| HS Code | 410618 |
| Productname | SABIC HDPE P5510 |
| Polymertype | High Density Polyethylene |
| Processingmethod | Injection Molding |
| Density | 0.954 g/cm³ |
| Meltflowrate 190c 2 16kg | 11 g/10 min |
| Tensilemodulus | 1200 MPa |
| Tensilestrengthatyield | 27 MPa |
| Tensileelongationatyield | 9 % |
| Tensileelongationatbreak | >1000 % |
| Flexuralmodulus | 1200 MPa |
| Notchedizodimpactat23c | 8 kJ/m² |
| Notchedizodimpactatminus30c | 3 kJ/m² |
| Vicatsofteningtemperature | 75 °C |
| Heatdeflectiontemperatureat0 45mpa | 70 °C |
| Brittlenesstemperature | -70 °C |
| Hardnessshored | 62 |
| Meltingtemperature | 132 °C |
| Waterabsorption | <0.01 % |
As an accredited SABIC HDPE P5510 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC HDPE P5510 is packaged in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg net per pallet. |
| Container Loading (20′ FCL) | SABIC HDPE P5510 loads in 20′ FCL containers at about 25 MT net, packed in 25 kg bags, floor-loaded. |
| Shipping | SABIC HDPE P5510 is a non-hazardous polyethylene resin supplied as pellets. It is typically shipped in 25 kg bags, jumbo bags, or bulk trucks/railcars. Store in a dry, cool area away from direct sunlight, heat, and moisture. Handle with standard PPE and keep containers sealed. Not classified as dangerous goods. |
| Storage | Store SABIC HDPE P5510 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Protect pallets from excessive stacking and UV exposure. Use first-in, first-out stock rotation. Maintain clean handling areas and avoid contact with incompatible chemicals or odorous materials. |
| Shelf Life | SABIC HDPE P5510 typically has a 24-month shelf life when stored in original packaging, dry, cool, and away from direct sunlight. |
Thin-wall dairy and spreadable-fat containers molded from SABIC HDPE P5510 at wall stocks between 0.40 mm and 0.65 mm fall under food-contact compliance clauses FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation (EU) No 10/2011, including Annex I and Annex II positive-list verification and overall migration limits below 10 mg/dm² under EN 1186-1 simulant testing. The resin itself is characterized by a nominal melt flow rate of 5.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1 and density of 0.955 g/cm³ per ISO 1183-1, which positions it for high-speed thin-wall filling without excessive injection pressure on accumulator-assisted hydraulic or hybrid machines with clamp forces between 2,500 kN and 6,500 kN. A production-validated formulation typically loads 96.5–99.0 wt% P5510 with 1.0–3.0 wt% food-grade white masterbatch—equivalent to final titanium dioxide content of 0.3–1.5 wt%—plus 0.02–0.06 wt% fluoroelastomer-based polymer processing aid, and a slip/antiblock masterbatch at 0.05–0.15 wt% when nested cups require automated de-nesting. The downstream injection process uses piston injection velocities above 250 mm/s, melt temperatures of 200–230 °C, mold temperatures of 10–35 °C, and cycle times of 4.5–8.5 s on 4- to 16-cavity hot-runner tools; tooling shrinkage allowances are commonly set at 1.5–2.5% for wall stock below 0.60 mm, though published data for P5510-specific anisotropic shrinkage is limited. Finished product types include 250–1,000 ml margarine tubs, dairy dessert cups, and spreadable cream cheese containers with tamper-evident snap lids, where low odor and taste transfer are verified by organoleptic panel testing under EN 1622 or equivalent internal methods.
Closure-specific compliance for drinking water and beverage contact includes FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011 including its subsequent amendments, and often NSF/ANSI 61 for potable water system components in North American supply chains; sensory acceptance is tested under EN 1622, while torque retention is measured on continuous-thread closures under ASTM D2063/D2063M-10(2018). In 28 mm and 30/25 mm closure compounds, P5510 is used at 94.0–97.5 wt%; color masterbatch is added at 1.5–3.0 wt%; erucamide slip is blended to a final amide concentration of 500–1,200 ppm; and an antioxidant/stabilizer masterbatch at 0.10–0.20 wt% is retained for regrind stability. Closed-loop regrind addition is limited to 20 wt% maximum and no more than three heat histories, because retained oxygen-containing species at higher regrind fractions elevate aldehyde and ketone odour thresholds during later organoleptic panels. Injection is performed on 24- to 48-cavity valve-gated hot-runner systems with melt temperatures of 210–235 °C, mold temperatures of 15–30 °C, injection pressures of 70–110 MPa, and hold pressures limited to 40–60 MPa; barrel residence times above 10 min at melt temperatures exceeding 240 °C are avoided by adjusting screw recovery to shot weight, and screw L/D ratios of 20:1 to 25:1 with compression ratios of 2.5:1 to 3.0:1 are typical. No pre-drying is required if internal moisture content is below 300 ppm, but after outdoor silo storage at relative humidity above 70% for more than 8 h, drying at 75 °C for 2 h in a desiccant dryer prevents splay and gate blush. Finished closure types include 28 mm PCO 1881 short-height still-water caps, 30/25 mm sports closures with tamper-evident bands, and single-piece 28 mm juice closures, with application torque values validated on closure equipment at 1.2–2.8 N·m depending on linerless or lined shell design.
When hypochlorite bleach or quaternary ammonium disinfectant formulations require linerless HDPE closures, stress-cracking resistance and torque retention after chemical exposure become the controlling specifications; materials are qualified under ASTM D1693-15 condition A or B with F50 values above 20 h in 10% Igepal CO-630, and closure systems for hazardous preparations are validated for child-resistant features under ISO 8317:2015 where applicable. Exposure testing at 50 °C for 48 h in 5% sodium hypochlorite solution is used as an internal stress-crack screening protocol on production closures because it reveals molded-in stress concentration at the tamper-evident bridge more severely than ambient-condition ESCR alone. The compound typically contains 96.0–98.0 wt% P5510, 1.5–3.0 wt% chemical-resistant pigment masterbatch, 500–1,000 ppm erucamide as torque-reducing slip, 0.08–0.15 wt% primary antioxidant masterbatch, and re-grind at 0–15 wt% only from closed-loop internal systems to avoid contamination by washer fluids or label adhesives. Production is carried out on 16- to 32-cavity cold-runner or hot-runner injection tools with melt temperatures of 210–235 °C, mold temperatures of 20–40 °C, back pressures of 0.5–1.5 MPa, and screw L/D ratios of 20:1 to 25:1; static decompression after plasticisation is limited because moisture uptake in outdoor silo storage can produce intermittent splay when barrel residence time exceeds 6 min. Terminal products include 28/410 and 38/400 detergent and bleach closures, drain cleaner closures, and child-resistant bottle adapters, where dimensional stability of the tamper-evident bridge is measured after 24 h at 40 °C per internal retention protocols.
Personal care jar closures and deodorant overcaps produced from P5510 must satisfy packaging safety obligations under Regulation (EC) No 1223/2009 for cosmetic article safety and REACH Annex XVII restrictions for phthalates and polycyclic aromatic hydrocarbons; where the closure contacts alcohol-based formulations, compatibility testing at 40 °C for 14 days in 50% ethanol is used as an internal extractable-shift screen aligned with the safety assessment requirements of Annex I to the Cosmetics Regulation. Formulation uses 95.5–98.0 wt% P5510, 1.5–3.5 wt% pre-dispersed pigment masterbatch, 0.05–0.20 wt% silicone-based friction modifier for consistent ejection from polished cavities, and 0.02–0.05 wt% fluoroelastomer processing aid to reduce melt fracture in thin hinge sections and narrow flow channels. Molding is executed on 32- to 64-cavity hot-runner platforms with melt temperatures of 200–230 °C, mold temperatures of 20–50 °C, injection speeds of 120–250 mm/s, and holding pressures of 35–55 MPa; cavity-to-cavity fill imbalance is held below 2% shot-weight variation by using rheologically balanced runner layouts, because unbalanced filling causes hinge-section warpage that is visible on high-gloss outer surfaces after lacquering or metallization. Terminal products include 15-ml to 50-ml cream jar lids, 30/25 mm serum bottle caps, and deodorant stick overcaps, where downstream decoration via pad printing or hot stamping requires surface tension above 38 mN/m after corona treatment.
Thin-wall industrial packaging molded from P5510 finds application where the chemical environment is a water-based lubricant additive, adhesive component, or non-solvent cleaner, but drop-impact requirements at wall thickness below 0.80 mm remain a process-defined boundary; published data for this specific configuration is limited, and each tool design is validated against ASTM D5276-19 or ISO 2248:1985 drop tests at customer-defined fill weights and temperature conditions. The compound usually combines 90.0–97.0 wt% P5510 with 3.0–10.0 wt% LLDPE or LDPE as impact modifier, 1.0–2.5 wt% compatible masterbatch, and 0.02–0.05 wt% polymer processing aid; for UN-certified dangerous goods packagings under ADR/RID Chapter 6.1, the formulation is fixed and re-qualification is required after any additive change above 0.1 wt%. Processing uses high-flow thin-wall injection molding machines with clamp forces of 3,500–8,000 kN, melt temperatures of 200–230 °C, mold temperatures of 10–30 °C, and injection velocities above 300 mm/s to avoid premature freeze-off in ribs and snap-fit undercuts; mold breathing is set below 0.10 mm to prevent flash at the parting line in multi-cavity layouts. Terminal product types include 0.5–5 L thin-wall industrial containers, lubricant additive bottles, and water-based adhesive buckets with closure lugs, where the polymer formulation is not recommended for aromatic or chlorinated solvent contact without mandatory barrier-layer insertion.
Competitive SABIC HDPE P5510 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC HDPE P5510 is a high-density polyethylene injection moulding grade. The numeric designation maps to a nominal density of 0.955 g/cm³ and a nominal melt flow rate of 10 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg. Density is determined according to ISO 1183-1:2019. The grade is supplied for rigid packaging, crates, trays, closures, and thin-walled industrial components in which injection pressure, cycle time, stacking stiffness, and dimensional stability control part cost.
The product is not a blow moulding or film extrusion grade. Melt strength is lower than high-molecular-weight HDPE used in extrusion blow moulding, and the high flow rate is intended for complex-flow-length injection moulding tooling. The material is typically processed on reciprocating-screw injection moulding machines with general-purpose polyolefin screws rather than on extrusion lines.
Blow moulding HDPE grades normally exhibit a melt flow rate below 1 g/10 min under ISO 1133-1:2022 and often use broad or bimodal molecular weight distributions to generate parison stability. P5510, at 10 g/10 min, has a substantially lower low-shear viscosity. This difference reduces injection pressure and clamp-force demand in multi-cavity tooling; for a projected part area of 0.1 m2, the lower viscosity can permit filling on a 120-ton clamp machine where a 1 g/10 min blow moulding grade may short-shot under the same runner geometry. The same molecular structure reduces melt strength and environmental stress crack resistance, so P5510 cannot be substituted into extrusion blow moulding tooling without parison die and accumulator programme changes.
At a density of 0.955 g/cm³, crystallinity is higher than in HDPE grades with density in the 0.940–0.950 g/cm³ range. Flexural modulus measured under ISO 178:2019 is therefore elevated, typically in the range of 1,200–1,400 MPa for this density class. The higher stiffness allows side-wall thickness reductions of approximately 10–15% compared with a 0.945 g/cm³ HDPE grade while maintaining top-load performance, provided the design is validated with finite-element analysis using the actual tensile stress–strain curve under ISO 527-2:2012.
In closure and crate applications, the grade fills thin sections at lower hydraulic pressure than blow moulding HDPE, but the reduction in entanglement density also means that aggressive surfactant contact can produce environmental stress cracking earlier than in a bimodal blow moulding grade. If ESCR is a release criterion, the relevant test for blow moulding grades, ASTM D1693-15, is not always reported for injection moulding grades; a comparative test against a reference material in the intended chemical environment should be conducted.
Representative datasheet values for SABIC HDPE P5510, as typically reported for an unfilled injection moulding HDPE of this density and flow class, are listed in the following table. The table is not a certificate of analysis; lot-specific release values should be obtained from the supplier.
| Property | Standard | Unit | Value |
| Density | ISO 1183-1:2019 | kg/m³ | 955 |
| Melt flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 | g/10 min | 10 |
| Tensile yield stress | ISO 527-2/1B/50 | MPa | 28 |
| Elongation at break | ISO 527-2/1B/50 | % | >200 |
| Flexural modulus | ISO 178:2019 | MPa | 1,200 |
| Notched Izod impact strength at 23 °C | ISO 180/A:2023 | kJ/m2 | 4 |
| Vicat softening temperature A50 | ISO 306:2022 | °C | 127 |
| Hardness Shore D | ISO 868:2003 | — | 62 |
These values reflect the high crystallinity associated with 0.955 g/cm³ density. The Vicat softening temperature of approximately 127 °C under ISO 306:2022 method A50 indicates short-term non-load-bearing contact should remain below that threshold. Continuous load-bearing service above 80 °C is not recommended for unfilled HDPE unless creep is calculated into the design.
Density measurements are influenced by pigment and masterbatch addition. A colour masterbatch level of 2 wt% can shift density by 0.002–0.005 g/cm³, altering part weight and stiffness. Converters should re-measure density when masterbatch loading changes, using a density gradient column or gas pycnometry after conditioning at 23 °C and 50% RH.
Thin-wall conversion of P5510 requires a controlled thermal profile. Barrel settings typically begin with a feed throat at 40–60 °C, a compression zone at 180–220 °C, a metering zone at 220–250 °C, and a nozzle at 230–260 °C. Mould temperature is commonly held between 20 °C and 40 °C to balance solidification rate against part warpage. At wall thicknesses below 2 mm, injection speed should be high enough to avoid premature freeze-off, with fill times between 0.1 s and 0.5 s for flow lengths below 150 mm. Published data for this specific configuration is limited for flow lengths above 150 mm, so mould-filling simulation using a measured viscosity curve is required.
At a melt flow rate of 10 g/10 min, the apparent melt viscosity at a shear rate of 100 s-1 and 220 °C is approximately 300–600 Pa·s for HDPE of this density class. The activation energy for flow is typically 25–29 kJ/mol; a barrel temperature increase from 220 °C to 250 °C therefore reduces viscosity by roughly 20–30%. Mould-filling simulation should use Cross or Bird-Carreau parameters rather than a single melt flow rate because the melt flow rate is measured at low shear and does not capture high-shear shear-thinning behaviour.
Cooling time scales with the square of wall thickness. For a 3 mm wall, a mould temperature of 30 °C and a melt temperature of 230 °C typically require a cooling time of 10–15 s for HDPE, although exact values depend on part geometry and cooling-channel placement. Conformal cooling can reduce this to 8–12 s but requires tooling investment. Crystallization shrinkage for HDPE of density 0.955 g/cm³ is approximately 1.5–2.5% in the flow direction and 2.0–3.0% in the transverse direction. Tooling dimensions must be corrected using a direction-dependent linear shrinkage factor, not a single global factor.
Observed production-line failure modes include splay when pellet surface moisture is present. Although HDPE is not hygroscopic, condensation formed during cold-powder transfer in unheated hoppers at relative humidity above 70% can produce visible splay. A short hopper-dryer cycle at 70 °C for 2 h removes surface water without thermal softening. Warpage occurs when mould temperature exceeds 50 °C in parts with section transitions greater than 3:1. Short shots result when nozzle temperature falls below 220 °C or when the non-return valve leaks due to wear; a ring non-return valve clearance greater than 0.15 mm may be sufficient to cause inconsistent shot size.
Mould temperature is a direct control variable for shrinkage and warpage. Mould temperatures below 20 °C reduce cycle time but increase frozen-in orientation, causing anisotropic shrinkage and post-mould dimensional drift. Mould temperatures above 40 °C improve stress relaxation and reduce warpage but increase cycle time and can cause sticking if the draft angle is below 0.5°. Ejection force is influenced by surface roughness; a polished core with surface roughness Ra below 0.4 µm allows lower draft, but textured cavity surfaces may increase ejection force by 15–30% compared with smooth tooling.
Compared with higher-flow HDPE injection grades above 20 g/10 min, P5510 retains a higher molecular weight fraction that improves notched impact strength and top-load retention. Compared with P5510, a 20 g/10 min grade fills longer flow paths at lower pressure but exhibits lower stress crack resistance and reduced low-temperature impact. In tooling with wall thickness below 1 mm, the higher-flow grade may be required; in structural crates with wall sections from 2 mm to 5 mm, P5510 provides a balance between flow and stiffness. Published data for this specific configuration is limited for exact quantitative comparisons across all grades; converter trials are required.
The base HDPE polymer is typically assessed under EU Regulation 10/2011 as amended for plastic food-contact materials and under FDA 21 CFR 177.1520 for olefin polymers. Compliance does not extend automatically to the final packaging article; colourants, masterbatches, recycled content, and processing aids introduced by the converter must be evaluated for migration limits. For non-food industrial packaging, the grade is normally outside the scope of specific substance restrictions under RoHS Directive 2011/65/EU when no intentionally added cadmium, lead, mercury, or hexavalent chromium is present.
Additive packages in P5510 include a stabilizer system to protect the polymer during melt processing and long-term oxidative ageing. The grade should not be blended with peroxides or pro-oxidant additives unless a controlled degradation step is expressly required, because uncontrolled lowering of molecular weight will shift the melt flow rate above 10 g/10 min and degrade impact. The material is not intended for outdoor exposure without a UV stabilizer package; if used in exterior crates, a UV stabilizer masterbatch should be added at the press at levels specified by the masterbatch supplier and verified by accelerated weathering under ISO 4892-2:2021.
In pallet and crate conversion, P5510 is processed with hot or cold runner systems. With a cold runner, sprue and runner regrind can be re-introduced at up to 20 wt% without substantial shift in density, provided the regrind is dry and contaminant-free. Above 20 wt% regrind, flow may vary due to molecular weight reduction from repeated extrusion; the melt flow rate should be re-measured under ISO 1133-1:2022 before adjusting hold pressure. For rigid industrial packaging, sink marks at bosses and ribs are controlled by gas counterpressure or by increasing pack pressure within the machine’s maximum hydraulic limit rather than by lowering mould temperature below 20 °C.
In applications requiring aggressive surfactant contact, P5510 is generally not selected without fluorination or multi-layer coextrusion because the high crystal content and low entanglement density reduce environmental stress crack resistance. Converters must not interpret the absence of a published ESCR value as suitability. If ESCR is a control criterion, a comparative test against a reference grade should be conducted in the intended chemical environment.