| HS Code | 518537 |
| Density | 1.53 g/cm³ |
| Glass Fiber Content | 30% |
| Color | Black |
| Tensile Modulus | 9500 MPa |
| Tensile Stress At Break | 135 MPa |
| Tensile Strain At Break | 2.5% |
| Flexural Modulus | 9000 MPa |
| Notched Izod Impact Strength At 23 C | 10 kJ/m² |
| Hdt At 1 82 Mpa | 205 °C |
| Hdt At 0 45 Mpa | 220 °C |
| Vicat Softening Temperature | 215 °C |
| Molding Shrinkage | 0.3-0.5% |
| Water Absorption | 0.07% |
| Ul 94 Flammability Rating | HB |
As an accredited SABIC VALOX™ PBT+GF 553-BK1006 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF 553-BK1006 is packaged in 25 kg moisture-barrier bags, palletized for safe industrial storage and transport. |
| Container Loading (20′ FCL) | 20′ FCL dry container: palletized 25 kg bags of SABIC VALOX™ PBT+GF 553-BK1006, shrink-wrapped and secured for ocean transport. |
| Shipping | SABIC VALOX™ PBT+GF 553-BK1006 is shipped as non-hazardous polymer pellets in moisture-barrier packaging, palletized and secured for transport. Keep dry and avoid heat or prolonged sunlight. Follow the SDS and local regulations; no UN number or hazard class is required. |
| Storage | Store SABIC VALOX™ PBT+GF 553-BK1006 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and moisture. Keep material in its original, sealed packaging until use to prevent contamination and moisture pickup. Avoid prolonged exposure to humid conditions, and follow first-in, first-out stock rotation. Observe local regulations and the manufacturer’s safety data sheet for handling and storage requirements. |
| Shelf Life | Shelf life is generally 2 years from manufacture in original sealed packaging under dry, cool storage conditions. |
Engine compartment connector bodies and sensor flanges are injection-moulded from VALOX™ PBT+GF 553-BK1006 when multi-cavity tools require lower moisture uptake than PA66 and higher dimensional precision than neat PBT. Published datasheet values place tensile stress at break in the range of 120 MPa to 135 MPa under ISO 527-2/1A and flexural modulus near 9,000 MPa under ISO 178. Heat deflection temperature measured to ISO 75-2/Af is reported above 200 °C. The resin absorbs roughly 0.1 % moisture at 23 °C and 50 % relative humidity under ISO 62, compared with approximately 0.8 % for PA66 under the same conditions. Component validation to SAE/USCAR-2 includes thermal cycling across -40 °C to 125 °C, humidity exposure, and terminal retention testing. In this application the moulded body is typically 1.0 mm to 2.0 mm thick, with shut-off faces that demand uniform packing. Glass fibres oriented parallel to flow reduce linear shrinkage but increase anisotropic warpage in ribbed sections. Predrying at 120 °C for 3 h to 4 h is applied to bring residual moisture below 0.02 %. Moulding is performed with a melt temperature between 245 °C and 255 °C and a mould surface temperature between 70 °C and 90 °C. Thermocouple placement in the nozzle and runner system prevents localised hot spots above 260 °C because the polybutylene terephthalate backbone degrades through ester cleavage and releases volatile by-products that deposit on tool cavities. Creep modulus measured to ISO 899-1 remains controlled by orientation of the 30 % glass fibre fraction; at weld lines strength retention is lower, and gate positioning must move knit lines away from latch arms and clip towers. Regulatory documentation for the grade covers RoHS 2011/65/EU and REACH SVHC disclosure. The finished connector bodies, sensor flanges, and ECU interconnect shells retain terminal insertion force after hot-oil immersion because the glass-reinforced PBT matrix resists creep at the contact interface under compressive preload.
The dominant process constraint is not flow length but the narrow thermal degradation window of the resin. Industrial control terminal blocks, relay sockets, and modular interface carriers are moulded with wall thicknesses below 1.2 mm. At these sections, filling pressure increases and the temptation to elevate melt temperature above 260 °C leads to molecular weight reduction and increased mould deposit formation. Published guidelines for glass-reinforced VALOX™ grades recommend melt temperature between 245 °C and 260 °C and recommend that total residence time at temperature does not exceed 8 min. Melt volume-flow rate measured to ISO 1133-1 at 250 °C and 5.0 kg is typically in the range of 12 cm³/10 min to 18 cm³/10 min. A reverse temperature profile is used, with the rear zone set 10 °C to 20 °C lower than the nozzle, to maintain feed-zone stability. The thin-wall geometry is gated with a valve-gated hot runner or a submarine gate, and hold pressure is staged to compensate for rapid crystallisation. Short-shot trials are conducted before production because glass-filled PBT exhibits a steep melt viscosity increase as solidification begins. Mould-filling simulation software with a fibre-orientation module is standard for optimising gate position. The black colourant package in BK1006 does not reduce weld-line mechanical properties below the unfilled PBT baseline when knitted edges are positioned in low-stress zones. Terminals are insert-moulded or staked after moulding. Compliance is verified under IEC 60695-2-11 for glow-wire resistance and IEC 60112 for comparative tracking index on finished parts, not raw resin plaques. The table below lists the conformity matrix applied to a modular industrial control platform.
| Application | Standard | Property or test condition |
|---|---|---|
| Engine-compartment connectors | SAE/USCAR-2 | Thermal cycling, humidity, terminal retention |
| Industrial terminal blocks | IEC 60695-2-11 | Glow wire at 650 °C / 30 s |
| Industrial terminal blocks | IEC 60112 | Comparative tracking index |
| Power tool housings | IEC 60745-1 | Mechanical strength, abnormal operation |
| Appliance pumps | IEC 60335-1 | Hot water immersion, leak resistance |
| Relay bobbins | IEC 61810-1 | Coil temperature endurance, dielectric withstand |
In hand-held power tools, the motor housing is not a single-material monolith; glass-reinforced PBT is used for the gear casing, brush holder frame, trigger housing, and ventilation grill. The material is selected because the 30 % glass fibre fraction raises tensile modulus to a level that supports rotor bearing seats without the low creep resistance of neat PBT. Impact testing is carried out on notched Charpy specimens to ISO 179-1/1eA at 23 °C; published values for glass-reinforced PBT grades are typically in the range of 7 kJ/m² to 10 kJ/m². The assembled housing must pass drop tests derived from IEC 60745-1, with the weakest point normally located at the weld line opposite the gate. Tool designers place sub-gates or overflow tabs at the end of flow to move the knit line to a high-mass rib intersection. Screw speed during plastication is limited to 80 rpm to 120 rpm to reduce fibre attrition; a general-purpose screw with 20:1 L/D ratio and low-compression feed zone is used on production machines. The mould surface is textured with a fine spark-eroded finish to reduce ejection drag on glass-rich surfaces. Production batches show that barrel temperature override in the compression zone causes resin yellowing and black speck formation; thermal imaging of purge material confirms local melt temperature above 265 °C. Cooling time is controlled by mould temperature at 80 °C, and cycle time is set by the thickest bearing boss, not by the nominal wall section. In this application the primary end products are angle grinder gear housings, drill motor end caps, and impact driver trigger frames.
Domestic washing machine drain pumps and dishwasher circulation pumps use glass-reinforced PBT impeller housings, volute covers, and mounting flanges. The failure mode in this application is not impact but differential shrinkage between longitudinal and transverse flow directions. Fibre orientation at the weld line and at the volute tongue creates a bow along the sealing face after demoulding. The part is typically moulded with wall thickness from 2.0 mm to 3.5 mm; a thick section increases differential shrinkage, while a thin section increases filling pressure. Mould temperature is held at 80 °C to 90 °C to slow crystallisation and improve dimensional stability. Pre-drying at 120 °C for 3 h is required before processing because hydrolytic degradation in the gate region weakens the sealing boss. The critical operational boundary is hot water immersion. PBT in hot water above 60 °C undergoes progressive hydrolysis at the ester linkage, and published data for this specific configuration is limited. Field experience from pump manufacturers shows that continuous service above 80 °C in aggressive detergent solutions favours high-temperature polyamide or PPE/PA66 blends over standard glass-reinforced PBT. For non-continuous drain pump duty at moderate temperature, the grade is compatible with short-term exposure to wash liquor at 40 °C to 60 °C. End-product validation includes pressure cycling and leak testing under IEC 60335-1; the sealing face is machined or ultrasonically welded to a thermoplastic elastomer gasket. Fibre-filled PBT can be joined by ultrasonic welding at the flange, but melt-down of the glass-rich skin reduces weld strength when amplitude exceeds 40 µm. The weld joint is therefore designed with a shear-joint geometry and low amplitude.
Solenoid valve bobbins occupy one of the narrowest tolerance windows in industrial fluid control. The bobbin is wound with copper magnet wire under tension, encapsulated, and then pressed into a steel armature bore. Glass-reinforced PBT is used because the coil flange must not creep under wire tension at elevated coil temperature. The moulded bobbin has wall sections from 0.6 mm to 1.5 mm; the thin flange is filled through a film gate at the core bore. The core pin is maintained at 70 °C to 85 °C because a cold core pin increases internal stress at the sharp corner between flange and core. Injection speed is set high in the first stage and reduced during packing to prevent jetting in the core bore. The material must survive dip soldering or wave soldering at 260 °C for 5 s to 10 s during coil termination. This thermal exposure is close to the upper processing limit; therefore the moulded bobbin is annealed at 150 °C for 30 min to release internal stress before soldering. Dielectric strength measured to ASTM D149 on moulded plaques is used for lot acceptance, and the finished coil must pass dielectric withstand testing under IEC 61810-1. The black glass-filled surface is non-conductive in dry service, but surface contamination from release agents or copper dust can produce tracking under voltage; therefore a non-silicone mould release is used and post-mould handling is automated.
Sealed relay bobbins expose the resin to continuous coil heat, mechanical shock from armature closure, and solder reflow temperatures. The temperature at the coil wire surface in a sealed miniature relay can range from 120 °C to 150 °C during continuous duty. The moulded bobbin is annealed after moulding; residual stress is measured qualitatively by immersion in a solvent that induces environmental stress cracking on stressed regions. Long-term heat ageing is evaluated to IEC 60216-1 or ISO 11346 using elongation at break retention. Published data for this specific configuration is limited, and the relay manufacturer establishes the thermal class by testing moulded bobbins at three ageing temperatures. The failure criterion is typically defined as 50 % retained elongation at break. Oxidative embrittlement of the PBT matrix precedes any glass-fibre degradation, and the bond between copper wire and bobbin flange becomes the mechanical weak point. Moulders pre-dry pellets to below 0.02 % moisture; otherwise steam at the gate produces voids in the thin flange and reduces dielectric withstand. Solder reflow at 260 °C for 10 s is survivable only if the part is dried and annealed, but outgassing from moisture or degraded oligomers can blister the encapsulation layer. In this application the grade is used for automotive relay bobbins, power relay bodies, and miniature signal relay spools, provided that the continuous coil temperature does not exceed 150 °C and that the part is not exposed to hot glycol-based brake fluids or alkaline cleaning agents. The end-product standard IEC 61810-1 determines coil endurance, dielectric withstand, and insulation resistance after thermal ageing.
Competitive SABIC VALOX™ PBT+GF 553-BK1006 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF 553-BK1006 is a black-pigmented, 30 wt% glass-fiber-reinforced polybutylene terephthalate injection molding grade. The published typical density is 1.53 g/cm³ per ISO 1183-1. Tensile stress at break is listed at 135 MPa per ISO 527-2/5, with tensile strain at break of 2.5%. Flexural modulus is 9500 MPa per ISO 178, and flexural stress at break is 190 MPa per ISO 178. Notched Izod impact toughness is 10 kJ/m² at 23°C and 8 kJ/m² at -30°C per ISO 180/1A. Heat deflection temperature under 1.8 MPa is 220°C per ISO 75-2/A.
The reinforcement package produces anisotropic mold shrinkage. Flow-direction shrinkage is typically 0.2% to 0.4%, while transverse shrinkage is 0.4% to 0.8% when measured according to ISO 294-4 after molding in a 60°C to 100°C mold-temperature range. The melt volume-flow rate is listed at 12 cm³/10 min under 250°C and 2.16 kg load per ISO 1133-1:2022. These values are typical material characterization data, not batch release limits.
| Property | Test method | Typical value |
|---|---|---|
| Density | ISO 1183-1 | 1.53 g/cm³ |
| Tensile stress at break | ISO 527-2/5 | 135 MPa |
| Tensile strain at break | ISO 527-2/5 | 2.5% |
| Flexural modulus | ISO 178 | 9500 MPa |
| Flexural stress at break | ISO 178 | 190 MPa |
| Notched Izod impact, 23°C | ISO 180/1A | 10 kJ/m² |
| Notched Izod impact, -30°C | ISO 180/1A | 8 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2/A | 220°C |
| Melt volume-flow rate, 250°C/2.16 kg | ISO 1133-1:2022 | 12 cm³/10 min |
| Mold shrinkage, flow / transverse | ISO 294-4 | 0.2–0.4% / 0.4–0.8% |
Compared with general-purpose unfilled PBT, which typically exhibits tensile stress at break in the 50 MPa to 60 MPa range, flexural modulus near 2500 MPa, and heat deflection temperature under 1.8 MPa below 70°C, the 30 wt% glass-fiber reinforcement in 553-BK1006 raises load-bearing stiffness and thermal deformation resistance substantially. Relative to a 15 wt% glass-fiber PBT grade, which may show tensile stress at break near 110 MPa and flexural modulus near 6000 MPa, this grade shifts the mechanical envelope upward while reducing ductility. The trade-off appears in tensile strain at break values below 5% and in reduced weld-line strength when flow fronts meet.
The shrinkage differential is a further distinction. Unfilled PBT typically exhibits isotropic mold shrinkage from 1.2% to 1.8%. In 553-BK1006, glass-fiber orientation reduces flow-direction shrinkage to 0.2–0.4%, but the transverse value remains higher at 0.4–0.8%. This anisotropy must be compensated in tooling design. For a 2 mm nominal wall thickness, a gate placed at one end promotes longitudinal fiber alignment and creates warpage risk in long, flat parts. Where dimensional tolerances below 0.1 mm are required on feature position, published data for this specific black lot should be supplemented with part-level studies on the intended gating layout.
Processing on a twin-screw compounding line with L/D 40:1 and barrel zones from 240°C to 265°C is used to disperse the glass fiber. The black pigment addition does not alter the documented tensile modulus at the 2 mm plaque level, but colorant dispersion must be verified by optical microscopy at 100× to rule out agglomerates larger than 20 µm that can act as crack-initiation sites.
Pre-drying is mandatory because the PBT ester backbone hydrolyzes under heat and moisture. Moisture content above 0.02% at the hopper will cause hydrolytic chain scission, reducing molecular weight and impact resistance before visible splay appears. The resin should be dried at 120°C for 3 h to 4 h in a desiccant dryer with a dew point below -30°C. At ambient relative humidity above 60%, open containers should not remain exposed for more than 30 min before processing. On a reciprocating screw injection molding machine with a general-purpose screw of L/D 20:1 to 24:1 and compression ratio 2.5:1 to 3.0:1, barrel temperatures from 240°C to 265°C and melt temperatures from 250°C to 270°C are typical. The mold temperature should be maintained between 60°C and 100°C. Lower mold temperatures shorten cycle time but reduce crystallization and lower the observed ISO 75-2/A heat deflection temperature of the molded part.
Production-scale defect modes include surface splay, internal voids, and local reductions in notched Izod impact. Residual moisture above 0.05% can reduce notched Izod impact by 15% to 25% before visible delamination occurs. Barrel residence time above 300°C or longer than 5 min accelerates thermal degradation. Purging with unfilled PBT or a commercial polyolefin purging compound is recommended after shutdown. Direct purging with PVC or acetal should be avoided because their decomposition products cause corrosion and cross-contamination.
The limiting processing variable is hydrolytic degradation at elevated temperature. Water attacks the ester linkage in the PBT backbone, generating carboxyl end groups. The reaction is autocatalytic because the generated carboxylic acid end groups further catalyze chain scission. At melt temperatures above 270°C with residual moisture above 0.02%, solution viscosity declines measurably. The molecular weight reduction translates into lower tensile elongation and lower notched Izod impact, even when the molded part shows no surface defects.
Barrel residence-time distribution becomes critical in hot-runner systems with high melt residence volume. A hot-runner manifold held at 260°C with local zones above 280°C can degrade material in stagnant boundary layers. The resulting black specks or streaks are distinct from carbon-black dispersion defects. When streak formation is observed, the hot-runner setpoint should be reduced in 5°C increments and the manifold pressure gradient checked against the supplier’s recommended melt-channel shear rate. Published data for hot-runner shear limits on this exact BK1006 color lot is limited; a starting shear rate below 50,000 s⁻¹ is typically used for glass-filled PBT grades.
For electrical connector and sensor housing applications, the material is evaluated against UL 94 HB at the manufacturer’s listed minimum thickness of 0.75 mm. Electrical property tests include comparative tracking index per IEC 60112 and dielectric strength per IEC 60243-1. Published values for this exact black lot should be verified from the supplier’s certificate of analysis. Compliance documentation is typically supplied against RoHS Directive 2011/65/EU as amended and REACH Regulation 1907/2006/EC. The grade is not intended for prolonged immersion in hot water or steam above 60°C unless the application has been validated by part-level testing for hydrolytic aging.
| Requirement | Standard or reference | Status or condition |
|---|---|---|
| Flammability | UL 94 HB | Listed at 0.75 mm minimum thickness; final part wall thickness and pigment loading can affect classification. |
| Comparative tracking index | IEC 60112 | Published value for this exact color lot is limited; verify lot-specific certificate. |
| Dielectric strength | IEC 60243-1 | Value varies with specimen thickness and conditioning; supplier data required. |
| EU RoHS | 2011/65/EU as amended | Supplier documentation typically confirms compliance for the black color lot; lot-specific certificate required. |
| REACH SVHC | 1907/2006/EC | Supplier SDS should be checked against the current Candidate List for substances above 0.1 wt%. |
The BK1006 designation denotes a black color package. In semi-crystalline PBT, pigment particles can influence nucleation and therefore shrinkage behavior. With glass-fiber reinforcement, the dominant dimensional control arises from fiber orientation, but the black colorant can alter the crystallization onset temperature by a few degrees. Tooling cut for natural 30% glass-filled PBT may still require shrinkage compensation when switching to 553-BK1006. A mold-temperature study at 60°C, 80°C, and 100°C is the accepted method for determining flow and transverse shrinkage for a specific tool. The resulting shrinkage coefficient is applied to cavity dimensions for critical fits below 0.1 mm.
The grade finds use in automotive underhood brackets, power distribution housings, electrical terminal blocks, and structural appliance components where heat deflection temperature up to 220°C per ISO 75-2/A and UL 94 HB at 0.75 mm are limiting requirements. The material is not recommended for continuous exposure to concentrated aqueous acids, strong bases, or hot-water environments above 60°C without end-use validation. For overmolded elastomer assemblies, adhesion to the PBT substrate must be tested under the intended thermal shock profile because the glass-fiber surface reduces available bond sites compared with unfilled PBT.
Where ASTM-based purchase specifications are used, the corresponding mechanical test methods are ASTM D638-14, ASTM D790-17, and ASTM D256-10e1. Conversion between ISO and ASTM values is not direct because specimen geometry and support span differ, particularly for flexural modulus and Izod impact.