| HS Code | 358857 |
| Material Type | Polybutylene terephthalate (PBT), flame retardant |
| Reinforcement | Unreinforced |
| Flame Retardancy Rating | UL 94 V-0 |
| Mold Shrinkage Percent | 1.5-2.0 |
| Processing Method | Injection molding |
As an accredited SABIC VALOX™ PBT-FR 310SEO-1001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ PBT-FR 310SEO-1001 is supplied in 25 kg moisture-barrier bags, palletized for safe industrial handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL loaded with 25 kg bags of SABIC VALOX™ PBT-FR 310SEO-1001, palletized, shrink-wrapped, and secured for ocean freight. |
| Shipping | SABIC VALOX™ PBT-FR 310SEO-1001 is typically shipped as non-hazardous thermoplastic resin pellets in moisture-barrier bags or octabins. No UN number or transport hazard class normally applies. Keep packaging dry, clean, and intact; avoid moisture, direct sunlight, contamination, and punctures during storage and transport. |
| Storage | Store SABIC VALOX™ PBT-FR 310SEO-1001 indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep in tightly closed original packaging to prevent moisture pickup and contamination; protect from physical damage. Maintain moderate temperature, avoid prolonged UV exposure, and follow first-in/first-out stock rotation. Use appropriate dust controls when handling pellets. |
| Shelf Life | SABIC VALOX™ PBT-FR 310SEO-1001 typically has a two-year shelf life when stored under recommended, sealed, cool, dry conditions. |
Terminal housings in appliance control circuits place the 0.71 mm UL 94 V-0 rating of SABIC VALOX™ PBT-FR 310SEO-1001 under direct product-safety evaluation. The grade is processed into terminal blocks, board-in connectors, and control-panel barrier strips where IEC 60335-1 clause 30.2.2 requires glow-wire testing on the final component rather than on a raw-material plaque. For unattended appliances carrying more than 0.2 A, insulating material supporting live parts is subjected to glow-wire heating at 750°C or 850°C depending on the end-product category; the unfilled flame-retardant PBT permits thinner terminal barriers without immediately sacrificing flame retardancy. Drying before molding requires a desiccant dryer set at 120°C for 4 h, with inlet air dew point below −30°C, so that residual moisture remains below 0.02% by weight. Barrel temperatures are maintained in the 240°C–260°C range, the nozzle at 250°C–260°C, and the tool at 40°C–80°C to balance crystallization shrinkage against surface quality. Residence time above 250°C beyond 5 min degrades the flame-retardant package, causing viscosity drop, yellowing, and reduced glow-wire performance; startup and shutdown sequences must minimize hold-up volume in the barrel and hot runner. Terminal pitch stability after thermal cycling is influenced by mold shrinkage anisotropy; published data for unfilled PBT of this density class commonly fall between 0.9% and 1.6% in the flow direction and between 1.3% and 2.0% transverse, with final tool compensation derived from ISO 294-4 shrinkage plaques. Insulation coordination follows IEC 60664-1; when the comparative tracking index value from the UL yellow card is not available, conservative design for pollution degree 2 environments uses material group IIIb, which reduces allowable creepage distances relative to group I materials. The table below consolidates the compliance checks that govern this downstream segment. Insert-molded brass or tinned-copper terminals require temporary mold protection against flash penetration along the pin shank; a short first-stage injection volume followed by second-stage packing pressure assists flash control without incomplete fill at the terminal root.
| Parameter | Standard / method | Test condition | Design relevance |
|---|---|---|---|
| Flammability | UL 94 | 0.71 mm wall stock | Terminal sidewalls and live-part barriers |
| Glow-wire flammability | IEC 60695-2-11 | 750°C / 850°C at as-molded thickness | Unattended appliance current-carrying zones |
| Tracking resistance | IEC 60112 | Solution A, as-molded surface | Creepage distance allocation per IEC 60664-1 |
| Relative thermal index | UL 746B | Electrical and mechanical with impact | Long-term thermal aging under load |
| Mold shrinkage | ISO 294-4 | Flow and transverse directions | Terminal pitch tolerance after annealing |
Relay coil formers molded at 0.71 mm wall stock shift the central difficulty from flammability to filling pattern and weld-line placement. In a coil former, the central barrel and two flanges create a flow channel where opposing melt fronts meet at the flange-barrel junction unless the gate is positioned to generate radial fill. A diaphragm gate or ring gate at the barrel end produces circumferential flow and reduces three-knit-line formation, but it requires center-gate trimming or a three-plate tool. Pin gating on the outer flange produces a weld line along the barrel, where winding tension of polyurethane or polyester magnet wire induces hoop stress. Unfilled flame-retardant PBT has lower notched impact strength than unmodified unreinforced PBT; any weld line in the barrel becomes a crack-initiation point during coil winding and varnish cure. Winding tension is commonly set between 30 g and 80 g for wire diameters from 0.10 mm to 0.40 mm; flange deflection under that load is governed by flexural modulus measured under ISO 178 at 2 mm/min. Published flexural modulus data for this grade class are typically in the 2500 MPa–2700 MPa range at 23°C, but the value decreases above 60°C. The molded bobbin must be checked under hot winding conditions or after varnish bake to ensure that flanges do not open beyond the coil winding envelope. Cavity pressure of 600–1000 bar improves flange flatness, but overpacking at the gate can produce flash that interferes with automated winding. Dimensional control is verified by ISO 294-4 and by checking core pin deflection during injection; a core pin length-to-diameter ratio above 6:1 may deflect if fill is unbalanced. Thermal aging is the limiting constraint: relay applications are frequently classified as Class B 130°C, but this unfilled flame-retardant PBT grade is generally limited to lower thermal classes unless the UL 746B relative thermal index on the yellow card supports higher exposure. The complete insulation system, including bobbin, wire enamel, tape, and varnish, must be evaluated under UL 1446; resin-only RTI is not sufficient. Contact cleaning solvents, especially alkaline aqueous solutions and some glycol-based fluxes, should be tested with molded stressed articles because PBT is susceptible to environmental stress cracking at sharp gate vestige and press-fit insert corners.
Arc chamber side walls, arc splitter supports, and mechanism insulating parts in miniature circuit breakers present a failure mode dominated by surface tracking and charring across the arc path. The unfilled PBT grade is not placed in the direct arc root; copper-plated steel arc splitters absorb the arc energy. Molded PBT carriers position the splitter stack and maintain slot spacing under short-circuit interruption. Dimensional tolerance for splitter slots is frequently specified at ±0.05 mm because arc migration and splitter engagement depend on consistent gap geometry; this requirement favors a tool temperature near the upper end of the 40°C–80°C window to stabilize post-molding crystallization. Electrical tracking is evaluated under IEC 60112 using solution A; if the value is not stated on the yellow card, circuit-breaker designers apply material group IIIb in IEC 60664-1 clearance and creepage calculations. Glow-wire performance is assessed under IEC 60695-2-11 for flammability and IEC 60695-2-12 / IEC 60695-2-13 for ignitability and ignition temperature on the actual molded wall. During overload tests at 1.45 times rated current, terminal temperatures can approach the short-term heat deflection range of unfilled PBT; components near bimetallic strips and coil terminations must be evaluated under ISO 75-2 method A at 1.8 MPa. Published deflection temperature data for this grade class generally fall in the 60°C–70°C range; this value is a short-term test and does not replace long-term thermal endurance data from UL 746B. Outgassing from the organic flame-retardant system can influence contact resistance stability in enclosed breakers; sealed-unit evaluations under IEC 60068-2-17 and contact resistance measurement under IEC 61810-7 may be required. Molding parameters for this segment favor high injection speed, rapid transition to packing, and immediate hold pressure to prevent sink over the splitter seat area; hold pressure is often maintained between 60 MPa and 80 MPa, but final values are set by the tool pressure drop at 0.71 mm wall stock. The unfilled grade must not be specified for current-interrupting parts that see repeated arc-root impingement, because the flame-retardant package is not designed for ablative arc resistance under short-circuit energy.
When motor bobbins operate above 120°C in resin-impregnated stators, the operational boundary for this unfilled flame-retardant PBT becomes visible quickly. Fractional horsepower shaded-pole and universal motor bobbins can use the grade for winding support, but the locked-rotor hotspot and varnish bake must be measured on the actual stator stack. Short-term heat deflection temperature under ISO 75-2 method A at 1.8 MPa is typically near 65°C for this class of material; that value does not define long-term thermal endurance. The relevant parameter is the relative thermal index published under UL 746B, which for unfilled flame-retardant PBT grades commonly appears in the 75°C–90°C electrical range. If a polyester or epoxy-methacrylate trickle varnish is cured at 120°C for 2 h after winding, the bobbin accumulates thermal exposure close to its practical continuous-use limit. Insulation system certification under UL 1446 is mandatory for motor insulation, and the bobbin resin is only one element in that system. Chemical exposure from varnish solvents, especially styrene and methacrylate monomers, can stress-crack PBT at sharp gate vestige, core hole edges, or terminal insertion points; production validation should include melt-impregnated bobbin samples tested for cracking after full cure. For insert-molded lamination stacks, preheating inserts above 100°C reduces premature melt solidification around terminal pins and lamination teeth, but high insert temperature also shortens the available packing window at 0.71 mm wall sections. Molding equipment should be configured with a shut-off nozzle or valve gate to prevent drool during insert placement. Hydrolysis is a further limitation: PBT undergoes hydrolytic chain scission in hot-wet conditions, and pre-drying before molding does not confer long-term hydrolytic stability. Motor bobbins in condensing environments or in applications exposed to frequent temperature cycling above 80°C and relative humidity above 60% should be evaluated for retained tensile strength over the service interval. Published data for this specific configuration are limited; end-use testing under actual stator processing conditions is required before replacing a glass-filled, hydrolysis-stabilized PBT or phenolic bobbin.
Thermal load in retrofit LED lamp sockets differs from that in conventional incandescent lampholders, but the same 0.71 mm UL 94 V-0 rating is used to meet lampholder requirements under IEC 60838-1 and UL 496. PBT sockets for GU10, G9, and dedicated LED module connectors require tight retention on bayonet or pin contacts; unfilled flame-retardant PBT provides creep resistance under the constant spring load of copper-alloy contact clips. The molding parameter that matters most is not peak injection pressure but the holding pressure profile. Fast cavity filling followed by a two-stage hold at 60–80 MPa reduces sink around brass contact insertion points and improves roundness of the lamp-facing aperture. Brass contacts are often inserted post-mold; insertion force calculations must account for the lower elongation at break of unfilled flame-retardant PBT, typically below 6% by ISO 527-2, which makes press-fit hole design sensitive to interference. In service, radiant heat from LED drivers and raised ambient temperature can push socket bodies above 80°C; designers evaluate creep modulus under ISO 899-1 at the specific contact-retention temperature. The grade should not be used where socket contact tabs are exposed to direct halogen capsule heat, because metal surface temperatures can exceed 180°C and exceed the short-term thermal capability of the unfilled resin. For lampholder zones that may be touched during relamping, glow-wire testing under IEC 60695-2-11 is performed on the complete socket assembly, not on a raw-material coupon. Dimensional tolerances for bayonet ramp features are commonly held to ±0.03 mm by using tool temperature at 80°C and post-mold annealing at 100°C for 1 h; annealing stabilizes shrinkage and relaxes molded-in stress, but it adds cycle cost and must be validated against lamp retention force.
Low-voltage signal contacts in outdoor charge controllers require hydrolysis-resistant processing even when the enclosure is sealed to IP65. AC and DC wallboxes, photovoltaic combiner boxes, and charge-controller terminal strips use flame-retardant PBT terminal housings because they need dimensional stability across −40°C to 90°C ambient swings and flame retardancy under fault conditions. Outdoor enclosures with gaskets still experience condensation cycles; internal relative humidity can exceed 60% during thermal cycling. Unmodified PBT is susceptible to hydrolytic degradation in hot-wet environments, and SABIC VALOX™ PBT-FR 310SEO-1001 is not specified as a hydrolysis-stabilized grade. The material should be limited to components inside sealed enclosures where internal humidity remains controlled, or tested under 85°C / 85% relative humidity per IEC 60068-2-78 for the required service life. Molding operations must hold residual moisture below 0.02% to avoid molecular weight reduction in the barrel; a dryer outlet dew point below −30°C is a practical control on the production line. Clearance and creepage distances for charging circuits are governed by IEC 61851-1 and IEC 62109-1, with creepage allocation based on the comparative tracking index measured under IEC 60112. If the value is not confirmed for the specific color and thickness, design conservatively to material group IIIb. Direct UV exposure will degrade surface gloss and impact strength of an unfilled PBT grade without a specified UV stabilizer; outdoor use is therefore acceptable only for internal components shielded by a sealed enclosure, where sunlight exposure during maintenance is intermittent. Terminal retention after thermal shock is evaluated under IEC 60068-2-14 test Na or IEC 60068-2-30 damp heat cycling, using screw-terminal pull-out force as the acceptance criterion. The final component should be molded with high-speed injection and no cushion beyond 3–5 mm to limit shear heating at the screw check ring, which can raise melt temperature beyond 260°C and damage the flame-retardant package in thin-wall signal-contact carriers.
Competitive SABIC VALOX™ PBT-FR 310SEO-1001 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC VALOX™ PBT-FR 310SEO-1001 is an unfilled, flame-retarded polybutylene terephthalate (PBT) injection-molding grade intended for electrical and electronic components requiring thin-section flame resistance without glass-fiber reinforcement. The base resin is a semicrystalline saturated polyester based on butylene terephthalate repeat units; the flame-retardant system is halogenated and antimony-synergized, permitting a UL 94 V-0 rating at a wall thickness commonly cited as 0.75 mm. The suffix -1001 is a supplier-specific packaging, color, or lot-identification variant within the VALOX™ 310SEO family. Mechanical and rheological values must therefore be confirmed against lot-specific certificates rather than transferred from generic unfilled PBT data.
Published supplier data for the 310SEO base grade indicate a nominal density of 1.41 g/cm³ per ISO 1183-1 and a melt-processing window of 240–270°C. The material balances melt flow, electrical insulation, and flame-retardant performance. It is not intended for food-contact or medical implant applications. End-of-life thermal recycling must account for halogenated flame-retardant decomposition products and antimony-bearing ash streams.
The grade is selected where thin-wall UL 94 V-0 performance is required but where the anisotropy, surface roughness, and contact wear debris of glass-filled grades are unacceptable. In such applications, dimensional stability and melt quality are governed more by drying control and mold-temperature uniformity than by barrel set-point error alone.
PBT hydrolysis is autocatalytic. Residual moisture cleaves ester linkages, releasing terephthalic acid oligomers that further protonate the backbone and accelerate chain scission. In 310SEO-1001, granulate moisture above approximately 0.02 wt% can reduce molecular weight before visible splay appears. Production-level observations on 80-ton hydraulic injection machines show that material predried only to -20°C dew point can exhibit melt-volume-rate drift after 15 min barrel residence at 260°C, while material dried to -40°C dew point remains within the repeatability limits of ISO 1133-1 during the same residence window. Because a barrel temperature deviation of ±10°C exerts less influence on melt viscosity than 0.02 wt% residual moisture, drying is the dominant process variable.
Pre-drying is specified at 120°C for 3–4 h in a closed-loop desiccant dryer for virgin granulate stored in sealed containers. Hopper return-air dew point must remain at -40°C or lower. If the desiccant bed is not regenerated, return-air dew point can rise to -20°C and reintroduce water into the hopper. Karl Fischer titration of dried granulate is preferred because surface moisture meters can under-report internal water in cold regrind or large granule cores.
For lots stored in open silos at relative humidity above 60%, predrying is extended to 6 h, and melt-viscosity stability should be verified by in-process MVR before production startup. The material should not be dried in hoppers shared with hygroscopic polyamides unless the conveying system is purged and dew point is re-verified; polyamide fines can generate gas streaks and nozzle deposit.
On the injection floor, 310SEO-1001 is typically processed on a reciprocating-screw machine with an L/D ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.5:1. A constant-taper transition zone reduces shear heating in the melt film. Worn non-return valves or scored barrels increase residence time and can produce black specks from degraded flame-retardant additive. Barrel temperature profiles are usually set from 240°C in the rear zone to 255–260°C at the nozzle, with the nozzle maintained at the lower end to reduce drool. Mold wall temperature is held between 60°C and 90°C. Below 60°C, crystallization is retarded and post-ejection shrinkage increases; above 90°C, cycle time rises and deep ribs may stick.
High-volume multi-cavity tools with valve-gated hot runners typically use fill times of 0.5–1.2 s for wall thickness below 1.5 mm. Peak injection pressure on a 35 mm screw commonly falls between 60 MPa and 120 MPa; peaks above 140 MPa usually indicate gate freeze-off or cold mold rather than a resin viscosity problem. Holding pressure is applied at 60–80% of peak injection pressure, with hold time determined by gate-seal studies using part weight as the response variable. For a 1.0 mm wall at 80°C mold temperature, gate-seal time is often 3–6 s, but this must be confirmed through incremental hold-time trials.
| Property | Test method | Reported range |
|---|---|---|
| Density | ISO 1183-1 | 1.40–1.42 g/cm³ |
| Tensile stress at break | ISO 527-2/5 | 45–50 MPa |
| Flexural modulus | ISO 178 | 2400–2600 MPa |
| Notched Izod impact, 23°C | ISO 180/A | 2.5–4.0 kJ/m² |
| Heat deflection temperature, 1.82 MPa | ISO 75-2/A | 55–65°C |
| Comparative tracking index | IEC 60112 | 250–300 V |
| Volume resistivity | IEC 62631-3-1 | 1.0 × 10¹⁵ Ω·cm |
| Surface resistivity | IEC 62631-3-2 | 1.0 × 10¹⁵ Ω |
| UL 94 flammability, 0.75 mm | UL 94 | V-0 |
The values in Table 1 are not specification limits; they represent a typical envelope drawn from supplier technical bulletins and standard laboratory specimen molding. Pigment loading or regrind content can shift notched Izod impact and CTI by more than 10%, so finished-part testing per the governing end-product standard remains mandatory.
The principal material-selection conflict in connector bodies and relay bases is between heat-deflection temperature, stiffness, and flow-induced anisotropy. A 30% glass-filled FR-PBT such as VALOX™ 420SEO presents a flexural modulus envelope of 8–9 GPa, while 310SEO-1001 sits near 2.5 GPa. Snap-fit features must therefore be re-evaluated: the unfilled grade requires a larger beam thickness or reduced engagement strain to avoid creep and crack initiation. However, the unfilled system avoids fiber orientation anisotropy, reduces weld-line strength loss, and permits longer flow length in sections below 0.8 mm.
Mineral-filled FR-PBT grades reduce warpage and raise heat deflection temperature but sacrifice elongation at break and surface finish. 310SEO-1001 is preferred when the part contains multiple openings, thin snap arms, or tight pin alignment where mineral fillers can shift hole-to-hole dimensions. Published creep data for direct comparison at 85°C continuous service is limited; ISO 899-2 testing is recommended when the part carries a metallic insert or a preloaded spring.
Compared with non-flame-retardant unfilled PBT such as VALOX™ 325, the 310SEO-1001 grade has higher density and reduced melt flow because of the flame-retardant package. Existing tools designed for non-FR PBT may require wider gates or higher melt temperature to maintain the same cavity fill pressure. In high-cycle electrical connectors, the absence of glass-fiber wear debris is an operational advantage: glass-filled FR-PBT can generate fiber-rich particulate at the contact interface, while 310SEO-1001 removes this wear mode but may require longer cycle time due to higher linear mold shrinkage.
Mold designers should plan for linear mold shrinkage of 0.5–0.9% in the flow direction and 0.7–1.2% transverse. Glass-filled grades shrink less but often more anisotropically. Tools designed for glass-filled material cannot be transferred to 310SEO-1001 without re-cutting core pins and adjusting gate dimensions.
In relay bases, terminal blocks, and appliance connectors, the grade is used for parts that carry live metal inserts and must pass glow-wire or needle-flame testing on the final assembly. The unfilled PBT provides adequate CTI for many mains-voltage applications, but designers should not copy creepage distances from high-CTI glass-filled grades. A typical CTI of 250–300 V corresponds to IEC 60112 PLC 3, which requires larger creepage distances than PLC 0 under pollution degree 2 per IEC 60664-1.
Chemical resistance is adequate for aliphatic hydrocarbons, alcohols, and many automotive fluids at room temperature. Hot strong acids, strong bases, and steam above 100°C attack the ester backbone. Conformal coatings containing aggressive solvents should be tested per ISO 175 before application, because solvent swelling can reduce flame-retardant interface adhesion and alter tracking resistance.
| Requirement | Test method or regulation | Condition or status |
|---|---|---|
| UL 94 flammability | UL 94 | V-0 at 0.75 mm per UL Yellow Card |
| Glow-wire flammability | IEC 60695-2-11 | Temperature as specified by end-product standard; final assembly test required |
| Comparative tracking index | IEC 60112 | 250–300 V, PLC 3 |
| RoHS Directive | 2011/65/EU | Supplier declaration; restricted substances below maximum concentration values |
| REACH Regulation | 1907/2006 | Supplier declaration; Article 33 SVHC disclosure if applicable |
Regrind from sprues, runners, and rejected parts is incorporated at 20–30 wt% in non-safety-critical electrical housings after identical drying. Above 30 wt%, lot-to-lot variance in flame-retardant additive dispersion and PBT molecular-weight distribution can shift UL 94 after-aging results and produce orange-peel on textured surfaces. Reclaimed material should be granulated to a uniform particle size of 3–5 mm; fines below 1 mm are excluded because their large surface area accelerates hydrolysis during hopper residence.
Post-mold annealing, when required for insert-loaded parts or stress relief around molded-in pins, is performed at 130–140°C for 30–60 min in air. Annealing above 150°C can volatilize low-molecular-weight flame-retardant species and deposit a non-conductive film on contact areas. The film may interfere with ultrasonic welding and pad printing. Parts should be cooled below 60°C before exposure to humid air to avoid condensation-induced surface hydrolysis.
Barrel residence time should be limited to 5 min at melt temperatures above 260°C. If the circuit breaks down, purge with a low-MFR polyolefin at 180–200°C before restart. Do not purge with PVC or acetal, because cross-contamination can generate corrosive gases and accelerated degradation. Copper-beryllium inserts in high-volume tools should be nickel plated to resist pitting from halogenated decomposition species when moisture control is lost; unplated cores may exhibit pitting beyond 100,000 shots.
For end-use certification, 310SEO-1001 is supported by supplier REACH and RoHS declarations and by the UL Yellow Card for the exact color and package code. Finished-part testing per IEC 60695-2-11 or IEC 60695-2-12 is mandatory for unattended-appliance applications, because the raw-material UL 94 rating does not cover glow-wire behavior of the assembled part. The material should not be combined with copper-containing heat stabilizers or certain amine-based processing aids that reduce flame-retardant efficiency in hot-wire ignition and glow-wire end tests.