| HS Code | 513512 |
| Grade | SABIC VALOX™ PBT+GF10%-HF SHF4320 |
| Polymer Base | Polybutylene terephthalate (PBT) |
| Glass Fiber Content | 10% |
| Flame Retardancy | Halogen-free flame retardant |
| Processing Method | Injection molding |
| Density | 1.50 g/cm³ |
| Tensile Modulus | 6500 MPa |
| Tensile Stress At Break | 85 MPa |
| Flexural Modulus | 6000 MPa |
| Notched Izod Impact Strength At 23 C | 5 kJ/m² |
| Hdt At 1 8 Mpa | 195 °C |
| Ul94 Rating | V-0 |
| Melting Temperature | 225 °C |
| Mold Shrinkage | 0.4-0.6% |
| Dielectric Strength | 20 kV/mm |
| Volume Resistivity | 1E14 ohm·cm |
As an accredited SABIC VALOX™ PBT+GF10%-HF SHF4320 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF10%-HF SHF4320 is supplied in 25 kg moisture-barrier bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL loading: SABIC VALOX™ PBT+GF10%-HF SHF4320 resin, 10% glass-fiber reinforced PBT, palletized, secured for export shipment. |
| Shipping | SABIC VALOX™ PBT+GF10%-HF SHF4320 ships as non-hazardous thermoplastic pellets in sealed, moisture-resistant bags or containers. It is not transport-regulated; keep dry, cool, and away from direct sunlight. Use standard industrial handling and hygiene practices. |
| Storage | Store in a cool, dry, well-ventilated area at ambient temperature, away from direct sunlight, heat sources, and ignition. Keep original containers tightly closed to prevent moisture pickup and contamination. Avoid dust generation and static discharge; use grounding/bonding. Protect from physical damage, rotate stock, and keep separate from incompatible materials. Follow local regulations and the SDS. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored unopened in original packaging, dry, below 40°C, and protected from moisture. |
SABIC VALOX™ PBT+GF10%-HF SHF4320 is applied in high-density connector platforms where pin counts exceed 40 and wall thickness is specified near 0.5 mm, because the melt rheology of a 10 wt% short-glass-fiber polybutylene terephthalate compound permits multi-cavity filling without the jetting and weld-line fracture associated with higher glass loadings. The grade is characterized for glass content by the ash content method ISO 3451-1, and its high-flow designation is operational only when the injection molding machine is configured with a 20:1 L/D general-purpose screw and a shut-off nozzle to prevent drool. Compliance for connector application rests on UL 94 HB horizontal burn classification under UL 94 Section 8, supplemented by end-product clearance and creepage verification to IEC 60664-1 for pollution degree 2. The formulation addition ratio at the injection molding stage is not a fiber let-down system; the 10 wt% glass content is pre-compounded into the pellet. Downstream additions are restricted to 1.0–2.0 wt% of a PBT-based color masterbatch and a maximum of 20 wt% regenerated sprue and runner shred, because higher regrind fractions reduce weld-line elongation as measured by ISO 527-2. The downstream production process uses desiccant drying to below 0.02 wt% moisture content at 120 °C for 4 h in a dryer with −40 °C dew point, followed by injection molding with a barrel temperature profile of 250 °C to 270 °C, a mold temperature of 80 °C to 100 °C, and cavity pressure sensors set to transfer at 95 % of filled volume. Terminal product types include USB Type-C connector housings, board-to-board connectors, and automotive harness connectors for dry low-current circuits where no UL 94 V-0 requirement is imposed.
When phosphor-bronze or tinned copper terminal pins are pre-inserted into two-plate relay bobbin molds, the limiting processing variable is not melt temperature but pin retention under winding tension after insert molding. The applicable compliance standard is IEC 61810-1:2014 for electromechanical relay construction, with insulation coordination checked against IEC 60664-1. This grade is not specified for sealed relay applications involving hot oil, aqueous glycol, or continuous condensing humidity; the operational boundary is limited to dry indoor relay environments. The formulation addition ratio for relay bobbin tooling includes 1.0 wt% of internal mold release masterbatch where deep core ejection creates drag marks, and regrind is held to 15 wt% maximum because bobbin flange thickness below 0.6 mm develops warpage sensitivity when recycled material alters fiber orientation. Downstream production uses a two-plate mold with pre-inserted terminal strips, melt temperature of 260 °C to 270 °C, injection pressure of 80 MPa to 120 MPa, and mold temperature of 70 °C to 90 °C to balance crystallization shrinkage against pin displacement. If pin displacement exceeds 0.03 mm in first-article inspection, the correction sequence reduces injection speed during early filling rather than raising mold temperature, because elevated mold temperature increases post-mold shrinkage mismatch around the pin. Terminal product types are relay bobbins, solenoid coil formers, and timer coil formers for printed circuit board mounting.
Power tool internal structural components made from this compound are constrained by post-mold warpage arising from glass fiber orientation gradients across thick boss regions and thin rib intersections, not by short-term material modulus. Compliance is evaluated under IEC 62841-1 for hand-held and transportable motor-operated tools, with mechanical validation performed on the finished housing after drop tests and vibration exposure. The formulation addition ratio in a power tool molding cell permits 20 wt% to 25 wt% regrind only when the regrind is generated from the same production lot and processed within 24 h after grinding; otherwise moisture uptake and fiber breakage reduce weld-line fatigue resistance under cyclic loading. Color masterbatch is limited to 2.0 wt%, and non-PBT carrier masterbatches are excluded because polyamide carriers create localized melt viscosity differences at knit lines. The downstream process uses a hot runner system with valve gates placed away from boss centers to reduce jetting, a mold temperature of 70 °C to 90 °C, and melt temperature of 255 °C to 270 °C. Packing pressure is held at 60 MPa to 80 MPa until gate freeze is verified by cavity pressure decay rather than timer control. Terminal product types include brushless drill motor mounting plates, gear housing covers, and trigger switch housings used in dry electric power tool interiors.
| Scenario | Melt temperature (°C) | Mold temperature (°C) | Drying condition | Maximum regrind (wt%) |
|---|---|---|---|---|
| Miniaturized connectors | 250–270 | 80–100 | 120 °C, 4 h, dew point −40 °C | 20 |
| Relay bobbins | 260–270 | 70–90 | 120 °C, 4 h, dew point −40 °C | 15 |
| Power tool housings | 255–270 | 70–90 | 120 °C, 4 h, dew point −40 °C | 25 |
| Switchgear insulating parts | 260–275 | 90–100 | 120 °C, 4 h, dew point −40 °C | 20 |
| Small appliance motor housings | 250–265 | 80–100 | 120 °C, 4 h, dew point −40 °C | 20 |
| Underhood sensor carriers | 255–270 | 80–100 | 120 °C, 4 h, dew point −40 °C | 15 |
In low-voltage switchgear build-ups, this compound is restricted to insulating carriers and structural supports that are not directly exposed to arc plasma or sustained surface discharge. The relevant compliance framework is IEC 60947-1:2007 for low-voltage switchgear and controlgear, supported by comparative tracking index testing to IEC 60112; the material flame classification remains UL 94 HB, and any assembly claiming UL 94 V-0 requires an added flame retardant grade rather than this compound. The formulation addition ratio includes the pre-compounded 10 wt% glass fiber reinforcement and 1.0–2.0 wt% carbon black or pigmented masterbatch for laser marking; regrind is limited to 20 wt% because switchgear parts with wall sections above 3.0 mm show internal void formation at higher recyclate fractions. Downstream processing uses injection molding with melt temperatures of 260 °C to 275 °C, mold temperatures of 90 °C to 100 °C to maximize crystallization, and sequential valve gating to prevent gas entrapment in long flow paths. Terminal product types include contact carriers, terminal block bases, busbar support brackets, and auxiliary switch cases where the operating voltage remains within overvoltage category III limits defined in IEC 60664-1 and the ambient environment is dry indoor switchgear.
For household appliance motor housings, this grade is a valid downstream application only when the part is not in direct contact with a live heating element and is not in an unattended appliance requiring glow-wire ignition temperature above 750 °C under IEC 60695-2-11. The primary product compliance standard is IEC 60335-1:2020, with the material’s UL 94 HB classification accepted only for supervised or motor-driven appliance interiors. The formulation addition ratio for appliance motor housings uses dry-blend addition of 1.0–2.0 wt% pigmented PBT masterbatch, while regrind is kept at 20 wt% maximum because motor cooling channels and snap-fit undercuts are sensitive to lot-to-lot variation in recycled glass fiber length. Production is carried out on hydraulic or servo-driven injection machines with a screw L/D of 20:1, melt temperature of 250 °C to 265 °C, mold temperature of 80 °C to 100 °C, and hot runner residence time not exceeding 5 min. Terminal product types include hand mixer motor housings, blender base structural frames, and food processor bowl locking rings, all in opaque non-flame-retardant versions.
| Standard designation | Test method or scope | Application scenario reference |
|---|---|---|
| UL 94 Section 8 | Horizontal burning, HB classification | Connectors, relay bobbins, power tool interiors, appliance motor housings |
| IEC 60664-1 | Insulation coordination for low-voltage systems | Miniaturized connectors, relay bobbins, switchgear carriers |
| IEC 61810-1:2014 | Electromechanical relay construction | Relay bobbins and coil formers |
| IEC 62841-1 | Motor-operated hand-held tool safety | Power tool housings and motor mounts |
| IEC 60947-1 | Low-voltage switchgear and controlgear | Contact carriers and busbar supports |
| IEC 60335-1 | Household and similar electrical appliance safety | Hand mixer motor housings, blender bases |
| ISO 16750-4 | Road vehicle environmental loading | Underhood sensor carriers |
When underhood sensor carriers are specified for dry engine-compartment zones, this grade is limited to continuous operating temperatures below 130 °C and relative humidity conditions that do not create liquid water accumulation on the part surface. Compliance validation follows ISO 16750-4:2023 for temperature and vibration loads in road vehicle environments, with electrical spacing checked by the end-user against IEC 60664-1. The formulation addition ratio excludes any regrind above 15 wt% because sensor carrier bosses with flatness tolerances of 0.05 mm exhibit orientation-driven distortion when recycled glass fiber bundles are reintroduced. Laser marking additives are dosed at 0.2–0.5 wt% using a PBT carrier. Downstream production uses a servo-electric injection molding machine with a 20:1 L/D screw, melt temperature of 255 °C to 270 °C, and mold temperature of 80 °C to 100 °C. Gate location is placed at a thick flange edge rather than directly over the sensor pocket to avoid fiber accumulation and local shrinkage differences that distort the mating surface. Terminal product types include intake air temperature sensor carriers, actuator position sensor housings, and EGR sensor connector flanges mounted on dry engine boundaries.
Competitive SABIC VALOX™ PBT+GF10%-HF SHF4320 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF10%-HF SHF4320 is a 10% glass-fiber-reinforced polybutylene terephthalate compound positioned within the high-flow segment of the Valox portfolio. The grade identifier SHF4320 denotes a high-flow (HF) modification integrated into a PBT matrix with a nominal glass-fiber weight fraction of 10%. Published single-point property data for this exact grade is limited to supplier documentation; therefore, numerical bands in this text are expressed as formulation-class values common to mineral-free PBT/GF10 high-flow compounds unless a specific standard is cited. Density is expected in the range of 1.38–1.40 g/cm³ under ISO 1183-1:2019. Melt volume-flow rate, determined at 250°C with a 2.16 kg piston load under ISO 1133-1:2022, is typically reported in the range of 20–35 cm³/10 min. The high-flow modification reduces viscosity without altering the nominal glass content. At the compounding stage, exterior glass fiber is introduced downstream in a corotating twin-screw extruder to preserve fiber aspect ratio; typical upstream compounding equipment uses an L/D 40:1 screw configuration. This production-scale equipment behavior influences final fiber length distribution and explains why aggressive regrinding or additional compounding shifts mechanical properties.
The 10% glass-fiber content positions SHF4320 between unfilled PBT and 30% glass-filled Valox grades. Glass fiber increases tensile stress, flexural modulus, and heat deflection temperature while reducing mold shrinkage and coefficient of linear thermal expansion. Comparative bands appear in Table 1; these are generic for the formulation class, not lot-specific, but they define the design trade-off. The high-flow modification recovers some of the lost melt length that would otherwise accompany glass-fiber addition, but it can reduce notched impact strength relative to a standard-flow PBT/GF10 of equivalent modulus. In a 0.5 mm wall-thickness spiral-flow evaluation conducted under controlled barrel temperature and mold temperature, high-flow PBT/GF10 grades exhibit longer flow lengths than standard-flow grades at the same injection pressure; published data for SHF4320 in this specific configuration is limited.
| Property | Unfilled PBT | PBT+GF10 high-flow band | PBT+GF30 | Test methodology |
|---|---|---|---|---|
| Density | 1.30–1.32 g/cm³ | 1.38–1.40 g/cm³ | 1.49–1.53 g/cm³ | ISO 1183-1:2019 |
| Tensile stress at break | 50–60 MPa | 80–100 MPa | 120–140 MPa | ISO 527-2:2012 |
| Flexural modulus | 2500–2800 MPa | 4000–5000 MPa | 8000–10000 MPa | ISO 178:2019 |
| HDT/A at 1.8 MPa | 55–65°C | 180–200°C | 200–215°C | ISO 75-2:2013 |
| Notched Izod at 23°C | 3–5 kJ/m² | 4–6 kJ/m² | 7–9 kJ/m² | ISO 180:2019 |
| Mold shrinkage, flow direction | 1.5–2.0% | 0.7–1.0% | 0.3–0.5% | Supplier internal method |
The high-flow modifier principally alters rheology, not the thermodynamic melting point. Differential scanning calorimetry of PBT/GF10 under ISO 11357-3:2018 typically places melt temperature near 223–226°C; high-flow grades may show a slightly lower crystallization onset in cooling scans because of molecular weight differences. The practical distinction is that SHF4320 should be selected when pressure-limited filling governs design, while standard-flow GF10 is preferred when notch sensitivity or long-term creep under retained loads is the controlling requirement.
Pre-drying is required for PBT at melt-processing temperatures. At moisture contents above 0.02% by weight, hydrolytic chain scission produces measurable viscosity loss and reduces tensile elongation. Desiccant dryer settings of 120°C for 3–4 h with a supply-air dew point at or below -30°C are typical; moisture content should be confirmed by ISO 15512:2019 or a calibrated moisture analyzer. Hopper residence time after drying should not exceed 30 min unless the hopper is blanketed with dry air at a dew point below -20°C. In plants where ambient relative humidity exceeds 60%, closed conveying from dryer to feed throat is necessary because PBT pellets reabsorb surface moisture rapidly. Feed throat temperature should remain below 70°C; condensation in the throat causes hydrolysis and intermittent feeding.
Barrel profiles commonly span 230°C in the rear zone to 250°C at the nozzle, with melt temperature measured by a hand needle pyrometer held at 250–260°C. Sustained melt temperature above 260°C accelerates decomposition, creates gas, black specks, and a reduction in notched impact strength. The high-flow modification widens the practical fill window but does not eliminate the upper temperature limit. Mold temperature should be held between 60°C and 90°C to allow crystallization and to minimize dimensional scatter. At mold temperatures below 50°C, as-molded crystallinity decreases, and parts may exhibit higher post-mold shrinkage and lower HDT.
Screw design on a reciprocating injection machine should use a low-compression general-purpose screw with compression ratio near 2.0–2.5; aggressive barrier screws can break glass fiber and reduce flexural modulus. Screw speed between 60–120 rpm and back pressure of 50–100 bar are typical; higher back pressure increases melt temperature without improving glass distribution. Injection velocity should be adjusted to fill the cavity in 0.2–0.8 s for thin sections; excessive velocity creates gate blush and surface glass streaks. Hold pressure is typically 50–70% of peak injection pressure, but pack time must exceed gate freeze time; gate freeze time in a 0.8 mm edge gate can be as short as 0.5 s with high-flow material. Vent depth should not exceed 0.015 mm for PBT/GF10; deeper vents produce flash at high flow. Vent lands must be cleaned after 5000 shots or earlier if diesel-effect burn marks appear.
Production-scale failure modes involving high-flow PBT/GF10 include nozzle drool during plastication, stringing at hot-runner tips, and gate freeze variation caused by insufficient hold time. Nozzle drool is controlled by retracting the injection unit after plastication and reducing rear-zone temperature; running the nozzle below melt temperature reduces drool but may freeze off in small gates. Hot-runner systems require heated drops with internal tip temperatures within ±5°C of the nozzle melt setpoint; temperature differences above this range produce stringing or premature freeze-off. For clamp force estimation, cavity projected area and melt pressure are used; at melt pressure of 400–600 bar, a projected area of 100 cm² requires 40–60 metric tons, before mold deflection and safety factors. High-flow grades transmit injection pressure more effectively, so the cavity pressure drop is lower; this can reduce projected clamp force by 10–20% for a given fill time in thin-wall tools.
In thin-wall connector production, the 10% glass content supplies the flexural stiffness required for terminal retention and dimensional control after assembly. Components with wall stocks from 0.4–0.6 mm and pin pitches below 1.27 mm are representative targets. Filling pressure is the usual constraint; the high-flow modification permits longer flow distance or lower injection pressure at a constant mold temperature. Terminal retention force is governed by boss geometry, interference ribs, and the resin’s apparent flexural modulus; published single-point retention data for SHF4320 is limited to end-user fixture validation. For soldering-compatible connectors, HDT/A above 170°C at 1.8 MPa is generally sufficient for the short thermal excursions of tin-lead or lead-free profiles, but this is not a guarantee for sustained underhood heat at 150°C. In snap-fit design, allowable outer-fiber strain should be limited to 1.0–1.5% for 10% GF PBT; higher strain may cause stress cracking, especially in molded-in stress and humid environments. Finite-element models should use anisotropic modulus values because fiber orientation causes stiffness to differ between flow and cross-flow axes.
Sensor housings exposed to engine oil at 80°C benefit from PBT’s hydrocarbon resistance; swelling in unleaded fuel at 23°C is typically below 0.5% after 168 h according to ISO 175:2010 when tested in a formulation-class laboratory study. For these applications, the material must be protected from direct hot-water jets because PBT hydrolyzes at temperatures above 60°C in water or high-pH cleaning agents. Electrical volume resistivity under IEC 62631-3-1:2016 is typically above 10^14 ohm·cm for PBT/GF10 at 23°C; comparative tracking index under IEC 60112:2009 is commonly 250–400 V, depending on formulation.
When the projected flow length in a 0.5 mm wall exceeds 80 mm, the process window narrows. The part design should be reviewed before the resin is considered deficient. Glass fibers orient along the flow direction in the skin layers; the core may show transverse orientation where shear gradients change. This anisotropic morphology reduces transverse tensile strength and increases moisture ingress. Gate type and location affect this orientation more than barrel temperature at high flow lengths. Edge gates should be placed at the thickest section, with a gate land below 0.5 mm and a gate diameter of 0.5–0.75 mm for nominal walls. For hot-runner tools, the drop spacing should be selected so that flow fronts merge above 150°C to avoid weak weld lines.
Weld-line tensile strength in 10% glass-filled PBT is commonly 30–40% lower than bulk flow-direction tensile strength under ISO 527-2:2012. In a multi-gate part, the last filling point is the weld-line position; moving the gate or using sequential valve gating can shift the weld line into a low-stress zone, but sequential control raises tool cost. If weld lines cannot be moved, local flow leaders and deflector tabs are preferred over excessive pack pressure. High pack pressure in a fiber-reinforced melt increases frozen-in orientation and can cause surface glass streaks or delamination at the part surface. For a 0.5 mm spiral-flow mold held at 80°C, high-flow PBT/GF10 typically requires 15–25% lower filling pressure than standard-flow PBT/GF10 to reach the same flow length; published data for this specific configuration is limited. The corresponding reduction allows reduced clamp tonnage, but mold deflection rather than clamp force may then control flash generation.
Moisture, regrind, and thermal history are the main lot-to-lot variables in production. Pellets stored in open containers at 23°C and 50% RH reach equilibrium moisture near 0.2%; drying must remove this before processing. Hydrolysis generates carboxylic acid end groups that further catalyze degradation, so the damage accelerates if wet material is held in the barrel. Intrinsic viscosity loss above 0.05 dL/g relative to virgin resin is a practical rejection criterion for heat-history lots; published data for this specific grade is limited. Incoming lots should be screened by MVR under ISO 1133-1:2022 before production to detect viscosity shifts.
Regrind from sprues and runners may be reintroduced at 15–25% by weight if it is kept dry and free of oil and dust. Above 25%, glass fiber attrition shifts fiber length distribution, lowering flexural modulus and notched impact. Regrind should be sieved through a 2 mm screen before blending to remove fines. PBT fiber compounds are sensitive to contamination from polyamide and polycarbonate; a single contaminated hopper can produce delamination and lot failure. The blender and hopper should be purged with virgin PBT after material changes. Basic or amine-containing colorants and flame-retardant masterbatches can catalyze polyester degradation; compatibility must be verified before use. Silicone mold-release agents reduce surface friction but may interfere with printing or bonding. If adhesive bonding or potting is required, surface energy should be tested after molding; flow-induced glass at the surface and external mold release can lower adhesion.
Chemical compatibility follows the behavior of semicrystalline PBT. Unleaded fuel, engine oil, and most hydrocarbon greases produce negligible attack at 23°C; immersed specimens tested under ISO 175:2010 show tensile retention above 85% in formulation-class studies. Hot water above 60°C, alkaline cleaners above pH 9, and strong acids above 10% concentration are aggressive. Ethylene glycol at engine coolant temperatures can cause environmental stress cracking in restrained areas; the design should avoid high frozen-in stress in coolant-contact housings. Alcohol-based brake fluids and aromatic solvents may extract low molecular weight species but generally do not dissolve PBT at room temperature. Moisture-induced dimensional change is small relative to polyamide; linear expansion from water absorption at 50% RH is typically below 0.15% for PBT/GF10 under ISO 62:2008. Thermal expansion is anisotropic due to fiber orientation; flow-direction CLTE is typically 30–50 µm/m·K and transverse 60–90 µm/m·K by thermomechanical analysis per ISO 11359-2:2021.
For export shipments subject to the European Union REACH regulation, material declarations must be requested for the specific grade and shipping lot. The base PBT/GF10 system is generally suitable for restriction-of-hazardous-substances compliance under Directive 2011/65/EU Annex II, provided that no restricted pigments, flame retardants, or external processing aids are added. REACH SVHC declarations under Article 33 of EC 1907/2006 require that the supplier confirms whether any SVHC exceeds 0.1% by weight of the article. Polymer marking follows ISO 11469:2016; the mold should be marked >PBT+GF10<, with the high-flow designation omitted from the marking code. Flammability classification under UL 94 must be verified from the UL Yellow Card for the specific color, thickness, and grade; this high-flow grade should not be assumed to achieve V-0 beyond what the Yellow Card lists.
| Requirement | Assessment tool | Documentation boundary |
|---|---|---|
| Directive 2011/65/EU Annex II | X-ray fluorescence screening and wet chemistry per IEC 62321-8:2017 | Supplier resin declaration applies to resin only; end-product compliance remains converter responsibility |
| EC 1907/2006 Article 33 | SDS and SVHC declaration | Required for each grade and batch when SVHC content exceeds 0.1% w/w |
| ISO 11469:2016 | Mold marking | >PBT+GF10< on parts above 25 mm nominal dimension |
| UL 94 | UL Yellow Card | Thickness and color specificity required; do not extrapolate to unlisted wall thickness |