| HS Code | 458853 |
| Material Type | PBT + glass fiber |
| Flame Retardancy | UL94 V-0 at 1.5 mm |
| Volume Resistivity Ohm Cm | 1E15 |
| Mold Shrinkage Flow Percent | 0.2-0.5 |
| Melt Temperature C | 250-270 |
| Mold Temperature C | 60-90 |
As an accredited SABIC VALOX™ PBT+GF 553-1001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF 553-1001 packaging consists of 25 kg moisture-resistant bags on pallets for safe industrial storage and handling. |
| Container Loading (20′ FCL) | SABIC VALOX™ PBT+GF 553-1001 is packed in palletized 25 kg bags and loaded into a 20′ FCL for export. |
| Shipping | SABIC VALOX™ PBT+GF 553-1001 is shipped as non-hazardous, glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags or octabins. It is not regulated as dangerous goods (no UN number, class, or packing group). Keep dry and avoid excessive heat during storage and transport. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and strong oxidizers. Keep containers tightly closed to prevent contamination and moisture pickup. Avoid dust generation and ignition sources; use grounding when handling bulk. Follow the manufacturer’s SDS and local regulations, and consult the supplier for shelf-life guidance. |
| Shelf Life | Typically 2 years from manufacture when stored unopened in original packaging, dry, at 10–30°C, away from sunlight and moisture. |
Within DC motor brush card carriers for fractional-horsepower HVAC blower modules, the granulate is pre-dried in a desiccant-bed dryer with return-air dew point below -40°C until residual moisture content falls below 0.02 wt%, determined by ISO 15512 Karl Fischer titration. A general-purpose reciprocating screw with 20:1 L/D ratio and 2.2:1 to 2.5:1 compression ratio is retained; barrel profile is set from 240°C at the feed zone to 260°C at the nozzle, with a melt temperature of 250–265°C. Mould temperature is maintained between 70°C and 90°C to promote crystallinity and reduce post-mould movement. Injection is staged with screw advance between 30 mm/s and 60 mm/s, followed by packing at 60–80 MPa hydraulic pressure for 0.5–1.0 s/mm of nominal wall thickness. For a 1.0 mm brush card wall, shrinkage is 0.2% to 0.5% in the flow direction and 0.6% to 0.9% transverse when measured per ISO 294-4 after 72 h at 23°C. The end product integrates commutator ring supports and brush tube pockets; moulded-in slot positions are held within ±0.05 mm using pin gages after conditioning. Dielectric integrity is validated at 1.5 kV AC for 60 s by IEC 60243-1, and comparative tracking index is evaluated at 250 V using IEC 60112 solution A. Continuous exposure to hot aqueous glycol above 85°C is not recommended because ester hydrolysis reduces molecular weight and accelerates stress cracking at rib roots.
The limiting factor is not UL 94 V-0 alone; IEC 60695-2-11 glow-wire testing at 750°C for unattended appliances under IEC 60335-1 is thickness-dependent because the flame-retardant package must quench afterglow at the char layer. In electronic thermostat control modules and line-voltage power-supply enclosures, moulded brackets from 30% glass-reinforced PBT are gated with a single sub-runner per cavity to avoid weld lines at boss-to-wall junctions. Melt temperature is limited to 250–265°C; excursions above 270°C accelerate release of the brominated flame-retardant synergist and produce gas splay at the flow front. A 0.8 mm nominal wall requires injection velocity not exceeding 100 mm/s to prevent jetting, and packing is held at 70–90 MPa for 1.0 s/mm to densify the crystalline lamellae adjacent to the core. Heat deflection under 1.82 MPa by ISO 75-2/A is near 200°C, permitting brief contact with metal-oxide varistor leads at 150°C without boss deformation. The end product is a snap-fit control-module carrier; snap arms are radiused to not less than 0.6 mm at the root to avoid notch initiation. The relationship between glow-wire pass and filler orientation is non-linear; published data for 0.4 mm V-0 performance in this specific grade are limited, so the design minimum remains 0.8 mm.
| Assessment | Standard | Condition | Acceptance Criterion |
|---|---|---|---|
| Flammability | UL 94 V-0 | 1.5 mm thickness, 48 h at 23°C/50% RH | individual afterflame ≤ 10 s; no cotton ignition |
| Glow-wire ignitability | IEC 60695-2-11 | 750°C, 30 s contact | no flame persisting > 2 s; no ignition of wrapping paper |
| Tracking resistance | IEC 60112 | solution A, 100 drops | ≥ 250 V at material group IIIa |
| Heat deflection | ISO 75-2/A | 1.82 MPa, flatwise | ≥ 195°C after conditioning |
In three-phase distribution boards rated up to 690 V AC, phase barriers and busbar supports are injection moulded from glass-reinforced PBT where creep resistance and dielectric rigidity are required under continuous current heating. Unlike polyamide 66, the material exhibits limited moisture absorption, so dimensional change at 80°C and 90% RH remains below 0.1% after 1,000 h of exposure per IEC 60068-2-78. Processing uses a hot-runner system with valve gates because exposed busbar slots require flatness within 0.15 mm over 150 mm of linear travel. Cavity-filling pressure is capped at 90 MPa and holding time is set to 1.0 s/mm of section; an eight-cavity family tool is run with a clamp force of 3,500 kN to counter the high projected area of flat barrier plates. Creepage and clearance distances through the moulded barrier are designed under IEC 61439-1, with through-surface tracking performance classified according to IEC 60112. The end product is a formed-phase barrier with integral snap-in busbar clips; after assembly, dielectric withstand between adjacent phases is tested at 2.5 kV AC for 60 s according to IEC 61439-1. Mechanical impact at low temperature is the primary failure mode, so ductile-brittle transition is evaluated by falling-dart impact at -20°C; glass orientation parallel to the barrier plane reduces through-thickness crack propagation.
Because under-hood electrical distribution centres experience thermal cycling from -40°C to 125°C with superimposed vibration, fuse panel substrates and relay mounting plates are moulded using sequential valve gates to counter perimeter-to-centre shrinkage. Four post-cavity pressure transducers are positioned at the last flow fronts; injection is transferred to packing when the melt pressure at the final transducer reaches 50 MPa, preventing over-packing of the gate area and reducing warpage at the connector footprints. A 30 wt% glass fibre content raises dynamic modulus at 125°C sufficiently to hold relay blade alignment within 0.5 mm, but weld-line tensile strength drops to 55–65% of the virgin value measured by ISO 527-2/5. Battery acid and hot ethylene glycol are the principal chemical constraints; at coolant temperatures above 90°C, hydrolysis at the PBT ester linkage reduces notched Izod impact by more than 30% within 1,000 h of continuous exposure. Consequently, the material is confined to dry-side components and bracketry isolated from direct fluid line weep. The component is validated under thermal shock and humidity cycling per ISO 16750-4, but published component-level data for 553-1001 in 85°C/85% RH service is limited; qualification therefore requires OEM-specific humidity exposure with electrical load.
Industrial solenoid coil bobbins are wound with 0.2–0.8 mm enamelled copper wire at winding tensions up to 15 N; the bobbin flange must resist cracking at the gate and at the core-pin weld. When the flange wall is reduced below 0.8 mm, injection speed is limited to 60 mm/s to maintain a stable melt front, and melt temperature is set at 255°C to compensate for shear heating across the sub-runner. Packing pressure is held at 75 MPa for 3.0 s, followed by a profiled drop to 30 MPa over 2.0 s to minimize gate stress. Weld lines formed at the core-pin merge are tensile tested per ISO 527-2/5 on specimens cut from the flange; acceptance is set at 70 MPa minimum because lower values correlate with flange fracture during winding. Wire termination is via pressed-in terminals that produce hoop stress at the bobbin ID; stress-cracking resistance is screened by immersion in 2% sodium hydroxide for 24 h followed by compressive loading at 0.5% outer-fibre strain. The end product—a pilot-operated solenoid valve bobbin—requires class F insulation thermal endurance to 155°C; the material is therefore used in short-cycle intermittent duty rather than continuous service above 140°C because oxidative degradation of the PBT matrix accelerates beyond that threshold.
Terminal spacers for alternating-current charging inlets are gated at the geometric centre of the part to orient glass fibre radially around the pilot-pin aperture, thereby reducing anisotropic electrical tracking across flow lines. The moulding is processed at 250–265°C melt temperature with a cold-runner mould at 80°C, and the part is packed at 80 MPa for 2.5 s. Creepage distances between power contacts are maintained above 8 mm for pollution degree 3 installations under IEC 60664-1, and the material is classified for tracking at 250 V minimum per IEC 60112. The terminal spacer must withstand 2.5 kV AC dielectric test for 60 s after a thermal shock cycle from -25°C to 60°C, as referenced in charging interface qualification. The end product—a pilot-pin retainer and phase terminal spacer—is exposed to low-temperature impact when cable flexing occurs during cold weather; therefore, the design avoids sharp internal corners and maintains 0.6 mm minimum radii at the terminal recess. Published long-term ultraviolet data for unfilled PBT indicate surface embrittlement after outdoor exposure, so the component is installed inside the charging inlet enclosure rather than on an external face.
Pressure-sensitive terminal block bodies are produced with a multi-cavity hot-runner manifold, using cavity-pressure-controlled hold to prevent insert displacement around embedded brass threaded sockets. Each cavity is fitted with a ceramic-pressure sensor that triggers packing at 45 MPa melt pressure; hold is maintained for 1.0 s/mm of wall thickness. Brass inserts are preheated to 120°C to reduce shear stress at the insert-to-polymer interface, and the screw is retracted with 20 mm of decompression to prevent stringing from the valve gate. The 30 wt% glass reinforcement permits screw torque retention above 2.5 N·m after 10 tightening cycles on M4 terminals, but successive installation at higher torque produces microcracking that is detectable by dye penetrant. Electrical clearance is verified after assembly under IEC 60998-2-1 for screw-type terminal blocks, while the housing is subjected to glow-wire testing at 750°C for uninsulated live parts. The PBT matrix limits continuous use to 130°C in dry conditions; prolonged exposure to hot humid environments above 85°C/85% RH reduces tensile strength through hydrolysis and is not recommended unless the terminal block is protected by an enclosure.
Competitive SABIC VALOX™ PBT+GF 553-1001 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF 553-1001 is a 30 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding compound. The generic designation under ISO 11469:2016 is PBT-GF30. The material consists of a semicrystalline PBT matrix containing 30 % by mass short glass fibre, which raises stiffness and short-term heat resistance while reducing overall mould shrinkage relative to unfilled PBT. The product is supplied as pellets for conventional injection moulding and is not intended for blow moulding or rotational moulding.
In the SABIC VALOX range, the 553-1001 suffix identifies a standard injection-moulding position. Natural-grade data are used below; custom colours can alter flow length, impact strength, warpage, and flammability rating. The exact additive and colour package should be confirmed from the lot-specific certificate of analysis.
The values in the following table are representative manufacturer-published figures for the natural grade at 23 °C unless otherwise stated. They should not be applied as specification limits without confirmation against the current SABIC technical datasheet and the production lot certificate of analysis.
| Property | Test standard | Representative published value |
|---|---|---|
| Density | ISO 1183-1:2019 | 1.53 g/cm³ |
| Tensile modulus | ISO 527-2/1A | 9500 MPa |
| Tensile stress at break | ISO 527-2/1A | 110 MPa |
| Tensile strain at break | ISO 527-2/1A | 3.0 % |
| Flexural strength | ISO 178:2019 | 170 MPa |
| Flexural modulus | ISO 178:2019 | 8300 MPa |
| Charpy notched impact strength | ISO 179-1/1eA | 7 kJ/m² |
| Izod notched impact strength | ISO 180/A | 8 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2/Af | 205 °C |
| Vicat softening temperature, B120 | ISO 306/B120 | 210 °C |
| Water absorption, 24 h immersion | ISO 62 | 0.06 % |
| Dielectric strength, 3.2 mm | IEC 60243-1 | 19 kV/mm |
| Volume resistivity | IEC 60093 | >1.0E15 Ω·cm |
The values are generated on injection-moulded specimens of the thickness specified in the relevant test standard, generally 4 mm for ISO tensile and flexural tests. Glass-fibre orientation caused by plaque edge gating can produce modulus values 5 % to 15 % higher than values measured on production parts with high transverse flow. This anisotropy is a material characteristic and not a lot defect. The notched impact value of 8 kJ/m² does not imply toughness in sharp-cornered designs; the material is notch-sensitive, and gate vestiges, knit lines, and sharp internal corners behave as stress concentrators. Cold-climate service below -40 °C should be qualified by part-level impact testing rather than by reference to room-temperature data alone.
Compliance with RoHS Directive 2011/65/EU Annex II and REACH Regulation EC 1907/2006 Annex XVII should be confirmed through current SABIC product documentation. Food-contact, medical, and potable-water clearances are not automatic for the standard product and require written confirmation from SABIC regulatory affairs before specification.
Drying is mandatory before injection moulding. Residual moisture above 0.02 % causes hydrolytic degradation of PBT ester linkages at melt temperatures. The reaction is autocatalytic because chain scission releases carboxylic acid end groups that accelerate further hydrolysis. Desiccant dryers with a dew point of -30 °C or lower are required; standard drying conditions for natural resin are 120 °C for 3 h to 4 h. Material stored in humid environments above 60 % RH should be dried for 4 h to 6 h. Closed-loop hopper residence time should not exceed 2 h at temperature if the dryer cannot maintain a dew point below -30 °C.
The melt-temperature window is normally set between 250 °C and 270 °C. A common barrel profile is 240 °C rear, 255 °C centre, 265 °C front, and 260 °C to 270 °C nozzle. At melt temperatures above 275 °C, colour shift, tensile loss, and gaseous decomposition products increase. If hot-runner temperatures exceed 280 °C, the manifold should be rebalanced rather than increasing barrel temperature to compensate for short shots.
A general-purpose screw with an L/D of 18:1 to 20:1 and a compression ratio of 2.5:1 to 3.0:1 is adequate for most machines. High-compression screws can reduce glass-fibre length and lower impact strength. Back pressure is set in the range 0.3 MPa to 0.7 MPa, and screw surface speed is typically 0.2 m/s to 0.5 m/s. Injection speed should be medium to fast in thin-wall tools; cavity fill times below 0.5 s improve glass-fibre distribution in walls below 1.0 mm.
Mould temperature is maintained at 80 °C to 100 °C. At mould temperatures below 80 °C, the skin freezes before full crystallinity develops, increasing post-mould shrinkage and warpage. Mould shrinkage is anisotropic: representative flow-direction shrinkage in natural grade is 0.2 % to 0.4 %, while transverse shrinkage is commonly two to three times that value. Precision parts should be qualified on the production tool using ISO 294-4 shrinkage plaques, not on generic datasheet ranges.
On multicavity tools with wall sections at 0.4 mm to 0.8 mm, production short shots are frequently traced to gate freeze-off or glass-fibre packing at the gate, not to incorrect barrel temperature. Increasing gate land length to 1.0 mm to 1.5 mm and using a wider submarine or tab gate can restore filling without raising melt temperature. Weld lines in glass-reinforced PBT typically retain only 50 % to 60 % of the parent tensile strength; gate locations on connector housings should be chosen so that weld lines are not placed at latch arms or terminal retention features.
Heat deflection temperature under 1.8 MPa is 205 °C by ISO 75-2/Af, and Vicat softening temperature is approximately 210 °C by ISO 306/B120. These values indicate short-term heat resistance but do not define continuous service temperature. In dry air at zero load, 130 °C to 150 °C is a practical service band for many 30 wt% glass-filled PBT compounds; above this band, oxidative embrittlement progresses. Published data for the 553-1001 position under creep loads above 140 °C is limited, and prototype testing is required. The crystalline melting point of PBT is approximately 225 °C, so any soldering or reflow excursion above this value will produce distortion.
Volume resistivity above 1.0E15 Ω·cm under IEC 60093 and dielectric strength of 19 kV/mm at 3.2 mm under IEC 60243-1 are typical for a dry glass-filled grade. Glass fibre can reduce dielectric strength at thin sections. Low-voltage insulation coordination must rely on creepage and clearance distances established by IEC 60664-1:2020 rather than on dielectric strength alone. The comparative tracking index should be verified under IEC 60112 for the specific colour; many 30 % glass-filled PBT formulations fall in the 250 V to 300 V range, but surface contamination and humid ageing can reduce this value.
Chemical resistance is typical of semicrystalline PBT. The material resists aliphatic hydrocarbons, mineral oils, glycols, and many dilute acids at room temperature. Hot water and steam above 60 °C are hydrolysis boundaries; pressurised hot-water contact above 80 °C can cause rapid tensile loss and should be avoided unless the specific part and service condition are qualified. Strong bases above pH 9 and high-concentration oxidising acids should be considered incompatible. For outdoor use, a UV-stabilised or painted product is required because the natural grade yellows and embrittles under sustained UV exposure.
Compared with an unfilled PBT, 553-1001 raises flexural modulus from a class-typical 2.5 GPa to approximately 8.3 GPa and heat deflection temperature under 1.8 MPa from below 70 °C to approximately 205 °C. This increase is achieved at the expense of elongation at break, which drops from greater than 20 % for many unfilled PBT grades to approximately 3.0 %. The glass-reinforced position is therefore unsuitable for snap-fit designs that require high post-yield deformation; snap-fit strain should be limited to below the elongation at break and analysed at the lowest service temperature.
Against a flame-retardant 30 % glass-reinforced PBT, 553-1001 generally retains higher tensile strength and better thermal ageing because it does not carry an FR additive package. It is not UL 94 V-0; published flammability for natural thicknesses is typically UL 94 HB. For applications where V-0 or 5VA at wall thicknesses below 1.5 mm is mandatory, a flame-retardant VALOX grade such as 420SEO should be evaluated. That evaluation should include comparative tracking index under IEC 60112, glow-wire ignition temperature under IEC 60695-2-13, and notched impact under ISO 180/A, because FR additives often move all three properties.
Replacement of a 15 % or 20 % glass-filled PBT with 553-1001 also changes shrinkage balance. The 30 % glass fibre reduces overall mould shrinkage but increases differential shrinkage between flow and transverse directions. Flat rectangular parts with an edge gate are therefore more prone to warp. Flow-direction coefficient of linear thermal expansion is typically on the order of 25 µm/m·°C, while transverse expansion may approach 80 µm/m·°C; these class-typical values should be replaced by measured values for the production tool and part geometry.
For thin-wall connector housings at 0.4 mm to 0.6 mm wall stock, tool venting often determines whether the mould runs at cycle. Vent depths of 0.02 mm to 0.03 mm are typical for PBT-GF30; blocked vents cause short shots, burn marks, and white deposits on the cavity surface. Dimensional control should be based on a capability study run at the production press with a hot-runner system, not on prototype tooling. Checks after 24 h post-moulding are necessary because PBT continues to crystallise and dimensions can shift by more than 0.05 % in the first day after demoulding.