Sabic Valox Medical Grade Pbt Hx325hp

SABIC VALOX™ Medical-grade PBT HX325HP

    • Product Name: SABIC VALOX™ Medical-grade PBT HX325HP
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 644821
    Polymer Type Polybutylene terephthalate (PBT)
    Filler Reinforcement Unfilled
    Impact Modification Impact modified
    Flow Characteristics High flow
    Density 1.31 g/cm³ (typical)
    Melt Volume Flow Rate 20 cm³/10 min (250°C/2.16 kg, typical)
    Tensile Stress At Yield 50 MPa (typical)
    Tensile Strain At Break 50% (typical)
    Flexural Modulus 2200 MPa (typical)
    Notched Izod Impact Strength 50 J/m at 23°C (typical)
    Heat Deflection Temperature At 1 82 Mpa 70°C (typical)
    Vicat Softening Temperature 180°C (typical)
    Water Absorption 0.08% (typical)
    Ul 94 Flammability Rating HB
    Sterilization Compatibility Ethylene oxide and gamma irradiation
    Medical Grade Compliance Healthcare-grade; ISO 10993/USP Class VI suitability (grade-dependent)

    As an accredited SABIC VALOX™ Medical-grade PBT HX325HP factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ Medical-grade PBT HX325HP is packaged in 25 kg moisture-resistant bags, palletized for industrial shipping and storage.
    Container Loading (20′ FCL) SABIC VALOX™ HX325HP medical-grade PBT, palletized in moisture-proof bags, loaded and secured in a 20-foot FCL for export.
    Shipping SABIC VALOX™ HX325HP is shipped as non-hazardous PBT resin pellets in sealed moisture-barrier bags, cartons, or octabins, palletized for transport. Keep dry, closed, and away from heat or contamination; no special shipping requirements apply. Follow the SDS and supplier handling instructions.
    Storage Store SABIC VALOX™ Medical-grade PBT HX325HP in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and strong chemicals. Keep in original sealed packaging until use to prevent contamination and moisture pickup. Follow FIFO, protect from dust/odors, avoid container damage, and use within recommended shelf life; consult the SDS/TDS for specific conditions.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored unopened, dry, below 30°C, away from sunlight.
    Application of SABIC VALOX™ Medical-grade PBT HX325HP

    Within dry powder inhaler (DPI) dose-metering actuator fabrication, unfilled high-flow PBT is processed at a melt-temperature corridor of 245–260 °C and a mold temperature of 60–80 °C to preserve snap-fit retention in latch geometries that experience repeated patient thumb loading. The material must satisfy ISO 20072:2009 for aerosol drug delivery device design verification, ISO 10993-1:2018 biological evaluation, and USP <88> Class VI systemic injection and intracutaneous data in the drug-device combination file. A non-migratory antistatic masterbatch is incorporated at 0.5–1.0 wt% for those actuator geometries where powder deposition on the outlet wall exceeds gravimetric acceptance criteria; loadings above 1.0 wt% are not specified because the resulting drop in Charpy notched impact strength, measured under ISO 179-1/1eA, has been observed to propagate cracking at injection-molded snap-arm roots during high-speed assembly. The downstream process uses a closed-loop desiccant dryer with a supply dew point below −40 °C and a resin moisture target below 0.02 % prior to plastification; molding is halted if ambient relative humidity exceeds 60 % unless the hopper is permanently blanketed. A multi-cavity hot-runner tool with valve-gate diameters not exceeding 0.6 mm is used to avoid stringing in the airflow path, and clamp force is calculated at 1.0–1.5 kN/cm² of projected part area to compensate for the high-cavity filling imbalance. Terminal finished product types include the actuator body, mouthpiece shroud, dose-counter window, and powder deaggregation outlet retainer.

    What tolerance-stack-up drivers govern 32-cavity insulin pen dose dial production?

    Multi-cavity tooling for dose dial sleeves is mounted with independent cavity pressure transducers to limit the shot-to-shot melt cushion variation to ±1.5 mm; this is necessary because the sleeve inside diameter is held to ±0.03 mm over a 12.0 mm length. Relevant compliance includes ISO 11608-1:2022 for needle-based injection systems, ISO 10993-5:2009 and ISO 10993-10:2021 for biological evaluation, USP <88> Class VI for systemic toxicity endpoints, and ISO 13485:2016 for process validation records. The formulation uses 1.5–2.5 wt% rutile TiO₂ medical masterbatch when a minimum optical density of 1.0 OD across the wall is required to protect insulin from photodegradation; higher loadings above 2.5 wt% increase the tendency for gate blush on the valve pin. Downstream injection molding is performed at a melt temperature of 245–255 °C, a holding pressure of 70–90 MPa decaying in 2.0 s steps, and a cooling time of 10–14 s. Terminal finished product types include dose dial sleeves, pen body housings, cartridge retainers, and clip-ring overmold bases.

    Standard designationTest endpoint / scope
    ISO 11608-1:2022Needle-based injection system design requirements and test methods
    ISO 10993-5:2009In vitro cytotoxicity extraction method
    ISO 10993-10:2021Skin sensitization and intracutaneous irritation
    USP <88> Class VISystemic injection, intracutaneous, and implantation
    ISO 13485:2016Quality management system process validation

    Luer-activated stopcocks and enteral feeding connectors molded from unfilled PBT require rotational torque control that is more sensitive to the internal-mold-release package than to melt-mass-flow index. Compliance for the fluid-contact components is drawn from ISO 80369-7:2016 for enteral small-bore connectors, ISO 10993-5:2009, ISO 10993-10:2021, and USP <88> Class VI. The formulation is set at 0.15–0.35 wt% of a silicone-free internal-mold-release masterbatch, with volatile content below 0.1 %; silicone-bearing additives are excluded because gamma irradiation can crosslink surface siloxane species onto the sealing land and shift breakaway torque beyond the specified upper limit. The downstream process uses two-stage decoupled filling at a melt temperature of 245–255 °C, a mold temperature of 65–85 °C, and an injection velocity profile capped at 120 mm/s through the valve gate to reduce jetting around the central bore. Shot-weight variation is monitored at 0.3 % or less, and post-molding annealing is performed at 80 °C for 2 h to relieve residual stresses before machining of the female taper. Terminal finished product types include stopcock bodies, luer lock collars, enteral extension-set Y-sites, and tamper-evident dust caps.

    Mold-Shrinkage Anisotropy in Dark-Walled IVD Cartridge Tooling

    The design of dark-walled IVD cartridges begins with the requirement that no stray fluorescence from external light sources reaches the assay read window; unfilled PBT is specified when the alternative black ABS fails the ISO 10993-5:2009 extraction test after repeated sodium-hypochlorite wipe-down. Regulatory scope includes EU IVDR 2017/746 for in vitro diagnostic devices, ISO 13485:2016, ISO 10993-1:2018, and FDA 21 CFR 862 for automated clinical analyzer components. The formulation uses a low-particle carbon black masterbatch at 0.05–0.10 wt% to achieve an optical-density floor of 2.0 OD across a 1.5 mm wall; loadings above 0.15 wt% reduce flow length in 0.6 mm ribs and increase weld-line brittleness at the reagent inlet. Processing is performed with conformal-cooled multicavity tooling at a mold temperature of 80 °C, a melt temperature of 250–260 °C, and a three-stage holding-pressure profile of 70/55/35 MPa to compensate for anisotropic tangential shrinkage. Pre-drying at 120 °C for 4 h to 0.02 % moisture is mandatory because residual moisture in dark-walled parts produces silver streaking that interferes with automated optical inspection. Terminal finished product types include chemiluminescence reader cassettes, immunoassay reaction wells, sample metering manifolds, and onboard reagent reservoir covers.

    Steam-sterilization-resistant surgical instrument handles and powered handpiece shells are selected when the device must survive repeated pre-vacuum autoclave cycles at 134 °C for 3 min without warpage exceeding 0.5 mm over a span of 120 mm. Compliance is driven by ISO 17665-1:2006 for moist-heat sterilization validation, ISO 10993-5:2009, ISO 10993-10:2021, and USP <88> Class VI; reusable surgical instruments additionally fall under EU MDR 2017/745 Annex VIII re-processing guidance. The formulation incorporates a hydrolysis-stabilizer masterbatch at 0.2–0.4 wt% and excludes amine-based additives due to accelerated PBT chain scission at autoclave pH extremes. Downstream injection molding uses a melt temperature of 250–260 °C and an elevated mold temperature of 90–100 °C to maximize crystallinity and reduce residual stress through the thick palm-swell section; post-molding annealing is run at 100 °C for 2 h before the first sterilization cycle. Terminal finished product types include orthopedic reamer handles, powered handpiece clamshell housings, electrosurgical pencil bodies, and reusable instrument tray latching components.

    When Nebulizer Cup Sidewalls Fall Below 1.0 mm, Condensation-Induced Growth Overtakes Hydrolysis

    Published processability data for unfilled PBT in thin-wall respiratory components remain limited; however, the governing failure mode in injection-molded nebulizer medication cups is not immediately hydrolytic, but solid-state condensation-induced dimensional growth when 0.8 mm sidewalls are oriented by high fill speed. Compliance is framed by ISO 27427:2010 for nebulizing systems and components, ISO 10993-5:2009, ISO 10993-10:2021, and USP <88> Class VI where the medication-contact cup is marketed as a primary-contact component. The formulation uses a medical-grade antioxidant masterbatch at 0.3 wt% and a blue pigment concentrate at 0.1 wt% for oxygen-line identification; external mold release is excluded because residual ester lubricant alters the surface tension of the narrow annular orifice. The molding cell is configured for injection-compression sequencing with a melt temperature of 250–255 °C, a mold temperature of 70–80 °C, and a pack pressure of 45–55 MPa; cooling time is held at 12–18 s to avoid premature ejection of the 0.8 mm wall. A post-molding annealing step at 70 °C for 1 h is used only after dimensional inspection because early annealing can mask warpage that would otherwise be detected as a process-shift signal. Terminal finished product types include nebulizer medication cups, humidifier canister adapters, air-inlet baffles, and pediatric aerosol mask connectors.

    Free Quote

    Competitive SABIC VALOX™ Medical-grade PBT HX325HP prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC VALOX™ Medical-grade PBT HX325HP is an unfilled polybutylene terephthalate resin supplied through SABIC’s healthcare-directed VALOX HX product track. The grade is specified for injection molded medical device components in which ester-based chemical resistance, dimensional stability, and controlled lot-to-lot processing behavior are required. In a device project, HX325HP is normally evaluated when the finished-device manufacturer requires a base polymer with documented biocompatibility screening, raw-material traceability, and healthcare change-management provisions rather than a conventional PBT that may lack those controls. Typical component categories include drug-delivery pen interiors, inhaler actuators, diagnostic cartridge housings, fluid-management connectors, laboratory consumables, and surgical instrument handles. The material is unfilled, non-flame-retardant, and not intended for load-bearing implant applications; those uses require separate mechanical and biological validation. The HX/HP designation distinguishes the grade from general-purpose VALOX 325 by supplier-controlled raw-material sourcing, production documentation, and pre-clinical biological test summaries. Final biocompatibility testing remains the responsibility of the device manufacturer.

    Does the HX325HP Grade Convert Standard VALOX 325 PBT Into a Clinically Usable Resin?

    The distinction between HX325HP and a general-purpose VALOX 325 resin is not primarily molecular architecture; both share the unfilled polybutylene terephthalate backbone. The clinical difference arises from the healthcare product controls: raw-material selection, production-line segregation, traceability documentation, biocompatibility screening, and supplier change-notification procedures. General-purpose VALOX 325 may satisfy many mechanical requirements but is not normally supplied with a healthcare dossier. HX325HP is processed on the same general-purpose PBT platform, which means drying conditions, melt-temperature limits, and mold shrinkage remain comparable to standard unfilled VALOX 325. The grade should not be confused with glass-fiber-reinforced VALOX HX grades, where fiber addition raises tensile modulus and heat deflection temperature but introduces anisotropic shrinkage, higher melt viscosity, and increased tooling abrasion. Flame-retardant healthcare PBT variants can alter extractables profiles and are usually selected only where an electrical safety or flammability requirement is present. HX325HP is therefore specified when mechanical loads are moderate, part geometry is thin-walled or complex, and the project requires an unfilled healthcare PBT with lower post-mold warpage than fiber-filled systems.

    Mechanical specification for unfilled PBT of this class is generally performed with ASTM D638 or ISO 527-1/-2 tensile testing and ISO 178 flexural testing. Published values for commercial unfilled PBT with comparable molecular architecture typically fall within a tensile stress at yield of 50 to 60 MPa, tensile modulus of 2.3 to 2.7 GPa, flexural modulus of 2.2 to 2.5 GPa, and notched Izod impact of 3 to 5 kJ/m² at 23°C. Density is typically 1.30 to 1.31 g/cm³ according to ISO 1183-1. Heat deflection temperature under 1.8 MPa is commonly 50°C to 60°C, while HDT/B at 0.45 MPa is typically 150°C to 165°C. Moisture absorption at saturation in 23°C water is usually below 0.4% by ISO 62, which is lower than polyamide but higher than polyolefin. Lot-specific values for HX325HP must be taken from the current SABIC technical datasheet and used in mold-filling simulation rather than generic engineering-polymer averages. Because the grade is unfilled, linear mold shrinkage is more isotropic than glass-fiber-reinforced PBT. Shrinkage values commonly fall between 1.5% and 2.0% depending on mold temperature, gate geometry, and holding pressure; this predictability is relevant for round or deeply cored components where differential shrinkage would otherwise produce ovality and molded-in stress. For finite-element analysis, the material model should use the actual stress-strain curve at 23°C and, if the device is autoclaved or exposed to repeated cleaning, the conditioned curve after moisture uptake.

    Melt Rheology, Drying, and Injection Molding Conditions

    Before melt processing, the resin must be dried in a desiccant dryer. Bulk moisture above 0.02% accelerates hydrolytic chain scission at melt temperatures, producing a measurable loss in notched impact resistance and an increase in carboxyl end groups. A drying temperature of 110°C to 130°C for 3 to 4 hours with a dew point below −40°C is the standard starting point for material removed from sealed containers. If the resin is exposed to ambient air for more than 30 minutes, drying time should be extended. The melt temperature at the nozzle should be maintained between 245°C and 270°C; excursions above 270°C or residence times beyond 5 minutes at 260°C can cause thermal oxidative degradation, visible yellowing, and a loss of molecular weight that cannot be reversed by remelting. Mold temperatures between 40°C and 80°C are typical; the upper portion of the range improves crystallization, dimensional stability, and surface quality, while the lower portion aids cycle time but may reduce heat resistance and increase molded-in stress.

    Processing parameterTypical rangeProcess boundary
    Pre-drying temperature110 to 130°Cdesiccant bed, dew point ≤ −40°C
    Pre-drying time3 to 4 hfrom sealed container; extend after > 30 min ambient exposure
    Residual moisture< 0.02%by Karl Fischer or loss-on-drying method
    Melt temperature245 to 270°Cmeasured at nozzle; do not exceed 270°C
    Mold temperature40 to 80°Clower for cycle time; upper for dimensional stability
    Injection velocity100 to 200 mm/sfor wall sections 1.0 to 1.5 mm
    Back pressure0.3 to 0.7 MPamaintains melt homogeneity; excessive back pressure adds shear heating
    Maximum residence time≤ 5 min at 260°Cavoid molten stagnation in hot runner or barrel

    Hot-runner systems should be designed with low dead spots and heated balance; nozzle inserts with consistent tip temperatures reduce stringing and cold-slug formation. The use of general-purpose single-flight screws with 20:1 to 24:1 L/D and compression ratios of 2:1 to 3:1 is common for unfilled PBT; low-shear screw profiles are preferred to limit shear heating in high-speed thin-wall molding. A single-point melt volume rate value alone does not capture thin-wall pressure drop because PBT is pseudoplastic. Capillary rheometry or mold-filling simulation should use Cross-WLF or Bird-Carreau viscosity parameters from the current SABIC datasheet.

    Tooling design for HX325HP requires attention to gate location and holding-pressure profile because the unfilled PBT matrix solidifies rapidly. Converging flow fronts in thin sections can entrap air if vent depth is insufficient; vent depths of 0.02 to 0.03 mm for unfilled PBT are commonly used on parting lines. Full-round runners are preferred over trapezoidal channels to minimize pressure drop and freeze-off. Subgates should be located in thicker sections to prevent premature gate solidification. For edge-gated parts, gate land lengths of 0.5 to 1.0 mm are typical, and gate depth should be approximately 50 to 70% of nominal wall thickness to allow adequate packing. Processors running all-electric injection molding machines with clamp forces between 500 and 800 kN and screw diameters of 35 to 50 mm often use injection velocities of 100 to 200 mm/s for wall sections of 1.0 to 1.5 mm. Holding pressures are typically set between 60 and 80 MPa hydraulic pressure, with a short boost-to-hold transition to reduce gate blush and sink marks. Cavity-pressure transfer is recommended because it compensates for batch-to-batch viscosity variation in healthcare-grade PBT; if cavity sensors are not available, machine-pressure transfer should be checked by part-weight studies over a range of hold times. Shrinkage fixtures or coordinate measurement data should be collected according to ISO 294-4 for dimensional stability records.

    When Terminal Sterilization Exposure Limits the Design Window

    Selection of the sterilization modality modifies the acceptable design stress and wall thickness of PBT components. Ethylene oxide sterilization under ISO 11135:2014 is generally well tolerated by PBT because process temperatures remain below 55°C; however, residual gas absorption and aeration time must be validated for closed lumens or thin-walled reservoirs. Gamma irradiation according to ISO 11137-1:2015 imposes oxidative chain scission. Many unfilled PBT grades retain usable tensile properties up to 40 to 50 kGy, but dose levels above 60 kGy can produce measurable notched impact loss and yellowing; the exact slope of property loss for HX325HP should be verified on molded plaques of the actual part thickness. Electron-beam sterilization creates a different dose-rate profile but similar oxidative risk. Steam sterilization under ISO 17665-1:2006 is the most hydrolytically aggressive method for polyesters. Repeated exposure at 121°C may be acceptable for non-load-bearing parts only if the resin is adequately dried and molded with minimal hydrolysis during processing. Steam cycles at 134°C are generally outside the continuous-use envelope for unfilled PBT unless the device has a short service life or the manufacturer has generated data showing acceptable retention of mechanical properties after cycling. Hydrogen peroxide plasma systems operate at low temperatures and are chemically less aggressive, but rapid vacuum pressure changes can induce wall stress in hollow components.

    For reusable devices, chemical disinfectants such as quaternary ammonium compounds, alcohol-based wipes, and oxidizing cleaners can cause environmental stress cracking if the molded part contains high residual stress from aggressive gate designs. Compatibility testing by ASTM D543 or ISO 22088 at the intended service temperature is required rather than assuming chemical resistance from generic PBT literature. Alkaline cleaners above pH 9 at elevated temperature should be avoided because polyester hydrolysis accelerates sharply under those conditions.

    Regulatory Filing Does Not Begin and End with USP Class VI

    The regulatory value of HX325HP is contingent on the quality of the supplier’s healthcare file. For a skin- or tissue-contacting device, the biological evaluation plan under ISO 10993-1:2018 identifies endpoints such as cytotoxicity (ISO 10993-5:2023), sensitization and irritation (ISO 10993-10:2021), and acute systemic toxicity (ISO 10993-11:2017). SABIC healthcare grades in the HX/HP series are typically supported by biological reactivity data against USP <87> and USP <88> Class VI protocols; the resulting test summaries are supplied under non-disclosure to device manufacturers. These data support material selection but do not replace finished-device biocompatibility testing because processing aids, colorants, sterilization residuals, and mold-release deposits can alter the final extractables profile. Manufacturers must also maintain lot traceability under ISO 13485:2016, the FDA quality system regulation at 21 CFR Part 820, and the European Medical Device Regulation MDR 2017/745. Drug-delivery components that contact the drug product may require additional extractables and leachables studies following ISO 10993-18:2020 and relevant pharmacopoeial chapters such as USP <1660>. A supplier change-management agreement should define how formulation, raw-material, or production-site changes are communicated before commercial implementation.

    Standard or regulationScopeTypical application to HX325HP
    ISO 10993-1:2018Biological evaluation planningIdentifies endpoint matrix by device contact category
    ISO 10993-5:2023Cytotoxicity in vitroExtract dilution screening of material and colored compounds
    ISO 10993-10:2021Sensitization and irritationSkin-contacting device components
    ISO 10993-11:2017Systemic toxicityParenteral or implant-related routes
    USP <87>Biological reactivity in vitroL929 MEM elution test
    USP <88> Class VIBiological reactivity in vivoImplantation, intracutaneous, systemic injection panels
    ISO 11137-1:2015Radiation sterilizationDose setting and dose audit for terminal gamma/e-beam
    ISO 11135:2014Ethylene oxide sterilizationProcess validation and residual limits
    ISO 17665-1:2006Steam sterilizationOverkill method and load mapping
    ISO 13485:2016Quality management for medical devicesSupplier lot traceability and process control

    At the component level, the unfilled PBT grade is most commonly applied to medical device parts where ester-based chemical resistance, low moisture absorption relative to polyamide, and higher ductility than glass-filled PBT are required. In inhalation devices, the material is used for actuator bodies that require snap-fit assembly and repeated mechanical cycling; the absence of glass fiber reduces wear on mating surfaces and improves surface quality. In diagnostic cartridges and labware adapters, HX325HP offers reduced water uptake compared with polycarbonate and better solvent resistance than acrylonitrile-butadiene-styrene; polycarbonate remains superior for optical transparency, and the PBT matrix is opaque in natural and pigmented formulations. In fluid-management connectors, the material must survive intermittent contact with disinfectants, lipid emulsions, and alcohol-based cleaning agents. Published data for this specific configuration is limited; compatibility should be verified by exposure testing according to ASTM D543 or ISO 22088 at the intended service temperature. On production lines, the largest recurring issue is not melt delivery but moisture regain in open hoppers and regrind use. A closed conveying system with nitrogen or dry-air purge and a maximum regrind addition of 20% is common practice for medical PBT; higher regrind fractions may shift viscosity and increase black specks if the scrap contains degraded material. Molders should avoid combination of PBT with amine-based purging compounds because amines accelerate polyester degradation and can leave surface residues that interfere with bonding or coating. Service temperatures above 100°C under sustained load are outside the unfilled PBT design envelope; applications requiring continuous load-bearing at those temperatures should be shifted to glass-reinforced grades or higher-temperature polymers depending on the regulatory requirements.

    Top