Sabic Valox Impact Modified Pbt 3706 1001

SABIC VALOX™ Impact-Modified PBT 3706-1001

    • Product Name: SABIC VALOX™ Impact-Modified PBT 3706-1001
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 374245
    Material Type Polybutylene terephthalate (PBT), impact modified
    Reinforcement 10% glass fiber
    Density 1.35 g/cm³
    Melt Volume Flow Rate 250 C 5 0 Kg 13 cm³/10 min
    Mold Shrinkage Flow 0.4 %
    Tensile Modulus 3900 MPa
    Tensile Stress At Break 80 MPa
    Tensile Strain At Break 4 %
    Flexural Modulus 3500 MPa
    Charpy Notched Impact Strength 23 C 10 kJ/m²
    Izod Notched Impact Strength 23 C 9 kJ/m²
    Hdt A 1 8 Mpa 190 °C
    Hdt B 0 45 Mpa 210 °C
    Vicat Softening Temperature 165 °C

    As an accredited SABIC VALOX™ Impact-Modified PBT 3706-1001 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC VALOX™ Impact-Modified PBT 3706-1001 is supplied in 25 kg moisture-barrier bags, palletized and shrink-wrapped for shipping.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized bags of SABIC VALOX™ 3706-1001 PBT resin, dry ambient conditions, secured for transport.
    Shipping SABIC VALOX™ Impact-Modified PBT 3706-1001 is typically shipped as dry resin pellets in sealed moisture-barrier bags or boxes, palletized and protected from humidity, heat, and contamination. It is generally not classified as dangerous goods; transport according to applicable local, national, and international regulations and supplier safety data sheets.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture absorption and contamination. Segregate from strong oxidizers. Maintain stable temperature, avoid prolonged high humidity, and follow first-in, first-out stock rotation. Use appropriate PPE and comply with local regulations.
    Shelf Life SABIC VALOX™ Impact-Modified PBT 3706-1001 typically has a 24-month shelf life when stored unopened, dry, below 50°C, and protected from sunlight.
    Application of SABIC VALOX™ Impact-Modified PBT 3706-1001

    Does 3706-1001 Retain Terminal Retention Through 1,000-Hour Underbonnet Thermal Cycling?

    Connector bodies and terminal retainers in engine-bay electrical systems require a combination of low-temperature ductility, hot oil mist resistance, and dimensional stability around press-fit brass terminals. VALOX™ 3706-1001 is selected when the connector must survive 1,000 h of thermal cycling from -40 °C to 125 °C without terminal back-out or latch fracture. The compliance boundary for engine-bay connectors is set by ISO 20860-1:2008 for dimensional and electrical interface requirements, USCAR-2 for durability and terminal retention, and UL 94 HB at 1.5 mm per the supplier Yellow Card. Formula addition ratio is 100 wt% prime VALOX™ 3706-1001; clean runner and gate regrind from the same lot is blended at a maximum of 20 wt% after granulation through a 6 mm screen. The downstream production process begins with desiccant drying at 120 °C for 4 h to a residual moisture ceiling of 0.02% by ASTM D7191, followed by injection molding on a reciprocating-screw machine with 20:1 L/D and 1,000–1,500 kN clamp force. Nozzle melt temperature is held between 245 °C and 260 °C; hot runner manifold temperature does not exceed 265 °C to limit transesterification and impact-modifier degradation. Terminal products in this tier include sealed connector bodies, terminal position assurance clips, relay socket housings, and fuse-box mounting brackets.

    Control pointSetpoint / toleranceAcceptance criterion
    Residual moisture after drying≤ 0.02%ASTM D7191
    Feed throat temperature40–60 °CNo pellet fusion
    Barrel mid-zones235–255 °CMelt thermocouple logging
    Nozzle melt temperature245–260 °C±5 °C lot audit
    Hot runner manifold≤ 265 °CDrop check after 5 min idle
    Mold surface temperature40–80 °CContact probe before shot
    Maximum full-melt residence time≤ 8 minReject if yellowness index delta > 4

    EV Charging Inlet Latch and Housing Load Paths

    In AC charging inlet and coupler production, latch release force after thermal conditioning at 85 °C and low-temperature impact after -40 °C exposure are decisive because the housing retains metallic sleeves and snap-in locking teeth. The governing standards are IEC 62196-1:2022 and IEC 62196-2:2022 for plugs and socket-outlets, SAE J1772:2021 for North American vehicle inlet geometry, and GB/T 20234.1-2023 for China-market interfaces. The formulation addition for black external charging connectors is 2 wt% carbon-black masterbatch in 98 wt% prime resin; regrind from sprues and rejected pre-assembly moldings is capped at 15 wt% because outdoor UV exposure and high-current thermal cycles amplify molecular-weight non-uniformity. Processing uses a 3-zone desiccant dryer at -30 °C dew point, 120 °C inlet temperature, and 4 h residence time, then injection molds into hot runner tools with valve gates near the latch boss; mold temperature is set between 60 °C and 80 °C to control sink at metal terminal inserts. Finished products include Type 1 and Type 2 AC charging inlet housings, charging coupler latch bodies, and temperature-sensor retaining tabs. Published data for some vehicle-specific latch geometries is limited; pre-production validation on the actual charging inlet tool is required where hot-runner shear heating raises the melt above 265 °C at the gate.

    Molding unfilled impact-modified PBT into cordless drill and impact driver battery-pack lower housings forces attention onto gate freeze time and weld-line impact strength, because a 2 m drop test onto concrete must not propagate cracks from the snap-fit engagement ribs. The relevant product-safety envelope is IEC 62841-1:2014 for hand-held motor-operated electric tools, with material flammability controlled to UL 94 HB at 1.6 mm where the pack shell is not acting as a flame barrier. Formula addition is 100 wt% prime VALOX™ 3706-1001; bulk color is introduced as 2–3 wt% pre-dried masterbatch, and clean internal regrind is limited to 15 wt% after in-line metal detection and 6 mm screening. Molding operations on 1,000–1,200 kN clamps use valve-gated multi-cavity tools with sequential opening from the gate nearest the battery cell retention rib to displace gas away from the weld plane; melt temperature is kept between 245 °C and 255 °C and maximum residence time is 7 min, because extension beyond 8 min is linked to batch-to-batch variation in impact durability. Terminal product types are cordless battery pack lower shells, charger base frames, motor end caps, and 18 V/20 V pack latch brackets. On production lines using vacuum hoppers without desiccant beds, intermittent impact failure has been traced to moisture above 0.04% before plastication.

    Espresso machine brew-unit carrier plates and pump mounting brackets are specified in impact-modified PBT where continuous contact with 60–85 °C water, citric acid descaler, and coffee oils excludes ABS/PC candidates. The controlling safety standard is IEC 60335-1:2016 together with IEC 60335-2-15:2012 for machines for preparing hot beverages. Food-contact status of the specific packaging lot must be confirmed against 21 CFR 177.1660 and EU 10/2011 documentation if regrind is excluded. Formulation addition is 100 wt% prime resin; where non-food immediate exterior parts allow internal regrind, the proportion is held to 10 wt% maximum, because the chain-length distribution after a second heat history can widen and reduce hydrolytic stability. The downstream process preheats pellets at 120 °C for 4 h and molds at 245–260 °C nozzle temperature with mold surface temperature 70–90 °C; elevated mold temperature is used to grow crystallinity at water-contact surfaces and to prevent post-molding creep at screw bosses. Terminal products are brew group carriers, drip-tray support frames, pump mounting flanges, and internal water-tank brackets. Published data for this specific grade under repeated citric acid exposure is limited; validation should include mechanical retention after 500 cycles of 85 °C water immersion with 1% citric acid descaling solution.

    When Chemical Cleaning Agents Attack Glass-Reinforced PBT Alternatives

    Where alkaline disinfectant wipedowns expose glass fibers on filled PBT surfaces, industrial process transmitter enclosures and valve position indicator covers are transferred to unfilled impact-modified VALOX™ 3706-1001. The standards governing the enclosure family are IEC 60529 for IP65/IP67 degrees of protection, NEMA 250 Type 4X for corrosion resistance, and ISO 9227:2017 neutral salt spray for exterior metallic insert validation. Formula addition for process-control housings is 100 wt% prime pellet; if RAL color coding is required, 2 wt% pre-colored masterbatch with outdoor-grade pigment is used, and no downstream impact modifier or filler is added because the resin already carries its impact modification. Production is run on 900–1,300 kN machines with a low-shear screw at compression ratio 2.2:1 and mold temperature 60–80 °C; surface texture is typically VDI 24 to 30 to mask flow lines around metal inserts. Operational boundary: the material is not specified for continuous immersion in pH 12 solutions above 80 °C, where hydrolysis at weld lines can reduce elongation below 5%; published data for this specific grade in the stated chemical solution is limited. Terminal products include proximity sensor housings, valve position indicator covers, fieldbus junction enclosures, and actuator inspection windows with overmolded gasket seats.

    Busbar Carrier Insert-Molding for Traction Battery Pack Insulation

    During cell stack assembly, low-voltage busbar carriers inside traction battery modules require a balance of dielectric strength, creepage resistance, and impact tolerance. The component class is governed by ISO 6469-1:2019 for electrically propelled road vehicles, IEC 60243-1:2013 for dielectric strength testing of solid insulating materials, and IEC 60664-1:2020 for clearances and creepage distances in low-voltage zones; the material carries UL 94 HB at 1.5 mm, so it is excluded from high-voltage barriers where V-0 or VTM-0 flame-retardant grades are mandated. Formulation is 100 wt% prime VALOX™ 3706-1001; regrind from post-industrial busbar carrier scrap is limited to 10 wt% when insulation resistance after 85 °C/85% RH conditioning must remain above 1 MΩ. Higher regrind ratios are not recommended because metallic fines from insert-loaded runners are difficult to separate. Downstream processing preheats copper busbars to 100 °C, dries resin to 0.02% moisture, and injects at 245–255 °C into a tool with 80 °C mold temperature and vacuum venting to avoid gas entrapment around the insert. Terminal products are busbar retention clips, module end-plate insulation carriers, and cell-interconnect alignment spacers for prismatic and pouch modules. Published data for this specific configuration at higher regrind ratios is limited; a screening trial at 10 wt% regrind is recommended before production release.

    Free Quote

    Competitive SABIC VALOX™ Impact-Modified PBT 3706-1001 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Designated as SABIC VALOX™ 3706-1001, the material is a semi-crystalline polybutylene terephthalate (PBT) compound modified with an elastomeric impact package. The 3706-1001 identifier denotes a non-reinforced impact-modified PBT supplied in pellet form for injection molding and specialized extrusion. Its primary differentiation from unmodified PBT is a measurable shift in low-temperature ductile failure behavior, obtained at the expense of room-temperature flexural modulus and heat deflection under load. Published manufacturer data place density at 1.31 g/cm³ by ISO 1183-1:2019. Equilibrium water absorption at 23 °C is approximately 0.4 % by ISO 62. The crystalline melting point by differential scanning calorimetry is approximately 225 °C per ISO 11357-3; the glass transition of the PBT phase is near 40–50 °C, while the elastomeric modifier introduces a sub-ambient transition that improves low-temperature toughness. The melt processing window is bounded by hydrolytic chain scission above 0.02 % moisture and by thermal degradation of the impact modifier above approximately 270 °C.

    Mechanical property data for the compound show a tensile stress at yield near 47 MPa when tested at 50 mm/min in accordance with ISO 527-2/5A/50. Tensile strain at break is typically above 100 % under the same method, which is higher than the 5–10 % break strain common for unmodified unfilled PBT. Notched Izod impact values by ISO 180/A are approximately 50 kJ/m² at 23 °C and 15 kJ/m² at -30 °C. The flexural modulus is reported near 1,900 MPa by ISO 178. These values should be treated as representative published values; lot-specific certificates of analysis govern final acceptance. In comparison, unmodified unfilled PBT typically exhibits flexural modulus near 2,500–2,800 MPa and tensile stress at yield near 55–60 MPa, but its notched Izod impact at -30 °C is often below 6 kJ/m².

    In automotive wiring-device housings and industrial enclosures, the grade is used for snap-fit closures and connector bodies where assembly occurs at subzero temperatures. Dimensional checks are normally made after conditioning at 23 °C and 50 % RH for 48 h; mold shrinkage by ISO 294-4 ranges from 0.9 % to 1.5 % depending on wall thickness and mold temperature. Flow-direction shrinkage is typically 0.9–1.2 %, while transverse shrinkage can reach 1.3–1.5 % for wall thicknesses of 2.0–3.0 mm. The material carries a UL 94 HB classification at 1.5 mm and 3.0 mm; it is not a flame-retarded grade and should not be substituted for V-0 or V-2 listed PBT products.

    What Drying and Melt-Processing Boundaries Govern Hydrolytic Stability?

    Hydrolysis is the principal process risk. Because the PBT backbone contains ester linkages, residual moisture above 0.02 % by weight accelerates molecular weight reduction, producing splay, lower nozzle melt viscosity, and loss of impact. A desiccant dryer with a dew point at or below -30 °C is required; pre-drying at 120 °C for 3–4 h is typical for sealed containers, while material exposed to ambient conditions above 60 % RH for more than 4 h is dried at 110 °C for 6–8 h. Tray ovens without a dry-air source are not recommended because the low air volume permits moisture re-absorption. The dried resin should be conveyed to the machine throat with a dry-air loader and processed within 30 min of hopper residence.

    Barrel zone setpoints on a conventional three-zone reciprocating screw are usually set at 230–240 °C in the rear, 240–250 °C in the center, and 250–260 °C at the front and nozzle. Melt temperatures above 270 °C or residence times exceeding 5 min at the high end of the range can cause the elastomeric phase to yellow and the melt to lose impact; machine heaters should be reduced or the barrel purged with a general-purpose PBT during interruptions. Mold temperature is maintained at 60–80 °C. The lower half of that range improves cycle time but can increase molded-in stress and reduce dimensional stability; the upper half improves crystallization but lengthens cycle. A screw with L/D 20:1–24:1 and compression ratio 2.5:1–3.0:1 is typical.

    On production-scale injection molding machines of 1,500–6,500 kN clamp force, the material has been run with a shot size between 25 % and 65 % of barrel capacity and a cushion of 3–6 mm. Published data for this specific configuration is limited; gate-seal time, switchover point, and hold pressure should be established by short-shot and gate-seal studies on each tool. Hot-runner systems should avoid restrictive gate diameters below 1.5 mm in thin-walled parts because excessive shear can degrade the impact modifier and reduce notched Izod energy. Peak injection pressure in typical connector tools is 70–120 MPa hydraulic, although cavity pressure is the preferred process variable. Cavity pressure at the end of fill is often held near 30–45 MPa for close-dimensional work.

    Observed process defects in production molding include splay streaks from incomplete drying, delamination at the gate from excessive shear, and gloss differences between the gate and flow front due to hot-runner thermal imbalance. These defects are corrected by lowering hot-tip temperature, increasing gate diameter, or raising mold temperature rather than by increasing melt temperature alone. Regrind addition up to 20 % by weight is typical in non-appearance parts, provided the regrind is dried and melt processed without additional thermal history. Higher regrind levels can reduce notched Izod impact at -30 °C and increase mold-fill variability. The use of recycled material should be validated by ISO 180/A impact testing at the lowest service temperature defined by the end-use application.

    Property Comparisons Against Unfilled and Glass-Filled PBT

    The difference in property profile is most visible in a comparison matrix. The table lists representative published values; they are not minimum specifications and may vary with pigmentation, regrind content, and conditioning.

    Representative published property comparison for PBT compounds
    Property and test methodVALOX™ 3706-1001 impact-modified PBTUnmodified unfilled PBT30% glass-fiber PBT
    Density (ISO 1183-1:2019)1.31 g/cm³1.31 g/cm³1.53 g/cm³
    Tensile stress at yield (ISO 527-2/5A/50)47 MPa58 MPa125 MPa
    Flexural modulus (ISO 178)1,900 MPa2,500 MPa9,500 MPa
    Notched Izod impact at 23 °C (ISO 180/A)50 kJ/m²5 kJ/m²10 kJ/m²
    Notched Izod impact at -30 °C (ISO 180/A)15 kJ/m²4 kJ/m²8 kJ/m²
    HDT/Af at 1.8 MPa (ISO 75/Af)55 °C55 °C205 °C

    Unmodified unfilled PBT offers higher flexural modulus and a sharper ductile-to-brittle transition. In snap-fit designs with insertion at -20 °C, unmodified PBT can fracture at notched Izod values below 5 kJ/m², whereas the impact-modified grade retains approximately 15 kJ/m². Glass-fiber-reinforced PBT inverts the trade: flexural modulus rises above 9,000 MPa, and HDT/Af at 1.8 MPa rises above 200 °C, but notched impact generally remains below 12 kJ/m² at 23 °C. The 3706-1001 grade is therefore selected when snap-fit insertion and impact loading govern the failure mode; glass-filled PBT is selected when creep, stiffness, and heat resistance under load govern.

    Chemical resistance data generated by ASTM D543-14 immersion show good retention of tensile strength in aliphatic hydrocarbons, mineral oils, diesel fuel, ethylene glycol, and dilute mineral acids at 23 °C. Alkaline solutions above pH 10 at 60 °C and hot concentrated sulfuric or nitric acid cause surface attack and embrittlement. The grade is not recommended for continuous immersion in hot water above 60 °C because hydrolytic degradation proceeds even without external load. Chlorinated solvents and phenols should be avoided; they may dissolve or stress-crack the part. For underhood connectors exposed to road-salt brines, occasional splash contact is acceptable, but continuous immersion under stress is not covered by standard PBT resistance data and must be validated on the component.

    Unlike PBT/PC blends, the absence of polycarbonate in 3706-1001 preserves resistance to aromatic hydrocarbon stress cracking; toluene and xylene immersion in ASTM D543-14 do not show the rapid crazing observed in many PC-containing blends. The trade is that PBT/PC blends may offer higher room-temperature notched impact in thick sections; the choice between the two depends on whether solvent exposure or ultimate impact is the dominant requirement.

    Typical electrical properties for unfilled impact-modified PBT include volume resistivity above 1E15 ohm·cm by IEC 60093 and a dielectric strength above 20 kV/mm by IEC 60243-1, but published values for this exact grade should be confirmed from the manufacturer datasheet before use in insulation applications. Regulatory status should also be verified against the latest SABIC product stewardship bulletin. Statements of compliance for RoHS 2011/65/EU and REACH (EC) No 1907/2006 are lot and region specific; the material is not presented here as a food-contact or medical-grade product.

    In electrical connector applications with wall thickness 1.0–2.5 mm, mold design should use gate widths of at least 0.8–1.0 mm and vent depths of 0.012–0.025 mm to prevent gas burn and jetting. Draft angles of 0.5–1.0° are common for textured surfaces. The grade has been used for wiring harness connectors, sensor housings, relay bases, power tool housings, and appliance handles where regulatory requirements do not demand a flame-retarded PBT. In each application, the final part must be tested to the relevant end-use standard, such as SAE J2030 for automotive connector performance or IEC 60695 for electrical flammability, because resin datasheet values alone do not establish component compliance.

    Top