| HS Code | 214095 |
| Productname | SABIC VALOX PBT+GF 420SEO-1001 |
| Polymerbase | PBT |
| Flameretardancy Ul94 | V-0 |
| Melttemperature C | 250-280 |
| Moldtemperature C | 40-80 |
| Volumeresistivity Ohm Cm | 1E15 |
As an accredited SABIC VALOX™ PBT+GF 420SEO-1001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT+GF 420SEO-1001 is supplied in 25 kg moisture-barrier bags, palletized and shrink-wrapped for industrial handling. |
| Container Loading (20′ FCL) | Loaded in a 20-foot FCL container, palletized and secured, with dry conditions maintained for SABIC VALOX™ PBT+GF 420SEO-1001. |
| Shipping | SABIC VALOX™ PBT+GF 420SEO-1001 is supplied as non-hazardous glass-filled PBT resin pellets, typically in moisture-barrier bags, boxes, or bulk containers. Ship under normal freight conditions; keep dry, avoid excessive heat/UV, and follow SDS storage and handling guidance. |
| Storage | Store SABIC VALOX™ PBT+GF 420SEO-1001 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, moisture, and oxidizing agents. Keep containers tightly closed in the original packaging when not in use to prevent contamination and moisture pickup. Avoid prolonged UV exposure, and follow the manufacturer’s SDS for specific temperature, handling, and shelf-life requirements. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored dry, in original sealed packaging, at ambient temperature. |
VALOX™ PBT+GF 420SEO-1001 is used in low-voltage terminal blocks and distribution connectors where UL 94 V-0 flammability at end-use thickness and predictable post-mold shrinkage govern cavity layout. The pellet carries a nominal 20 wt% glass fiber reinforcement; for terminal block production, closed-loop sprue and runner regrind is typically limited to 20 wt% after ignition resistance has been re-verified because fiber length attrition and flame-retardant distribution shift the UL 94 V-0 margin at living hinge and snap-fit sections. Compliance for this segment is assessed against IEC 60947-7-1 for terminal blocks, IEC 60695-2-12 glow wire at 850 °C for unattended current-carrying parts under IEC 60335-1 clause 30.2.3, and IEC 60112 comparative tracking index to support creepage distances under IEC 60664-1. The molding process typically runs on 150–220 t hydraulic or servo-hydraulic injection machines with 8–32 cavity cold runner or hot tip tools; melt temperature is held at 250–265 °C, mold temperature at 80–90 °C, and pre-drying at 120 °C for 3–4 h to a dew-point-derived moisture content below 0.02%. Production experience shows that gate blush and flash at the wire entrance slot appear when hold pressure exceeds 60–70 MPa on thin terminal wings, while insufficient hold below 45 MPa increases sink at the screw boss. The resin enters the cavity with pronounced glass fiber orientation: flow-direction shrinkage is typically 0.3–0.5% and transverse shrinkage 0.7–1.0% when measured under ISO 294-4, requiring asymmetric steel sizing in multi-cavity terminal block tools. Finished component types include 5.08 mm pitch PCB terminal blocks, DIN rail feed-through blocks, panel-mount barrier strips, relay sockets, and distribution block bases.
When a 6–63 A miniature circuit breaker interrupts overload or short-circuit current, the arc chamber and contact carrier are exposed to rapid localized heating and mechanical pressure from gas expansion. 420SEO-1001 is employed in arc side plates, moving contact carriers, and arc barriers because its combustion behavior under UL 94 V-0 at 0.75 mm combines with a nominal 20 wt% glass reinforcement to hold post-mold flatness in walls that define the arc gap. Industry compliance for this application is linked to IEC 60898-1 and UL 489 for device performance, with material-level verification through UL 94 V-0, IEC 60695-2-12 glow wire at 750 °C, and IEC 60243-1 dielectric strength above 18 kV/mm on 2.0 mm plaques. The preferred molding setup uses 80–120 t injection machines with single-cavity or two-cavity tools; screw L/D ratio between 20:1 and 25:1; nozzle melt temperature 255–270 °C; and mold surface temperature 90–100 °C to accelerate crystallization and reduce post-mold warpage in 0.8–1.2 mm walls. Regrind addition is restricted to 10 wt% because arc chamber components require homogeneous flame-retardant distribution; higher recycled content increases the standard deviation of UL 94 V-0 results across shot-to-shot production. Molding rhythm is set by pressure-holding requirements: hold pressure between 50–80 MPa for 4–8 s eliminates vacuum voids at the intersection of the arc splitter retention ribs, with injection velocity staged from 80–120 mm/s at the gate to 30–50 mm/s at the end of fill to prevent jetting and gas entrapment. Terminal finished parts include arc chamber side plates, arc splitter pockets, contact carrier slides, and trip lever linkages integrated into MCB and RCBO devices.
In underhood power distribution boxes, sealed connector housings, and relay and fuse box bases, VALOX™ PBT+GF 420SEO-1001 is selected where the ambient temperature profile remains below 130 °C and adjacent wire insulation does not drive continuous exposure above the PBT heat deflection window. The material’s nominal 20 wt% glass reinforcement provides the dimensional repeatability needed for terminal position assurance clip retention, while the flame-retardant package supports UL 94 V-0 listings at 1.5 mm in engine compartment electrical devices. Compliance testing for this sector follows SAE/USCAR-2 for connector mechanical and environmental performance, ISO 16750-4 for thermal cycle profiles, and IEC 60529 sealing-level verification on assembled connectors. Formulation practice in first-tier molding often combines 85 wt% virgin resin with 15 wt% closed-loop regrind after the reground fraction passes thermal shock testing from -40 °C to 125 °C for 100 cycles and humidity aging at 85 °C/85% RH for 1000 h. Downstream molding occurs on 200–350 t electric injection machines using sequential valve-gated hot runners; fill time is kept between 1.2–1.8 s across 8–16 cavity tools, mold temperature is maintained at 100–110 °C, and pre-drying is set to 120 °C for 3–4 h or until moisture reaches 0.02%. Gate placement must counter anisotropic shrinkage: flow-direction shrinkage of 0.3–0.5% versus transverse shrinkage of 0.7–1.0% under ISO 294-4 can distort pin header openings if cavity steel is not adjusted per gate orientation. Finished components include sealed ECU connectors, fuse and relay box bases, terminal position assurance clips, and wheel speed sensor connector bodies.
AC and DC charging infrastructure inserts 420SEO-1001 into the electrical path as contact carriers, locking latches, inner retainers, and wallbox terminal guards, not as outdoor plug bodies where UV stabilization and hydrolytic resistance dominate selection. The core processing conflict is that the 20 wt% glass reinforcement lowers linear shrinkage but intensifies anisotropic warpage, which shifts contact pin positions and changes plug engagement forces under IEC 62196-2 and UL 2251 mechanical tests. Compliance for charging contact carriers requires IEC 61851-1 for creepage and clearance under pollution degree 3, IEC 60664-1 for insulation coordination, UL 94 V-0 at 1.5 mm, and IEC 60112 comparative tracking index sufficient for the operating voltage class. Because the comparative tracking index is sensitive to flame-retardant decomposition byproducts and fiber-rich surface layers, regrind addition is held to 10 wt% maximum; higher regrind percentages have been observed in production trials to increase CTI variability and to lower the UL 94 V-0 pass margin at the thin latch wall of 0.8 mm.
Molding is typically executed on 250–400 t electric injection machines with 4–8 cavity sequential valve gates. Pre-drying at 120 °C for 3–4 h to 0.02% moisture is mandatory; residual moisture above 0.04% reduces tensile elongation at break under ISO 527-2 and creates gas splay at the contact socket end. The melt profile is held at 255–270 °C, with the hot runner set 5–10 °C lower than the nozzle to minimize residence time degradation of the flame-retardant package. Mold surface temperature is set at 90–110 °C; values below 80 °C produce a dull surface finish and increase post-mold crystallization drift, while values above 120 °C extend cycle time without proportional shrinkage gain. Fill is staged: initial injection at 100–140 mm/s through the gate, followed by 40–60 mm/s packing to prevent overpacking at the thin latch. Hold pressure between 60–90 MPa is maintained for 6–10 s; gate freeze-off time in a 1.0 mm diameter tunnel gate is approximately 7–9 s at these mold temperatures. Post-mold shrinkage measured under ISO 294-4 shows flow-direction values of 0.3–0.5% and transverse values of 0.7–1.0%, requiring separate scaling factors for the pin pitch and latch seat. Finished parts include Type 2 AC connector inner carriers, DC fast-charge contact retainers, latch pawls, wallbox terminal guards, and charging inlet rear housings.
| Sector | Primary material-level compliance standards | Typical end-use thickness |
|---|---|---|
| Terminal blocks and distribution connectors | UL 94 V-0, IEC 60695-2-12, IEC 60947-7-1, IEC 60112 | 0.75–1.5 mm |
| Miniature circuit breaker arc chambers | UL 94 V-0, IEC 60695-2-12, IEC 60898-1, IEC 60243-1 | 0.75–2.0 mm |
| Underhood connectors and relay boxes | UL 94 V-0, SAE/USCAR-2, ISO 16750-4, IEC 60529 | 1.5 mm |
| EV charging contact carriers and retainers | UL 94 V-0, IEC 62196-2, UL 2251, IEC 61851-1, IEC 60664-1 | 0.8–1.5 mm |
| Motor insulation components | UL 1446, IEC 61857-1, IEC 60335-1, IEC 60243-1 | 0.8–2.0 mm |
| Appliance switches and controls | UL 94 V-0, IEC 61058-1, IEC 60730-1, IEC 60335-1 | 0.75–1.5 mm |
The incorporation of 420SEO-1001 into small motor electrical insulation is constrained less by melt flow than by the thermal aging condition in the resin-rich zones adjacent to coil windings. A nominal glass fiber content of 20 wt% is present in the pellet; in bobbin and end cap molding, regrind content is typically limited to 15 wt% after insulation resistance testing under IEC 62631-3-1 at 500 V DC and dielectric breakdown testing under IEC 60243-1 remain within specified limits. Material compliance is evaluated as part of an insulation system recognized under UL 1446, with component-level tests following IEC 61857-1 and IEC 60335-1 for motorized appliance applications. The process involves insert molding around copper coil forms and steel bearing sleeves, which demands low residual stress: melt temperature is kept at 250–265 °C, mold temperature at 80–100 °C, and fill speed is limited to 30–60 mm/s at the insert wall to avoid displacing fine magnet wire. Production equipment is normally a 120–200 t hydraulic injection machine with vertical clamp for insert-loaded tools or a shuttle tool. Gate placement on the end cap rim, not on the hub, reduces knit lines at the bearing bore; knit line strength is measured under ISO 527-2 tensile testing at 5 mm/min, with acceptance typically requiring retention of at least 60% of the unfilled knit line value. Terminal finished parts include class B insulated end caps, coil bobbins, brush card holders, terminal boards, and commutator support rings.
Within appliance power controls and electromechanical switch housings, VALOX™ PBT+GF 420SEO-1001 replaces unfilled flame-retardant PBT where rocker switch bodies, rotary switch bases, and power selector knobs require higher creep resistance under contact spring load. The material carries 20 wt% glass reinforcement; switch manufacturers often add 20 wt% closed-loop regrind for non-load-bearing housing walls, but safety-related barriers and actuator frames remain virgin or use a 10 wt% regrind limit to preserve UL 94 V-0 at 0.75 mm. Compliance is evaluated under IEC 61058-1 for switches, IEC 60730-1 for automatic electrical controls, and IEC 60335-1 for household appliance end use. Molding is performed on 80–150 t injection machines with 8–24 cavity tools; melt temperature is set at 250–265 °C, mold temperature at 60–80 °C to shorten cycle time, and hold pressure at 40–60 MPa to prevent sink at screw bosses. Finished parts include rocker switch housings, rotary switch bases, power selector knobs, control panel brackets, and interlock strike plates.
Competitive SABIC VALOX™ PBT+GF 420SEO-1001 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT+GF 420SEO-1001 is a 20% glass-fiber-reinforced polybutylene terephthalate injection molding grade in which the SEO designation identifies a self-extinguishing formulation. The product is specified for electrical and electronic component manufacturing where a UL 94 V-0 rating is required at 0.75 mm wall thickness. Representative datasheet values place the density at 1.61 g/cm³ (ISO 1183) and the tensile stress at break at 95 MPa (ISO 527-2/5). The compound is supplied as pellets and must be dried in a closed-loop desiccant dryer before melt processing.
The 20% glass fiber content raises the flexural modulus to approximately 6000 MPa (ISO 178) relative to an unreinforced flame-retardant PBT such as VALOX 310SE0, where the modulus is approximately 2500 MPa. The same fiber loading reduces tensile strain at break to 2.5% (ISO 527-2/5) and produces a notched Charpy impact value near 4 kJ/m² (ISO 179-1/1eA). The heat deflection temperature under 1.8 MPa load is reported near 203°C (ISO 75-2/Af). The flame-retardant system shifts the vertical burn classification to V-0 at 0.75 mm; however, the same system raises melt viscosity relative to a non-flame-retardant 20% glass-filled PBT and narrows the permissible barrel-temperature window.
| Property | Standard | Representative value |
|---|---|---|
| Density | ISO 1183 | 1.61 g/cm³ |
| Tensile stress at break | ISO 527-2/5 | 95 MPa |
| Tensile strain at break | ISO 527-2/5 | 2.5% |
| Flexural strength | ISO 178 | 145 MPa |
| Flexural modulus | ISO 178 | 6000 MPa |
| Charpy notched impact, 23°C | ISO 179-1/1eA | 4 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2/Af | 203°C |
| Flammability rating | UL 94 | V-0 at 0.75 mm |
| Comparative tracking index | IEC 60112 | 250 V |
| Dielectric strength | IEC 60243-1 | 15 kV/mm |
| Volume resistivity | IEC 60093 | 1.0×10¹⁵ Ω·cm |
| Water absorption, 24 h | ISO 62 | <0.1% |
Data in the table are representative values reported for natural-grade material at 23°C and 50% relative humidity after conditioning to ISO 291. They are not specification limits; lot-to-lot variance and colorant effects can shift the values. The -1001 suffix is an internal product variant identifier. Published data for the -1001 suffix as a distinctly characterized grade are limited beyond the base VALOX 420SEO datasheet.
Pre-drying is the first processing constraint. PBT undergoes hydrolytic degradation at melt temperatures above 250°C when residual moisture exceeds 0.02% by mass. A desiccant dryer set to 120°C with a dew point of -30°C or lower for 3–4 h is standard preparation. Dried pellets exposed to ambient air at relative humidity above 60% should be reprocessed within 2 h or returned to the dryer. Production-scale compounding of glass-filled PBT typically uses co-rotating twin-screw extruders with L/D 40:1, downstream fiber feeding, and vacuum venting to preserve fiber length and remove volatiles. Published data for the -1001 variant under specific compounding configurations are limited.
Rear barrel zones are set between 240°C and 255°C, middle zones between 255°C and 270°C, and the nozzle between 255°C and 270°C. The melt temperature at the nozzle should not exceed 275°C. Holding molten material above 275°C or allowing residence time beyond 5 min can decompose the flame-retardant system, visible as black specks in molded parts and measurable as a reduction in tensile stress at break. Mold temperature is maintained between 60°C and 95°C. Below 60°C, rapid crystallization reduces knit-line strength; above 95°C, cycle time increases without a corresponding gain in heat deflection performance. A screw back pressure of 0.3–0.7 MPa and a screw speed of 30–80 rpm are typical for glass-filled PBT compounds. Hydraulic injection pressures of 80–120 MPa are common for connector geometries with wall thickness from 0.8 mm to 2.5 mm. The screw should have a low compression ratio of 2.0:1 to 2.5:1, and the barrel and screw flights should be hardened or bimetallic because 20% glass fiber is abrasive.
Mold filling is shear-sensitive. At wall thickness below 0.8 mm, the glass-fiber network increases apparent melt viscosity and can produce short shots if gate diameters are below 0.8 mm or if flow length exceeds 150 mm from the gate. Submarine and tunnel gates should be sized at 60–70% of the nominal wall thickness for glass-filled PBT. Vent depth should not exceed 0.02 mm to prevent flash while allowing air evacuation; inadequate venting produces burn marks and blackened flow fronts that compromise the UL 94 rating on molded parts. Shrinkage is anisotropic. In glass-filled PBT grades, flow-direction mold shrinkage is typically lower than cross-flow shrinkage because fibers align along the melt-flow direction. Tool designers should apply supplier shrinkage data specific to the color and wall thickness rather than generic unfilled-PBT values; published data for the -1001 suffix across all colors are limited.
Connector housings, relay bases, and switch bodies are processed from this grade because the UL 94 V-0 classification at 0.75 mm and the comparative tracking index of 250 V (IEC 60112) reduce ignition and tracking failure risk in live-part separation. The volume resistivity of approximately 1.0×10¹⁵ Ω·cm (IEC 60093) and dielectric strength near 15 kV/mm (IEC 60243-1) provide predictable electrical isolation in dry indoor service. The PBT matrix limits 24 h water absorption to less than 0.1% (ISO 62), which preserves dimensional stability in humid assembly environments. Because the notched Charpy value is near 4 kJ/m², parts must be designed with wall-to-rib transitions of at least 0.5:1 and radiused corners; sharp steps create stress concentrations that can produce brittle field failures.
Compared with VALOX 420, a 20% glass-filled PBT without the SEO flame-retardant system, 420SEO-1001 trades a minor reduction in flow length and tensile elongation for the UL 94 V-0 classification. The non-flame-retardant grade typically exhibits a lower melt pressure during filling and a wider barrel-temperature window. Against VALOX 310SE0, an unreinforced flame-retardant PBT, 420SEO-1001 raises flexural modulus from approximately 2500 MPa to 6000 MPa and heat deflection temperature by roughly 30°C, but lowers notched impact and increases directionally dependent shrinkage. Against VALOX 430SE0, a 30% glass-filled flame-retardant PBT, 420SEO-1001 reduces glass content, lowering density, transverse warpage, tool wear, and melt viscosity. The trade-off is a lower flexural modulus and lower heat deflection temperature than the 30% grade. These comparisons are derived from published supplier datasheets and should be re-verified for the specific color and lot.
Regulatory compliance cannot be assumed from the base polymer alone. The flame-retardant system may contain halogenated organic components. The material must be checked against RoHS 2011/65/EU Annex II restrictions and any customer-specific low-halogen specification. The supplier’s certification for the exact 420SEO-1001 compound and color is the authoritative document. The REACH 1907/2006 Article 33 communication requirement applies to substances of very high concern above 0.1% w/w. The grade is not intended for food-contact or medical-device applications; no FDA 21 CFR compliance statement is implied by the standard electrical-grade datasheet.
| Domain | Standard or regulation | Typical status |
|---|---|---|
| Flammability | UL 94 | V-0 at 0.75 mm |
| Electrical tracking | IEC 60112 | 250 V |
| Dielectric strength | IEC 60243-1 | 15 kV/mm |
| Long-term thermal index | UL 746B | Consult current UL Yellow Card |
| EU restriction of hazardous substances | RoHS 2011/65/EU | Requires current supplier certification |
| EU chemical registration | REACH 1907/2006 | Requires current supplier certification |
In high-humidity electrical applications, the comparative tracking index of 250 V (IEC 60112) and low water absorption limit surface leakage current. However, the material is not corona-resistant; partial discharge in inverter-driven motor windings can degrade the organic matrix. For components exposed to voltage spikes above 1 kV, terminal-to-terminal creepage distance should be evaluated under IEC 60664-1. The flame-retardant system operates through vapor-phase and condensed-phase mechanisms during combustion. The UL 94 V-0 rating is thickness-dependent: at wall thickness below 0.75 mm, the reduced char structure and higher surface-to-volume ratio can lead to a downgrade to V-1 or V-2. Therefore, 0.75 mm is a critical dimensional threshold, not a conservative guideline.
Operational boundaries include a restriction on regrind fractions above 20% by mass unless end-use mechanical testing confirms otherwise. Re-drying of regrind is mandatory. The grade is not recommended for continuous immersion in hot water above 60°C because hydrolytic attack on the PBT matrix accelerates with temperature and becomes a failure mode in pressure-bearing or snap-fit components. Nitrogen-containing organic additives, especially amine-based colorants and lubricants, can interfere with the flame-retardant decomposition chemistry; any such additive must be evaluated by UL 94 testing on the final part geometry. Long-term thermal aging performance is governed by UL 746B; the current UL Yellow Card should be consulted before specifying the grade in outdoor or load-bearing electrical enclosures.
Motor end caps and coil bobbins represent a second application envelope. The grade provides the stiffness required to hold wound copper assemblies under torsion. The heat deflection temperature of 203°C at 1.8 MPa permits short-term exposure to varnish curing cycles, but the maximum continuous use temperature must be confirmed against UL 746B data specific to the end-use wall thickness. Published data for the -1001 suffix in continuous-use motor environments is limited.