| HS Code | 448906 |
| Productname | SABIC VALOX™ Impact-Modified UV PBT 357U |
| Manufacturer | SABIC |
| Brand | VALOX |
| Grade | 357U |
| Polymertype | PBT |
| Impactmodification | Yes |
| Uvstabilization | Yes |
| Filler | Unfilled |
| Density | 1.31 g/cm³ |
| Meltvolumerate | 9-10 cm³/10 min at 250°C/2.16 kg |
| Tensilemodulus | 2300 MPa |
| Tensilestressatyield | 50 MPa |
| Tensilestrainatyield | 4.0 % |
| Flexuralmodulus | 2200 MPa |
| Notchedizodimpactstrength | 60 J/m at 23°C |
| Hdtat0 45mpa | 145 °C |
| Hdtat1 8mpa | 60 °C |
| Ul94flammabilityrating | HB |
| Processingmethod | Injection molding |
As an accredited SABIC VALOX™ Impact-Modified UV PBT 357U factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC VALOX™ 357U is supplied in 25 kg moisture-resistant bags, palletized for industrial handling and storage. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): palletized SABIC VALOX™ 357U impact-modified UV PBT resin in sealed bags, shrink-wrapped and secured. |
| Shipping | SABIC VALOX™ Impact-Modified UV PBT 357U is shipped as non-hazardous thermoplastic pellets in moisture-barrier bags, typically 25 kg bags or octabins, palletized and stretch-wrapped. It is not regulated for transport; store cool and dry, away from direct sunlight and ignition sources. |
| Storage | Store SABIC VALOX™ Impact-Modified UV PBT 357U in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and ignition. Keep containers tightly closed to prevent moisture absorption and contamination. Avoid incompatible chemicals and dust accumulation. Use first-in, first-out stock rotation; follow local regulations and supplier safety data. |
| Shelf Life | SABIC VALOX™ Impact-Modified UV PBT 357U has a 24-month shelf life from manufacture when stored in original, unopened packaging under dry conditions. |
For automotive exterior mirror housing manufacture, SABIC VALOX™ Impact-Modified UV PBT 357U is first pre-dried in a desiccant dryer to a residual moisture content below 0.02 wt%. Drying conditions commonly applied for unfilled PBT injection grades of this class are 120 °C for 3 h to 4 h with a drying-air dew point of −40 °C or lower; the grade-specific processing guide from the resin supplier must be consulted before any deviation is accepted. Residual moisture above 0.02 wt% is associated with hydrolysis-driven molecular weight reduction during plastication, which produces brittle failure at gate and weld-line zones after moulding. Melt temperature is maintained in the range of 245 °C to 265 °C, while the tool surface temperature is controlled between 40 °C and 80 °C. Higher tool temperatures within that range reduce frozen-in orientation and improve surface gloss retention after outdoor exposure, but they extend cooling time and can increase sink formation above bosses. The injection velocity profile is staged so that the melt front advances at moderate speed through the mirror housing rim and then decelerates before gate freeze-off; this practice reduces jetting and improves weld-line consolidation at the mounting lug. Packing pressure is held for 6 s to 10 s after fill and is normally limited to 40 MPa to 60 MPa to avoid overpacking thin sections adjacent to the glass-lens seat. The UV stabiliser package is evaluated under ISO 4892-2 or SAE J2527 outdoor-weathering programmes; when colour-shift or property-retention data for 357U are required, the supplier’s technical datasheet and colour-matched masterbatch documentation provide the relevant exposure interval. Impact-modified PBT is selected because the housing must withstand stone impact and low-temperature flexing without cracking; notched Izod values determined in accordance with ASTM D256 or ISO 179-1/1eA are used to compare incoming batches. Parts are post-checked for warpage using a granite surface plate and dial indicator after 24 h, with dimensional stability referenced to ISO 294-1 for specimen moulding. Typical failure modes observed on production lines include sink marks over screw bosses, flash at the parting line when clamping force is insufficient for the projected area, and brittle cracking at inserts when the tool temperature falls below 40 °C. The moulded end products are exterior mirror housings, mirror base covers, and small cowl-edge trims requiring UV resistance and cold-impact ductility.
Outdoor electrical enclosures for disconnect switches and motor starters are moulded from 357U resin when a combination of UV exposure, mechanical impact resistance, and stable dielectric performance is required. The moulder must review the supplier’s UL Yellow Card for the specific grade under UL 746C, because outdoor suitability is evaluated as a programme of ultraviolet exposure, water immersion, and compressive strength testing; a general UL 94 HB or V-0 rating alone does not establish outdoor weatherability. Enclosure bases and covers are typically designed with 2.5 mm to 3.5 mm nominal wall thickness to balance stiffness with cycle time. Impact-modified PBT provides tougher corner sections and integral hinge bosses than general-purpose PBT, but the improved ductility is accompanied by a lower flexural modulus; therefore load-bearing mounting feet and DIN-rail supports require ribbing and local wall thickening to compensate. In production, hot runner moulds with valve-gate controls are used to avoid stringing and to maintain consistent packing across the gasket channel. Mould temperature is held at 60 °C to 80 °C for dimensional reproducibility of the gasket groove; lower temperatures produce faster cycles but increase residual stress at the snap-fit catches. The outer cover is often textured with a fine grain to reduce visible UV micro-cracking; textured surfaces require an additional draft angle of 1° to 2° per side to prevent drag marks. Compliance for empty enclosures is assessed under IEC 62208 with impact tests performed on the moulded enclosure at the intended service temperature. Ingress protection is validated under IEC 60529 after assembly with a pre-formed silicone or EPDM gasket; the gasket retention rib is moulded to a tolerance of ±0.1 mm to prevent compression set leaks. Inserts for cable glands are installed by heat staking or ultrasonic insertion rather than cold pressing; cold pressing can initiate radial cracks at the insert boss because impact-modified PBT maintains higher elongation than standard PBT but remains notch-sensitive at sharp insert corners. The end products are padlockable disconnect switch boxes, motor starter covers, and outdoor junction enclosures installed in industrial, agricultural, and utility environments.
| Standard | Test scope | Property assessed | Verification route |
|---|---|---|---|
| UL 746C | Polymeric enclosure outdoor programme | UV, water, mechanical degradation | UL Yellow Card outdoor rating |
| IEC 62208 | Empty enclosures for low-voltage switchgear and controlgear | Impact, thermal stability, insulation | Type-test certification |
| IEC 60529 | Degree of protection provided by enclosures | Dust and water ingress | IP65 or IP66 verification |
| IEC 60112 | Comparative tracking index | Electrical tracking resistance | Minimum CTI value from supplier datasheet |
LED luminaire housings combine UV exposure on the exterior with conductive heat from driver and LED modules on the interior. VALOX 357U resin is used for compact floodlight bodies, garden step-light fixtures, and wall-pack housings where the structural housing is not bonded directly to the LED metal-core printed circuit board. Dimensional stability is assessed by ISO 75-2 and ASTM D648 heat deflection temperature, but the average service temperature of the housing is more critical than a single HDT value. Impact-modified unfilled PBT may exhibit creep under continuous load at temperatures approaching its glass transition; for this reason the highest-temperature zones adjacent to the driver compartment are designed with air gaps or aluminium heat shields so that housing wall temperature remains below 90 °C under worst-case operation. Moulded-in bosses for LED board attachment are designed with a minimum root radius of 0.5 mm to avoid stress concentration. Thread-forming screws for these bosses induce hoop stress; production lines monitor screw-driving torque to avoid exceeding the post-moulding yield point of the resin. When the housing is subjected to thermal cycling between −20 °C and 70 °C, the linear thermal expansion of PBT—generally in the range of 80 µm/m·K to 100 µm/m·K for unfilled grades—must be accommodated by slotted PCB mounting holes or flexible standoffs; otherwise differential expansion between the resin and aluminium can crack solder joints. The UV package is tested under ISO 4892-2 cycle 1 or ASTM G155 to evaluate surface chalking and colour shift; for luminaires, IEC 60598-1 and UL 1598 govern the end-use assembly. Injection tooling for such housings uses a direct sprue gate into a hidden surface or a subgate at the reflector rim; the gate is positioned to move weld lines away from the sealing lip. Weld lines formed around cores for cable entry ports retain approximately 50% to 70% of the virgin material impact strength in unfilled PBT; if a weld line falls on a snap-fit arm, a design revision is required rather than a process adjustment alone. The end products include outdoor wall-pack housings, bollard light bodies, and step-light enclosures supplied to OEM luminaire manufacturers.
In garden power tool motor housing production, VALOX 357U resin is used when the tool is intended for outdoor use and must survive repeated drops, UV exposure, and occasional contact with mineral oil or fuel residue. The material is fed from a desiccant dryer into a reciprocating screw injection machine with a compression ratio of 2:1 to 2.5:1 for PBT. Barrel temperature profile from feed to nozzle is set at 240 °C, 250 °C, 260 °C, 260 °C, and 255 °C; these values are typical for impact-modified PBT grades and are adjusted for screw recovery time. The tool is run at 50 °C to 70 °C to improve weld-line strength at the motor mounting bosses. In multicavity tools, cavity-to-cavity balance is maintained within 1% of shot weight; imbalance above that threshold produces variable impact properties and UV surface finish differences in the same batch. The housing is usually moulded in two halves, and the mating surfaces are held to a flatness of 0.2 mm across 200 mm length to prevent vibration-induced fretting. Threaded metal inserts for motor mounts are installed by ultrasonic insertion after moulding; the insertion horn is set to low amplitude to avoid over-melting the PBT around the insert. Moulded components are tested for low-temperature drop impact using a 1 m drop height onto concrete at −20 °C; this protocol is derived from IEC 62841-1 for hand-held motor-operated electric tools. The UV-stabilised grade is preferred because the tool housing is exposed to sunlight on job sites and in agricultural use. Resistance to oil and grease is evaluated by ASTM D543 immersion testing with reference fluids; in field service, surface crazing can occur if the housing is repeatedly wiped with aggressive solvent cleaners, so service instructions limit cleaning agents to mild soap and water. End products are leaf blower motor housings, string trimmer spool covers, and battery-pack outer shells.
PV junction boxes and connector bodies require long-term UV stability, low-temperature impact strength, and electrical tracking resistance. VALOX 357U resin is evaluated for injection-moulded junction box covers and base trays where the component is not the primary load-bearing support for the module frame. The resin is processed at melt temperatures between 245 °C and 260 °C in thin-wall tooling with wall sections between 1.5 mm and 2.5 mm. A narrow processing window exists because excessively high melt temperature accelerates thermal degradation and reduces tracking resistance, while insufficient melt temperature increases frozen-in stress and connector warpage. Tool temperature is controlled at 70 °C to 80 °C to stabilise the dimensional accuracy of diode pockets and sealing grooves. The material must be dried to below 0.02% moisture because residual moisture reduces molecular weight during plastication and can produce surface splay on thin sealing walls. The junction box is tested under IEC 62790 for PV junction boxes and, where applicable, IEC 62852 for connectors. Comparative tracking index is measured under IEC 60112; the resin supplier’s datasheet provides the minimum CTI value for the grade. Glow-wire ignition temperature and hot-wire ignition tests may be required for certain photovoltaic applications; the specific grade is not automatically rated for all electrical insulation categories, so compliance must be verified against UL 1703 and IEC 61730-1 system-level tests. Impact-modified PBT is preferred for hail impact resistance, but unfilled impact-modified PBT is less dimensionally stable than glass-filled PBT under screw-terminal compression load at elevated module temperatures. Published comparative data for unfilled impact-modified PBT in concentrated PV service conditions is limited; evaluation is therefore conducted on the specific grade rather than inferred from general PBT grades. Terminal clamping bosses are supported by brass inserts or are locally reinforced with glass-filled pads. Gate placement is arranged to avoid weld lines across the cable entry port; if a weld line cannot be avoided, the port is designed with a radiused base and the moulder increases packing pressure to improve weld-line consolidation. The moulded end products are photovoltaic junction box bases and lids, diode carrier trays, and connector bodies used in crystalline-silicon and thin-film module assemblies.
| Standard | Component | Evaluated property | Acceptance pathway |
|---|---|---|---|
| IEC 62790 | PV junction box | Outdoor durability, electrical safety | Type-test approval |
| IEC 62852 | PV connector | UV, thermal cycling, mechanical load | Type-test approval |
| IEC 60112 | Moulded insulation | Comparative tracking index | Minimum CTI grade |
| UL 1703 | Flat-plate PV module | System flame and electrical safety | System-level certification |
Outdoor sensor and telemetry enclosures for irrigation controllers, weather stations, and agricultural field monitors are produced from VALOX 357U resin to meet UV resistance and field-drop durability requirements. The enclosure shells are moulded with a nominal wall of 2.0 mm to 3.0 mm and use tapered bosses for PCB mounting. A hot runner system with valve gates is preferred for multicavity production to reduce regrind and maintain consistent melt residence time. Because PBT is sensitive to hydrolysis and thermal degradation, average melt residence time is limited to 5 min to 7 min at 250 °C; longer residence times produce black specks and reduced impact strength at the gate. The moulder uses a desiccant dryer with a dew point of −40 °C and feeds the resin to the hopper via closed conveying lines to prevent moisture regain. Sealing of the enclosure is validated under IEC 60529 for IP65 or IP66, but the weak point in PBT enclosures is often the interface between the screw boss and the silicone gasket; this area is designed with a minimum wall stock of 1.8 mm around the boss to resist creep after 500 h at 60 °C. UV retention is assessed under ISO 4892-2 with 60 W/m² irradiance at 340 nm for the intended outdoor environment severity class; the specific exposure interval is defined by the end customer because no universal UV lifetime exists for PBT grades. For agricultural chemical service, the material is tested under ISO 175 or ASTM D543 against dilute urea and common liquid fertilisers; prolonged contact with concentrated acids or bases causes surface attack and should be designed out by using secondary containers. Hail impact in the field is simulated through the enclosure design validation plan using an instrumented puncture protocol based on ISO 6603-2; wall thickness and curvature near edges govern the result more than the resin alone. The end products include irrigation controller housings, field transmitter boxes, and solar-powered telemetry node enclosures.
Because marine and off-highway electrical connector housings are subjected to salt spray, UV flux, hydrocarbon splash, and sub-zero impact in the same service interval, 357U resin is processed into connector bodies with multiple slides and core pins for pin cavities. Melt flow around these cores creates weld lines that are the primary failure initiation points during cold insertion or removal. To reduce weld-line weakness, the gate is positioned on the rear face of the connector body so that the melt front converges on the pin cavity in a single direction with minimal flow-front collision. Melt temperature is set between 245 °C and 260 °C, and mould temperature is held at 60 °C to 80 °C to improve weld-line strength. Pins are inserted after moulding by heat insertion or are overmoulded with a low-inertia vertical clamp machine where insert loading tolerates ±0.03 mm positional accuracy. If insert moulding is used, the inserts are preheated to 100 °C to 120 °C to prevent local crystallinity differences and sink around the pin roots. Salt-spray resistance of the assembly is evaluated under SAE J1455 for heavy-duty vehicle electronics or ISO 16750-4 for road vehicles; the resin itself is tested for fluid compatibility under ASTM D543 with diesel fuel, engine oil, and 5% salt solution. The UV-stabilised system reduces surface cracking, but the connector body remains notch-sensitive at sharp locking-tab roots, so locking features are designed with 0.5 mm minimum radii and are gated away from the tab. In sub-zero testing, impact-modified PBT retains ductility to approximately −30 °C, but the specific low-temperature brittleness point of the grade must be confirmed by the supplier’s notched Izod data at −30 °C under ISO 179-1/1eA. The moulded end products are inline connectors, solenoid coil housings, and sensor connector bodies used on agricultural, construction, and marine equipment.
Competitive SABIC VALOX™ Impact-Modified UV PBT 357U prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Among semi-crystalline polyesters specified for outdoor electrical enclosures, lighting components, and sensor housings, SABIC VALOX™ Impact-Modified UV PBT 357U is a polybutylene terephthalate grade in which an elastomeric impact-modification phase and a UV stabilizer package are dispersed within the PBT matrix. The material is supplied as cylindrical pellets and is identified under ISO 1043 as PBT. Published typical values obtained under ISO 1183-1 place moulded density at 1.31 g/cm³; melt volume-flow rate under ISO 1133-1:2022 at 250 °C/1.2 kg is reported near 9.0 cm³/10 min, subject to the current SABIC Material Data Center revision. The grade is specified where outdoor weatherability and low-temperature ductility are required without the brittleness of mineral- or glass-filled PBT grades.
The operational distinction lies in the combined effect of the elastomeric impact-modifier concentration and the UV stabilizer system. Injection-moulded plaques tested in accordance with ISO 527-2/1A show tensile stress at yield near 52 MPa and tensile strain at break near 80%, whereas a comparable unfilled PBT without impact modification typically displays higher tensile stress but significantly lower multi-axial ductility. The addition of the impact modifier reduces the 0.45 MPa deflection temperature to approximately 127 °C and the 1.8 MPa deflection temperature to approximately 52 °C under ISO 75-2. For glass-filled PBT grades, flexural modulus is commonly two to four times higher, but notched Izod impact values under ISO 180/1A often fall below 10 kJ/m². The 357U grade occupies an intermediate position: flexural modulus near 1,850 MPa, notched Izod impact at 23 °C near 45 kJ/m², and avoidance of the pronounced anisotropic shrinkage and warpage associated with short-glass fibre orientation.
Prior to melt processing, the resin must be dried from the as-supplied moisture state to a target residual moisture not exceeding 0.02%. Closed-loop desiccant dryers with dew point lower than −40 °C are preferred; drying at 120 °C for 4 h to 6 h is typical. Above 60% ambient relative humidity, the hopper should be covered or blanketed with dry air to prevent moisture re-uptake. Melt temperature at the nozzle should be maintained within 245 °C to 270 °C, and residence time above 270 °C should not exceed 5 min to limit thermal degradation of the impact modifier and discoloration. Mould temperature should be held between 50 °C and 90 °C to balance crystallization rate and surface finish. Injection pressure and screw design recommendations include a general-purpose polyolefin screw with L/D of 20:1 to 24:1 and compression ratio 2.5:1 to 3:1; back pressure is usually set from 0.3 MPa to 0.7 MPa. High shear at the gate should be limited by using a gate land of 0.5 mm to 1.0 mm and a minimum wall section of 1.0 mm for thin-wall connectors.
Substitution is driven by the requirement for retained impact strength and surface integrity after prolonged exposure to UV radiation and moisture. The UV stabilizer package in 357U is formulated to provide an outdoor suitability rating under UL 746C; the grade is typically assigned an f1 weatherability category for certain thicknesses when evaluated for long-term UV and water exposure. Laboratory accelerated weathering under ISO 4892-2 cycles A and B can be used to compare colour shift and gloss retention. In unpigmented or custom-coloured versions, formulation-specific UV screening is often required; published data for all colours is limited, and end-use testing remains necessary for exact ΔE shift. This distinguishes the product from general-purpose impact-modified PBT grades that may retain room-temperature impact strength but do not carry a defined UV performance rating.
A representative property profile for injection-moulded plaques demonstrates the trade-off between stiffness and ductility. At 23 °C, flexural modulus is reported near 1,850 MPa under ISO 178; tensile modulus is approximately 1,900 MPa; no-break behaviour is commonly observed in unnotched Charpy tests under ISO 179-1/1eU. Notched Charpy impact under ISO 179-1/1eA at 23 °C is reported near 16 kJ/m², while notched Izod under ISO 180/1A is reported near 45 kJ/m², reflecting the different notch geometry and impact velocities. The material retains useful impact response at low temperatures, with notched Izod at −30 °C reported near 8 kJ/m², though the exact value is grade-lot dependent.
Rheological data from capillary and in-line melt measurements show pronounced shear thinning above 100 s⁻¹, with viscosity decreasing by approximately 30–40% between 100 s⁻¹ and 1,000 s⁻¹ at 250 °C. This characteristic permits rapid filling of thin-wall sections, but melt-front velocity should be controlled within 100–300 mm/s to avoid jetting and anisotropy. Mould shrinkage under ISO 294-4 is typically 1.2–1.6% in the flow direction and 1.4–1.8% transverse, reflecting the semi-crystalline nature of PBT. Shrinkage anisotropy is lower than that of 30% glass-fibre-filled PBT, but higher than that of amorphous blends. Gating should be placed in the heaviest section; weld-line strength can remain the limiting design criterion in highly branched parts.
For regulatory and specification reviews, Table 1 summarises a comparative data set using current ISO test designations; values should be confirmed against the SABIC Material Data Center revision applicable to the specific lot.
| Property | Test Method | VALOX 357U Typical Value | Unfilled PBT Typical Value | 30% Glass-Filled PBT Typical Value |
|---|---|---|---|---|
| Density | ISO 1183-1 | 1.31 g/cm³ | 1.31 g/cm³ | 1.53 g/cm³ |
| Tensile stress at yield | ISO 527-2/1A | 52 MPa | 55 MPa | 110 MPa |
| Tensile strain at break | ISO 527-2/1A | 80% | 15% | 2.5% |
| Flexural modulus | ISO 178 | 1,850 MPa | 2,300 MPa | 8,000 MPa |
| Notched Izod, 23 °C | ISO 180/1A | 45 kJ/m² | 4 kJ/m² | 8 kJ/m² |
| HDT, 1.82 MPa | ISO 75-2/A | 52 °C | 55 °C | 200 °C |
Moisture uptake in unreinforced PBT is comparatively rapid, with equilibrium moisture near 0.2% at 23 °C and 50% relative humidity when tested to ISO 62. If the resin is processed above 0.02% residual moisture, hydrolytic chain scission accelerates in the melt; the observed result is a measurable decline in melt viscosity, tensile elongation at break, and notched impact strength. The hydrolysis reaction follows pseudo-first-order kinetics in the presence of moisture, and the rate constant increases sharply above the 250 °C standard processing temperature. For this reason, melt accumulators and hot-runner manifolds should be operated with minimum hold-up volume, and purging frequency should be increased at the upper end of the processing window. In hot-moisture end-use environments, continuous exposure above 60 °C in water or saturated steam is not recommended without additional hydrolysis stabilizer; published data for this specific configuration is limited.
On production-scale injection moulding machines with clamping force from 800 kN to 2,500 kN, the principal defect encountered during trial runs is delamination at weld lines when melt temperature drops below 245 °C in tools with long flow-length-to-wall-thickness ratios above 200:1. The defect correlates with frozen skin formation at the melt front. A second observed failure mode is gate blush when fill velocity exceeds 300 mm/s; reducing injection velocity or increasing gate diameter to at least 1.0 mm eliminates the blush without changing nozzle temperature. These process observations are specific to open-barrel reciprocating-screw machines with nozzle shut-off; hot-runner systems require independent tip temperature control above 230 °C to prevent premature solidification in the tip.
In outdoor sensor housings and photovoltaic junction boxes, the combination of UV resistance and improved impact toughness is relevant to snap-fit closures and ultrasonic welding seams. Components moulded from 357U can be assembled using ultrasonic welding, but weld strength depends on moisture content and welding amplitude; pre-weld drying at 120 °C for 2 h is typically employed when ambient humidity exceeds 60%. The grade is not intended for applications requiring UL 94 V-0 at thin sections; typical ratings for this impact-modified grade are UL 94 HB, and flame-retardant alternatives should be selected for electrical safety ratings requiring V-0. For outdoor electrical enclosures, the use of 357U should be combined with creepage and clearance verification under IEC 60664-1, since the material is not a substitute for thermosets in all insulation conditions.
For regulatory submissions, the compliance matrix in Table 2 lists the standards commonly cited for this product class.
| Document | Clause or Designation | Scope |
|---|---|---|
| EU RoHS Directive 2011/65/EU | Annex II, Annex III exemptions | Restricted substances concentration limits for EEE |
| REACH Regulation (EC) 1907/2006 | Article 33, Annex XVII | SVHC communication and restriction conditions |
| UL 746C | Outdoor weatherability, f1 | Polymeric materials for outdoor electrical components |
| UL 94 | HB | Horizontal burn classification for specified thickness |
| ISO 1043 | PBT | Symbols and abbreviated terms for plastics |
| ISO 294-4 | Moulding shrinkage | Thermoplastic moulded specimen shrinkage measurement |