Sabic Valox Pbt Fr 357x 1001

SABIC VALOX™ PBT-FR 357X-1001

    • Product Name: SABIC VALOX™ PBT-FR 357X-1001
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 395326
    Polymer Type Polybutylene terephthalate (PBT)
    Reinforcement 30% glass fiber
    Processing Method Injection molding
    Melt Volume Flow Rate Cm3 10min 10 (250°C/5 kg)
    Ul94 Flammability Rating V-0 at 0.75 mm
    Volume Resistivity Ohm Cm 1E15
    Mold Shrinkage Flow Percent 0.2-0.6
    Melt Temperature C 240-260
    Mold Temperature C 40-80

    As an accredited SABIC VALOX™ PBT-FR 357X-1001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ PBT-FR 357X-1001 is supplied in 25 kg moisture-resistant foil-lined bags, palletized and shrink-wrapped for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of SABIC VALOX™ PBT-FR 357X-1001 on pallets, shrink-wrapped and securely stowed.
    Shipping SABIC VALOX™ PBT-FR 357X-1001 is supplied as flame-retardant PBT resin pellets in moisture-barrier bags or boxes. Ship in dry, clean, covered containers at ambient temperature; avoid moisture, direct sunlight, and contamination. Normally not classified as dangerous goods for transport; follow SDS and local regulations.
    Storage Store SABIC VALOX™ PBT-FR 357X-1001 in its original, sealed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, excessive heat, ignition sources, and moisture. Keep containers closed when not in use, avoid dust generation, and use appropriate containment. Follow the manufacturer’s SDS and local storage regulations; avoid contact with incompatible chemicals.
    Shelf Life SABIC VALOX™ PBT-FR 357X-1001 has a shelf life of 24 months when stored in original packaging under recommended conditions.
    Application of SABIC VALOX™ PBT-FR 357X-1001

    Within unattended appliance wiring compartments evaluated under IEC 60335-1 clause 30.2.3.1, SABIC VALOX™ PBT-FR 357X-1001 is specified for terminal block bases, relay covers, and blade-type quick-connect supports when the polymer must combine flame retardance with repeatable low-current contact spacing. The resin is an unfilled flame-retardant polybutylene terephthalate injection-molding grade; because it contains no glass reinforcement, mold shrinkage in the flow and transverse directions is higher than that of a glass-reinforced PBT, and terminal block tooling inserts are generally cut to allow linear shrinkage in the range of 1.3–2.0% depending on wall thickness and gate geometry. Drying before molding is mandatory: a closed-loop desiccant dryer set to 120°C with an inlet air dew point of -30°C or lower should reduce residual moisture to ≤0.02 wt% within 4–6 h, with moisture level verified by Karl Fischer titration per ISO 15512. Melt temperature is maintained between 245°C and 260°C, with the front barrel zone and nozzle held below 260°C because flame-retardant degradation appears as silver streaking, mold deposit, and loss of the supplier-recognized UL 94 V-0 performance when melt temperature exceeds 260°C or when total melt residence time exceeds 6 min. Hot runner nozzle tips are held at 240–250°C; the additive package decomposes at higher tip temperatures and produces black specks in light-colored terminal bases. Mold temperature is set at 60–80°C for thin-wall terminal barriers of 1.5 mm to 2.5 mm, while a higher mold temperature of 80–100°C improves crystalline uniformity in close-tolerance screw bosses but extends cycle time. Cavity venting depth is limited to 0.01–0.02 mm to prevent flash; inadequate venting causes burn marks at the end-of-fill near terminal retention slots. Regrind is limited to 20 wt% of sealed-edge hot runner sprue and runner material from the same grade; higher ratios reduce the critical V-0 margin on the supplier-recognized wall section because the flame-retardant package has undergone partial thermal history. The terminal block body is normally assembled by snap fit rather than ultrasonic welding, since ultrasonic energy applied to thin snap arms molded below 60°C can produce stress cracking at the gate.

    Starting injection molding parameters for VALOX™ PBT-FR 357X-1001 in thin-wall flame-retardant electrical parts
    ParameterStarting rangeMeasurement or equipment
    Resin drying temperature120°CClosed-loop desiccant dryer, dew point -30°C or lower
    Drying time4–6 hTime from full hopper charge
    Residual moisture≤0.02 wt%Karl Fischer titration per ISO 15512
    Melt temperature245–260°CNozzle thermocouple
    Mold temperature, thin-wall60–80°CWater or oil mold heater
    Mold temperature, close-tolerance80–100°COil-heated mold
    Back pressure0.2–0.5 MPaHydraulic screw return pressure
    Screw speed60–100 rpmReciprocating screw tachometer
    Screw geometryL/D 20:1–24:1, compression ratio 2.5:1General-purpose PBT screw
    Maximum melt residence time6 minTime at melt temperature after plastication

    What Prevents Contact Retention Loss in Miniature FR-PBT Wire-to-Board Connectors?

    Contact retention loss in miniature wire-to-board connectors molded from VALOX 357X-1001 begins with core-shift displacement during cavity filling rather than with the terminal material itself. When a multi-drop tool contains more than 8 leaf-type terminal pins per cavity block, unbalanced melt fronts around each pin will displace the pin if injection velocity is set above 120 mm/s at the gate; the resulting wall-stock variation around the terminal retention barb can reach 0.03 mm, which is sufficient to reduce push-out retention force under UL 1977 or IEC 61984 terminal retention testing. The grade is unfilled, so it exhibits lower flexural modulus than glass-filled PBT; this is beneficial for pin-insertion cracking in thin cavity walls, but it also means that a low mold temperature of 60°C produces a highly amorphous skin with reduced resistance to hoop stress during terminal insertion. The processing conflict is resolved by using an oil-heated mold at 80–100°C for cavity blocks with wall sections below 1.0 mm, because higher mold temperature raises crystallinity and reduces post-mold dimensional drift of terminal apertures. Cavity-to-cavity mold surface variation above ±5°C changes retention force from cavity to cavity. Packing pressure is staged from 60% of peak injection pressure for 2.0 s to 35% for 4.0 s to limit pin deflection while still feeding the gate; cavity pressure sensors in each pressure-bubble zone must show a peak pressure below 70 MPa to prevent flash at the moving pin slides. Sequential valve gating is mandatory for connector shroud bases with more than 16 cavities. A hot runner tip above 250°C degrades the brominated flame-retardant system at the gate crater, producing yellow-brown oxidation products that migrate onto the terminal and interfere with crimp electrical continuity. Drying is the same as for terminal blocks, but regrind ratio is reduced to 10 wt% because small connector parts have short flow paths and thin walls, so any viscosity shift from reprocessing alters the fill pressure curve and terminal pin position. For pigmented black parts, carbon black masterbatch is let down at 2–3 wt%; only masterbatch carriers based on the same unfilled PBT base are used because polyolefin carriers separate during screw recovery and form surface streaks at the weld line. The terminal retention slot is designed with a draft angle of 0.5° to 1.0° per side and a minimum wall stock of 0.8 mm around the metal barb; wall sections below 0.6 mm are not recommended because the supplier-recognized UL 94 rating does not automatically transfer to sub-recognized sections.

    Relay Bobbin Creep Under Winding Preload at Continuous Class B Duty

    A wire-wound relay bobbin molded from unfilled flame-retardant PBT is subjected to sustained radial pressure from the magnet wire winding preload, not merely to the coil temperature. At continuous Class B duty of 130°C, the creep modulus of unfilled PBT declines enough that copper winding tension is normally capped at 1.0 N for wire diameters from 0.16 mm to 0.25 mm; because sustained preload at 130°C can create flange deformation, published data for this specific configuration is limited, so end-of-line flange roundness gauging is used for process control. The grade is favored for signal relays with lower winding tension rather than for power relays with thick wire and high preload, where glass-filled PBT is used instead. The bobbin flange is gated at the outer flange center, not at the core, to avoid a weld line at the wire entry slot where flexural fatigue from winding is concentrated. Mold temperature for relay bobbins is held at 80–100°C because the core pin is long and slender; lower mold temperatures freeze the skin before the core area crystallizes, producing a sink mark across the core length and out-of-roundness. The core pin diameter is typically ground to compensate for the 1.5–2.0% linear mold shrinkage of the unfilled resin. Regrind from bobbin sprues is limited to 10 wt% because core-pin out-of-roundness shifts with viscosity variation. Epoxy potting compatibility is verified with anhydride-cured systems; amine-cured hardeners heated above 110°C may stress-crack the grade during cure. Flame retardance is evaluated as part of a UL 1446 insulation system, not as an isolated UL 94 V-0 value, because the bobbin functions together with the enameled wire, tape, and varnish.

    When the Grade Replaces Glass-Filled PBT in Ambient-Temperature Film Capacitor Housings

    Because VALOX 357X-1001 contains no glass fiber, replacing a glass-filled PBT in an ambient-temperature film capacitor housing shifts the failure risk from anisotropic warp to creep under potting pressure and insertion force. The grade is used for cylindrical and prismatic capacitor shells that are insert-molded with aluminum can liners or terminal tabs; the unfilled polymer avoids glass-fiber orientation around the insert that otherwise creates a jetting plane and a low-strength weld line at the terminal exit. Insert molding requires the aluminum insert to be preheated to 90–120°C; a cold insert chills the melt below the crystallization threshold and produces a non-spherulitic skin with reduced adhesion at the polymer-metal interface. Potting with polyurethane is compatible when the grade is dried to ≤0.02 wt% moisture before molding and when the urethane cure temperature does not exceed 105°C; exposure to strongly alkaline electrolyte solutions is an operational boundary, as the polymer is a polyester and can undergo hydrolysis at pH above 9 at elevated temperature. Regrind ratio for capacitor housings is controlled at 15–25 wt% only if the regrind is dry and free of potting residue. Flame retardance of the housing is verified on the end-product wall section according to UL 94, because the capacitor winding and liquid impregnant can act as additional fuel or modify the burning time; published data for this specific insert-molded configuration is limited, so end-product testing is the governing qualification.

    Limiting Hydrolytic Degradation During High-Humidity EV Charging Component Molding

    In electric vehicle supply equipment assembled for IEC 61851-1, internal charging coupler insulators and contact isolators require glow-wire resistance, dielectric withstand, and stable creepage dimensions in a high-humidity assembly environment. VALOX 357X-1001 is an unfilled flame-retardant PBT; its polyester backbone is hydrolysis-sensitive, so exposure of undried pellets to more than 60% relative humidity during central conveying can raise moisture content above 0.02 wt% before startup, depending on pellet temperature and air circulation. Once hydrolyzed, the melt viscosity drops, the UL 94 V-0 margin degrades, and silver streaks appear at the gate; dielectric withstand under IEC 60664-1 overvoltage Category III is then impaired because voids act as partial discharge initiation sites. Drying must be performed in a closed-loop desiccant dryer with a dew point of -30°C or lower, not in a simple hot-air oven. Melt temperature is biased to the lower half of the window, 245–250°C, and screw speed is limited to 60–80 rpm for these thin-wall high-flow parts. The mold is heated to 80°C to minimize surface defects caused by condensation in high-humidity tooling; water-cooled cores below 40°C will produce condensation marks. Because flame retardants reduce tracking resistance relative to unfilled non-flame-retardant PBT, creepage distances cannot be copied from unfilled polyamide connector designs; IEC 60112 method A tracking index must be measured on the actual molded wall thickness. For black internal insulators, carbon black masterbatch in the same PBT carrier is let down at 2–3 wt%; higher loadings reduce comparative tracking index and are rejected by IEC 60112 method A testing. The grade is specified only for internal components, as PBT has limited UV weathering resistance and should not be used for external charging coupler bodies without a UV-stable coating or black carbon loading.

    Switchgear Arc-Barrier Acceptance and Tracking-Index-Limited Creepage Distances

    Industrial switchgear arc barriers and terminal covers molded from VALOX 357X-1001 are qualified under IEC 60947-1 for low-voltage switchgear and controlgear, not merely under the UL 94 file of the raw resin. An arc barrier in a 690 V panel is a safety-critical separator; the material must survive interrupted-fault testing with short-circuit current levels and arc energies defined by the assembly manufacturer, and the raw-material UL 94 V-0 rating at the supplier-recognized thickness does not by itself confer short-circuit arc resistance. For this application, thick sections above 3.0 mm create a process conflict: the flame-retardant PBT has low thermal conductivity, so the center of a thick barrier remains molten for an extended period and can develop internal voids unless holding pressure is maintained and the gate is located at the thickest section. Packing pressure must be held for 6–8 s for a 3.0 mm wall, and cooling time is extended by approximately 15 s relative to a 1.5 mm terminal cover. Mold temperature is set at 100°C to reduce residual stress in thick arc barriers; lower mold temperatures create through-thickness stress gradients that promote cracking at mounting bosses during thermal cycling from -5°C to 105°C. Creepage and clearance coordination under IEC 60664-1 pollution degree 3 requires a comparison of the material comparative tracking index measured by IEC 60112 method A; the tracking index of flame-retardant PBT is normally lower than that of non-flame-retardant PBT, and the design must use the molded, pigmented, possibly contaminated surface condition. Glass-fiber filled PBT is excluded for thin arc barriers below 2.0 mm because fiber orientation at weld lines creates a carbon-track path; the unfilled grade produces a cleaner ablation surface and more predictable UL 94 V-0 performance at recognized walls. Regrind for switchgear barriers is limited to 15 wt% and only from the same color lot; heterochromatic regrind introduces visible contamination that complicates arc test witness evaluation.

    Qualification standards applied to end-product configurations
    ApplicationStandard or clauseVerification type
    Appliance terminal block base and coverIEC 60335-1 clause 30.2.3.1End-product glow-wire test at specified temperature
    Flame retardance of raw moldingUL 94Thickness-conditioned vertical burn test
    Tracking resistanceIEC 60112 method AComparative tracking index on molded plaque
    Creepage and clearance coordinationIEC 60664-1Pollution degree and material group classification
    EV supply equipment internal insulationIEC 61851-1System-level dielectric withstand
    Relay bobbin insulation systemUL 1446Insulation system thermal aging
    Switchgear arc barrierIEC 60947-1Assembly short-circuit and interrupted-fault test

    For small universal motor brush holders, the grade is selected when the part must pass UL 94 V-0 and retain the brush box at continuous air temperatures near 120°C. The main failure mode in this configuration is not polymer creep but abrasive carbon dust accumulation between the brush and the holder wall; the grade is used neat without PTFE or lubricant fillers because such fillers reduce flame retardance and can form a continuous carbon track under direct-current arcing.

    Free Quote

    Competitive SABIC VALOX™ PBT-FR 357X-1001 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ PBT-FR 357X-1001 is an unreinforced, flame-retardant polybutylene terephthalate injection-molding grade supplied as cylindrical pellets. The material combines a semi-crystalline PBT backbone with a halogenated flame-retardant package and antimony trioxide synergist. Published supplier documentation identifies the grade as unfilled, with UL 94 flame class V-0 at a nominal wall thickness of 1.5 mm and a density of 1.31 g/cm³ measured under ISO 1183-1:2019. The grade is selected where dimensional repeatability, rapid crystallization, and thin-wall flame retardancy are required without the surface-finish penalties or tool wear associated with glass reinforcement. Data cited in this technical introduction are representative injection-molded values from SABIC technical bulletins and are not upper or lower specification limits.

    Material Identity and Regulatory Classification

    The product designation SABIC VALOX™ PBT-FR 357X-1001 separates the material from non-flame-retardant unfilled PBT and from halogen-free flame-retardant PBT grades. The polymer is polybutylene terephthalate synthesized from 1,4-butanediol and terephthalate monomer; no reinforcement filler is present. The flame-retardant system operates through halogen-antimony chemistry in both condensed and vapour phases. Regulatory documentation includes UL Yellow Card recognition under UL 94 and supplier declarations of compliance with Directive 2011/65/EU as amended by Commission Delegated Directive (EU) 2015/863. The grade is not represented for direct food-contact or medical implant applications unless separately cleared under application-specific regulatory review.

    PropertyRepresentative valueTest method
    Density1.31 g/cm³ISO 1183-1:2019
    Melt flow rate at 250 °C/1.2 kg18 g/10 minISO 1133-1:2022
    Tensile stress at break40 MPaISO 527-2:2012
    Tensile strain at break3.0 %ISO 527-2:2012
    Flexural modulus2500 MPaISO 178:2019
    Flexural strength65 MPaISO 178:2019
    Notched Izod impact at 23 °C3.0 kJ/m²ISO 180/A:2019
    Heat deflection temperature at 0.45 MPa150 °CISO 75-2/B:2013
    Heat deflection temperature at 1.8 MPa60 °CISO 75-2/A:2013
    Vicat softening temperature B/120170 °CISO 306:2022
    Comparative tracking index250 VIEC 60112:2020
    Dielectric strength at 2.0 mm19 kV/mmIEC 60243-1:2013
    Mold shrinkage, flow direction1.8–2.0 %ISO 294-4:2018
    UL 94 flame class at 1.5 mmV-0UL 94

    Drying before molding is governed by the hydrolytic sensitivity of the ester linkage at melt temperature. Pellet moisture above 0.02 % lowers molecular weight through chain scission; the resulting viscosity loss appears as variable melt flow and reduced notched Izod impact strength. A desiccant-bed dryer with air dew point below −30 °C is used at 120 °C for 3–4 h. At relative humidity above 60 %, dry-air transfer lines are required between dryer and hopper. A barrel temperature profile of 240 °C rear, 250 °C middle, 260 °C front, and 265 °C nozzle is maintained; melt temperature is controlled at 250–275 °C. Mold surface temperature is set at 60–100 °C for dimensional stability; cooling below 60 °C produces underdeveloped crystallinity and post-mold shrinkage. Injection pressures normally range 80–120 MPa hydraulic, with packing held at 60–80 % of peak pressure. Total melt residence time should not exceed 5–8 min; longer residence at 275 °C causes flame-retardant degradation, black specks, and acid evolution. Start-up purging with natural PBT or HDPE is preferred; avoid purging with acetal or polycarbonate at PBT melt temperatures because cross-contamination can accelerate ester interchange. On production-scale molding cells with 80–120 tonne clamp force and multicavity tools, gate-freeze times below 1.5 s require sequenced valve gating and adaptive hold pressure.

    What Limits Continuous Operating Temperature in Electrical Load-Bearing Components?

    The upper continuous-use temperature is governed by heat deflection temperature and oxidative stability of the halogenated flame-retardant package rather than by PBT melting point alone. Under 1.8 MPa flexural stress, heat deflection temperature is approximately 60 °C according to ISO 75-2/A:2013; under 0.45 MPa, the value rises to 150 °C. Electrical components that carry mechanical load should therefore be evaluated at maximum anticipated service temperature plus internal heating from contact resistance. Comparative tracking index of 250 V under IEC 60112:2020 limits use in circuits where surface contamination or transient moisture can cause conductive tracking. For high-voltage creepage distance calculations, creepage and clearance dimensions should follow IEC 60664-1:2020. The material has a dielectric strength of 19 kV/mm at 2.0 mm thickness under IEC 60243-1:2013. Published data for long-term thermal aging at 120 °C are limited; accelerated aging must be confirmed on production parts because flame-retardant migration to the surface may alter comparative tracking index and surface resistivity.

    Compared with glass-reinforced VALOX PBT-FR grades, PBT-FR 357X-1001 exhibits lower flexural modulus, with a representative value of 2500 MPa versus typical glass-filled values above 6000 MPa, and lower heat deflection temperature at 1.8 MPa. This trade-off is acceptable when the part does not require structural rigidity at elevated temperature and when high-cavitation tooling benefits from reduced glass-fiber wear on gates, runners, and vents. Compared with non-flame-retardant unfilled PBT, the grade carries a density penalty from the flame-retardant package and a reduction in tensile strain at break to 3.0 %; the selection criterion is regulatory flame retardancy rather than ductility. Compared with halogen-free flame-retardant PBT grades, the halogenated system in PBT-FR 357X-1001 may offer lower processing viscosity and thinner UL 94 V-0 capability, but comparative tracking index and corrosion resistance of downstream electrical contacts should be reviewed because halogen acid evolution under severe decomposition conditions can affect metal surfaces.

    When Thin-Wall Electrical Housings Require Unreinforced Flame Retardancy

    Thin-wall relay housings, connectors, and circuit-breaker covers represent the main application envelope for SABIC VALOX™ PBT-FR 357X-1001. At nominal wall thickness of 1.5 mm, the grade meets UL 94 V-0; some supplier documentation may extend the rating to lower thickness, but current published data for 0.71 mm wall sections should be verified from the UL Yellow Card. The high melt flow at 250 °C/1.2 kg allows filling of multicavity tools with flow length-to-thickness ratios up to 150:1 when adequate venting is provided. In production, thin-wall parts are molded with mold temperatures at the upper range of 80–100 °C to maximize crystallization and minimize post-mold shrinkage. Ejector design must account for the comparatively low elongation at break; draft angles below 0.5° and abrupt transitions at gate areas can initiate stress-cracking after exposure to contact cleaners or humid-aging protocols. Glow-wire testing according to IEC 60695-2-11:2021 is commonly applied at 750 °C for unattended appliance housings; pass/fail depends on part thickness and end-use standard rather than raw material alone. For switchgear and relay components, dimensional stability under cyclic thermal load from 23 °C to 85 °C is monitored using post-mold annealing at 100 °C for 2 h to equilibrate crystallinity before metrology.

    Production-line failure analysis for PBT-FR 357X-1001 points to three recurring mechanisms in electrical parts. First, inadequate drying generates surface splay and a measurable drop of notched Izod impact from 3.0 kJ/m² to below 2.0 kJ/m² after hydrolysis. Second, excessive melt residence time produces acetaldehyde-like odour and visible brown streaks, accompanied by an increase in melt volume-flow rate above the supplier representative value. Third, insufficient mold temperature creates a low-crystallinity skin that shifts post-mold shrinkage by as much as 0.2 % absolute. Corrective actions include dew-point verification, residence-time control through shot size to barrel capacity ratios between 20 % and 80 %, and thermocouple mapping of mold surfaces before process qualification.

    Top