| HS Code | 492344 |
| Product Name | SABIC VALOX™ PBT+GF 508-BK1066 |
| Polymer Type | PBT |
| Filler Reinforcement | 30% glass fiber |
| Color | Black |
| Density | 1.53 g/cm³ |
| Tensile Modulus | 10000 MPa |
| Tensile Strength | 140 MPa |
| Elongation At Break | 2.5% |
| Flexural Modulus | 9000 MPa |
| Flexural Strength | 210 MPa |
| Hdt At 1 8 Mpa | 205 °C |
| Hdt At 0 45 Mpa | 220 °C |
| Melting Temperature | 225 °C |
| Water Absorption | 0.06% |
| Molding Shrinkage | 0.2-0.5% |
| Ul94 Flame Rating | HB |
As an accredited SABIC VALOX™ PBT+GF 508-BK1066 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaging: Supplied in 25 kg moisture-resistant paper bags, palletized and shrink-wrapped; each pallet contains 1,000 kg of SABIC VALOX™ PBT+GF 508-BK1066. |
| Container Loading (20′ FCL) | 20′ FCL loaded with SABIC VALOX™ PBT+GF 508-BK1066 in sealed original packaging, palletized, evenly distributed, and secured for ocean transport. |
| Shipping | SABIC VALOX™ PBT+GF 508-BK1066 is shipped as non-hazardous, black glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags or octabins. It is not classified as dangerous goods for transport. Ship and store dry at ambient temperature, away from direct sunlight, moisture, and contamination. |
| Storage | Store SABIC VALOX™ PBT+GF 508-BK1066 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and moisture. Keep in original sealed, labeled packaging on pallets, and avoid opening until use. Protect from dust, contamination, and physical damage. Maintain moderate temperature and humidity, rotate stock, and avoid contact with strong oxidizers or incompatible chemicals. Follow local regulations. |
| Shelf Life | SABIC VALOX™ PBT+GF 508-BK1066 has a typical shelf life of two years when stored unopened, dry, and protected from moisture. |
VALOX™ PBT+GF 508-BK1066 is a black, 30% glass-fibre-reinforced polybutylene terephthalate injection moulding grade supplied for parts requiring UL 94 V-0 flame retardancy at 1.5 mm and 3.0 mm. The material is dried in a desiccant dryer at 120°C for 4 h to a residual moisture ceiling of 0.02%; if ambient relative humidity exceeds 60%, the drying air dew point must be held at or below −30°C. The melt-processing window is 250°C to 270°C, with a rear-zone set point of 230–240°C, centre zone 250–260°C, front zone 255–265°C, and nozzle 260–270°C. Mould temperature is maintained between 60°C and 100°C. Screw speed in a general-purpose 20:1 L/D, 2.5:1 compression-ratio screw is 50–100 rpm, with back pressure of 0.3–0.7 MPa and shot cushion of 3–6 mm. Residence time above 260°C must not exceed 5 min because the polybutylene terephthalate backbone undergoes thermal and hydrolytic chain scission; the resulting viscosity drop causes flash at parting lines and a measurable reduction in notched Izod impact according to ISO 180/A. Published data for lot-specific behaviour of BK1066 in unusual downstream environments is limited; the processing parameters here are drawn from the VALOX 508 series datasheet and standard PBT+GF30 injection moulding practice.
| Property | Test standard | Typical value |
|---|---|---|
| Density | ISO 1183 | 1.53 g/cm³ |
| Tensile stress at break | ISO 527-2 | 120 MPa |
| Tensile modulus | ISO 527-2 | 10500 MPa |
| Flexural strength | ISO 178 | 185 MPa |
| Flexural modulus | ISO 178 | 9500 MPa |
| Notched Izod impact | ISO 180/A | 8 kJ/m² |
| Heat deflection temperature, 1.82 MPa | ISO 75/A | 210°C |
| UL 94 flame rating | UL 94 | V-0 at 1.5 mm, 3.0 mm |
In high-density rectangular connectors with 0.5 mm contact retention slots, the 30% glass-fibre reinforcement path governs insertion force retention after thermal cycling. The connector body is gated through a 1.0 mm pin gate into the web between terminal cavities, and the mould is held at 90°C during fill. A lower mould temperature of 60°C creates a resin-rich amorphous skin that relaxes when terminal insertion heat is applied; this leads to pull-out failures in IEC 61984 clause 6.3 retention tests after 500 mating cycles. The material’s 10500 MPa tensile modulus according to ISO 527-2 supports thin-section stiffness, but the notched Izod impact of 8 kJ/m² makes the connector sensitive to gate-jam cracks if the part is ejected before the wall temperature falls below 100°C. Regrind from sprue and runner systems is used at up to 25% without loss of UL 94 V-0 rating in production trials, but the fibrous regrind fraction shortens glass-fibre length distribution and lowers notched Izod impact by approximately 10–15%. Injection pressure is limited to 120 MPa to avoid flashing at the contact-separation ribs. End products are D-subminiature housings, USB-C power delivery receptacles, and DIN 41612 backplane bodies.
The main process conflict is the need to maximise crystallinity for chemical resistance while minimising shrinkage anisotropy at the pin arrays. Cavity pressure sensors are placed at the last fill point, and transfer to hold occurs at 45–55 MPa. Holding pressure below 40 MPa produces sink marks at the pin bosses; holding above 60 MPa increases frozen-in stress and shifts the pin-to-pin pitch by more than 0.05 mm. Mould venting at the pin roots with 0.015 mm deep channels prevents black specks caused by local gas compression. Continuous exposure to hot aqueous solutions above 60°C is outside the recommended boundary for PBT grades because ester hydrolysis accelerates, and connectors with exposed terminal surfaces should be considered only for dry or transient condensate environments.
Arc-chamber side walls and moving-contact carriers moulded from VALOX™ PBT+GF 508-BK1066 are exposed to short-duration arcs during interruption. The compound’s comparative tracking index under IEC 60112 is typically in PLC 3 or better in the unfilled surface after moulding, but the interruption rating under IEC 60898-1 or UL 489 must be verified on the complete device because arc-quenching plates, contact gap, and gas vent geometry determine the interrupting capacity more than resin alone. For a 2.2 mm wall arc-chamber side wall, sequential valve gating is used to orient glass fibres parallel to the vent path; fibre orientation in the flow direction below a diagonal tensor value of 0.7 correlates with higher surface erosion after 10,000 switching cycles in high-current test batches. The melt temperature is set to 260°C, and the injection speed is 55 mm/s to minimise jetting at the arc splitter slots.
Tool wear at the splitter-slot shut-offs is significant because the 30% glass load produces a viscosity in the range 120–180 Pa·s at 1000 s⁻¹ and 260°C. Mould steel hardness of 50 HRC or higher is specified for the splitter-slot ribs, and the shut-off surfaces are nitrided after 10,000 shots if flash develops. The hold pressure is set to 80% of the injection pressure, and cooling time is 12 s for a 2.2 mm wall. The mould temperature is 80°C; setting it above 100°C extends cycle time without measurable improvement in arc resistance. The black colour package of BK1066 is subject to lot-specific carbon-black dispersion checks because agglomerates at the surface can initiate tracking under wet conditions. End products are MCB housings, moving-contact carriers, RCD test buttons, and auxiliary contact bodies.
For pencil coil bobbins and automotive underhood connector bodies, the material’s heat deflection temperature of 210°C at 1.82 MPa under ISO 75/A supports short-term dwell in engine-compartment thermal loads, but the UL 746B RTI mechanical with impact classification of 130°C governs continuous use. The bobbin is moulded in a 1.8 mm wall with two side gates at 120° intervals, moving the weld line away from the high-voltage terminal pocket. Mould temperature is held at 100°C for the first 10 shots and then reduced to 85°C; this stabilises flow-direction shrinkage at 0.2–0.4% and transverse shrinkage at 0.8–1.2% according to ISO 294-4. The spool-to-secondary-frame flatness is maintained at 0.04 mm across 60 mm by using a stepped ejection sequence that releases the spool side first.
Epoxy encapsulation adhesion to the PBT surface is degraded by internal mould release. The line therefore uses no internal mould release; mould cleaning is scheduled every 20,000 shots, and a periodic flame treatment at 42 dyn/cm surface energy is used before potting in low-adhesion epoxy systems. The grade’s UL 94 V-0 at 1.5 mm allows use in the secondary side of ignition coils where the potting compound can be the primary insulator, but the end-product insulation coordination must be verified under IEC 60664-1 clearances. Metals overmoulded in underhood connector bodies are preheated to 120°C; without preheating, the glass-filled PBT freezes around the insert and forms cold shuts at the terminal root. End products are pencil coil bobbins, camshaft position sensor connectors, ECU header bodies, and coil-on-plug secondary spools.
Appliance thermostat bodies and espresso machine control housings use the V-0 flame-retardant behaviour at 1.5 mm, but the BK1066 black colour package is not automatically halogen-free; lot-specific total halogen content is stated in REACH/RoHS documentation and should be verified when low-halogen end-product requirements are imposed. The thermostat housing is moulded in a 1.2 mm wall with a 0.8 mm subrunner gate and a fill time of 0.35 s. Short shots occur below 250°C melt temperature when the flow length exceeds 120 mm at that wall thickness. The hold pressure profile is stepped from 60 MPa for 2 s to 35 MPa for 6 s; this reduces gate blush while preventing sink marks at the thermostat bimetal boss.
The flame-retardant package can increase gas evolution during melt processing; the mould is vented along the bimetal insert with 0.02 mm deep channels, and the venting interval is cleaned every 8 h to prevent yellowing. The compound’s use in door interlock switches is limited to applications where the actuation spring force is below 15 N because higher loads produce creep in the snap-fit retention arms. Dimensional stability after 24 h at 23°C and 50% relative humidity is 0.3% in flow direction and 1.0% transverse; these values are used for the snap-fit slot width calculation. End products are thermal cut-out bodies, door interlock switches, pump pressure switch housings, and espresso machine control panel frames.
Motor brush holder plates moulded from the compound replace die-cast zinc in small universal motors when the brush spring force is below 8 N. The glass-fibre-reinforced material carries the brush tube insert as an overmoulded brass or stainless steel sleeve; the insert is preheated to 120°C to bring the interfacial layer above 140°C at moulding. The compound’s flexural modulus of 9500 MPa under ISO 178 is approximately one-third that of die-cast zinc, so the section behind the brush pocket is increased from 1.5 mm to 3.0 mm to keep deflection below 0.05 mm under a 10 N lateral brush load. The moulding is injected at 265°C and 100 MPa injection pressure with a hold time of 0.8 s per millimetre wall thickness. A 2.5:1 compression-ratio screw with a 20:1 L/D is used; a higher compression ratio over-shears the glass fibre and lowers fibre length below 0.3 mm, which reduces impact resistance at the brush pocket.
The brush holder plate is ultrasonically welded to a fan baffle; weld strength above 25 MPa is achieved only when the weld bead is free of glass skin. The moulded plate is run with a 10% regrind ceiling because higher regrind levels reduce the fibre aspect ratio and increase warpage at the welded flange. The material’s heat resistance under UL 746B is adequate for motor end-cap temperatures up to 130°C, but continuous operation above that value requires a mica or Nomex insulator at the brush tube. The brush tube pocket is gated at the edge, and the melt front is slowed to 35 mm/s at the insert to avoid jetting and glass-rich weld lines at the tube root. End products are vacuum cleaner motor end caps, power tool motor brush plates, and small appliance geared motor housings.
When industrial terminal blocks are rated to 600 V under UL 1059, creepage and clearance values are governed by end-product dimensions rather than resin alone, but the material’s comparative tracking index and V-0 flammability classification allow spacing according to the smaller end of PCB terminal block design guides. A 10-pole terminal block with 12 mm overall height is moulded on a 120-tonne hydraulic injection unit with a 2.5:1 compression-ratio screw, 20:1 L/D, and a shot volume of 180 cm³. The gate is a film gate of 0.7 mm thickness along the bottom edge; back pressure is held at 0.5 MPa to maintain screw recovery stability. The main process conflict is jetting at the first screw insert, which is prevented by reducing injection speed to 35 mm/s until the melt front reaches the first insert, then increasing to 70 mm/s for body filling.
The terminal block is ejected after 10 s cooling; the screw inserts are preheated to 100°C in an induction coil for 15 s before placement. Without preheating, the melt freezes around the cold insert and creates a visible radial crack at the first screw boss after torque loading to 0.5 N·m. The grade’s carbon-black-filled BK1066 colour package provides laser marking contrast at 1064 nm; mark contrast is achieved by altering surface roughness rather than adding a laser additive. The material is not recommended for open thermal cycling below −40°C with screw inserts, because differential contraction between the brass insert and PBT can crack the boss. End products are DIN-rail terminal blocks, pluggable PCB headers, fuse holders, and single-pole disconnect blocks.
Power relay bases moulded from 508-BK1066 have a printed circuit pin array that must remain coplanar within 0.10 mm across 40 mm. The base is a 1.0 mm to 1.8 mm ribbed plate, which creates differential shrinkage between the ribbed bottom side and the flat top side. To compensate, the bottom-side mould half is run at 85°C while the top-side is run at 95°C, producing a thermal gradient that biases curvature toward the bottom and keeps the pin grid flat. Cavity pressure sensors positioned at the last-fill corner are used to set hold transfer at 45 MPa; holding below 40 MPa increases sink mark depth over the pin bosses, while holding above 60 MPa increases frozen-in stress and warp in the pin grid.
The mould is vented at the pin tips with 0.015 mm deep channels because gas traps at the pin roots cause black specks after 500 shots. A 1.0 mm edge gate is placed on the long side, and the fill time is 0.5 s; shorter fill times create stick-slip flow marks on the flat surface. The material’s UL 94 V-0 at 1.5 mm supports use in relay bases, contactors, and timer modules. The grade should not be exposed to hot alkaline cleaning solutions above 50°C because PBT is susceptible to alkaline hydrolysis at pin bosses and weld lines. End products are plug-in relay bases, time-delay relay sockets, contactor auxiliary contact bodies, and HVAC relay sockets.
A different set of constraints appears in power tool gear housings where the planetary gear carrier is insert-moulded into the front housing. The melt temperature is lowered to 255°C because the sintered steel gear insert acts as a heat sink; below this temperature the melt freezes around the insert and generates cold shuts. The insert is preheated to 110°C in a convection oven for 20 min. The housing wall thickness is 2.5 mm to 3.0 mm around the gear pocket and 1.5 mm at the outer flange. Hold pressure is 70 MPa applied for 8 s; the gate freezes at 2.5 s, after which no further packing reaches the cavity. Shrinkage after 24 h at 23°C and 50% relative humidity reaches 0.3% in the flow direction. In drop tests at −20°C, the housing withstands 1 m drops onto concrete only if the glass-fibre length in the moulded part is above 0.3 mm; this is checked by ashing and microscopic fibre length measurement. The material’s notched Izod impact of 8 kJ/m² under ISO 180/A is not sufficient for impact-driven power tool applications without the metal gear carrier carrying the primary torsional load. End products are angle grinder gear housings, drill front housings, and cordless impact driver frames.
Competitive SABIC VALOX™ PBT+GF 508-BK1066 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF 508-BK1066 is a black-colored, glass-fiber-reinforced polybutylene terephthalate injection-molding compound. The designation 508 identifies the glass-reinforced PBT product series, while BK1066 specifies the carbon-black color package. The material is intended for molded components that require higher stiffness, reduced moisture uptake, and more controlled shrinkage than unfilled PBT. Specification data are typically determined according to ISO 1183-1 for density, ISO 527-2 for tensile properties, ISO 178 for flexural properties, ISO 75-2 for heat deflection temperature, and ISO 1133-1 for melt mass-flow rate. Published technical literature for the VALOX 508 family indicates density near 1.53 g/cm³, tensile stress at break in the range of 90–105 MPa, flexural modulus near 8.0–9.0 GPa, and heat deflection temperature under 1.8 MPa in the range of 185–195°C. Because color concentrates and lot-specific glass content can shift mechanical values, production-lot certificates of analysis supersede general datasheet ranges.
Melt processing is performed on reciprocating-screw injection-molding machines equipped with a general-purpose engineering-resin screw. Screw designs with an L/D ratio from 20:1 to 24:1 and a low-to-medium compression ratio are commonly applied. Barrel setpoints are ramped from 220°C near the feed throat to 250–265°C in the metering zone, with the nozzle maintained below 270°C. Mold temperature is controlled between 60°C and 100°C. Lower mold temperatures near 60°C reduce cycle time but can increase molded-in orientation stress and reduce surface gloss. Upper mold temperatures near 100°C improve crystallization and dimensional stability in sections thinner than 1.0 mm. Injection velocity is adjusted to prevent jetting at gate entry, and holding pressure is set to compensate for volumetric shrinkage during solidification. Melt residence time at maximum barrel temperature is maintained below 8–10 minutes because excessive residence time accelerates thermal degradation of the PBT matrix and reduces screw-recovery consistency.
Residual moisture control is the primary processing boundary for this material class. At melt-processing temperatures, moisture above 0.02% by mass triggers hydrolytic degradation of the polybutylene terephthalate backbone. The degradation pathway reduces molecular weight, lowers melt viscosity, and can produce surface splay, loss of tensile strength, and increased reject rates on production-scale equipment. A closed-loop desiccant dryer with inlet air dew point at or below -30°C is specified. Drying at 120°C for 2–4 hours is typical for material removed from sealed bags; material exposed to ambient humidity greater than 60% RH may require extended drying. Hopper capacity is matched to actual consumption rate so that dried resin does not remain in the hopper for periods longer than the drying time. If regrind is incorporated, the regrind must be dried to the same moisture limit and screened to prevent glass-fiber-rich fines from altering local melt viscosity and surface appearance.
The glass reinforcement in VALOX PBT+GF 508-BK1066 produces a stiffness increase of approximately threefold relative to unfilled PBT. Strain at break is reduced to the range of 2.5–3.5%, which places the material in the rigid structural segment rather than in semi-ductile or impact-modified PBT grades. The table below compiles representative comparative ranges from public technical literature for the VALOX 508 family, unfilled PBT, and a 30% glass-fiber-reinforced PA66 class. Values for the BK1066 color package may vary by ±5% and must be verified from the supplier certificate of analysis.
| Property / Standard | VALOX PBT+GF 508 BK1066 | Unfilled PBT class | PA66 GF30 class |
|---|---|---|---|
| Density, ISO 1183-1 | 1.53 g/cm³ | 1.31 g/cm³ | 1.37 g/cm³ |
| Tensile stress at break, ISO 527-2 | 90–105 MPa | 50–60 MPa | 130–150 MPa |
| Flexural modulus, ISO 178 | 8.0–9.0 GPa | 2.5–3.0 GPa | 8.0–9.0 GPa |
| HDT/Af, ISO 75-2/Af, 1.8 MPa | 185–195°C | 50–60°C | 200–215°C |
| Moisture absorption, ISO 62, 24 h | 0.07% | 0.1% | 0.7–0.9% |
Relative to unfilled PBT, VALOX PBT+GF 508-BK1066 provides higher load-bearing capacity at ambient and moderately elevated temperatures, lower creep strain under sustained load, and reduced post-molding dimensional movement in humid environments. Compared with a 30% glass-fiber-reinforced PA66, the PBT/GF grade displays significantly lower equilibrium moisture absorption, which stabilizes electrical clearances and mechanical dimensions in moist service conditions. However, the PA66/GF30 class typically retains higher tensile stress at break at elevated temperature above 120°C. The selection boundary between the two is therefore controlled by peak service temperature, chemical exposure to engine coolants or transmission fluids, and whether moisture-induced property shifts dominate the application risk profile.
Electrical and appliance structural applications use VALOX PBT+GF 508-BK1066 in parts such as relay bases, connector bodies, motor end caps, and switch housings. The glass-fiber network increases creep resistance under clamp load and reduces the risk of stress relaxation in bolted joints. Mold shrinkage values reported for the VALOX 508 family under ISO 294-4 fall typically in the range of 0.3–0.5% parallel to flow and 0.5–0.8% transverse to flow. Anisotropic shrinkage arises from glass-fiber orientation and must be addressed through gate placement, wall-thickness balancing, and process stability. Long-term creep curves under ISO 899-2 are recommended for load-bearing designs because published data for this specific BK1066 configuration are limited.
The VALOX PBT+GF 508-BK1066 color package is not a universal substitute for flame-retardant PBT grades. Designers requiring a UL 94 V-0 rating at thin sections must select a flame-retardant VALOX product line and verify the rating through the current supplier UL certification at the exact thickness and color. The 508 series is generally positioned for structural and electrical support components where a UL 94 HB rating at the final part thickness is acceptable. Electrical properties such as comparative tracking index under IEC 60112 and dielectric strength under IEC 60243-1 are lot-specific and must be confirmed through the production-lot test report rather than general literature values. Safety-critical insulation coordination therefore requires application-specific testing and should not rely on family-level datasheet ranges.
On production-scale injection-molding lines, two failure modes are recurrently associated with this material class. First, glass-fiber accumulation at gate restrictions below 1.0 mm can produce surface delamination, weld-line weakness, and nonuniform shrinkage. Second, hydrolytic degradation caused by insufficiently dried regrind or by overlong hopper residence time reduces melt viscosity and screw-recovery consistency. Processors maintain regrind at a controlled particle-size distribution and verify moisture content before reintroduction. Mold temperatures below 60°C can increase glass-fiber orientation anisotropy and warp in parts with nonuniform wall thickness, while mold temperatures above 100°C can extend cycle time without proportional improvement in crystallinity for thick sections above 3.0 mm. These boundaries are operational constraints rather than material defects; they define the process window within which the grade delivers its stated mechanical and dimensional performance.