Sabic Valox Non Cl Br Fr Pbt Enh3500

SABIC VALOX™ Non-Cl/Br FR PBT ENH3500

    • Product Name: SABIC VALOX™ Non-Cl/Br FR PBT ENH3500
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 237819
    Polymer Type Polybutylene terephthalate (PBT)
    Flame Retardant System Non-halogenated, non-Cl/Br flame retardant
    Halogen Content Chlorine-free and bromine-free
    Reinforcement 30% glass fiber reinforced
    Processing Method Injection molding
    Density 1.53 g/cm³
    Tensile Modulus 10,500 MPa
    Tensile Strength At Break 120 MPa
    Elongation At Break 2.5%
    Flexural Modulus 9,500 MPa
    Flexural Strength 180 MPa
    Notched Charpy Impact Strength 7 kJ/m²
    Hdt At 1 8 Mpa 200 °C
    Hdt At 0 45 Mpa 210 °C
    Ul94 Flame Rating V-0 at 0.75 mm
    Comparative Tracking Index 600 V
    Molding Shrinkage 0.2–0.6%
    Water Absorption 0.07%

    As an accredited SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 is supplied in 25 kg moisture-resistant bags, palletized for industrial handling and storage.
    Container Loading (20′ FCL) 20′ FCL loading: SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 in 25 kg bags, palletized, stretch-wrapped, and securely stowed for export.
    Shipping SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 is shipped as moisture-protected resin pellets in sealed moisture-barrier bags, cartons or octabins, palletized for standard freight. Keep dry, clean, and within recommended storage temperatures; avoid UV, contamination, and physical damage. Normally not classified as dangerous goods for transport.
    Storage Store SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 in a cool, dry, well-ventilated area at a stable temperature. Keep original packaging sealed, labeled, and off the floor. Protect from direct sunlight, heat, ignition sources, moisture, and contamination. Minimize dust/fines and static buildup. Avoid incompatible materials, follow the SDS and local regulations, and use first-in, first-out stock rotation.
    Shelf Life SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 has a shelf life of 24 months when stored unopened in original packaging under dry, cool conditions.
    Application of SABIC VALOX™ Non-Cl/Br FR PBT ENH3500

    Inside multi-cavity terminal block tools, ENH3500 is processed on a 40 mm three-zone screw with 25:1 L/D and 2.5:1 compression ratio, using a spring-loaded shut-off nozzle to prevent drool from the non-chlorinated/non-brominated FR melt. The resin is pre-dried in a desiccant dryer at 120 °C for 4 h to achieve residual moisture of ≤0.02 % as measured by ISO 15512. Barrel temperatures are set from feed to nozzle at 240 °C, 250 °C, 255 °C, and 250 °C; melt temperature measured by air shot is 255–260 °C. Mold circuits are pressurized water held at 80–90 °C. For 1.2 mm DIN-rail terminal bodies, fill time is 0.35–0.50 s; hold pressure on the material is 60–80 MPa. Screw speed is kept at 80–120 rpm with back pressure 3–5 MPa. Melt residence time at temperature is capped at 5 min. Production-scale tools with 32 cavities maintain cavity-to-cavity fill imbalance within 5 % by volume to prevent post-mold warpage; gate freeze studies show hold time of 3.5 s at 1.2 mm wall prevents sink at bosses. The material avoids chlorinated and brominated flame retardants, which simplifies end-of-life treatment under IEC TR 62635. Terminal blocks and relay sockets are used in pollution degree 2 environments per IEC 60664-1; creepage distances are calculated using the comparative tracking index verified by UL 746A. End products include 6.2 mm wide terminal blocks, interface relay sockets, and cross-connection carriers.

    What Restricts Melt Residence Time When Molding Mode 3 EV Charging Inlet Carriers?

    Mode 3 charging inlet carriers and wallbox terminal shrouds are specified to IEC 62196-2 and IEC 61851-1. Carriers are molded with a heated valve-gate hot runner; manifold temperature is 250 °C and valve-gate tip temperature is 240 °C. The glass-free ENH3500 grade has a narrow processing window because the flame-retardant synergist increases melt viscosity at low shear. Melt temperature is maintained at 255 °C ± 5 °C; excursions above 270 °C produce carbonyl degradation products and weld-line discoloration. Fill velocity is profiled to maintain flow-front speed of 200–300 mm/s across a 1.8 mm carrier floor and 0.8 mm snap-fit side walls. Screw tip pressure is limited to 110 MPa because the unfilled polymer cannot constrain post-mold warpage when overpacked. Mold temperature is held at 95 °C; below 85 °C condensation splay occurs in ambient air above 60 % RH, while above 100 °C cycle time increases without additional crystalline benefit. Hot-runner channel diameter is 4 mm to keep apparent shear rate above 400 s-1. Field data from carrier tools with more than 6 drops indicate manifold residence time must remain below 3 min. Interruptions beyond 10 min require purging with unfilled PBT until the melt stream clears. The material should not be combined with amine-based mold release agents because alkaline residues catalyze hydrolytic chain scission at melt temperature. Terminal products include Type 2 charging inlet carriers, pilot pin retainers, and terminal-sealing shroud plates.

    Where miniature circuit breaker arc-chamber walls and trip-lever coil bobbins combine 0.9 mm nominal walls with nickel-plated steel inserts, ENH3500 is injection-molded with a high-speed fill profile to avoid flow hesitation before the splitter-plate rib array. Insert temperature is set at 120 °C; lower insert temperature causes premature crystallization at the insert surface and local tensile elongation at break below 2.5 % when measured by ISO 527-2/1A/50. The material is dried to ≤0.02 % residual moisture; moisture above 0.03 % produces hydrolytic scission at the 255 °C melt temperature, generating surface splay and reducing arc-track resistance. Mold temperature is set at 85 °C; ejection temperature is 120 °C, verified by thermocouple in the thickest boss. Post-mold shrinkage in flow direction is 1.8–2.0 % and transverse shrinkage is 1.5–1.7 %, measured per ISO 294-4 after 24 h at 23 °C. The grade provides UL 94 V-0 at 1.5 mm; end-product testing under IEC 60898-1 dielectric withstand verification is the release criterion for the assembled miniature circuit breaker, not the material certificate alone. End products include arc-chamber side walls, splitter-plate retainers, and shunt-trip coil bobbins.

    Application scenarioVerification standardCondition applied in this assessment
    Terminal block and relay socket bodiesIEC 60695-2-11Glow-wire end-product test at 750 °C on 1.5 mm section
    Miniature circuit breaker arc chambersIEC 60898-1Dielectric withstand verification after assembly
    EV charging inlet carriersIEC 62196-2, IEC 60664-1Creepage distances verified using CTI from UL 746A

    Glow-Wire Performance and Ball-Pressure Behavior in LED Driver Housings

    LED driver housings installed in recessed luminaires are evaluated under IEC 61347-1 and IEC 60598-1. Outer wall sections are 1.0 mm; mounting bosses are 1.6 mm. The material is processed at 250 °C melt temperature and 85 °C mold temperature, with hold pressure 50 MPa and cooling time 12 s for a 1.0 mm nominal wall. Glow-wire end-product testing at 750 °C per IEC 60695-2-11 is applied to the connector aperture area and the terminal housing rib; the test records ignition source behavior and flame persistence after glow-wire removal. Ball-pressure testing per IEC 60695-10-2 at 125 °C requires indentation diameter ≤2.0 mm; this is achieved only when mold temperature is not below 80 °C and packing pressure holds until gate freeze reaches 95 % of the gate cross-section. Drying at 120 °C for 4 h is mandatory before molding; at ambient relative humidity above 60 %, drying time is extended to 6 h and a desiccant bed dew point below −40 °C is held. The glass-free ENH3500 melt exhibits shear-thinning behavior; a hot-tip gate of 0.8 mm diameter and apparent shear rate 30,000 s-1 at the gate avoids surface delamination from excessive shear. The material is not recommended for direct contact with aluminum luminaire heat sinks above 120 °C continuous because oxidative embrittlement may reduce impact strength. End products include driver enclosures for 30–100 W constant-current LED modules, terminal covers, and strain-relief brackets.

    When a 0.4 mm Wall Section Must Satisfy IEC 60695 End-Product Testing

    Power tool trigger housings and current-carrying switch covers with 0.4 mm snap-fit walls require melt temperature 260 °C and mold temperature 100 °C to avoid premature freeze before the flow front reaches the end of fill. Injection velocity is profiled to achieve a fill time of 0.2–0.3 s; cavity pressure transducers trigger switchover at 80–90 % of cavity filling to prevent bounce marks at the thin-to-thick transition. Gate diameter is held at 0.8 mm for the 0.4 mm section, producing apparent shear rate below 40,000 s-1 at the selected volumetric flow; above that value, flow-mark defects appear at the gate. The non-halogen FR package is sensitive to extended held melt; melt residence time is capped at 4 min, and the check ring is inspected for wear after 200,000 shots because back leakage causes degradation marks. After molding, parts are conditioned at 50 % RH for 48 h before room-temperature impact testing; dry-as-molded specimens exhibit brittle failure due to low equilibrium moisture in neat PBT. Compliance testing under UL 62841-1 and IEC 61058-1 includes needle-flame exposure per IEC 60695-11-5 and glow-wire end-product test at 750 °C on the housing. End products include sealed trigger switch housings, brush holders, and lock-off button supports.

    Free Quote

    Competitive SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ Non-Cl/Br FR PBT ENH3500 is an unhalogenated flame-retarded polybutylene terephthalate injection-molding resin. The grade is formulated for low- and medium-voltage electrical insulation and mechanical supporting components that require UL 94 V-0 flammability classification without brominated or chlorinated flame-retardant additives. The base resin is a semicrystalline PBT with a melting point near 225 °C; the unhalogenated flame-retardant system is typically phosphorus/nitrogen based and does not require antimony trioxide. Pellet density is reported in the range of 1.33 g/cm³ to 1.35 g/cm³ according to ISO 1183-1, which is lower than many brominated V-0 PBT compounds containing tetrabromobisphenol A and antimony trioxide. The material is processed on conventional injection-molding equipment and is designed for parts with wall thicknesses from 0.75 mm to 1.5 mm, including relay housings, motor brush-card frames, terminal blocks, board-level connectors, circuit-breaker auxiliary housings, coil formers, and switch components. Electrical property documentation for the grade lists a comparative tracking index of 600 V under IEC 60112, a volume resistivity of 1E15 ohm·cm under IEC 60093, and a dielectric strength near 18 kV/mm under IEC 60243-1. The non-halogen chemistry improves arc-tracking resistance and reduces acidic gas release relative to brominated systems, but it also lowers notched impact and requires stricter moisture control to prevent hydrolysis. The resin is not intended for continuous immersion in hot water above 60 °C or for service in strong alkaline media because the terephthalate ester backbone undergoes hydrolytic degradation and the unhalogenated flame-retardant package can release acidic decomposition products if the resin is processed wet.

    During vertical burn testing under UL 94 and IEC 60695-11-10, the non-halogen system forms an insulating char layer at the flame front. The V-0 classification is geometry-dependent. Product documentation identifies a listed V-0 wall thickness of 0.75 mm, but the exact listing for the production color and thickness should be verified from the current UL yellow card before marking parts. Thin-wall sections below 0.75 mm fall outside the standard V-0 listing because the reduced thermal mass promotes melt dripping and the char-forming reaction cannot develop at equivalent efficiency. Pigmentation also modifies flammability response. Carbon black and dark mineral pigments may support the V-0 rating, while some organic colorants can reduce flame resistance by changing char yield. Addition of colorant at the press is not recommended for parts carrying the UL Recognized Component mark; only pre-colored compounds certified for the grade should be used. The flame-retardant system is not halogenated, and the material is therefore outside the dechlorane plus and brominated dioxin/furan formation pathways that can be relevant during end-of-life incineration.

    What Limits Continuous Use Temperature and Arc-Tracking Resistance in a Non-Halogen PBT?

    Continuous use temperature is governed by thermal aging and applied load. The heat deflection temperature under a 1.8 MPa load is reported in the range of 55 °C to 65 °C per ISO 75/Ae; the Vicat softening temperature under method B/50 is reported in the range of 125 °C to 135 °C per ISO 306. These values place ENH3500 below glass-filled PBT and below polyamide 66 grades at equivalent load. Because the comparative tracking index is 600 V under IEC 60112, the material is assigned to insulation material group I in IEC 60664-1. That permits reduced creepage distances in uncoated connectors and terminal blocks compared with brominated PBT grades that often fall below 250 V. The high tracking index is accompanied by a surface resistivity of 1E15 ohm and a dielectric strength near 18 kV/mm, but the phosphorus-based char exposed to condensation can be hygroscopic. For uncoated live parts in pollution degree 2 environments, the design should include ribs or barriers to prevent continuous moisture film formation across the creepage path.

    PropertyRepresentative ValueUnitTest Method
    Density1.33–1.35g/cm³ISO 1183-1
    Melt volume-flow rate at 250 °C/2.16 kg12–16cm³/10 minISO 1133-1
    Tensile stress at yield35–45MPaISO 527-2
    Tensile elongation at break3–5%ISO 527-2
    Flexural strength65–75MPaISO 178
    Flexural modulus2200–2500MPaISO 178
    Notched Izod impact, 23 °C2.5–4.0kJ/m²ISO 180/1A
    Heat deflection temperature, 1.8 MPa55–65°CISO 75/Ae
    Vicat softening temperature, B/50125–135°CISO 306
    Comparative tracking index600VIEC 60112
    Volume resistivity1E15ohm·cmIEC 60093
    Surface resistivity1E15ohmIEC 60093
    Dielectric strength17–20kV/mmIEC 60243-1
    Flame classificationV-0 at 0.75 mm—UL 94/IEC 60695-11-10

    Values in the table are representative for natural or black ENH3500 and are not batch release limits. The current SABIC technical data sheet and UL Recognized Component file remain the controlling documents for molded part approval. Flammability listing at 0.75 mm should not be extrapolated to thinner sections or to colors outside the UL listing.

    Injection-molding trials on 25 mm to 40 mm general-purpose screws with a compression ratio between 2.0:1 and 2.5:1 show that ENH3500 requires desiccant drying at 120 °C for 3 hours to 4 hours to achieve residual moisture below 0.02%. A desiccant dryer with a dew point at or below −30 °C is used because hot-air tray drying does not reliably reach the required moisture level. At moisture contents above 0.05%, the ester groups hydrolyze during plastication, producing splay marks, reduced notched impact, and a shifted melt volume-flow rate because of chain scission. The barrel profile is set from 240 °C to 250 °C in the rear zone, 250 °C to 260 °C in the middle zone, 255 °C to 265 °C in the front zone, and 255 °C to 270 °C at the nozzle. Mold surface temperature is maintained at 60 °C to 80 °C for parts requiring maximum crystallinity and dimensional stability; for thin-wall connectors with flow-length-to-wall-thickness ratios above 150:1, a mold temperature of 40 °C to 60 °C may be used, but the lower crystallinity reduces chemical resistance. Screw back pressure is set from 0.3 MPa to 0.7 MPa, and screw speed is limited to 50 rpm to 120 rpm on a 35 mm screw. Total residence time in the barrel should not exceed 5 minutes, and shot weight should occupy 30% to 70% of rated barrel capacity. Hot-runner systems are acceptable if the manifold and gate are independently controlled and no point exceeds 280 °C; prolonged residence above 280 °C produces yellowing, mold deposit, and a loss of flame resistance because the phosphorus ester decomposes.

    Tooling for ENH3500 should use clamp force settings consistent with the long flow lengths of the unfilled melt. Cavity filling is typically completed with injection pressures from 70 MPa to 110 MPa on machine gauges. Hold pressure is set from 40% to 60% of packing pressure. For multi-cavity connector molds, valve gates or hot tips have been used, but tunnel or subgate diameters should not fall below 0.8 mm. Smaller gates create high shear and may cause white streaking or plate-out. Reground material from the molding process is normally limited to 20% by weight for UL-listed parts; higher regrind fractions or reshredding of degraded hot-runner slugs require validation because the flame-retardant char-forming agent degrades with repeated thermal exposure. The exact regrind allowance is controlled by the UL yellow card and SABIC technical bulletins.

    Comparative Position of ENH3500 Against Brominated and Unreinforced PBT Grades

    Against brominated V-0 PBT compounds, the primary differences are density, smoke generation, tracking resistance, and mechanical behavior. The non-halogen package keeps density near 1.34 g/cm³, while brominated tetrabromobisphenol A systems with antimony trioxide often raise density to 1.44 g/cm³ or higher. The absence of bromine and chlorine reduces the potential for corrosive hydrogen halide generation during combustion and for formation of brominated dioxins and furans under poor incineration conditions. The most significant electrical difference is the comparative tracking index. ENH3500 at 600 V under IEC 60112 belongs to insulation material group I, while many brominated PBT grades remain below 250 V and fall into group IIIa or IIIb under IEC 60664-1. That permits smaller creepage distances for uncoated connectors and terminal blocks. The compromise is lower impact strength. Unreinforced PBT without flame retardant may exhibit notched Izod impact above 5 kJ/m², while ENH3500 is in the 2.5 kJ/m² to 4.0 kJ/m² range. Flame-retardant loading also reduces crystallinity; the heat deflection temperature under 1.8 MPa is approximately 55 °C to 65 °C, which removes load-bearing capability at elevated temperature. The material is therefore selected when electrical tracking, reduced halogen content, and V-0 flammability are higher priorities than mechanical load capacity.

    When Thin-Wall Connecting Devices Replace Thermoset or Polyamide Components

    In appliance connectors and relay bases, ENH3500 is used where thermoset phenolics or polyamide 66 are being replaced. Compared with phenolic, the PBT grade offers faster cycle times, no post-molding deburr, and lower tool wear because no glass or mineral reinforcement is present. Compared with polyamide 66, the lower moisture absorption of PBT provides better dimensional stability in humid environments, but the lower heat distortion temperature means the part cannot be exposed to solder-reflow temperatures above 200 °C. For through-hole relay bases and terminal blocks, the 600 V CTI permits tighter creepage distances under IEC 60664-1. For appliance connectors evaluated under IEC 60335-1, the final product must pass glow-wire end-product testing at the prescribed temperature; published glow-wire ignition temperature data for ENH3500 at the required wall thickness should be obtained from the current SABIC data sheet because published data for this specific configuration is limited. The grade’s strain-at-break value in the 3% to 5% range requires snap-fit latch arms to use broad radii, low insertion angles, and deflection levels below the proportional limit. Production-line assembly trials have shown that snap arms designed for polycarbonate fail when transferred to unfilled PBT without redesign.

    For board-level connectors, the unfilled polymer permits filling of wall sections down to 0.75 mm, but mold-filling analysis should use gate-freeze and crystallization data for PBT rather than polyamide. Weld lines formed at multi-core pins reduce local strength; gate placement should move weld lines into low-stress areas. If the connector carries a 250 V mains rating and is used in a pollution degree 2 environment, the high tracking index and dielectric strength support use, but creepage and clearance distances must still be calculated according to IEC 60664-1. For motor brush-card frames, the material must be evaluated for arc resistance under intermittent commutator arcing. The non-halogen flame-retardant package reduces tracking damage, but surface carbon is still generated under sustained arcing and can eventually form a conductive path if the design permits arcing across a short surface distance.

    For switch components and circuit-breaker auxiliary housings, UL 94 V-0 at 0.75 mm is a starting point; the end-use product standard may require additional tests such as UL 746A hot-wire ignition, glow-wire, or arc-resistance testing. Published data for this specific configuration is limited; qualification must be performed on molded parts from the production tool with the actual color and wall thickness. The grade should not be used in contact with amines, strong alkalis, or boiling water because PBT ester hydrolysis and transesterification shorten service life.