| HS Code | 572667 |
| Density | 1.58 g/cm³ |
| Tensile Modulus | 11000 MPa |
| Tensile Stress At Break | 120 MPa |
| Tensile Strain At Break | 2.0 % |
| Flexural Modulus | 10000 MPa |
| Flexural Strength | 180 MPa |
| Charpy Notched Impact Strength 23 C | 8 kJ/m² |
| Charpy Unnotched Impact Strength 23 C | 40 kJ/m² |
| Hdt At 1 8 Mpa | 200 °C |
| Hdt At 0 45 Mpa | 210 °C |
| Vicat Softening Temperature | 210 °C |
| Ul94 Flammability Rating | V-0 at 0.75 mm |
| Coefficient Of Linear Thermal Expansion | 2.5E-5 /°C |
| Dielectric Strength | 20 kV/mm |
| Volume Resistivity | >1E15 ohm·cm |
| Water Absorption | 0.1 % |
| Mold Shrinkage | 0.2-0.5 % |
As an accredited SABIC VALOX™ PBT-FR 357-1001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT-FR 357-1001 is supplied in 25 kg sealed moisture-barrier bags, palletized at 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loaded with SABIC VALOX™ PBT-FR 357-1001 in original sealed bags on pallets, dry container, ambient, secured for transport. |
| Shipping | SABIC VALOX™ PBT-FR 357-1001 is a flame-retardant polybutylene terephthalate resin supplied as pellets. For transport, it is normally non-hazardous and not regulated as dangerous goods. Ship in dry, sealed packaging (bags/octabins) at ambient temperature, avoiding moisture, heat, and contamination. |
| Storage | Store SABIC VALOX™ PBT-FR 357-1001 indoors in a cool, dry, well-ventilated warehouse, preferably below 40°C, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers sealed and palletized to prevent moisture pickup, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures; do not stack excessively, rotate stock, and follow the SDS and local regulations. |
| Shelf Life | SABIC VALOX™ PBT-FR 357-1001 has a shelf life of two years when stored dry, cool, and in original unopened packaging. |
Inside a 160 A DIN-rail terminal block carrier, the insulating body is molded from an unfilled flame-retardant polybutylene terephthalate because the part must retain steel screw inserts, maintain creepage distances under IEC 60947-7-1, and pass a UL 94 V-0 flame rating at a wall thickness of 0.71 mm without the warpage penalty of a glass-filled alternative. The material is dried to a residual moisture content below 0.02 wt% in a desiccant dryer with a dew point of −30 °C, typically at 110 °C for 4 h; moisture above 0.04 wt% at the hopper causes hydrolysis during plastication, measurable as a drop in tensile elongation at break according to ISO 527-2 and as an increase in variance across a 12-cavity production tool. Melt preparation on a general-purpose injection unit with screw L/D 20:1 and compression ratio 2.5:1 uses a melt temperature of 245–260 °C, with barrel set points biased toward the front zone to limit residence time above 250 °C to fewer than 6 min. Mold temperature is held at 80–90 °C; below 60 °C the surface solidifies before full crystallization, and post-mold shrinkage continues after assembly, changing terminal pitch and field-reported screw torque retention. Hydraulic holding pressure in the range 50–70 MPa for a part with a nominal wall of 1.8 mm suppresses internal voids around brass inserts, while a short hold time below 4 s produces gate sink and voids detectable by X-ray. Because terminal block carriers are assembled with copper busbars, the comparative tracking index of the grade should be evaluated by IEC 60112; if the datasheet value is at or below 250 V, creepage distance compensation is required under IEC 60664-1 for pollution degree 2 or higher.
Automotive relay bases molded from VALOX PBT-FR 357-1001 are exposed to terminal insertion stresses, underhood thermal cycling, and condensed moisture during vehicle soak tests. The material's low equilibrium water uptake relative to polyamide 66—typically reported in ISO 62 datasheet values—reduces the dimensional swelling that would otherwise loosen molded-in blade terminals and change contact spring alignment. Dielectric withstand after aging is not a bulk property alone; it is controlled by wall thickness, weld-line integrity, and the absence of volatiles trapped near metal pins. On an 8-cavity mold with copper alloy terminals inserted, processing at a mold temperature below 70 °C creates a low-crystallinity surface layer that increases moisture ingress and can produce partial discharge sites under 1500 V AC testing after 500 h at 85 °C and 85% RH. Venting depth at the end-of-fill must be maintained between 0.02 mm and 0.03 mm; deeper vents flash, while shallower vents trap volatiles that leave carbonized tracks under dielectric test. The gate should be placed on a non-cosmetic surface away from thinned webs around relay coil pins because the flame-retardant additive reduces melt strength and makes weld lines at the last fill point more susceptible to crack propagation during terminal staking. Packing pressure between 60 MPa and 80 MPa with a hold time of 1.5 s/mm of nominal wall is used to maintain contact between the polymer melt and the insert shank during solidification; insufficient packing produces shrinkage gaps around the metal that reduce breakdown resistance.
| Processing parameter | Working set point | Critical threshold | Observed failure mode outside threshold |
|---|---|---|---|
| Residual moisture after drying | 0.01–0.02 wt% | 0.04 wt% | Hydrolysis at melt state; tensile elongation loss per ISO 527-2; silver streaks |
| Melt temperature | 245–260 °C | 270 °C | Flame-retardant degradation; yellowing; dielectric strength loss |
| Mold temperature | 70–90 °C | 60 °C | Low crystallinity; post-mold dimensional drift; reduced chemical resistance |
| Holding pressure | 50–80 MPa | 40 MPa | Sink marks; voids around inserts; pin retention scatter |
| Back pressure | 0.3–0.7 MPa | 1.0 MPa | Shear heating of flame-retardant package; melt temperature override |
| Residence time above 250 °C | 3–6 min | 8 min | Discoloration; volatile generation; inconsistent flame retardancy |
Winding tension applied to solenoid coil formers transfers compressive hoop stress into the bobbin core and flange root; if the bobbin wall thickness is below 1.0 mm, creep under a Class B operating temperature can permit the coil winding to loosen, producing audible noise and shorted turns. Unfilled flame-retardant PBT is selected for bobbins because it fills thin wall sections and resists mineral oil and potting compounds, but its creep modulus is lower than that of glass-fiber reinforced grades. Short-term flexural modulus measured by ISO 178 is not an adequate design input; tensile creep modulus and stress relaxation data from ISO 899-1 should be used for flange deflection calculations at continuous operating temperatures above 90 °C. In a production environment, a 16-cavity bobbin mold with a 0.8 mm wall and a single submarine gate is run with a fast injection speed to fill the core before freeze-off, while a melt temperature at the upper end of the allowed range—260 °C—keeps fill pressure below 90 MPa. The mold is circulated at 85 °C to maximize crystallinity and flatten the post-mold shrinkage curve. Winding tension is separately limited by the bobbin flange design; with a flange thickness of 1.2 mm, tension above 1.5 N on 0.2 mm copper wire has been observed to cause visible flange deflection on the unwound side, but published data for this exact grade and coil configuration is limited. The molder rejects parts that show gate blush or weld lines across the flange root because both defects reduce creep resistance under sustained load. After molding, parts should be allowed to stabilize for 24 h at 23 °C before winding; immediate winding can shift dimensions by several tenths of a percent as post-crystallization and moisture equilibrium proceed.
The substitution is driven by the need for stable contact pitch at elevated humidity because glass-filled nylon can absorb enough water to alter connector engagement and terminal retention after aging. The unfilled PBT grade has a lower notched impact strength and a higher coefficient of linear thermal expansion than a 30% glass-filled PBT; ISO 180/A and ISO 11359-2 values from the current datasheet should be compared directly before a drop-in replacement. Pin retention is not governed by bulk modulus alone: the interference between the metal contact barb and the plastic cavity produces local hoop stress that relaxes over time. A design that works in glass-filled nylon with a 0.6 mm wall around the contact may develop cracks after insertion in unfilled PBT if the barb depth exceeds the available elongation. On a 32-cavity connector mold with a hot runner system, cycle time is set by the gate freeze time; a gate diameter of 0.8 mm freezes too quickly at melt temperature 250 °C, causing erratic packing and inconsistent pin retention across cavities. Increasing gate diameter to 1.2 mm and holding pressure to 70 MPa reduces cavity-to-cavity variation in pull-out force measured by a vertical tensile tester. The latch arm root radius should be enlarged from 0.2 mm to at least 0.4 mm, and the latch thickness increased if the part is exposed to side-load during harness assembly. Thermal cycling from −40 °C to 125 °C per ISO 16750-4 produces lower retention loss in low-moisture PBT than in polyamide, but the initial insertion force may rise because of the lower elongation at yield. End-use terminal retention values should be measured according to the harness maker's specification rather than extrapolated from standard mechanical properties.
Arc interruption in a miniature circuit breaker places contradictory demands on the thermoplastic insulating parts: the arc chute must survive transient thermal loading without igniting, while the barrier plates must preserve creepage distances after exposure to ionized gases and metal vapor. VALOX PBT-FR 357-1001 is used in these internal parts because its UL 94 V-0 rating at 0.71 mm supports thin-wall designs, and the unfilled composition avoids the conductive carbon path that can develop when arc erosion exposes glass fibers. Critical to this application is the comparative tracking index measured by IEC 60112; a flame-retardant package can lower CTI, so the circuit breaker designer must verify that the listed CTI exceeds the minimum required for the pollution degree and voltage class of the device under IEC 60664-1. A wall thickness of 0.4 mm is below the UL-listed thickness and requires end-use testing of the final part. Molding of barrier plates with thickness 0.6 mm in a 4-cavity tool uses a melt temperature of 255 °C, mold temperature of 80 °C, and injection speed high enough to fill the thin section before the flow front freezes. The tool is equipped with vacuum venting because the flame-retardant system can produce volatiles at the upper processing temperature; residual gas must be evacuated before the cavity can be packed. Field failure modes in this part family are linked to jetting at blind pockets and to excessive residence time above 260 °C, which darkens the polymer and can reduce dielectric strength. Process control limits in production should include screw speed below 100 rpm and back pressure between 0.3 MPa and 0.7 MPa to limit shear heating of the flame-retardant additive.
Appliance power strip housings are frequently subjected to glow-wire testing at 750 °C or 850 °C per IEC 60335-1 clause 30.2.3, depending on current supervision and proximity to live parts. The material selection must consider not only UL 94 V-0 but also glow-wire flammability index and glow-wire ignition temperature from IEC 60695-2-11 and IEC 60695-2-12; these values are thickness-dependent and should be taken from the product datasheet at the planned wall section. In a power strip body with a nominal wall of 2.0 mm, molding at a melt temperature of 250 °C and a mold temperature of 80 °C produces a crystalline structure that resists post-mold shrinkage when the strip is assembled with snap-fit covers and screw bosses. The lower heat distortion temperature of unfilled PBT compared with reinforced grades means that the design should keep internal copper busbars separated from the polymer by a minimum air gap of 1.0 mm and should avoid clamping the busbar directly against the housing wall. Creepage and clearance dimensions per IEC 60664-1 must be maintained after mold shrinkage; for an unfilled PBT, linear mold shrinkage is higher and more isotropic than for a glass-filled grade, so the tool should be cut using the shrinkage value from the datasheet and verified by a first-article dimensional layout on a coordinate measuring machine after 48 h aging at 23 °C. The production molder checks moisture content at the hopper every 4 h when ambient humidity exceeds 60% RH because regrind from sprues and runners can absorb surface moisture rapidly. Published data for this specific power strip configuration is limited; therefore, full glowing-wire and tracking tests on the final assembly are required by the appliance standard regardless of the base resin rating.
| Standard | Test method | Parameter of interest | Application condition |
|---|---|---|---|
| UL 94 | 20 mm vertical burn | V-0 at 0.71 mm | Thin-wall electrical enclosures and barriers |
| IEC 60695-2-11 | Glow-wire flammability index | GWFI at target thickness | Appliance housings under IEC 60335-1 |
| IEC 60695-2-12 | Glow-wire ignition temperature | GWIT at target thickness | Unattended appliance end product |
| IEC 60112 | Comparative tracking index | CTI in volts | Creepage distance selection under IEC 60664-1 |
| IEC 60243-1 | Electric strength | kV/mm | Relay bases and terminal blocks |
| ISO 527-2 | Tensile strength and elongation | MPa, % | Load-bearing snap-fit and latch arms |
| ISO 178 | Flexural modulus | MPa | Bobbin flange deflection |
| ISO 180/A | Notched Izod impact | kJ/m² | Cold impact in EV accessories |
In EV charging coupler accessories such as locking actuator housings, signal pin carriers, and interior retaining brackets, the polymer must survive condensation after thermal cycling, low-temperature impact, and tracking current across surfaces that may collect dust and moisture. VALOX PBT-FR 357-1001 is considered for these parts because it combines V-0 performance at 0.71 mm with low moisture absorption, but the designer must separate signal-level insulating parts from power contact carriers that require higher CTI and possibly higher continuous operating temperature. The clearance and creepage distances defined in IEC 62196-1 and IEC 60664-1 for pollution degree 3 with overvoltage category II often exceed those required in indoor appliances; if the material has a CTI between 175 V and 250 V, creepage distances may need to be enlarged relative to a material with CTI above 600 V. In a 2-cavity mold for a locking actuator housing with wall thickness 1.5 mm, mold temperature is held at 85 °C to reduce warpage at the bearing surface that slides against the locking pin. The part is dried at 110 °C for 4 h and molded with a residual moisture content below 0.02 wt%; storage of dried pellets in open air longer than 1 h at 60% RH or higher starts to reintroduce surface moisture. Dimensional checks are made after 24 h because PBT continues to crystallize and shrink after demolding; measurements taken immediately at the press understate final assembly dimensions. For cold impact, the material's ISO 180/A notched impact value at −30 °C should be compared with the mechanical shock expected during charging cable drop and vehicle drive-over events. Published data for this specific EV accessory configuration is limited; qualification should include thermal cycling from −40 °C to 85 °C, damp heat at 85 °C/85% RH, and tracking tests on the final assembly.
Competitive SABIC VALOX™ PBT-FR 357-1001 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT-FR 357-1001 is a flame-retarded, unreinforced polybutylene terephthalate (PBT) injection-molding grade specified for thin-wall electrical connectors, relay bases, bobbin housings, and power-distribution components requiring a UL 94 V-0 classification at reduced wall thickness. The material is built on a semi-crystalline polyester backbone with a peak melting point of approximately 225 °C by differential scanning calorimetry. The -1001 suffix identifies a controlled additive and color variant within the VALOX 357 family; it does not define a separate polymer composition. The flame-retardant package typically consists of a brominated aromatic compound with antimony trioxide synergist, which raises melt viscosity and compound density relative to unfilled general-purpose PBT while retaining the low equilibrium moisture absorption and rapid crystallization behavior of the polyester matrix. The product is therefore positioned between general-purpose PBT resins that meet only UL 94 HB and glass-reinforced PBT compounds that provide higher stiffness but introduce anisotropic shrinkage and warpage.
The principal differentiation of 357-1001 from non-flame-retardant PBT grades appears in thin-wall flammability response and melt stability. Under UL 94 vertical burn, a flame-retardant PBT compound of this class typically achieves V-0 at 0.8 mm or 0.75 mm, whereas a general-purpose unfilled PBT of the same thickness remains in the HB classification. The formulation change also modifies processing: the melt must be kept within a narrower residence-time window because brominated flame-retardant decomposition products can form at hot-runner temperatures above 265 °C and after more than 6 minutes of hold-up. Published data for the exact additive chemistry of this specific configuration are limited; the current UL Yellow Card and supplier technical datasheet should be confirmed before tool release.
Moisture control is the first processing constraint. The resin must be dried in a desiccant-bed dryer with a supply air dew point of -30 °C or lower and a hopper temperature of 120 °C for 4 hours; the residual moisture target is below 0.020 wt% by ISO 15512. If pellets are exposed to ambient air above 60 % RH for more than 2 hours, hydrolysis of the PBT backbone begins, and subsequent molding can cause surface silver streaking, reduced tensile stress at break, and loss of UL 94 V-0 performance. The hopper capacity should be sized to no more than 1.5 h of material consumption at the selected shot weight. The dryer return-air cooler should be inspected at the beginning of each shift because an overloaded desiccant wheel raises the drying dew point and introduces batch-to-batch moisture variance.
Injection unit settings for a general-purpose screw of 20:1 to 24:1 L/D should maintain barrel zones from 230 °C rear to 260 °C front, with a nozzle setpoint of 250–265 °C and a measured melt temperature of 240–260 °C. Mold temperature should be held at 60–90 °C; temperatures below 50 °C produce low crystallinity and understated dimensional maturity, while temperatures above 100 °C extend cycle time and may overheat the flame-retardant package in hot spots. Hot-runner systems must use fully round flow channels without blind plugs, balanced manifolds, and externally heated nozzles with thermocouple control to ±3 °C. Dead-volume zones in valve-gate bodies or nozzle tips are a documented source of black specks and flame-retardant degradation. If the hot-runner volume exceeds 1.5 shots, a purge protocol of 3–5 shots after every 20 min idle period is recommended. Residence time at melt temperature should not exceed 6 minutes; if cycle interruption exceeds this threshold, the screw should be retracted and the barrel cooled to 200 °C after purging with general-purpose PBT.
Table 1 compares representative property ranges for VALOX PBT-FR 357-1001, an unfilled general-purpose PBT, and a 30 wt% glass-reinforced PBT. The values are distilled from supplier datasheets and ISO test methods; they are intended for initial candidate screening rather than final part validation.
| Property and test method | VALOX PBT-FR 357-1001 | Unfilled general-purpose PBT | 30 wt% glass-reinforced PBT |
|---|---|---|---|
| Density, ISO 1183-1 | 1.40–1.43 g/cm³ | 1.31 g/cm³ | 1.52–1.56 g/cm³ |
| Tensile stress at yield, ISO 527-2 | 55–60 MPa | 55–60 MPa | 120–130 MPa |
| Tensile elongation at break, ISO 527-2 | 4–8 % | 15–30 % | 2–4 % |
| Flexural modulus, ISO 178 | 2500–2700 MPa | 2200–2400 MPa | 7000–8000 MPa |
| Notched Izod impact, ISO 180/1A | 3–5 kJ/m² | 4–6 kJ/m² | 8–10 kJ/m² |
| HDT/A at 1.80 MPa, ISO 75-1/-2 | 50–60 °C | 50–60 °C | 200–210 °C |
| Melt volume rate, ISO 1133-1 at 250 °C/2.16 kg | 12–18 cm³/10 min | 30–40 cm³/10 min | 8–12 cm³/10 min |
| UL 94 at 0.8 mm | V-0 | HB | HB |
After molding, the post-shrinkage of 357-1001 is significantly more isotropic than that of glass-reinforced PBT. Typical mold shrinkage measured by ISO 294-4 after 48 h at 23 °C is 0.014–0.020 mm/mm in the flow direction and 0.014–0.022 mm/mm transverse to flow; the ratio remains closer to unity than the flow-to-cross-flow behavior associated with high-glass grades. This reduces out-of-plane warpage in flat terminal strips and snap-fit lids, but it also means the unreinforced compound cannot compensate for high applied bending moments. Tooling should therefore use a minimum draft angle of 0.5 °, a wall-thickness target of 1.0–2.5 mm, and generous radii at bosses; unreinforced flame-retardant PBT grades are notch-sensitive under impact, so the section behind snap fingers should not be sharp-cornered.
Replacement of an unfilled, non-FR PBT with the flame-retarded grade usually requires a review of the pressure-demand envelope rather than a complete tool rebuild. The brominated flame-retardant package raises low-shear viscosity because the additive particles increase internal friction and because the compound has a lower melt volume rate than many general-purpose grades. Injection pressure at a given flow length is typically 10–20 % higher. For multi-cavity connectors with wall thickness below 1.0 mm, the screw injection speed should be raised to 200–400 mm/s, and the changeover from velocity to pressure control should occur before the part is fully packed. A cushion of 3–6 mm should be maintained; if the cushion falls below 2 mm, the holding-pressure profile may be lost and short shots or sink marks can appear. A spring shut-off nozzle or hydraulic nozzle is preferred over a reciprocating nozzle because the flame-retardant melt drools at front zones above 250 °C.
In relay bases, terminal blocks, and connector housing applications, the comparative tracking index of a brominated FR PBT is commonly below that of unfilled PBT. For this grade, the supplier datasheet should be checked for the exact CTI; values around 250 V on a 3.0 mm plaque are typical for brominated/antimony systems, which limits use in high-creepage designs where insulation materials require CTI of ≥400 V under IEC 60112. Glow-wire performance under IEC 60695-2-12 is also end-product specific; a molded insulating part may pass a GWFI of 960 °C at 1.0 mm if supported by appropriate plate thickness, but sections below 0.5 mm are less likely to meet the same ignition threshold. Published data for this specific configuration at all wall thicknesses is limited; therefore testing on the final part is mandatory under EN 60695-2-12.
Compliance claims must be secured from the SABIC technical datasheet, the UL Yellow Card, and the Safety Data Sheet for the version supplied. The resin is typically documented under REACH regulation 1907/2006/EC and may be certified under the recast RoHS Directive 2011/65/EU and its delegated amendments. Many flame-retarded PBT compounds use a brominated non-PBB/non-PBDE additive that is outside the original RoHS restriction list, but verification remains with the molder because color concentrates, regrind, and processing aids can introduce non-compliant substances. For applications involving direct food contact, the grade is generally not recommended unless the specific additives and pigments are confirmed under FDA 21 CFR 177.1660 or equivalent national approvals; this confirmation is not automatic with the flame-retardant package.
The grade should not be combined with copper-based color concentrates at melt temperatures above 260 °C, because copper ions can accelerate polyester degradation and reduce UL 94 V-0 pass rates. It is also incompatible with strong alkaline hot-water service; continuous exposure to aqueous solutions above pH 9 at temperatures above 60 °C produces surface hydrolysis and a measurable reduction in tensile strength within 500 hours. For outdoor UV exposure, the natural variant exhibits chalking and embrittlement unless carbon black or UV-stabilized black is specified; the flame-retardant package alone does not provide weathering resistance. Storage of unopened containers is recommended at 10–30 °C and below 60 % RH for no more than 12 months; after opening, the remaining material should be resealed and re-dried before use.