Sabic Hdpe M40053s

SABIC HDPE M40053S

    • Product Name: SABIC HDPE M40053S
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 578742
    Product Name SABIC HDPE M40053S
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.953 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.4 g/10 min
    Melt Flow Rate 190 C 21 6 Kg 10 g/10 min
    Tensile Strength At Yield 25 MPa
    Tensile Elongation At Break >600%
    Tensile Modulus 1200 MPa
    Flexural Modulus 1100 MPa
    Izod Notched Impact Strength 23 C 20 kJ/m²
    Izod Notched Impact Strength 30 C 8 kJ/m²
    Shore D Hardness 64
    Vicat Softening Temperature 125 °C
    Melting Temperature 130 °C
    Deflection Temperature At 0 46 Mpa 75 °C
    Thermal Expansion 1.5E-4 /°C
    Environmental Stress Cracking Resistance Escr >1000 h
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Dissipation Factor 0.0002
    Volume Resistivity >1E15 ohm·cm
    Uv Stabilization Yes

    As an accredited SABIC HDPE M40053S factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC HDPE M40053S is supplied in 25 kg polyethylene bags, typically palletized, with optional 1,000 kg jumbo bags.
    Container Loading (20′ FCL) SABIC HDPE M40053S is loaded in 20′ FCL containers as palletized 25 kg bags, typically 20–22 metric tons per container.
    Shipping SABIC HDPE M40053S is shipped as non-hazardous, free-flowing polyethylene pellets in 25 kg bags, octabins, or bulk containers. Transport in clean, dry trucks or railcars. Protect from moisture, contamination, direct sunlight, and excessive heat; store in a cool, dry, ventilated area. No special hazardous-materials handling required. Standard freight regulations apply.
    Storage Store SABIC HDPE M40053S in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Use pallets off the floor, avoid excessive stacking, and follow first-in, first-out rotation. Protect from prolonged UV exposure and maintain normal ambient temperatures. Refer to SDS for detailed guidance.
    Shelf Life SABIC HDPE M40053S shelf life: two years from production date when stored unopened in original packaging, dry, cool, away from direct sunlight.
    Application of SABIC HDPE M40053S

    In high-cavitation injection moulds for 28 mm tamper-evident beverage closures, process stability is governed by the interaction between the narrow molecular weight distribution of SABIC HDPE M40053S and the cooling channel layout. The grade is typically processed at a nozzle set temperature of 220–250°C, with an injection velocity profile that fills the cap shell within 0.2–0.4 s and a switch-over point from velocity control to pressure control set at 95–98% of the screw stroke. Cavity packing pressure in the range of 60–80 MPa is maintained for 0.5–1.2 s, after which the gate freezes and the part enters the cooling phase. Melt flow rate measured according to ISO 1133-1:2022 at 190°C/2.16 kg is reported as 4.0 g/10 min on the product datasheet, a value that permits flow length-to-wall-thickness ratios above 120:1 in closure walls of 0.8–1.2 mm. Cooling water at 8–14°C is directed through bubblers in the core pins to maintain the core steel surface below 25°C; this prevents sink opposite the sealing bead and limits diametric shrinkage after demoulding. Cycle times in production tools with 32–64 cavities are normally constrained by the cooling of the sealing ring, and recorded values for cap shells of 1.0 mm nominal wall thickness fall between 5 s and 9 s, though published data for this specific configuration is limited. Screws with an L/D ratio of 20:1 to 24:1 and a barrier flight design provide sufficient melt homogeneity without excessive shear heating; melt residence time should not exceed 5 min at temperatures below 250°C because thermal oxidation above 280°C initiates chain scission and generates off-odour compounds. Material handling requires no pre-drying unless the granulate has been stored opened under ambient humidity for more than 6 months or surface condensation is visible; HDPE is not hygroscopic, but moisture on pellet surfaces can create streaking on the gate lands. The grade is formulated without intentionally added slip or antistatic packages according to the manufacturer’s technical data sheet, so external lubrication of the mould and post-mould surface treatment may be required for high-speed cap sorting.

    What Mould Cooling Parameters Control Warpage in Thin-Wall Dairy Containers?

    For injection moulded round dairy cups with rim diameters of 70–95 mm and wall thickness between 0.5 mm and 1.2 mm, SABIC HDPE M40053S is processed against a lower melt temperature boundary of 200°C and an upper boundary of 240°C to avoid pressure-limited filling in long flow paths. The critical warpage mechanism in these parts is differential shrinkage between the highly oriented gate area and the slower-cooled sidewall; mould temperature mapping therefore specifies separate cooling zones: gate-side inserts are held at 10–15°C, sidewall channels at 20–25°C, and rim channels at 8–12°C. The difference in surface temperature across the cavity must not exceed 5 K at the time of ejection, because asymmetric crystallisation produces a radial bow that exceeds 1.5 mm on a 95 mm diameter rim. Packing pressure is applied for 1.0–2.0 s with a specific packing pressure of 40–60 MPa on the melt, followed by holding at 20–30 MPa to control sink at the rim stacking ledge. Mould filling uses a central sprue with a hot runner or a three-plate cold runner with pinpoint gates; the selected gate diameter of 0.8–1.0 mm must be below the wall thickness to limit gate vestige height. Ejection must occur only after the core surface temperature has fallen below 50°C; ejection at higher temperatures leads to rim ovality outside the ±0.5 mm tolerance required by cup sealing equipment. SABIC HDPE M40053S has a density reported as 954 kg/m³, and typical notched Charpy impact strength values for high-flow HDPE injection grades in this density class fall between 4 kJ/m² and 7 kJ/m², but the certificate of analysis for the supplied lot must be consulted for the exact value. Food contact conformity is verified under Regulation (EU) No 10/2011, including overall migration testing in 10% ethanol, 3% acetic acid, and 20% ethanol simulants, and under FDA 21 CFR 177.1520 for olefin polymers in contact with aqueous and acidic foods up to Condition of Use B. The processor must control odour and taste carryover by purging with a high-viscosity polypropylene after colour changes and by limiting melt residence time to 4 min; aldhehyde formation from oxidised high-density polyethylene can create off-odour carryover, and sensory panel evaluation under ISO 13302:2018 is used to confirm headspace quality, though published data for this specific configuration is limited.

    Compliance matrix for SABIC HDPE M40053S in injection-moulded food-contact articles
    Regulation/StandardDesignationTest conditionCriterion
    FDA 21 CFR177.1520Distilled water, 10% ethanol, 3% acetic acid, 20% ethanol simulants; Conditions of Use B through H as applicableMaximum extractable fraction as specified in 177.1520(c); no migration of residual monomers above threshold
    EU Regulation(EU) No 10/2011Food simulants A, B, C, D1; OM1 through OM7 as applicableOverall migration < 10 mg/dm²
    REACHRegulation (EC) No 1907/2006SVHC screening, Annex XVII restrictionsNo SVHC above 0.1 wt% in the article
    RoHSDirective 2011/65/EUXRF screening, IEC 62321-5:2013Cd < 100 mg/kg, Pb < 1000 mg/kg, Hg < 1000 mg/kg, Cr(VI) < 1000 mg/kg
    China GB food contactGB 4806.7-2016Aqueous, acidic, alcoholic simulants; total migration testTotal migration < 10 mg/dm² or 60 mg/kg depending on article shape

    Where storage boxes, totes, and household articles are injection moulded on hydraulic machines with clamp forces between 1,500 kN and 5,000 kN, SABIC HDPE M40053S is selected for stiffness and environmental stress-crack resistance rather than low-temperature impact. Wall stock is typically 1.8–3.0 mm, melt temperature is maintained at 210–240°C, and gate land thickness is limited to 0.6–0.8 mm to keep flatness within 1 mm per 100 mm of span. Mould shrinkage values of 1.8–2.2% in the flow direction and 1.5–1.8% across flow, determined under ISO 294-4:2018, are used in cavity dimensioning, with draft angles of 1.5–2.0° on stacking ribs. The material is not suited to high-frequency living hinges; flexural fatigue validation is required and published data for this specific configuration is limited. Environmental stress cracking resistance under ASTM D1693-15a, Condition B exceeds 10 h in 100% Igepal CO-630 at 50°C, but masterbatch carriers above 2 wt% can degrade ESCR. The processor should avoid exposing moulded articles to aromatic solvents or oxidising chemicals at temperatures above 23°C because these agents accelerate environmental stress cracking in household end-use conditions.

    When Impact Loading at Low Temperature Governs Crate Wall Thickness

    Industrial crates and logistics totes moulded from SABIC HDPE M40053S are typically used at temperatures as low as -20°C in cold-chain distribution, which shifts the design criterion from static stiffness to notched impact resistance. In side-wall sections of 2.5–3.5 mm, the material retains sufficient Charpy impact strength under ISO 179-1/1eA at -20°C, but the transition to brittle failure is strongly influenced by injection speed and weld-line geometry. On production lines, the processing window is set at a melt temperature of 230–250°C and an injection velocity that fills the cavity in 1.5–2.5 s; slower injection produces cold weld lines at the junction of the grid wall and the solid rim and may reduce low-temperature impact strength significantly, with production trials on similar high-flow HDPE grades showing losses exceeding 25%, though data for this specific grade should be confirmed. The tooling design for crates uses multiple pin gates arranged symmetrically around the base centre to avoid a single long flow path; when a single sprue gate is used, the continuous-flow length exceeds 600 mm and the melt front temperature falls below 190°C at the far rim, creating a weak boundary layer. Wall thickness is usually not reduced below 2.5 mm for open-mesh crates because the notch sensitivity of the intersection between vertical and horizontal ribs increases below this value, and ejector pin marks must be positioned on thicker ribs to avoid forming local stress concentrators. The mould shrinkage allowance for unfilled HDPE crates is set at 1.8–2.3% in the flow direction and 1.6–2.0% in the transverse direction, with additional compensation for the rim where effective cooling time is longer. Industrial crates are often tested according to ISO 8611-1:2011 for pallet and crate top-load performance; top-load capacity at 40°C is lower than at 23°C due to reduced creep modulus, and the specific derating factor must be established by ISO 899-2:2003 testing. The material is not suitable for heavy-duty pallets with unsupported racking spans above 800 mm; published data for this specific configuration is limited. The processor should avoid adding regrind above 20 wt% because repeated heat history reduces the notched Charpy impact strength at -20°C by increasing the crystalline fraction and removing low-molecular-weight fractions that act as internal plasticisers. In addition, the use of post-consumer recycled blending stock must be validated against REACH Annex XVII restrictions and the end-user's food-contact requirements if crates are used in direct food transport.

    Open-Top Industrial Pail Moulding with Conical Wall Draft

    Open-top pails of 10–25 L capacity are injection moulded from SABIC HDPE M40053S with a nominal sidewall thickness of 2.0–3.0 mm and a draft angle of 1.0–1.5° per side to allow high-speed demoulding. The gate is usually a direct sprue into the base centre or a film gate at the rim, and the filling phase uses a profiled velocity of 60–90 mm/s screw speed with a switch-over at 98% fill volume. Because the pail base is thicker than the sidewall to meet drop height requirements, a packing pressure of 50–70 MPa is held for 3–5 s to prevent vacuum voids at the base-to-wall transition. Mould cooling is set to 10–15°C in the base core and 20–25°C in the sidewall channels, producing a cycle time between 18 s and 25 s for a 10 L pail on a 4,000 kN injection moulding machine. The pail's stacking interface, moulded as an external rim and an internal ledge, is the critical dimensional feature; radial shrinkage of the rim after ejection must be compensated by a cavity diameter allowance of 1.8–2.2%, and any ovality above 1.5 mm results in unstable stacking and lid sealing failure. For UN-certified dangerous goods packaging, the design must pass a drop test from 1.2 m at -18°C after conditioning in accordance with ADR 6.1.5.3; SABIC HDPE M40053S can meet this requirement in pails of up to 20 L only when the wall thickness is not reduced below 2.5 mm and the base corner radius is at least 5 mm. The material is not suitable for open-top pails used with oxidising substances above 50°C or for prolonged exposure to aromatic hydrocarbons, which cause environmental stress cracking around the sidewall gate area. Processors should avoid adding excessive external mould release agents because residue accumulates on the sealing rim and interferes with induction sealing of foil laminates; if release is required, silicone-free stearate-based agents are used at a dilution below 0.5%.

    In non-implantable medical device housings and personal care component carriers, SABIC HDPE M40053S is used only where the part is not subjected to repeated steam sterilisation above 100°C, because heat deflection temperature under ISO 75-2/B is below 80°C and the material distorts under autoclave loads. The melt temperature in these tools is held at 200–230°C and the mould surface at 10–20°C; gate diameter is kept at 0.6–0.9 mm to prevent gloss variation on textured surfaces. Cytotoxicity, sensitisation, and irritation are evaluated on the final article according to ISO 10993-5:2009, ISO 10993-10:2010, and ISO 10993-23:2021. The grade is not recommended for components exposed to alcohol-based formulations above 30% ethanol because environmental stress cracking may occur at the gate; published data for this specific configuration is limited.

    Free Quote

    Competitive SABIC HDPE M40053S prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC® HDPE M40053S is a medium-flow high-density polyethylene injection-molding grade. The material is specified with a nominal melt flow rate of 4.0 g/10 min at 190°C/2.16 kg according to ISO 1133-1 and a nominal density of 0.953 g/cm³ according to ISO 1183-1. The grade is used in rigid packaging, closures, overcaps, crates, pails, housewares, and industrial containers where a balance of melt processability, impact strength, and moderate stiffness is required. Compared with higher-density HDPE injection grades, M40053S provides lower flexural modulus but generally better stress-crack tolerance and notched impact behaviour. Compared with higher-flow HDPE grades, M40053S requires higher injection pressure for thin-wall parts and is less suitable for wall sections below approximately 0.8 mm.

    Nominal Physical and Rheological Specification Profile

    The following nominal values are drawn from published manufacturer data for SABIC HDPE M40053S. They are not to be interpreted as lot-to-lot specification limits, and compliance for a particular production batch must be confirmed against the applicable technical datasheet.

    PropertyTest standardNominal valueUnit
    Melt flow rateISO 1133-14.0g/10 min
    DensityISO 1183-10.953g/cm³
    Tensile yield stressISO 527-226MPa
    Tensile modulusISO 527-21150MPa
    Flexural modulusISO 1781250MPa
    Charpy notched impact, 23°CISO 179-1/1eA6.0kJ/m²
    Vicat softening point, A120ISO 306127°C
    HardnessISO 86862Shore D

    The melt flow rate of 4.0 g/10 min places M40053S in the medium-flow injection-molding window. The density of 0.953 g/cm³ is at the lower end of the high-density polyethylene range. This lower density reduces flexural modulus and top-load resistance compared with 0.960–0.964 g/cm³ grades, but it contributes to improved notched impact and environmental stress crack resistance in non-aggressive service fluids. The Vicat softening point of 127°C indicates that continuous load-bearing service should remain well below 70°C unless creep data for the specific application support a higher temperature.

    Processing on conventional injection molding equipment is carried out with a three-zone general-purpose screw having an L/D ratio of 20:1–25:1 and a compression ratio of 2.5:1–3.0:1. The melt temperature measured at the nozzle is normally 210–250°C, with a mould temperature of 20–40°C. Lower mould temperatures reduce cycle time but increase frozen-in orientation and post-mould shrinkage anisotropy. Drying is not normally required when the packaging is intact. If surface moisture is present after condensation in cold silos or exposure to relative humidity above 60%, a desiccant dryer at 80°C for 2–3 h is used. Back pressure should be maintained at 0.5–1.5 MPa to avoid excessive shear heating. For screw diameters of 25–60 mm, screw rotation speed should not exceed 100 rpm, because high shear can generate local melt temperatures above the recommended upper limit and cause yellowing or molecular weight loss. Required clamp force can be estimated from projected area and cavity pressure; for a cavity pressure of 30–40 MPa, the clamp requirement is approximately 0.3–0.4 tonnes per cm² of projected area.

    What Limits Closure Dimensional Stability at High Cavitation Counts?

    In closure applications, dimensional stability is controlled by shrinkage, part-weight repeatability, gate sealing, and flow balance. Semicrystalline HDPE such as M40053S exhibits post-mould shrinkage generally in the range of 1.5–2.5% in the flow direction and 1.0–2.0% transverse to flow, depending on packing pressure, mould temperature, and gate geometry. With valve-gated hot runners, a hydraulic holding pressure of 40–60 MPa or 60–80% of peak injection pressure is commonly required to keep part mass within ±0.5% across cavities. Cavitation counts above 32 require carefully balanced melt delivery because manifold shear-induced temperature differences above 5°C can produce preferential shrinkage and warpage.

    Top-load resistance of closures is frequently evaluated under ASTM D2659-16, a standard test for column crush resistance of plastic containers. Because M40053S has a lower flexural modulus than higher-density HDPE grades, closure top-load strength at equal wall section is lower. Design compensation may require increasing wall thickness by 0.1–0.2 mm or adding gussets to tamper-evident bands. Gate design also influences closure performance: a sharp gate freeze-off threshold below the holding-pressure time produces sink marks and higher part-weight variation. Published data for this specific configuration in high-cavitation closure tools is limited; mould-filling simulation is recommended to map pressure drop, weld-line location, and shrinkage across the manifold.

    When Environmental Stress Crack Resistance Determines Additive Selection

    Environmental stress crack resistance of HDPE is evaluated under ASTM D1693 or ISO 22088-3, typically using a notched bent-strip method in 10% Igepal CO-630 solution at 50°C. M40053S, with lower density and a higher molecular-weight fraction than high-flow injection grades, provides better stress-crack resistance in slow-cooling or non-aggressive surfactant environments. However, HDPE is not resistant to strong oxidizers, chlorinated solvents, or aromatic hydrocarbons. Prolonged contact with these media can cause swelling, stress cracking, or chemical attack. Additive selection must avoid amine-based processing aids where full food-contact compliance under Commission Regulation (EU) No 10/2011 is required, as migration of low-molecular-weight amine components may exceed specific migration limits. For service involving oxygenated alcohols above 40°C, ESCR should be measured on moulded parts rather than compression-moulded plaques, because weld lines and frozen-in orientation reduce failure time compared with plaque data.

    Comparing Medium-Flow M40053S Against High-Flow Injection Grades

    Compared with SABIC HDPE M80064S, a higher-flow HDPE with nominal density of 0.964 g/cm³ and melt flow rate of 8.0 g/10 min, M40053S has a melt flow rate lower by 4 g/10 min and density lower by 0.011 g/cm³. The practical consequences are twofold. For the same cavity fill time, M40053S requires higher injection pressure or a thicker wall, which increases clamp force demand and may lengthen cycle time. The lower density also produces lower flexural modulus by approximately 15–20%. Therefore, structural parts designed for M80064S should not be converted to M40053S without reevaluating stiffness, top-load, and creep. Conversely, M40053S may provide better notched impact and stress-crack resistance than the higher-density grade, making it more suitable for closures with thick tamper bands or industrial containers subjected to drop impact at 0–5°C.

    For ultra-thin-wall packaging below 0.8 mm, a high-flow grade such as SABIC HDPE M200056 with nominal melt flow rate of 20 g/10 min is preferred because M40053S may not fill consistently at conventional injection velocities. The difference in melt flow rate is not merely a cycle-time variable; at equivalent wall thickness, the lower-flow material generates higher shear stress and greater pressure loss, which can push the process toward short-shot conditions in thin sections. Published data for this specific configuration is limited.

    Thermal Oxidation and Moisture Establish the Upper Processing Limits

    The upper melt temperature for M40053S is limited by thermo-oxidative degradation. At nozzle temperatures above 250°C, prolonged residence in hot-runner channels can cause chain scission, viscosity reduction, and generation of carbonyl groups, leading to off-taste and odour in sensitive packaging. The maximum recommended melt temperature is 250°C, with short-term excursions to 270°C permitted for start-up purging only if residence time is less than 5 min. If machine stoppages exceed 10 min, barrel temperatures should be reduced to 150–180°C or the machine purged with a higher-melt-stability HDPE. Moisture is rarely a process issue, but pellets stored in unheated silos at below 5°C can develop surface condensation above 0.05% moisture; this may produce splay or bubbles in thick sections. Drying at 80°C for 2–3 h is used in such cases.

    SABIC may provide compliance documentation for food-contact use under 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011, but the grade should be validated for each end use with respect to migration, organoleptic, and sensory performance. For non-food industrial applications, compliance with REACH and RoHS Directive 2011/65/EU is typically stated on the regulatory datasheet. The material is not intended for medical implants or prolonged skin contact without separate biocompatibility assessment. For outdoor service, a UV-stabilized variant or addition of 2–3% carbon black masterbatch is required because natural HDPE embrittles under extended UV exposure according to ISO 4892-2. Avoid processing at melt temperatures above the stated limit and avoid blending with incompatible amine-based additives unless the final article is fully reassessed for food-contact migration and colour stability.

    Top