Sabic Valox Pbt Gf 420seo Bk1066

SABIC VALOX™ PBT+GF 420SEO-BK1066

    • Product Name: SABIC VALOX™ PBT+GF 420SEO-BK1066
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 463371
    Density 1.53 g/cm³
    Glass Fiber Content 30 %
    Tensile Modulus 11000 MPa
    Tensile Stress At Break 120 MPa
    Tensile Strain At Break 2.5 %
    Flexural Modulus 10000 MPa
    Flexural Strength 180 MPa
    Notched Izod Impact Strength 80 J/m
    Heat Deflection Temperature At 1 8 Mpa 200 °C
    Heat Deflection Temperature At 0 45 Mpa 210 °C
    Vicat Softening Temperature 210 °C
    Ul 94 Flammability Rating V-0 at 0.75 mm
    Volume Resistivity 1E15 ohm·cm
    Dielectric Strength 20 kV/mm
    Coefficient Of Linear Thermal Expansion 2.5E-5 /°C

    As an accredited SABIC VALOX™ PBT+GF 420SEO-BK1066 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ PBT+GF 420SEO-BK1066 black resin pellets packaged in 25 kg moisture-barrier bags, 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of SABIC VALOX™ PBT+GF 420SEO-BK1066, palletized and secured for shipment.
    Shipping SABIC VALOX™ PBT+GF 420SEO-BK1066 is supplied as black glass-fiber-reinforced PBT pellets. It is non-hazardous and not regulated for transport. Ship in sealed moisture-barrier bags or containers under dry conditions, avoiding moisture, heat, and contamination.
    Storage Store SABIC VALOX™ PBT+GF 420SEO-BK1066 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep containers tightly closed and avoid contamination, dust, and physical damage. Protect from humid air; do not store near incompatible chemicals or oxidizing agents. Use appropriate PPE and follow the supplier’s SDS and local regulations.
    Shelf Life Shelf life is two years from date of manufacture when stored cool and dry in original unopened packaging.
    Application of SABIC VALOX™ PBT+GF 420SEO-BK1066

    In low-voltage switchgear manufacturing, arc-shield and terminal-support components are injection moulded from SABIC VALOX™ PBT+GF 420SEO-BK1066 at a nominal glass-fibre fraction of 20 wt%. The material is specified where an ignitable polymeric part must satisfy UL 94 V-0 at 0.8 mm nominal wall thickness without secondary flame-retardant coatings. Compliance for the populated assembly is evaluated under IEC 60898-1:2015 for miniature circuit breakers and under IEC 60695-2-11:2014 glow-wire testing, with the glow-wire acceptance temperature governed by the final part geometry and contact arrangement rather than by the compound alone. Formulation addition ratio in this downstream segment is constrained by closed-loop regrind from sprues and runners; the maximum recommended re-introduction rate is 20 wt% regrind blended into virgin pellets, provided the re-granulated fraction is dried to below 0.02% moisture and its dust fraction remains below 0.5 wt%. The production process begins with desiccant drying at 120°C for 4 h using a dryer dew point of -30°C or lower, followed by injection moulding on a screw machine with a barrel profile of 250–270°C and a mould temperature of 80–90°C. Hold pressure is typically set between 60 MPa and 80 MPa, with an average cavity pressure of 40–60 MPa recorded at the gate-seal point. Failure modes observed on production-scale equipment include short shots in thin arc-barrier ribs below 0.8 mm where glass-fibre orientation restricts melt front progression, and burn marks at the end of fill when vent depth exceeds 0.02 mm or when melt residence time exceeds 8 min. Terminal finished product types in this segment include miniature circuit breaker housings, residual current device bases, busbar retainers, and terminal-block sub-assemblies for DIN rail installations.

    Why Do Underhood Automotive Connector Housings Require Pre-Dried PBT-GF20 FR?

    Underhood automotive connector housings, fuse-box covers, and transmission sensor connectors moulded in this grade demand moisture control because PBT is a condensation polymer; at melt temperature, residual moisture above 0.02% accelerates hydrolytic chain scission, lowering molecular weight, reducing weld-line tensile strength measured to ISO 527-1:2019, and causing batch-to-batch variation in flame-retardant certification. Production-scale experience on 1,800 kN electric toggle-clamp injection machines with 25 mm diameter screws at L/D 20:1 shows that drying at 120°C for 4 h is the minimum; when ambient relative humidity exceeds 60%, hopper residence is extended to 6 h and dryer dew point is maintained below -40°C. Barrel-zone set points are profiled at 245°C, 255°C, 265°C, and 260°C from feed to nozzle, with measured melt temperature kept at 255–260°C to balance fill of multi-cavity connector tools against flame-retardant decomposition. Mould temperature is held at 70–90°C; lower mould temperatures create surface delamination at knit lines, while higher temperatures increase flash risk on 0.8 mm connector latch features. Addition ratio for automotive rework is limited to 15 wt% post-industrial regrind when the programme is qualified to USCAR-2 mechanical durability requirements; closed-loop recycled PBT-GF20 FR above this threshold widens injection-pressure variation in multi-cavity hot-runner tools by more than 5% and can alter terminal retention after thermal cycling. Compliance testing for the finished wire-to-device connector assembly references ISO 8092-2:2005 for on-board electrical wiring harness connections, with material flammability documented by UL 94 V-0 at 0.8 mm. Continuous-use temperatures above 140°C are not recommended for this PBT-GF20 FR grade; under sustained underhood exposure, polyamide or PPS grades are substituted when the heat-aging test defined in the OEM specification exceeds 1,000 h at 135°C. Terminal finished product types include engine control module connector shells, underhood junction boxes, fuse-box covers, and transmission speed-sensor connector shrouds.

    Angle grinder gearcase covers and drill motor end caps moulded in VALOX™ 420SEO-BK1066 experience differential shrinkage between longitudinal and transverse glass-fibre orientation; this produces warpage in rectangular covers with wall thickness below 1.5 mm. The applicable product safety framework is IEC 62841-1:2014 with material flammability certification to UL 94 V-0 at 0.8 mm. Flexural modulus for design verification is tested to ISO 178:2019, but end-use drop-test survival is highly dependent on gate location and weld-line placement. Addition ratio is set by part thickness: for gearcase covers with nominal wall above 1.5 mm, recycled PBT-GF20 FR from the in-house gating system is introduced at up to 25 wt%; for motor end caps with 0.8 mm walls, regrind is limited to 10 wt% because the recycled fraction raises peak injection pressure and creates flow hesitation at thin cooling ribs. The preferred downstream production process uses sequential valve-gate injection with a fill time of 2.0 s to 2.5 s, followed by packing at 70–100 MPa for 4–6 s. Mould temperature is maintained at 80–90°C with turbulent water channels sized to remove 12–15 W/cm² from the cavity surface. On production lines, ejection-side cracking occurs when part ejection temperature exceeds 100°C; cycle-time optimisation therefore monitors post-ejection surface temperature with infrared sensors. Finished component types include angle grinder gearcase covers, drill motor end caps, orbital sander base plates, and switch housings for double-insulated power tools.

    Battery Management System Cell-Sensing Connector Carrier Moulding in VALOX 420SEO-BK1066

    Cell-sensing connector carriers and low-voltage harness headers for battery management systems are moulded in this compound at nominal wall thicknesses of 0.8–1.2 mm, where the 20 wt% glass reinforcement provides sufficient plate stiffness for terminal insertion but reduces spiral-flow length compared with unreinforced PBT. Compliance for the battery-pack electrical architecture references ISO 6469-1:2019 for electrically propelled road vehicles and UL 94 V-0 at 0.8 mm; connector-level harness requirements are evaluated against the applicable IPC/WHMA-A-620 class criteria for wire preparation and terminal retention. The black colour package BK1066 is already compounded into the feedstock, so no additional carbon black masterbatch is introduced at the press. Addition ratio is intentionally conservative: closed-loop regrind is held to 10 wt% maximum in 0.8 mm pitch connector wafers, and many BMS moulders eliminate recycled material entirely from first-shot production because lot-to-lot melt-viscosity variation beyond ±3% shifts fill behaviour in thin terminal-retention windows. The injection moulding process uses fast-fill parameters with melt temperature at 255–265°C and injection velocity of 120–180 mm/s; cavity pressure sensors at the end of fill record a switchover point between 70 MPa and 90 MPa. Vent land depth is maintained at 0.015–0.02 mm to prevent flash on terminal insertion faces while avoiding burn marks at the last-filled cavity region. Published productivity data for 0.4 mm connector walls in this specific configuration is limited; end-use validation is therefore required before retracting steel from a 0.8 mm baseline. Finished terminal product types include BMS cell-sensing connector carriers, wire-to-board harness headers, battery-pack signal connector housings, and module terminal covers. The grade is not specified for high-voltage power-distribution connectors where arc-tracking resistance and 600 V creepage requirements demand PPS-GF or PPA-GF alternatives.

    When Switching Arc Suppression Relays Move to 0.75 mm Wall Stocks

    Power relay bases, armature cradles, and arc-barrier isolators moulded at 0.75 mm wall stock impose a narrow processing window because the flame-retardant package in PBT-GF20 FR decomposes under excessive melt residence and shear heating. Relay-specific compliance is evaluated under IEC 61810-1:2019 for electromechanical elementary relays, with the moulded insulation body subject to glow-wire testing at 850°C according to IEC 60695-2-11:2014 when the relay is installed in unattended equipment. The material flammability marking remains UL 94 V-0 at 0.75 mm, but part geometry and hole spacing affect the thermal incident outcome independent of the base-resin listing. Addition ratio in this segment is restricted to 10 wt% maximum recycled PBT-GF20 FR for 0.75 mm relay bases; moulding trial records from relay production show that recycled content above 15 wt% increases injection-pressure scatter by approximately 12% in cold-runner tools and produces inconsistent armature-cradle flatness after 24 h moisture conditioning. The downstream process uses a two-plate cold-runner mould with gate diameter of 0.6–0.8 mm, barrel temperatures from 245°C to 260°C, and mould temperature of 70–80°C. Melt residence time is limited to 8 min; production interruptions exceeding 15 min require purging with the same grade to displace degraded flame-retardant material from the screw channel. The principal processing failure on production lines is not burn marks but post-mould warpage in the armature cradles caused by differential glass orientation around ejector bosses. Terminal finished product types in this segment include power relay bases, armature cradles, arc barriers, and coil formers for contactors used in elevator control cabinets and HVAC compressor switching panels.

    Field-mounted industrial sensor enclosures operating in oil-mist and high-vibration environments are moulded with metal threaded inserts preheated to 150°C before insert moulding; insert displacement and hoop stress cracking around the threads are controlled by slowing injection speed to 60–100 mm/s until the melt front passes the insert plane. The applicable safety standard for the enclosure is IEC 61010-1:2010 with ingress protection normally specified at IP65 or IP67 when the cover is ultrasonically welded to the base. Material flammability is certified to UL 94 V-0 at 0.8 mm, and the compound meets the restricted-substance reporting obligations under REACH and RoHS Directive 2011/65/EU as amended by (EU) 2015/863. Formulation addition ratio for this segment is governed by the welding interface: external mould-release sprays are limited to 0.05 wt% maximum and restricted to non-bonding surfaces, because release-agent carryover into the ultrasonic weld zone reduces weld burst pressure. The glass-fibre content in the finished polymer remains 20±1 wt%; closed-loop recycled material is held at or below 20 wt% only when the downstream processor has verified that recycled content does not shift the ultrasonic horn frequency response above ±100 Hz from virgin material. Production processing uses a mould temperature of 65–80°C, packing pressure of 50–70 MPa, and post-mould dimensional conditioning at 23°C/50% relative humidity for 24 h before lid-to-base assembly. Terminal finished product types include proximity sensor housings, limit switch bodies, flow-meter terminal lids, and field-transmitter junction enclosures for measurement and control installations.

    Free Quote

    Competitive SABIC VALOX™ PBT+GF 420SEO-BK1066 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ PBT+GF 420SEO-BK1066 is a black-pigmented, 30% glass-fiber-reinforced, flame-retardant polybutylene terephthalate injection molding grade. The product designation identifies the polymer base as polybutylene terephthalate, the reinforcement as discontinuous glass fiber, and the color package as black. Typical supplier datasheet values include density of 1.60 g/cm³ (ISO 1183), tensile stress at break of 120 MPa (ISO 527-1/-2), flexural modulus of 9000 MPa (ISO 178), and heat deflection temperature under 1.8 MPa of 205 °C (ISO 75-2/A). These values are not specification limits; they are typical values measured on molded plaques and may vary with tool design, wall thickness, regrind content, and process conditions. The supplier-documented flammability rating for the 420SEO series is V-0 at 1.5 mm under UL 94.

    Does 30% Glass Fiber Reinforcement Alter the Failure Mode of Flame-Retardant PBT?

    In dry-as-molded components, the glass-fiber network raises tensile stress at break and flexural modulus relative to unfilled flame-retardant PBT. The same reinforcement reduces elongation at break to approximately 2.4% (ISO 527-1/-2); tensile failure therefore occurs through fiber-matrix debonding and brittle fracture rather than the ductile yielding observed in unfilled PBT. Notched Izod impact at 23 °C is typically 8 kJ/m² (ISO 180/A). The notch sensitivity of this grade is higher than that of unfilled PBT because fiber ends act as stress concentrators; this limits the use of sharp internal radii in molded parts. The reinforcement also lowers isotropic mold shrinkage to 0.2–0.4% (ISO 294-4), which supports precision electrical connector production, but anisotropic fiber orientation produces differential shrinkage parallel and perpendicular to flow, and this must be compensated by gate positioning and cooling-channel layout. Creep data for the BK1066 black formulation under high-temperature, load-bearing service are less commonly published; therefore, load-bearing designs at elevated temperatures should be confirmed by application-specific testing under ISO 899-1 or component-level load tests.

    Desiccant Drying and Melt Temperature Control for 420SEO-BK1066

    Because polybutylene terephthalate undergoes hydrolytic chain scission at melt temperature in the presence of moisture, pellets must be dried before processing. The supplier-recommended drying condition is 120 °C for 4 h in a desiccant dryer, with a maximum residual moisture content of 0.02%. Failure to observe this boundary produces silver streaks on the part surface, loss of melt strength, and reduced tensile elongation. Processing barrels are maintained at 250–270 °C, and the mold surface temperature is held at 60–100 °C. Barrel residence time should be limited because melt temperatures above 280 °C accelerate thermal degradation and may increase volatile by-products. The use of a general-purpose injection screw with an 18:1 to 22:1 L/D ratio is common; high-compression screws and high back pressures can fracture glass fiber and reduce impact performance. For hot-runner systems, dead spots and long residence zones should be avoided because black-pigmented material can generate carbonized specks after extended hold periods.

    When Unfilled PBT Is Replaced in Electrical Enclosure Applications

    Replacement of an unfilled flame-retardant PBT with 420SEO-BK1066 changes the design envelope. Wall thickness can often be reduced while retaining a UL 94 V-0 classification at 1.5 mm, although black pigmentation and processing conditions may shift the minimum thickness for a given tool. Creep and thermal distortion performance improve with the glass-fiber network; this is reflected in the 205 °C HDT/A value compared with unfilled PBT grades commonly reported near 60–80 °C. The trade-offs are higher density, higher notch sensitivity, and anisotropic mold shrinkage. The grade is used in electrical enclosures, relay housings, motor end caps, terminal blocks, circuit-breaker components, and solenoid valve bodies. In these applications, the part must often pass needle-flame or glow-wire testing under IEC 60695-2-11 or IEC 60335-1; the documented UL94 rating supports compliance, but end-product testing is required because UL94 is a material flammability classification, not an end-product fire-performance certification.

    Comparative Datasheet Matrix and Test Method Designations

    The following matrix consolidates representative values for 420SEO-BK1066 from supplier-published data. Because color concentrates, regrind, and molding parameters shift measured values, the matrix should not be used as an incoming-product specification without reviewing the current SABIC technical datasheet.

    PropertyTypical valueTest method
    Density1.60 g/cm³ISO 1183
    Glass fiber content30 %Supplier formulation
    Tensile stress at break120 MPaISO 527-1/-2
    Elongation at break2.4 %ISO 527-1/-2
    Flexural modulus9000 MPaISO 178
    Flexural strength175 MPaISO 178
    Notched Izod impact at 23 °C8 kJ/m²ISO 180/A
    Heat deflection temperature at 1.8 MPa205 °CISO 75-2/A
    Mold shrinkage0.2–0.4 %ISO 294-4
    FlammabilityV-0 at 1.5 mmUL 94
    Dielectric strength17 kV/mmIEC 60243-1

    Compared with non-flame-retardant VALOX 420, the 420SEO variant supplies the flammability documentation required by electrical and appliance standards; compared with unfilled flame-retardant PBT, the glass-fiber content increases tensile modulus and heat deflection temperature while reducing elongation and mold shrinkage. The BK1066 black package can influence tracking resistance; the comparative tracking index of pigmented material should be obtained from the current supplier datasheet because carbon black can reduce tracking resistance relative to natural formulations.

    Processing parameterRecommended conditionUnit or criterion
    Predrying temperature120°C
    Predrying time4h
    Residual moisture<0.02%
    Melt temperature250–270°C
    Mold temperature60–100°C
    Hot-runner temperature250–270°C

    On production-scale horizontal injection molding machines, process technicians typically set shot size between 50% and 70% of barrel capacity to limit melt residence time. A melt cushion of 3–5 mm is maintained after hold-pressure transfer. Fiber attrition in the screw plastication zone is a known production bottleneck; excessive screw speed or back pressure can reduce glass-fiber length and lower notched impact strength, even when the pellet remains dry. When regrind is used, addition levels above 20% can increase variance in melt viscosity and fiber-length distribution; for critical electrical components, regrind content should be validated by mechanical testing per ISO 527-1/-2 and ISO 180/A. The material is not intended for continuous hot-water or steam service; hydrolytic stability is inferior to polyphenylene sulfide or high-temperature nylons, and the fiber-matrix interface is susceptible to exposure. Published data for long-term hydrolysis in BK1066 black is limited. The material is also not indicated for medical or food-contact use unless a specific regulatory letter is provided by the supplier. Cleaning between the black grade and light-colored materials on production equipment requires purging with a glass-filled PBT or dedicated purging compound until no visible streaking or speck contamination remains; this is a practical line-conditioning concern when multiple colors are run on one injection press.

    Top