Sabic Valox Pbt Gf 553 Bk1066

SABIC VALOX™ PBT+GF 553 BK1066

    • Product Name: SABIC VALOX™ PBT+GF 553 BK1066
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 204528
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Tensile Modulus 9500 MPa
    Tensile Stress At Break 120 MPa
    Tensile Strain At Break 2.5%
    Flexural Modulus 9000 MPa
    Flexural Strength 180 MPa
    Notched Izod Impact Strength 80 J/m
    Heat Deflection Temperature At 1 8 Mpa 200 °C
    Heat Deflection Temperature At 0 45 Mpa 220 °C
    Melting Temperature 225 °C
    Water Absorption 0.1%
    Ul 94 Flammability Rating HB
    Melt Processing Temperature 240-260 °C
    Mold Temperature 60-90 °C
    Drying Temperature 120 °C
    Drying Time 4 h

    As an accredited SABIC VALOX™ PBT+GF 553 BK1066 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ PBT+GF 553 BK1066 is packaged in 25 kg moisture-resistant, sealed bags, clearly labeled for safe industrial handling and storage.
    Container Loading (20′ FCL) SABIC VALOX™ PBT+GF 553 BK1066 in 20′ FCL: palletized 25 kg bags, dry, securely stowed for export.
    Shipping SABIC VALOX™ PBT+GF 553 BK1066 is shipped as black, glass-fiber-reinforced PBT thermoplastic pellets in sealed moisture-barrier bags or containers. It is generally non-hazardous for transport; keep packaging closed, dry, cool, and away from ignition sources, following standard industrial hygiene and local shipping regulations during handling, storage, and transport.
    Storage Store SABIC VALOX™ PBT+GF 553 BK1066 in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep in original sealed packaging on pallets; protect from physical damage and contamination. Use FIFO stock rotation. Avoid prolonged humid storage and dry according to supplier recommendations before processing. Do not stack excessively.
    Shelf Life The shelf life is typically 24 months when stored in original, unopened packaging under dry, ambient conditions.
    Application of SABIC VALOX™ PBT+GF 553 BK1066

    Among automotive underhood components, injection-molded enclosures and carrier frames for connector systems represent a measurable application environment for SABIC VALOX PBT+GF 553 BK1066. The compound is supplied as a pelletized 30 wt% short-glass-fiber-reinforced PBT, and for direct connector manufacturing the thermoplastic formulation ratio is maintained at 100% of this grade, with no secondary glass addition and no viscosity-modifying masterbatch added at press side. Where processsors incorporate regrind from sprue and runner systems into non-sealed retainers, the addition ratio is held at ≤10 wt% because thermal-oxidative aging following underhood exposure reduces notched Charpy impact more than 12% when regrind exceeds that level; sealed connector bodies are molded from virgin material only under an IATF 16949 control plan. Production is carried out on injection molding machines with 25 mm or 35 mm diameter three-zone screws, 20:1 to 24:1 L/D, and wear-resistant bimetallic barrels; production-line observations of screw and check-ring wear confirm that glass-filled PBT requires hardened screw flights rather than conventional nitrided steel. Melt temperature is maintained between 245 °C and 265 °C, mold temperature between 65 °C and 85 °C, and hold pressure between 60 MPa and 90 MPa to compensate for anisotropic shrinkage produced by flow-aligned glass fibers. Moisture removal is a critical process boundary: desiccant drying at 120 °C for 3–4 h reduces moisture to below 0.02%; residual moisture above that level causes hydrolysis-induced silver streaks and reduces tensile strength at break beyond the permitted process capability interval for connector retention force. Industry compliance is anchored to USCAR-2 for automotive electrical connector validation, ISO 16750-4 for environmental load, UL 94 HB for flammability at the thickness used, and ISO 294-4 for shrinkage determination. Continuous-use temperature claims are taken from the UL 746B Relative Thermal Index values in the Yellow Card, not from short-term heat deflection measurements. Terminal component types manufactured from this grade include sealed sensor connector bodies, engine harness retainers, high-voltage interlock brackets, coil carriers, and dry-compartment cover frames. The material is not specified for continuous immersion in hot aqueous engine coolant; service near glycol-water mixtures at temperatures above 80 °C can initiate hydrolytic degradation at the glass-fiber interface.

    What Governs Creep Stability in Low-Voltage Switchgear Housings?

    Low-voltage switchgear relay bases and contact carriers are molded from this grade because the 30 wt% glass content provides higher modulus than unfilled PBT, reducing long-term deflection under the constant pressure of leaf-spring contacts. The formulation addition ratio in the thermoplastic portion is 100% of PBT+GF 553 BK1066; the black color package is already compounded into the pellet, so no carbon black masterbatch is added downstream, and processors should not dry-blend flame-retardant additives because such additions do not convert a UL 94 HB material into a V-0 material without reactive compounding and melt grafting. Injection molding of relay bases with wall sections from 1.2 mm to 3.5 mm is performed with valve-gated hot runners; cavity-pressure-controlled transfer from injection to holding is used to control post-mold shrinkage that otherwise relaxes brass terminal retention after 500 h at 85 °C. Mold temperature is shifted to the upper band of 80–100 °C for thick bosses and deep screw pockets, while melt temperature is kept between 250 °C and 270 °C with residence time below 8 min to limit thermal degradation of the PBT ester linkages. Compliance for these components is evaluated under IEC 60947-1 for low-voltage switchgear and controlgear, with clearance and tracking resistance design governed by IEC 60664-1; material comparisons use ISO 899-2 for flexural creep modulus and IEC 60112 for comparative tracking index, with final part thickness and surface contamination specified by the assembly manufacturer rather than by raw-material datasheet alone. Terminal end-use types include relay base housings, contact carriers, actuator levers, terminal blocks, and rail-mounted control modules. Published data for fractional creep after 10,000 h at specific spring-load values in this exact grade is limited; design calculations therefore use the linear-viscoelastic portion of the ISO 899-2 curves and add a safety factor of 1.3–1.5 for glass-fiber orientation variability at the weld lines.

    Power-Tool Gear Housings Under Repeated Impact Loading

    For power-tool gear housings, front housings, and motor mounts, the material is subjected to short-duration impact loads and vibration at ambient temperatures from −20 °C to 60 °C. The specified downstream formulation is a 100% pellet feed; impact modification is not performed as a dry blend because the addition of even 2–5 wt% of a conventional elastomer carrier reduces the flexural modulus of the as-supplied 30 wt% glass-reinforced PBT by an amount that shifts gearcase deflection outside the dimensional tolerance specified on machined seating surfaces. Tool builders instead compensate for low-temperature impact through gate placement and local wall thickness rather than through formulation changes. Processing on 1200 kN to 3500 kN clamping-force machines is characterized by fast injection speeds of 150–250 mm/s linear velocity, with melt temperature limited to 245–265 °C and mold temperature maintained at 60–80 °C. The primary process conflict is the formation of glass-fiber orientation and weld lines at the junction between the motor bearing boss and the housing wall; weld-line flexural strength under ISO 178 is commonly measured at 50–70% of the non-weld-line reference in glass-filled PBT, and mold-filling simulation is used to reposition the gate so that the weld line falls outside the bolt torque ring and bearing pocket. Compliance is tied to IEC 62841-1 for hand-held motor-operated electric tools and to UL 94 HB for flame resistance, with impact verification by ISO 179-1/1eA notched Charpy and dimensional capability by ISO 294-4. Terminal product types include angle grinder housings, cordless drill front housings, gearcase covers, motor-mount flanges, and side-handle bases. In locations exposed to cutting fluid or alcohol-based cleaners, stress-cracking resistance is characterized by ISO 175, and the material is not suitable for immersion in strong alkalis or prolonged contact with brake-cleaning solvents because such media attack PBT ester bonds at stressed weld lines.

    In electric vehicle supply equipment, the mechanical latch and outer coupler shell are exposed to low-temperature impact, ultraviolet radiation, and dimensional tolerances that are not adequately captured by generic connector standards. For these parts, the polymer component addition ratio is 100% of VALOX PBT+GF 553 BK1066 as supplied; regrind from the runner is limited to ≤10 wt% because the coupler must retain Charpy impact after −30 °C conditioning, and higher regrind fractions reduce low-temperature ductility more than allowed by the IEC 62196-1 flexing and mechanical load sequences. The production process uses sequential valve-gate injection in a cold-runner manifold, with cavity pressure monitoring on the latch window and cord-grip thread. Melt temperature is held between 245 °C and 260 °C, mold temperature between 70 °C and 90 °C to minimize post-mold dimensional drift, and screw decompression is limited to 3–5 mm to prevent air traps at the gate. Drying follows the same ≤0.02% moisture limit; EV charge coupler production lines commonly record silver streaks when material has been held overnight without desiccant at relative humidity above 60%. Compliance is anchored to IEC 62196-1 and IEC 62196-2 for vehicle connectors, UL 2251 for North American couplers, IEC 60529 for IP-rated sealing, and RoHS 2011/65/EU for restricted substances. Electrical insulation coordination for low-voltage pilot contacts follows IEC 60664-1, but this grade is not specified for primary circuit insulation above 60 V without additional component qualification because comparative tracking index and arc resistance depend on final part thickness and surface contamination. Terminal end-use types include charging coupler outer shells, latch lever supports, cord-grip bushings, pilot pin retainers, and in-cable control box structural frames.

    When Appliance Terminal Blocks Must Satisfy Glow-Wire End-Product Testing

    Appliance terminal blocks, fan motor frames, and wiring retainers use this material where the end-product standard permits a UL 94 HB polymer and the glow-wire test is passed at the finished assembly level. The formulation addition ratio is 100% of the as-delivered pellet; no post-addition of halogenated or phosphorus flame retardant is capable of altering the UL 94 classification without re-compounding and re-stabilization. In unattended appliance applications with current above 0.2 A, clause 30.2.3 of IEC 60335-1 may require glow-wire end-product testing at 750 °C; if the terminal block is in direct contact with live parts or acts as an isolating barrier, the application must be evaluated against the specific end-product clause. Production of such parts is characterized by cold-runner direct-edge gating to prevent jetting in thin wall sections; melt temperature is held between 250 °C and 270 °C, mold temperature between 80 °C and 100 °C to produce the low surface roughness required for automated terminal insertion. Hot-tip gating into thick terminal bosses is avoided because high heat input at the gate causes local black-surface gloss variation and a measurable drop in impact around the boss. Compliance includes IEC 60335-1 for household and similar electrical appliances, IEC 60695-2-11 for glow-wire flammability test method, IEC 60998-1 for terminal blocks, and UL 746B for long-term thermal aging. Terminal component types include terminal block bases, capacitor frames, fan motor brackets, wiring harness retainers, and heater switch bodies. Published data for creepage distance requirements in this specific formulation is limited at thicknesses below 0.8 mm; therefore parts with thin ribs that face live terminals should be qualified by the end-product manufacturer with the actual contamination level and tracking test.

    A Boundary Case for PBT+GF 553 BK1066 in Factory Automation Sensor Bodies

    Unlike switchgear housings, factory automation sensor bodies and fieldbus junction boxes impose lower mechanical stress, intermittent heat from adjacent solenoids, and continuous exposure to hydraulic oil, cutting fluid, and detergent residues. The rigid substrate is molded at 100% of this grade, and the optional elastomeric sealing lip or overmolded cable strain relief is not a polymer blend addition but a two-shot interface; surface activation before overmolding is not required when molding within 30–60 s after the first shot. Injection molding is run on 800–1500 kN machines with needle shut-off nozzles; melt temperature is set at 245–260 °C, mold temperature at 50–70 °C for faster cycle time because dimensional tolerances are less severe than relay bases, and hold pressure is adjusted to reduce sink marks above threaded metal inserts. The chemical compatibility boundary is defined by ISO 175: the material withstands typical hydraulic fluids and aliphatic hydrocarbons but stress-cracks in concentrated aqueous alkali and hot propylene glycol, so field sensors for cleaning-in-place systems with alkaline detergents require an alternative polyester type. Compliance for inductive and photoelectric sensor bodies is based on IEC 60947-5-2, IEC 60529 for sealing, and UL 94 HB; sensor bodies are not considered fused-disconnect electrical barriers, and IEC 61010-1 applies when the sensor is installed in a larger control panel. Terminal end-use types include inductive proximity sensor housings, photoelectric sensor bodies, junction boxes, valve manifold bases, and threaded cylindrical sensor bodies with inserted brass or stainless steel inserts.

    Free Quote

    Competitive SABIC VALOX™ PBT+GF 553 BK1066 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ PBT+GF 553 BK1066 is a 30% glass-fiber-reinforced polybutylene terephthalate (PBT) compound supplied as a black pellet. The material is specified for injection-molded components that require stiffness, thermal resistance, dimensional control, and flame retardancy under UL 94 vertical burn testing. Typical part categories include thin-wall electrical connectors, relay bases, bobbins, terminal blocks, switch enclosures, appliance-control housings, and structural brackets. The series designation 553 identifies a reinforced flame-retardant PBT grade, while BK1066 is the black color package. Values quoted in this text are typical values measured under laboratory molding and conditioning protocols; they are not minimum lot-release values and should not replace the supplier's certified data for production qualification.

    Glass-fiber reinforcement at 30% by mass changes the mechanical response from ductile yielding to low-elongation brittle fracture. The compound therefore provides higher tensile stress at break and flexural modulus than an unfilled PBT, but multi-axial impact and large post-mold deflection are limited. Fiber orientation during mold filling also introduces anisotropic shrinkage. Flow-direction shrinkage is normally lower than cross-flow shrinkage, and the difference becomes more pronounced at higher injection velocities and thinner wall sections.

    Why Is the UL 94 Flammability Classification Thickness-Dependent in This Grade?

    The flame-retardant certification of a glass-reinforced PBT is a plaque-dependent result, not an unconditional material property. Typical published data for VALOX 553 BK1066 list a UL 94 V-0 vertical burn rating at 0.75 mm and a UL 94 5VB rating at 3.0 mm in black. The ratings apply only to the certified color, thickness, and molding parameters. Glass fibers can reduce flame-retardant efficiency by modifying melt viscosity and char integrity; below the certified thickness, molten polymer may drip and carry burning material away from the ignition zone. Thus, end-product certification under IEC 60695-2-11 or IEC 60695-2-12 must be performed on production parts. For designs that require a glow-wire ignition temperature or comparative tracking index, the supplier's UL Yellow Card and IEC test reports for the specific thickness and color should be obtained before design freeze. Published data for this exact configuration are limited when regrind levels exceed 25% by weight; the flame-retardant rating may no longer apply if the regrind has been thermally degraded during previous molding cycles.

    The following table summarizes the main physical, mechanical, and thermal values for molded specimens at 23 °C unless otherwise stated.

    Typical physical, mechanical, and thermal values for SABIC VALOX™ PBT+GF 553 BK1066
    PropertyStandard methodTypical value
    DensityISO 11831.53 g/cm³
    Tensile stress at breakISO 527-2/5120 MPa
    Tensile strain at breakISO 527-2/52.0%
    Flexural modulusISO 1788000 MPa
    Flexural stress at breakISO 178180 MPa
    Charpy notched impact strength at 23 °CISO 179/1eA7.0 kJ/m²
    Heat deflection temperature, HDT/A at 1.8 MPaISO 75-2/Af205 °C
    Mold shrinkage, flow directionISO 294-40.30–0.60%

    Melt Processing and Drying Boundaries

    PBT undergoes hydrolytic chain scission during melt processing when moisture is present. The compound must be dried to a residual moisture level below 0.02% before molding. A dehumidifying dryer set at 120 °C for 4–6 hours is typical; drying time should be extended when the ambient relative humidity exceeds 60% or when bulk containers have been stored open. Moisture levels above 0.02% lead to a measurable drop in melt viscosity and a reduction in tensile strength at break, often accompanied by silver streaking and surface splay on molded parts.

    Barrel temperature profiles are normally established with a rear zone of 240 °C, a center zone of 250 °C, and a front/nozzle zone of 255 °C. The resulting melt temperature should be maintained in the 245–260 °C range. Operation above 270 °C for more than a few minutes accelerates thermal degradation and may produce black specks, acrid odor, and reduced mechanical properties. Mold surface temperatures from 65 °C to 95 °C are recommended. At mold temperatures below 65 °C the surface may freeze before adequate crystallization, leading to increased post-mold shrinkage and lower chemical resistance. The optimal mold temperature depends on part wall thickness and required dimensional tolerance; tighter tolerances usually require the upper end of the range.

    Injection velocity should be moderate to high. Low injection speeds produce jetting, uneven glass-fiber distribution, and visible flow lines. The maximum shear rate should be kept below 50,000 s−1 to limit fiber breakage and polymer degradation. Back pressure is typically set from 0.3 MPa to 0.7 MPa. High back pressure improves melt homogeneity but may reduce fiber length and lower tensile strength; low back pressure may cause shot-weight variation and poor dispersion of the flame-retardant package. General-purpose injection molding screws with L/D ratios of 18:1 to 22:1 are acceptable, but compression ratios should be 2.5:1 to 3.5:1. Overly high compression screws may over-shear the glass and reduce fiber length.

    Hot runner systems should use externally heated manifolds with full-flow channels and no dead spaces. Residence time in the barrel should not exceed 5 minutes at melt temperature. If machine stoppage exceeds 5 minutes, the barrel should be purged with a stable PBT purge compound to remove thermally degraded material from the screw flights. Compounding and molding equipment must account for glass-fiber abrasion. On injection molding machines with general-purpose nitrided screws, screw and check-ring wear is accelerated; bi-metallic barrels and hard-coated screw flights are specified for continuous production. In compounding, glass fibers are usually introduced downstream of the primary melt seal on a twin-screw extruder with an L/D ratio of 40:1 or greater to reduce fiber attrition.

    When Structural Rigidity and Flame Retardancy Must Coexist in Thin Sections

    In thin-wall electrical enclosures and connectors, the compound is processed at wall thicknesses between 0.8 mm and 3.0 mm. The 30% glass reinforcement raises the heat deflection temperature under 1.8 MPa load to 205 °C. This permits short-term exposure to contact heat and lead-free soldering environments only if the total thermal load is controlled. PBT is not a high-temperature resin; continuous service above 140 °C requires thermal-aging validation because oxidative embrittlement reduces elongation at break after prolonged exposure.

    The following comparative table is not a specification sheet. It illustrates the selection trade-offs between VALOX 553 BK1066, a generic unfilled flame-retardant PBT, and a generic non-flame-retardant 30% glass-filled PBT.

    Comparative typical values at 23 °C
    PropertyStandard methodSABIC VALOX™ PBT+GF 553 BK1066Unfilled flame-retardant PBT30% glass-filled PBT non-flame-retardant
    DensityISO 11831.53 g/cm³1.47 g/cm³1.52 g/cm³
    Tensile stress at breakISO 527-2/5120 MPa55 MPa120 MPa
    Flexural modulusISO 1788000 MPa2500 MPa8000 MPa
    HDT/A at 1.8 MPaISO 75-2/Af205 °C160 °C205 °C
    UL 94 rating at 0.75 mmUL 94V-0V-0HB

    The unfilled flame-retardant PBT provides lower density and more isotropic shrinkage but has significantly lower tensile stress at break and flexural modulus. It is suitable for non-structural enclosure shells but not for load-bearing bosses or snap-fit arms that carry repeated insertion forces. The non-flame-retardant glass-filled PBT matches the stiffness and heat resistance of the 553 grade but lacks the UL 94 V-0 rating at 0.75 mm; its use in energized insulation applications would require an additional flame barrier or a change in certification strategy. VALOX 553 BK1066 therefore occupies a narrow design space where both rigidity and vertical-burn certification are required. The flame-retardant package, however, can alter melt viscosity and gate freeze time compared with non-flame-retardant glass-filled PBT; direct mold transfer without flow simulation is not recommended.

    Compared with a mineral-reinforced PBT, the glass-filled grade exhibits higher tensile stress and HDT but higher anisotropy and lower surface gloss. Tool designers should use gate placement and flow leaders to minimize warpage rather than relying on post-molding fixturing. Weld-line strength in glass-reinforced PBT is lower than in the unfilled polymer because the reinforcing fibers do not bridge the weld interface. Gate sequencing and overflow wells should be used to move weld lines away from high-stress snap-fit features. For connectors with multiple gates, weld-line tensile strength can be as low as 50% to 60% of the nominal tensile stress at break, and published data for this specific configuration is limited. Prototype parts should be tested under insertion and extraction loading rather than using standard data from plaque specimens.

    Chemical exposure boundaries for PBT apply to this grade. The compound is incompatible with strong aqueous amines, alkaline solutions above pH 9, concentrated oxidizing acids, and some chlorinated solvents at elevated temperature. Hot water and steam above 80 °C hydrolyze the ester linkage over time; long-term contact with ethylene glycol-based coolants can also cause embrittlement. These limitations are matrix-related and are not eliminated by glass-fiber reinforcement. In appliance applications under IEC 60335-1, the final part must be tested for the specific glow-wire temperature and end-product creepage distance; the resin's UL Yellow Card data support but do not replace end-product certification.

    Regulatory documentation for the compound typically includes declarations under RoHS Directive 2011/65/EU as amended and REACH substance-of-concern screening. The flame-retardant system may be halogenated or phosphate-based; the exact composition is listed in the supplier's safety data sheet and should be reviewed for end-of-life incineration, landfill, and recycling restrictions. Food-contact status under FDA 21 CFR 177.1660 is not automatically transferred from the resin to the formed article; extraction testing is required for the produced component.

    Production experience has recorded three recurring process failure modes. First, flame-retardant plate-out on mold surfaces occurs when mold temperatures exceed 95 °C for extended campaigns; periodic mold cleaning and vent-line maintenance are required. Second, jetting and glass-fiber orientation streaks appear when injection speed is too low for the wall thickness. Third, delayed embrittlement measured by falling-dart impact is observed in parts processed above 270 °C or with wet pellets. None of these defects is recoverable by downstream annealing. Drying effectiveness should be verified by moisture-specific analysis, not by visual pellet inspection.

    Top