Sabic Valox Pbt Fr 310se0 Bk

SABIC VALOX™ PBT-FR 310SE0-BK

    • Product Name: SABIC VALOX™ PBT-FR 310SE0-BK
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 915510
    Color Black
    Material Type PBT, flame retardant, unfilled
    Density 1.31 g/cm³
    Melt Volume Rate 10 cm³/10 min (250°C/2.16 kg)
    Mold Shrinkage 1.1-1.5 %
    Tensile Modulus 2600 MPa
    Tensile Stress At Break 50 MPa
    Tensile Strain At Break 20 %
    Flexural Modulus 2300 MPa
    Flexural Strength 80 MPa
    Notched Izod Impact 23c 35 J/m
    Hdt 0 45mpa 150 °C
    Hdt 1 82mpa 70 °C
    Vicat Softening Temperature 170 °C
    Ul94 Flame Rating V-0 at 0.75 mm
    Volume Resistivity >1E15 ohm·cm
    Dielectric Strength 20 kV/mm
    Comparative Tracking Index 600 V

    As an accredited SABIC VALOX™ PBT-FR 310SE0-BK factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ PBT-FR 310SE0-BK is supplied in 25 kg moisture-barrier bags, palletized for industrial handling.
    Container Loading (20′ FCL) SABIC VALOX™ PBT-FR 310SE0-BK is palletized in bags and loaded into a 20-foot FCL container, secured and protected from moisture.
    Shipping Shipping description for SABIC VALOX™ PBT-FR 310SE0-BK: Flame-retardant PBT resin pellets, normally supplied in moisture-barrier bags within cartons/pallets. Transport as non-hazardous general cargo; keep dry and avoid direct sunlight, heat, and contamination. Follow the SDS and local transport regulations for classification and labeling.
    Storage Store SABIC VALOX™ PBT-FR 310SE0-BK in its original, tightly closed containers in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Protect the resin from moisture, dust, and contamination. Avoid prolonged exposure to elevated temperatures. Keep containers clearly labeled and use first-in, first-out stock rotation. Follow the supplier’s SDS and local storage regulations.
    Shelf Life SABIC VALOX™ PBT-FR 310SE0-BK typically has a 24-month shelf life when stored in original, unopened packaging under cool, dry conditions.
    Application of SABIC VALOX™ PBT-FR 310SE0-BK

    Terminal block housings moulded from SABIC VALOX™ PBT-FR 310SE0-BK are processed as a 100 wt% virgin resin without secondary flame-retardant masterbatch; regrind from the same production line may be introduced up to 20 wt% only after desiccant drying to a moisture content below 0.02% and after documented confirmation that the regrind has not exceeded three heat histories. Compliance for panel-mount and DIN-rail terminal blocks is assessed under IEC 60947-7-1 and UL 1059, while the polymer contributes a UL 94 V-0 classification at 0.71 mm and the end device is subjected to glow wire testing according to IEC 60695-2-11 at 750°C or 850°C as determined by the equipment standard. Injection moulding on an 80–120 t hydraulic machine with a 20:1 L/D three-zone screw, chrome-plated barrel, and non-return ring should maintain melt temperature 250–265°C at the nozzle and mould temperature 70–85°C; shot volume should occupy 40–60% of barrel capacity to limit residence time below 8 min. Medium to fast injection speed of 60–110 mm/s is typical for wall thicknesses 1.5–3.0 mm, with holding pressure at 45–60 MPa for 4–6 s per millimetre of nominal wall to reduce sink marks around metallic inserts. Finished part types include screw-clamp terminal block bodies, DIN-rail mounting feet, insulating partitions, and terminal covers, with dimensional verification performed after conditioning for 24 h at 23°C/50% RH against ISO 294-4 shrinkage data.

    What Limits Regrind Ratios in Relay Bobbin Moulding When Winding Tension Creates Radial Creep?

    Relay bobbin flanges and coil former bodies moulded from the unfilled FR PBT grade are typically run at 100 wt% virgin resin; regrind is constrained to 15 wt% maximum because repeated extrusion can shift as-moulded flange flatness beyond the ±0.05 mm tolerance typical across a 25 mm flange span. The component is commonly qualified to IEC 61810-1, EN 61810-1, and UL 508, with coil insulation systems evaluated under UL 1446 or thermal endurance according to IEC 60216-1 at Class F (155°C) service temperatures. Production tooling uses a central sub-gate feeding a cold runner, with vent depths of 0.015–0.025 mm to permit gas discharge from the flame-retardant package without flash; mould temperature is held at 80°C because flange sections crystallize sufficiently to resist radial creep from automated winding tension of 0.3–1.0 N in fine-wire bobbins. Pre-drying at 120°C for 3–4 h to below 0.02% moisture is mandatory, and machine settings of 250–265°C melt temperature, 5–7 bar back pressure, and screw speed 60–100 rpm prevent splay at the gate. Terminal finished parts include telecommunications relay bobbins, power relay housings, timer relay coil formers, and miniature PCB relay bases.

    When Appliance Connector Moulding Must Satisfy Glow Wire End-Part Testing After Thermal Cycling

    Appliance power-entry connectors and internal terminal blocks for washing machines, dishwashers, and induction cookers use the grade as 100 wt% as-supplied pellets; regrind addition is permitted up to 20 wt% only after desiccant drying and when final glow wire results are re-qualified on plaques of identical wall thickness. Compliance is dominated by IEC 60335-1 clause 30.2 and IEC 60695-2-11:2021, with end-product glow wire tests conducted at 750°C for unattended appliances above 0.2 A and 850°C for parts intended to retain live parts. Processing requires a mould temperature of at least 75°C; at 60°C or below, thin-wall sections below 0.8 mm may show lower crystallinity and higher moulded-in stress, and glow wire end-product verification is therefore more sensitive to these variables. A 25 mm barrier screw with L/D 22:1 and low-compression check ring keeps melt temperature at 255–270°C measured by nozzle probe; barrel temperatures from rear to nozzle are set at 250/260/265/270°C. Injection speed is set at 80–130 mm/s for 0.8–1.5 mm walls; holding pressure of 60–75 MPa is held for 3–5 s, followed by cooling time of 8–12 s to maintain gate seal before ejection. Mould surfaces should be chrome-plated or stainless because flame-retardant decomposition condensates can corrode P20 steel during extended runs. Terminal finished part types include IEC 60320 appliance inlets, internal wiring harness connectors, sensor terminal housings, and control board brackets.

    Baseline injection moulding set points for VALOX PBT-FR 310SE0-BK in electrical component production
    ParameterSet pointMeasurement or source
    Pre-drying temperature120°CDesiccant dryer, return air dew point ≤ -30°C
    Pre-drying time3–4 hClosed-loop hopper dryer
    Residual moisture≤ 0.02 wt%Karl Fischer ISO 15512:2019
    Melt temperature at nozzle250–270°CIR or contact nozzle probe
    Mould surface temperature60–100°C; thin-wall preferred 75–100°CMould surface thermocouple
    Back pressure3–7 barHydraulic pressure, 25 mm screw
    Screw surface speed50–120 rpmGeneral-purpose 18:1–22:1 L/D screw
    Shot volume utilization40–60%Barrel capacity basis
    Maximum residence time8 min at 265°CMoulding cell timer

    Motor brush holder assemblies and switch housings for hand-operated power tools present a different set of constraints because the part must survive vibration, repeated impact, and service temperatures near the thermal class of the motor. The material is processed as 100 wt% virgin resin for brush holder plates; regrind up to 10 wt% may be used only in external housings, not in brush holder insulating plates, because contamination from brass inserts and carbon dust in plant regrind can reduce dielectric strength by creating conductive paths. Compliance is tied to IEC 62841-1 for hand-held motor-operated tools and the legacy IEC 60745-1 requirements, with material flammability carrying UL 94 V-0 at 0.71 mm and comparative tracking index measured according to IEC 60112 method A. Injection moulding on 60–100 t machines with a 20:1 L/D general-purpose screw should keep melt temperature at 250–265°C, mould temperature at 65–85°C, and back pressure at 2–5 bar; higher back pressure above 8 bar raises shear heating and may accelerate degradation of the flame-retardant package, producing acrid fumes and surface splay. Insert moulding of brass brush holders requires preheating inserts to 80–100°C and using 0.5–1.0 mm radius on insert edges to avoid microcracks at the polymer-metal boundary. Finished parts include brush holder plates, switch trigger housings, terminal supports, and dust-sealed gearcase covers.

    Circuit Breaker Arc Chamber Components and Comparative Tracking Index Shift

    Miniature circuit breaker arc chamber partitions, side plates, and insulating barriers are the most process-sensitive applications because the unfilled PBT-FR grade acts as structural insulation and arc-containment surface. Formulation is normally 100 wt% virgin VALOX PBT-FR 310SE0-BK, and regrind is excluded from any part located within 10 mm of the arc path because repeated heat history and metallic contamination alter comparative tracking index and increase the probability of carbon tracking failure under short-circuit let-through energy. Applicable standards are IEC 60947-2 for low-voltage switchgear and controlgear, UL 489 for moulded-case breakers, and IEC 60695-2-11 for glow wire; long-term thermal performance is additionally evaluated by UL 746B RTI and tracking resistance by IEC 60112. Processing requires a 45–60 t injection moulding machine with a three-zone screw of 18:1–20:1 L/D, chrome-plated to resist acidic gas generation during long production runs. Melt temperature is held at 250–260°C, and mould temperature is held at 80–95°C to maximize crystallization and reduce post-mould warpage in flat barrier plates with length-to-thickness ratios above 80:1. Slow initial injection of 30–50 mm/s for the first 20% of fill, followed by 80–120 mm/s for the remainder, prevents jetting at the sub-gate and reduces internal stress near the arc chamber vent slots; photoelastic inspection is used to confirm that no high-fringe-order regions remain within the vent slot root. Quantitative residual stress thresholds are tool-specific, and published data for this specific configuration is limited; OEM validation on instrumented moulds is required before series release. Finished part types include MCB side plates, arc splitter supports, solenoid plunger guides, and DIN rail latching levers where UL 94 V-0 performance is required at 0.71 mm.

    Lamp Holder Moulding at Thin-Wall Flow Lengths Above 100:1 Demands Gate Land Control

    Edison-screw lamp holders and linear fluorescent lampholder bodies moulded from VALOX PBT-FR 310SE0-BK use 100 wt% virgin resin; 15 wt% regrind may be used only for non-current-carrying covers after approval against IEC 60238 dimensional stability. Compliance is dominated by IEC 60238 for lampholders and IEC 60598-1 for luminaires, with flammability assessed by UL 94 V-0 at 0.71 mm and moulded parts subjected to ball-pressure testing per IEC 60695-10-2 at 125°C or 145°C depending on insulation class. The processing window demands high melt temperature of 260–270°C and mould temperature of 80–100°C to fill flow lengths up to 120:1; when mould temperature falls below 70°C, the unheated thin-wall flow front freezes prematurely and creates weld-line weakness opposite the side gate. A hot runner system with externally heated manifold and valve gates is used for multi-cavity production, with hot drop set points at 265°C and gate land controlled to 0.8–1.2 mm. Gate blush at the side gate is reduced by a 0.5 mm radius on the gate entrance. Finished parts include E26/E27 lamp sockets, GU10 twist-lock bases, fluorescent starter bodies, and LED driver housings.

    Engine compartment connector housings moulded from the black unfilled flame-retardant PBT grade are usually processed from 100 wt% virgin resin; regrind is not recommended above 5 wt% because USCAR-2 thermal shock cycles from -40°C to 100°C can open knit lines near wire seal retention features. Compliance is assessed under USCAR-2 Class 2 or Class 3, SAE J2030 for automotive electrical cable, and REACH/ELV substance restrictions; flammability remains UL 94 V-0 at 0.71 mm. Moulding is performed on 100–150 t machines with a 20:1 L/D chrome-plated screw and closed-loop process monitoring; melt temperature is set at 255–270°C, mould temperature at 85–100°C. Pre-drying at 120°C for 4 h to below 0.02% moisture with a dew point of -30°C or lower is critical. Finished parts include engine compartment connector housings, fuse/junction block bodies, sensor connector shrouds, and CAN bus connector shells; prolonged exposure to hot automotive fluids above 80°C should be validated by immersion testing per ISO 16750-5.

    Free Quote

    Competitive SABIC VALOX™ PBT-FR 310SE0-BK prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ PBT-FR 310SE0-BK is an unreinforced, flame-retardant polybutylene terephthalate injection-molding resin supplied in black. The 310 series carries a UL 94 V-0 flammability classification at 0.71 mm wall thickness, and the -BK suffix identifies the black pigmentation. The material is specified for thin-wall electrical insulator housings, relay sockets, coil formers, switch components, and motor end caps in which flame must self-extinguish after the ignition source is removed. Table 1 lists typical values generated under ISO 294-4 specimen preparation and the cited methods. These values are not minimum specification limits; lot release is governed by the supplier’s certificate of analysis.

    Table 1: Typical physical, rheological, mechanical, electrical, and flammability values for VALOX 310SE0-BK
    Property Test method Typical value
    Density ISO 1183-1:2019 1.41 g/cm³
    Melt volume rate, 250 °C/2.16 kg ISO 1133-1:2022 13 cm³/10 min
    Tensile stress at yield, 50 mm/min ISO 527-2/1A/50 55 MPa
    Tensile modulus, 1 mm/min ISO 527-2/1A/1 2600 MPa
    Flexural modulus, 2 mm/min ISO 178:2019 2400 MPa
    Charpy notched impact strength, 23 °C ISO 179-1/1eA 4.0 kJ/m²
    Heat deflection temperature, 1.80 MPa flatwise ISO 75-2/A:2020 65 °C
    Volume resistivity IEC 62631-3-1 >1.0E+13 Ω·m
    Comparative tracking index IEC 60112:2020 250 V
    Flammability rating at 0.71 mm UL 94 V-0

    The 1.41 g/cm³ density and 13 cm³/10 min melt volume rate place the material among unfilled PBT-FR resins with moderate melt viscosity. The flexural modulus of 2400 MPa is lower than glass-filled flame-retardant PBT, which reduces snap-fit stiffness but also avoids fiber orientation-induced warpage in flat connectors. The heat deflection temperature of 65 °C under 1.80 MPa indicates that load-bearing use above 60 °C ambient requires mechanical derating. The 250 V comparative tracking index under IEC 60112:2020 supports insulation coordination in pollution degree 1 and 2 environments, provided creepage and clearance distances are calculated to IEC 60664-1:2020.

    Predrying is mandatory to limit hydrolysis of the PBT ester bond. The resin is dried for 4 h at 120 °C in a desiccant dryer with a dew point of −40 °C or lower. If pellet moisture exceeds 0.02% by weight at the feed throat, hydrolytic molecular-weight reduction produces splay, lowered melt strength, and variable UL 94 V-0 performance in walls below 1.0 mm. On injection molding machines with 20:1 to 25:1 L/D three-zone screws and compression ratios between 2.0:1 and 2.5:1, barrel temperatures are set from 240 °C to 270 °C from feed to nozzle. The melt temperature is maintained at 250 °C for stable processing. The upper limit of 270 °C is not a continuous production target because the halogenated flame-retardant package can release acidic decomposition products above 270 °C. Mold temperature is held at 60 °C to 90 °C, with the upper half of that range used for maximum crystallization and dimensional stability. Shot size is maintained at 40% to 60% of barrel capacity, and cumulative residence time at 250 °C should not exceed 8 minutes. Hot-runner manifolds are set 5 °C to 10 °C below the nozzle melt set-point to reduce static degradation in stagnant melt regions.

    In thin-wall mold filling, shear rates from 1000 s−1 to 5000 s−1 are typical for connector housings. Above 10000 s−1, shear heating can raise local melt temperature above 270 °C and degrade the flame-retardant package. Melt-pressure sensors should be used in hot-runner drops to detect shear-induced temperature rise. On production lines, drooling at the nozzle and black specks in molded parts indicate residence-time exceedance or dead spots. The corrective action is a reduction in barrel temperature or shot size, not an increase in backpressure. Molders transitioning from polycarbonate should not purge with polycarbonate because ester-carbonate transesterification can generate copolymers with uncontrolled flow behavior. A low-MFR PBT purge compound or a commercial barrel-cleaning compound rated above 270 °C is used instead.

    Does UL 94 V-0 at 0.71 mm satisfy glow-wire and hot-wire ignition tests for appliance components?

    Material flammability classification under UL 94 is not equivalent to end-product glow-wire compliance. A V-0 rating at 0.71 mm does not automatically pass IEC 60695-2-12 glow-wire ignition temperature or IEC 60695-2-13 glow-wire ignitability for unattended appliance enclosures. Glow-wire performance depends on part thickness, contact force, and final colorant system. Published data for this exact unfilled black PBT-FR configuration under glow-wire testing is limited, so appliance end-product testing is mandatory. Similarly, the 250 V CTI under IEC 60112:2020 is a resin coupon value; creepage and clearance distances on printed circuit board spacing must be derived from IEC 60664-1:2020 using the pollution degree and overvoltage category of the final assembly.

    Designers evaluating relay bases or terminal blocks should not extrapolate UL 94 V-0 at 0.71 mm to thicknesses below 0.40 mm without additional testing. In thin-wall mold trials, cavity thickness variation of ±0.05 mm can shift UL 94 test outcomes, particularly when the flame-retardant additive is not fully dispersed. Gate blush and weld lines in multi-cavity tools can also create local regions with reduced flame-retardant concentration; weld-line UL 94 performance should be confirmed on molded parts, not on edge-gated plaques alone.

    In comparison with glass-reinforced VALOX 420SE0, 310SE0-BK exhibits lower melt viscosity, lower tensile and flexural modulus, and lower notched impact strength but more isotropic shrinkage and reduced tool abrasion. The glass-filled grade raises flexural modulus above 8000 MPa and heat deflection temperature under 1.80 MPa to approximately 200 °C, whereas the unfilled grade remains near 2400 MPa and 65 °C. For thin-wall connectors with long flat bridge sections, the unfilled grade is used because it avoids fiber orientation-induced warpage in the flow direction. However, the unfilled grade requires thicker sections or ribbing to compensate for lower stiffness. The absence of glass fiber also permits lower injection pressure and reduced mold wear in high-cavitation tooling.

    Compared with non-flame-retardant PBT, the FR package narrows the processing window and increases density from approximately 1.31 g/cm³ to 1.41 g/cm³. The upper processing temperature is reduced by 20 °C to 30 °C. Overheating or extended residence generates acidic decomposition products that can corrode mold surfaces and produce black specks. Regrind use is allowed at 20% by weight with dry virgin material if the regrind has not experienced more than one heat history and is free of contamination. Higher regrind fractions reduce the UL 94 V-0 margin and should be requalified at the same 0.71 mm wall thickness before series production.

    The PBT ester backbone is sensitive to strong alkaline additives. Compounding with primary amine-containing colorants or flame retardants is not recommended because residual alkalinity catalyzes ester hydrolysis above 240 °C, producing lower molecular weight and reduced impact strength. Continuous contact with aqueous acids above 80 °C or hot water and steam above 85 °C promotes hydrolysis, and the grade should not be used in those environments without hydrolysis-stabilized PBT grades or approval testing. The black pigmentation provides surface ultraviolet screening, but the material is not marketed as a weatherable resin for prolonged outdoor exposure.

    Table 2: Regulatory and standard-designation checklist for VALOX 310SE0-BK
    Requirement Standard or regulation Condition or test method
    Flammability rating UL 94 V-0 at 0.71 mm
    Restriction of hazardous substances EU RoHS 2011/65/EU as amended by (EU) 2015/863 Supplier declaration required for homogeneous material limits
    REACH candidate list EC 1907/2006, Article 33 No SVHC intentionally added above 0.1% w/w per supplier statement
    Comparative tracking index IEC 60112:2020 250 V
    Relative thermal index UL 746B Consult current UL Yellow Card for thickness and color
    Insulation coordination IEC 60664-1:2020 Creepage and clearance calculated on final part geometry

    Regulatory documentation for electrical and electronic equipment should include the supplier declaration under EU RoHS 2011/65/EU as amended by (EU) 2015/863. REACH status under EC 1907/2006, Article 33, should be confirmed against the current candidate list. The UL Yellow Card file E121562 provides thickness-specific UL 94 and UL 746B relative thermal index data. The material is not intended for direct food-contact use under FDA 21 CFR 177.1660 unless a specific grade and color are certified for that application.

    When halogen-free classification is a design prerequisite, what trade-offs occur with 310SE0-BK?

    Because 310SE0-BK contains a halogenated flame-retardant package, it is not suitable for applications that require halogen-free printed-circuit board laminates under IEC 61249-2-21 or equivalent OEM low-halogen component criteria. Halogen-free PBT alternatives may carry UL 94 V-0 ratings at thicker sections, often 1.5 mm or 3.0 mm, rather than 0.71 mm. Substitution into existing tools designed for 310SE0-BK requires verification of melt-temperature limits, mold shrinkage, CTI, and glow-wire performance because halogen-free flame-retardant packages can be more shear-sensitive and may require lower melt residence time. The thinner the wall, the greater the difference in UL 94 rating between halogenated and halogen-free systems; at 0.71 mm, halogen-free PBT often cannot match the V-0 rating of this grade. This trade-off is the primary reason 310SE0-BK remains specified for miniaturized electrical connectors where wall thickness is below 1.0 mm and end-product standards do not penalize halogen content.

    Top