| HS Code | 156128 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate Mfr 190 C 2 16 Kg | 30 g/10 min |
| Tensile Modulus | 1100 MPa |
| Tensile Stress At Yield | 27 MPa |
| Tensile Strain At Break | 100% |
| Flexural Modulus | 1200 MPa |
| Charpy Notched Impact Strength 23 C | 4 kJ/m² |
| Notched Izod Impact Strength 23 C | 40 J/m |
| Vicat Softening Temperature | 124 °C |
| Heat Deflection Temperature 0 45 Mpa | 75 °C |
| Shore D Hardness | 60 |
| Mold Shrinkage | 1.5% |
| Water Absorption | <0.01% |
As an accredited SABIC HDPE M300054 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SABIC HDPE M300054 packaging: 25 kg polyethylene bags, 55 bags per pallet, total 1,375 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading for SABIC HDPE M300054: 25 kg bags, palletized, shrink-wrapped, strapped; approx. 18–20 MT net per container. |
| Shipping | SABIC HDPE M300054 is a non-hazardous polyethylene resin. It is typically shipped in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Keep containers dry, clean, and protected from heat, moisture, and direct sunlight. No special dangerous goods labeling is required. |
| Storage | Store SABIC HDPE M300054 in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Use FIFO rotation; spilled pellets are slippery. |
| Shelf Life | SABIC HDPE M300054 has a two-year shelf life when stored sealed in a cool, dry place, away from direct sunlight. |
At a melt flow rate of 30 g/10 min when tested to ISO 1133-1:2022 at 190°C under 2.16 kg and a density of 0.954 g/cm³ under ISO 1183-1:2019, SABIC HDPE M300054 enters thin-wall food packaging tooling as a high-flow injection grade with measurable processing advantages on sidewalls between 0.45 mm and 0.8 mm. Materials intended for dairy spread tubs, frozen dessert cups, and snack containers require compliance with FDA 21 CFR 177.1520(c) 1.1 and EU Regulation 10/2011/EC as amended by EU 2020/1245, including overall migration below 10 mg/dm² under the intended time-temperature condition and use of colorants listed in Annex I of the EU positive list. A typical dry blend formulation for opaque rigid containers comprises 2.5–3.5 wt% titanium dioxide masterbatch at 60% pigment loading in an LLDPE carrier, 0.03–0.06 wt% fluoropolymer processing aid for shear-induced wall slip, and 0.05–0.1 wt% silicone-based mold release when ejection force on a 16-cavity stack tool exceeds 15 kN. Production-scale high-speed accumulator injection molding is performed with a barrier screw at L/D 25:1 and compression ratio 2.2:1, with barrel zones profiled from 200°C near the feed throat to 230°C at the nozzle, mold temperature held at 8–18°C, injection speed set at 180–250 mm/s, holding pressure applied at 35–55 MPa for 0.6–1.2 s, and total cycle time controlled at 3.8–5.5 s in 4+4 stack tooling with valve-gated hot runners. Finished product types include 250–500 ml dairy spread tubs, 100–200 ml frozen dessert cups, 0.5–0.7 mm sidewall lids, and shallow snack food containers where sustained hot fill above 80°C is not required because the heat deflection temperature under 0.45 MPa is near 70°C in ISO 75-2:2013; for retort or hot-fill lines, polypropylene should be selected instead.
Beverage and dairy closures molded in 28 mm PCO 1881 neck finishes use the high flow of M300054 to fill high-cavitation tooling with reduced pressure drop, but the lower molecular weight of this grade imposes measurable limits on environmental stress crack resistance and sealing torque retention. Closure interiors intended for food contact must comply with EU 10/2011/EC and FDA 21 CFR 177.1520(c) 1.1, while removal torque stability is evaluated under ASTM D2063 after three application/removal cycles. The formulation window is narrower than that of lower-flow HDPE grades: erucamide slip is added at 500–900 ppm, behenamide at 200–400 ppm, primary phenolic antioxidant at 300–700 ppm, secondary phosphite at 500–1000 ppm, and zinc stearate acid scavenger at 300–600 ppm; if removal torque after 24 h seasoning falls below 1.0 N·m, back-off risk increases in distribution, while values above 2.0 N·m generate consumer complaint levels. Production tooling uses 48–72 cavities with collapsing core or mechanical unscrewing, barrel temperatures profiled from 210°C to 235°C at the nozzle, mold temperature at 10–20°C, injection pressure of 80–110 MPa, holding time of 1.0–2.0 s, and total cycle time of 4.5–6.5 s. Terminal products include 28 mm PCO 1881 two-piece closures for still water, UHT milk, and juice, as well as 38 mm tamper-evident closures for dairy and edible oil. Operational boundary: closures used with detergent or surfactant-containing liquids should not be specified with M300054 without extended testing under ASTM D1693-21 Condition B because high-flow HDPE exhibits reduced ESCR relative to grades with melt flow rates below 10 g/10 min, and published F50 data for this specific configuration should be confirmed against the manufacturer’s lot-specific certificate.
When cosmetic packaging components are injection-molded for skin-contact applications, Regulation (EC) 1223/2009 Annex I governs the safety assessment of the finished cosmetic product, while the packaging article itself is evaluated under REACH EC 1907/2006 Annex XVII and, when sold in the EU market, Directive 94/62/EC Article 11 heavy metal restrictions. For opaque cream jar bases, pump collar housings, and compact trays, a typical addition package contains 2.0–3.0 wt% white masterbatch with rutile TiO₂ content of 55–65% in an LDPE/LLDPE carrier, 0.15–0.35 wt% UV absorber of the 2-(2′-hydroxyphenyl)benzotriazole class, and 0.05–0.12 wt% phosphite-based synergist; if phthalate-free processing is specified, carrier resins and wetting agents must be verified against REACH Annex XVII entries 51 and 52. Injection molding uses high-gloss mold inserts and 8–16 cavity hot-runner tools, with nozzle temperature held at 205–230°C, mold temperature elevated to 25–40°C to improve surface replication and reduce flow lines on curved jar walls, injection speed reduced to 60–120 mm/s on thick-walled jar bases to avoid jetting, and holding pressure maintained at 40–60 MPa for 6–10 s; on production lines, ejection force rises above 15 kN when mold release concentration is omitted from the dry blend. Finished products include 30–100 ml cream jar bases, treatment pump collars, compact trays, and overcaps for fragrance and personal care sets. Operational incompatibility: colorants containing free aromatic amines or packages with high levels of migratory processing aids should be excluded when the container will contact alcohol-based formulations or ester-rich emulsions because migration testing under EU 10/2011/EC is not automatically demonstrated by the polymer’s olefin clearance.
For 2–10 L industrial pail bodies molded from M300054, the primary technical decision is whether the finished container will be classified as dangerous goods packaging; if so, ADR 6.1.5.2.4 drop testing and ADR 6.1.5.2.5 stacking test requirements apply, with drop heights of 1.2 m for Packaging Group II and 0.8 m for Packaging Group III when relative density does not exceed 1.2. For black lubricant and construction chemical pails intended for outdoor storage, a robust additive package comprises 2.0–2.5 wt% carbon black masterbatch at 50% loading in LDPE, 0.2–0.4 wt% hindered amine light stabilizer, 0.1–0.2 wt% phenolic primary antioxidant, and 0.03–0.06 wt% fluoropolymer processing aid to stabilize pressure demand across a single top sprue. Production processing on 500–1000 t hydraulic clamp injection molding machines uses single-cavity pail tooling with conformal cooling in the rim and handle boss, melt temperature at 220–250°C, injection speed at 100–160 mm/s, injection pressure at 90–120 MPa, holding pressure at 50–70 MPa, cooling time at 15–25 s, and mold temperature at 10–18°C; short shots are observed on rim-lock versions when injection speed falls below 100 mm/s. Terminal product types include 5 L and 10 L pails for lubricants, detergents, inks, and water-based construction chemicals, together with lids featuring tear-tab or gasket seats. Operational boundary: M300054 should not be specified for UN Packaging Group I products or for sustained stacked storage above 60°C because the heat deflection temperature under 0.45 MPa is near 70°C in ISO 75-2:2013, and sidewall deflection under load must be validated by 28-day stack creep data before approval for export shipment.
Logistics crates and returnable transit packaging manufactured from HDPE M300054 fall under Directive 94/62/EC Article 11 heavy metal restrictions—the sum of lead, cadmium, mercury, and hexavalent chromium must remain below 100 ppm—alongside REACH EC 1907/2006 Annex XVII restricted substance obligations and, for crates that contact unpacked fruit or vegetables, EU 10/2011/EC and FDA 21 CFR 177.1520(c) 1.1. Ventilated agricultural crates and bakery trays use a formulation with 2.5–3.5 wt% UV-stabilized green or black masterbatch, 0.2–0.5 wt% hindered amine light stabilizer, 0.1–0.2 wt% processing aid, and 0.05–0.2 wt% chemical foaming agent if wall thickness is reduced by structural foam molding; if pellets are stored in unheated silos with condensation risk, drying at 70–80°C for 1–2 h is required to prevent surface splay. Injection molding is performed with multiple hot-to-cold runner systems, melt pool temperature at 215–240°C, mold temperature at 20–35°C, injection speed at 80–140 mm/s, back pressure at 3–6 bar, and total cycle time of 20–32 s depending on rib density and wall thickness of 2.0–3.5 mm; cavity-to-cavity fill imbalance above 3% on 4-cavity produce crate tools produces inconsistent handle boss dimensions and stack misalignment. Terminal products include stack-and-nest produce crates, bakery trays, bottle transport trays, and returnable automotive parts dunnage. Living hinge designs are not recommended because high-flow HDPE has lower flexural fatigue resistance than polypropylene; if folding crate hinges are unavoidable, the hinge radius should exceed 1.5 mm and the design should be tested to 10⁴ flex cycles under ISO 178:2019 bending evaluation before field use.
| Obligation | Standard or clause | Test parameter | Threshold |
|---|---|---|---|
| EU packaging heavy metals | Directive 94/62/EC Article 11 | Sum of Pb, Cd, Hg, Cr(VI) | <100 ppm |
| US food contact produce crate | FDA 21 CFR 177.1520(c) 1.1 | Extraction under intended conditions | Conformance with 21 CFR 177.1520 |
| EU food contact produce crate | EU 10/2011/EC Annex I | Overall migration | 10 mg/dm² |
| REACH restricted substances | REACH EC 1907/2006 Annex XVII | Substance-specific restriction | As listed by CAS number |
In household storage and organization products, the processing window of M300054 interacts with large projected areas, thin nominal walls, and the need for stable stacking geometry under repeated use. General product safety obligations under Directive 2001/95/EC apply, and if a product is marketed as children’s storage furniture, EN 71-3 migration of elements testing may be triggered; RoHS Directive 2011/65/EU Annex II applies only when the article incorporates electrical components. A typical compound for nesting storage totes and laundry baskets includes 2.5–4.0 wt% color masterbatch in a PE carrier, 0.02–0.06 wt% fluoropolymer processing aid, 0.1–0.3 wt% glycerin monostearate antistatic additive, and 0.05–0.1 wt% slip additive to reduce stacking friction; production lots with melt flow variation outside ±2 g/10 min have been observed to produce shot weight drift in 1,500–2,500 g parts. Injection molding uses large-area tooling with sequential valve gating on 700–1300 t clamp machines, nozzle temperature at 205–225°C, mold temperature at 15–25°C, injection pressure at 80–100 MPa, and clamp force per projected area at 3–4 kN/cm²; jetting is controlled by staging valve gate opening from center to outer gates. Terminal products include nesting storage totes, laundry baskets, clothes hangers, and under-bed containers. At wall thickness below 0.8 mm and with high post-consumer recycled content, the ductile-to-brittle transition may shift above −10°C, so low-temperature drop impact should be tested under ISO 6603-2:2000 before specifying freezer-adjacent storage applications; published data for thin-wall hanger hook designs in this exact configuration is limited, and instrumented ejection force measurement during piloted tool trials is required.
Competitive SABIC HDPE M300054 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SABIC HDPE M300054 is a high-density polyethylene resin intended for injection moulding applications in which short cycle times, thin-wall filling, and post-mould dimensional stability are the primary production targets. The grade is characterised by a nominal density of 954 kg/m³ under ISO 1183-1:2019 and a melt flow rate of 30 g/10 min at 190°C and 2.16 kg under ISO 1133-1:2022. The narrow molecular weight distribution produces a low-viscosity melt that can fill multicavity tools at lower hydraulic pressure than standard low-flow injection HDPE grades. Typical single-stage reciprocating screw injection moulding machines with L/D ratios of 20:1 to 25:1 and non-return valve assemblies are sufficient for processing. Application areas include thin-wall food packaging, overcaps, closures, pails, and housewares, where the melt flow permits reduced pack pressure and earlier gate freeze while still maintaining acceptable part weight. M300054 is not designed for extrusion blow moulding, pipe, or rotational moulding, because its low melt elasticity cannot provide the required parison stability or long-term hydrostatic strength.
The density of 954 kg/m³ places the grade at the lower end of the high-density polyethylene density interval. Compared with stiff injection HDPE grades in the 960 kg/m³ to 970 kg/m³ range, M300054 offers slightly lower tensile modulus but lower melt viscosity and reduced residual stress when cooled at typical mould temperatures. In semicrystalline solidification from a melt temperature of 200°C to 230°C to a mould wall at 10°C to 30°C, the specific volume change is compensated by hold pressure before gate freeze. If hold pressure is removed too early, volumetric shrinkage produces sink marks and vacuum voids, particularly in rib intersections and thick bosses. Cavity-to-cavity differential shrinkage is controlled by keeping mould surface temperature variation below ±5°C; this value is not a material property but a processing boundary observed in multicavity HDPE moulding when conformal cooling is unavailable.
The 30 g/10 min melt flow rate is a standardised capillary flow value under ISO 1133-1:2022 and does not directly represent injection shear rates. At typical injection shear rates of 100 s⁻¹ to 1000 s⁻¹, high-flow HDPE exhibits shear-thinning behaviour, lowering apparent viscosity and reducing pressure drop through hot-runner manifolds and gate lands. The practical result is that a thin-wall part with a nominal wall thickness of 0.8 mm to 1.2 mm can be filled at lower injection pressure than an 8 g/10 min injection grade, but published quantitative comparisons for specific mould geometries are limited. Melt temperature should be set at 200°C to 230°C as measured in the purged melt. Higher temperatures above 250°C accelerate molecular weight reduction and produce yellowing; a barrel residence time above 250°C should be less than 5 minutes.
Because the melt has low elasticity, jetting can occur when the gate diameter is too large relative to wall thickness or when the gate is located in an open cavity without a flow diverter. The preferred gate geometry is a side gate or edge gate that directs the melt against the cavity wall. The gate diameter should be 0.5 to 0.8 times the nominal wall thickness. Hot-runner systems with thermal gate tips are acceptable if tip temperature is controlled below 250°C. Cold runner diameters of 3 mm to 4 mm are typical for medium-sized tools, but the final runner balance must be verified with short-shot progression, because high-flow HDPE will preferentially fill low-pressure drop cavities and can amplify runner imbalance in multicavity layouts. Venting depths of 0.02 mm to 0.03 mm are recommended to evacuate gas without flash, as the low-viscosity melt penetrates small clearances more readily than lower-melt-flow grades.
| Property | Test method | Typical value |
|---|---|---|
| Density | ISO 1183-1:2019 | 954 kg/m³ |
| Melt flow rate, 190°C/2.16 kg | ISO 1133-1:2022 | 30 g/10 min |
| Tensile stress at yield | ISO 527-2:2012 | 23 MPa |
| Tensile strain at yield | ISO 527-2:2012 | 9 % |
| Flexural modulus | ISO 178:2019 | 1000 MPa |
| Charpy notched impact strength at 23°C | ISO 179-1:2020/1eA | 3 kJ/m² |
| Vicat softening temperature, A50 | ISO 306:2022 | 123°C |
| Heat deflection temperature at 0.45 MPa | ISO 75-2:2013/B | 65°C |
| Shore D hardness, 15 s | ISO 868:2003 | 59 |
| Mould shrinkage | ISO 294-4:2018 | 1.2 %–1.8 % |
The values listed in the table are typical values from standard test specimens and must not be used as minimum specification limits. Tensile stress at yield, flexural modulus, and Charpy notched impact are affected by gate geometry, weld line position, cooling rate, and post-mould crystallinity. The tensile strain at yield of 9% reflects a stiff response with limited yielding before cold drawing. Environmental stress cracking resistance is not provided in the public datasheet for this specific configuration; applications involving detergents, surfactants, or solvent contact should require supplementary testing under ASTM D1693 or ISO 22088-2:2006 on finished articles or representative plaques processed under production conditions.
For food-contact end uses, M300054 is generally considered suitable under EU Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 for olefin polymers when used as supplied, but the final article must be tested for overall migration, specific migration limits, and sensorial properties because added masterbatches, processing aids, and regrind alter the compliance profile. REACH and RoHS 2011/65/EU declarations are grade-specific and should be obtained from SABIC’s regulatory documentation portal. Drying is not normally required for HDPE, but condensation on pellet surfaces stored in humid warehouses can produce surface splay and silver streaks at low melt temperatures. When those defects appear, drying at 80°C for 2 hours in a desiccant dryer is a corrective action. If regrind is used, its content should be kept below 30 wt% unless impact testing under ISO 179-1:2020 confirms that the finished article still meets the application requirement. Because high-flow HDPE is more sensitive to molecular weight reduction and contamination than lower-flow grades, the use of mixed post-consumer recyclate is not recommended without melt filtration and laboratory evaluation of melt flow stability.
| Property | M300054 | Lower-flow HDPE reference class, 8 g/10 min MFR |
|---|---|---|
| Density | 954 kg/m³ | 960–965 kg/m³ |
| Melt flow rate, 190°C/2.16 kg | 30 g/10 min | 8 g/10 min |
| Tensile stress at yield | 23 MPa | 25–27 MPa |
| Flexural modulus | 1000 MPa | 1100–1200 MPa |
| Charpy notched impact strength at 23°C | 3 kJ/m² | 4–6 kJ/m² |
| Vicat softening temperature, A50 | 123°C | 125–127°C |
| Mould shrinkage | 1.2 %–1.8 % | 1.5 %–2.0 % |
Reference-class values are drawn from publicly available datasheets for lower-flow injection HDPE grades and are provided for directional comparison only. The primary process difference is melt viscosity: M300054 can reduce filling pressure and permit shorter fill time in thin walls, but the lower molecular weight reduces impact strength and stiffness. The narrow molecular weight distribution of M300054 reduces die swell and post-mould warpage in flat parts but also reduces melt elastic memory. In closure and thin-wall container applications, the high-flow grade supports higher cavitation and reduced cycle time; in stackable crates or load-bearing components exposed to impact below -20°C, a lower-flow HDPE with higher Charpy notched impact is preferred.
M300054 is not a direct replacement for high molecular weight HDPE blow moulding grades, PE100 pipe resins, or high-stiffness HDPE compounds used for industrial crates. Its high MFR and narrow molecular weight distribution do not provide the melt strength required for continuous extrusion blow moulding; parison sag and thinning are significant processing hazards. For pressure pipe, the resin lacks the long-term creep rupture strength and slow crack growth resistance expected under ISO 9080:2022 and ISO 13479:2022. Attempting to use M300054 in these applications would require complete redesign of processing equipment and cannot be compensated by mould temperature or screw speed changes.
M300054 is processed on conventional hydraulic, servo-electric, or hybrid injection moulding machines with shot sizing between 30% and 70% of barrel capacity. The melt temperature at the nozzle should be 200°C to 230°C, with a lower limit of 190°C for very thin sections and a maximum of 250°C. Mould wall temperature is typically 10°C to 30°C to obtain short cooling times; raising the mould temperature to 40°C to 50°C improves gloss and weld-line strength but increases cooling time. Holding pressure is usually set at 50% to 70% of peak injection pressure, and holding time is determined by gate seal time from part weight stability. Back pressure should be limited to 0.5 to 1.5 MPa, and screw speed should be selected to avoid adiabatic overheating; a screw surface speed below 0.3 m/s is a typical starting point. Excessive shear heating from high screw speed and high back pressure can produce local melt temperatures above 250°C even when barrel setpoints are lower, leading to molecular degradation.
Mould design for M300054 must account for higher volumetric shrinkage than amorphous resins and lower internal stress than high-molecular-weight HDPE. Uniform cooling is therefore more important than extreme steel temperatures. Differential mould temperature above ±5°C across a cavity can create visible gloss banding, warpage, and inconsistent dimensions in flat lids or thin containers. If conformal cooling is not used, the circuit layout should provide independent control for core and cavity, with flow rates sufficient to produce a Reynolds number above 4000 in the cooling channel. Venting depth should be 0.02 mm to 0.03 mm, and vents should be placed along the last-filled regions and weld lines. Hot-runner valve gates are preferable when gate vestige or stringing is unacceptable; however, needle temperature must be controlled to avoid local degradation. Gate freeze time is short, so cavity pressure sensors are recommended for setting hold pressure switch-over by part weight rather than by timer alone.
Troubleshooting field issues with M300054 usually involves verifying melt temperature, gate geometry, and mould temperature uniformity before changing material grade. Surface splay at low melt temperature is corrected by drying or raising the nozzle temperature within the specified window. Short shots in thin sections indicate insufficient injection velocity or gate size below 0.5 times wall thickness. Sink marks indicate gate freeze before packing completion or insufficient holding pressure. Warpage indicates non-uniform cooling or excessive orientation; reducing melt temperature and increasing mould temperature within the specified range often reduces frozen-in stress. Flash with this low-viscosity grade is controlled by reducing injection velocity or clamp force adjustment and by ensuring vent depth does not exceed 0.03 mm. These corrective actions are standard process controls, not material accept/reject criteria.