Sabic Hdpe F01552

SABIC HDPE F01552

    • Product Name: SABIC HDPE F01552
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 402572
    Density 0.952 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.15 g/10 min
    Melt Flow Rate 190 C 5 Kg 0.5 g/10 min
    Melt Flow Rate 190 C 21 6 Kg 8 g/10 min
    Tensile Modulus 1000 MPa
    Tensile Stress At Yield 25 MPa
    Tensile Strain At Yield 10 %
    Tensile Strain At Break >600 %
    Flexural Modulus 1000 MPa
    Notched Charpy Impact Strength At 23 C 20 kJ/m²
    Notched Charpy Impact Strength At 30 C 5 kJ/m²
    Escr 10 Igepal 50 C >1000 h
    Vicat Softening Temperature 125 °C
    Melting Temperature 130 °C
    Thermal Conductivity 0.4 W/mK
    Coefficient Of Linear Thermal Expansion 1.5E-4 /°C
    Water Absorption <0.01 %
    Hardness Shore D 60
    Dielectric Constant 1 Mhz 2.3
    Volume Resistivity >1E14 ohm·cm

    As an accredited SABIC HDPE F01552 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC HDPE F01552 is supplied in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg per pallet.
    Container Loading (20′ FCL) Container Loading (20′ FCL) for SABIC HDPE F01552: 25 kg bags, approximately 20 MT net, securely stowed for export.
    Shipping SABIC HDPE F01552 is typically shipped as non-hazardous, solid polyethylene pellets in 25 kg bags, FIBCs, octabins, or bulk trucks/railcars. Keep packaging dry, cool, clean, and away from direct sunlight, heat, moisture, and contamination during transit. Use standard material handling; no special dangerous goods transport regulations apply.
    Storage Store SABIC HDPE F01552 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and ignition sources. Keep original bags or octabins tightly closed, palletized, and off the floor. Protect from moisture, dust, contamination, and prolonged UV exposure. Avoid extreme temperatures and strong oxidizers. Follow local regulations and supplier storage recommendations. Ensure good ventilation and avoid smoking.
    Shelf Life SABIC HDPE F01552 has a 24-month shelf life when stored unopened in original packaging, dry, cool, and protected from direct sunlight.
    Application of SABIC HDPE F01552

    SABIC HDPE F01552 is an extrusion-grade high-molecular-weight high-density polyethylene with a density of 0.952 g/cm³ (ISO 1183-1:2019) and a melt flow rate of 15 g/10 min at 190°C/21.6 kg (ISO 1133-1:2022). The resin is specified for high-stalk blown film extrusion where melt strength, thin-gauge down-gauging, and bubble stability govern line yield. Pre-drying is not required when silo storage remains below 60% RH; surface condensation from hopper temperature swings is the main loss of bubble stability. The following application records cover blown film and downstream converting only, not injection molding or thermoforming.

    In single-layer HMW-HDPE blown film lines converting T-shirt carrier sacks at 12–25 μm final gauge, the formulation remains 100% F01552 plus 2–4 wt% of a low-viscosity LDPE-carrier color masterbatch added by gravimetric dosing. Food-contact retail sacks used for produce or bread are covered under FDA 21 CFR 177.1520(c) 3.2a and EU Regulation 10/2011, with overall migration below 10 mg/dm²; non-food retail sacks are mechanically checked against EN 13590:2003 for single-use carrier bag tensile and weld strength. Processing on a grooved-feed extruder with 65 mm screw and 30:1 L/D typically uses die gap 0.9 mm, blow-up ratio 4:1, frost line height 8–12 die diameters, melt temperature 193–204°C, and bubble internal cooling air at 8–12°C. If die gap is narrowed below 0.8 mm without raising melt temperature above 204°C, shark-skin melt fracture appears on the inner bubble surface and propagates into tear anisotropy. Finished products include bottom-sealed T-shirt sacks, side-gusseted grocery sacks, and block-bottom retail bags at 10–25 μm, with in-line perforation and side-weld sealing at 120–140°C.

    What Drives the Layer Distribution in Three-Layer Cereal Liner Coextrusion?

    The three-layer structure for cereal liners is specified around F01552 skins for stiffness and moisture barrier and a butene-LLDPE core for dart drop and seal strength. Skin layers are formulated at 100% F01552 with 2–3 wt% white masterbatch; the core is a 1.0 g/10 min (190°C/2.16 kg, ISO 1133-1:2022) butene-LLDPE, and the layer thickness ratio is held at 20/60/20 or 30/40/30 depending on whether the liner is for dry cereal or powdered beverage. Food-contact compliance is governed by FDA 21 CFR 177.1520(c) 3.2a and EU Regulation 10/2011, with the LLDPE core also meeting the same polyolefin restrictions; converters submit the final laminate to overall migration testing below 10 mg/dm² in food simulant A. The coextrusion line uses a 200 mm three-layer die, die gap 1.2 mm, blow-up ratio 3:1, skin melt temperature 199°C, and core melt temperature 204°C to maintain layer viscosity match. Core melt above 210°C accelerates LLDPE gel formation, while skin melt below 193°C raises die pressure and induces gauge bands. Finished product types include cereal box liners at 40–50 μm, dry food pouch stock at 50–60 μm, and bag-in-box inner liners for dry beverage, where the HDPE skin reduces blocking and improves machine-direction stiffness on vertical seal jaws.

    Outside food contact, single-layer industrial liner production shifts the formulation tolerance toward internal regrind and antistatic additives. A running formulation of 85 wt% F01552, 5 wt% LDPE, and 10 wt% clean in-house HDPE trim scrap is used, with 2 wt% carbon black masterbatch for ultraviolet screening and 0.1–0.3 wt% non-amine antistat when cement or gypsum dust adhesion must be controlled. Because no food-contact declaration is required, mechanical acceptance is written against ASTM D1709-16a dart drop, ISO 6383-2:1983 Elmendorf tear, and ASTM D882-18 tensile properties; a minimum machine-direction Elmendorf tear of 1.5 N at 50 μm is common in purchase specifications. Processing on a 55 mm barrier-screw blown film line uses die gap 1.0 mm, blow-up ratio 3:1, melt temperature 188–196°C, and collapsing frame hip angle 18–22°. Regrind above 10 wt% narrows the tear balance and increases film blocking on the roll, especially in thicknesses above 60 μm. Finished product types include drum liners for powdered resins, box liners for adhesive-coated industrial goods, and construction dust partitioning film in 50–80 μm thicknesses.

    Lamination Films for Woven Polypropylene Sacks and Kraft Ream Wrappers

    A 20–30 μm F01552 blown film is used as the reverse-printed outer ply in adhesive-laminated woven polypropylene sacks where pet food, bird seed, or paper ream wrap requires surface strength and moisture resistance. The film layer is formulated at 100% F01552 with 2 wt% opacity masterbatch; no slip additive is used when the outer surface is to be corona treated and printed. For pet food contact, the HDPE layer is covered under FDA 21 CFR 177.1520(c) 3.2a and EU Regulation 10/2011, but the full laminate must be migration-tested as a finished structure under EU Regulation 10/2011 because the adhesive and woven substrate are part of the food-contact article. Blown film production on a single-layer line with die gap 1.0 mm, blow-up ratio 3:1, and melt temperature 190–196°C is followed by in-line corona treatment to 38–40 mN/m; surface energy is measured by ISO 8296:2003. Lamination is performed with a 1.5–2.5 g/m² solventless polyurethane adhesive on a flat-bed laminator at 40–60 m/min, using nip roll temperature 50–60°C. Corona treatment above 40 mN/m can oxidize the outer surface and reduce adhesion strength under humid storage. Finished product types include laminated woven sacks for pet food and horticultural seeds, kraft ream wrappers, and moisture-resistant outer wraps for roll goods.

    Where a 150 μm Class A vapor retarder is specified under a concrete slab, F01552 is extrusion-blown at the upper end of its thickness capability with a wider die gap and lower blow-up ratio to reduce transverse gauge variation. The formulation is 97–98 wt% F01552, 2–3 wt% carbon black masterbatch for opacity and ultraviolet screening, and 0.05–0.1 wt% hindered amine light stabilizer when the sheet remains exposed to site sunlight for more than 14 days. Compliance is set by ASTM E1745-17 Class A, which limits water vapor permeance to 0.1 perm tested by ASTM E96/E96M-21 at 23°C and 50% RH, with tensile and puncture requirements referenced in the same specification. The film is blown on a 75 mm grooved-feed extruder with die gap 1.2–1.5 mm, blow-up ratio 3:1, melt temperature 199–210°C, and chilled collapsing air at 10°C to reduce blocking in rolled stock. Installation over sharp aggregate without a geotextile cushion produces puncture tears; the sheet is therefore bid with a puncture-probability note and tested against ASTM D1709-16a for film dart drop. Finished product types include under-slab vapor retarder sheets in 150 μm and 250 μm thicknesses, supplied in rolls up to 3 m wide and 60 m long.

    When Form-Fill-Seal Powder Sachets Demand Seal Integrity Across Contaminated Seals

    Powdered drink mix sachets produced on vertical form-fill-seal equipment expose the seal area to product dust, so a 100% HDPE film frequently fails on hot tack because the seal initiation temperature is too high and the melt does not flow around powder particles. The running blend is 70 wt% F01552 and 30 wt% of a C6-LLDPE with melt index 1.0 g/10 min (190°C/2.16 kg, ISO 1133-1:2022) to lower seal initiation temperature to 112–118°C and improve hot tack measured by ASTM F1921-20. Food-contact compliance for the final sachet is derived from FDA 21 CFR 177.1520(c) 3.2a and EU Regulation 10/2011; if a non-amine permanent antistat is added at 0.1–0.3 wt%, its specific migration is verified under EU Regulation 10/2011 before release. Blown film production uses die gap 1.0 mm, blow-up ratio 3.5:1, melt temperature 190–198°C, and frost line height 6–9 die diameters to balance dart drop and stiffness. Conversion on vertical form-fill-seal machines uses jaw seal temperature 130–150°C, dwell 0.2–0.5 s, and film surface energy 38 mN/m after corona treatment for print adhesion. Amine-based migratory antistats are avoided because they can elevate seal contamination and organoleptic migration into dry food powders. Finished product types include sachets for powdered drink mixes, seasoning powders, and effervescent salts at total film thickness 30–45 μm.

    Free Quote

    Competitive SABIC HDPE F01552 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC HDPE F01552 is a high-density polyethylene resin supplied as pelletized feedstock for blown-film extrusion. The grade is characterized by a nominal density of 0.952 g/cm³ measured under ISO 1183 and a melt flow rate of 0.15 g/10 min at 190 °C/2.16 kg under ISO 1133-1. These values place the material in the medium-molecular-weight segment of the SABIC high-density polyethylene film range. The alphanumeric grade code embeds nominal flow and density information, but the exact decoding should be confirmed against the current manufacturer technical bulletin. Typical pellet bulk density and stabilizer composition are not part of the public specification and should be requested as certificate-of-analysis parameters when silo capacity or food-contact declarations are critical.

    Table 1 — Typical physical properties published for SABIC HDPE F01552
    PropertyTypical valueTest method
    Density0.952 g/cm³ISO 1183
    Melt flow rate0.15 g/10 minISO 1133-1 at 190 °C/2.16 kg
    Tensile modulus1250 MPaISO 527-2
    Tensile yield stress28 MPaISO 527-2
    Elongation at break>300%ISO 527-2
    Vicat softening temperature127 °CISO 306/A120

    The values in Table 1 are typical single-point values obtained by standardized laboratory methods and do not constitute a product specification. Lot-to-lot variation may occur within the manufacturer’s published control limits.

    What separates SABIC HDPE F01552 from adjacent film-grade HDPE resins?

    Within the SABIC HDPE film portfolio, F01552 is best understood by comparison with F00952 and F04660. Table 2 summarizes the grade-level differences in melt flow rate and density. The 0.15 g/10 min melt flow rate of F01552 is higher than the 0.09 g/10 min of F00952 and lower than the 0.60 g/10 min of F04660. The molecular weight implications are direct: higher melt flow rate correlates with lower average molecular weight and lower zero-shear viscosity. On extrusion lines, F01552 therefore consumes less specific mechanical energy than F00952 but more than F04660 at the same screw speed and output. Bubble stability generally follows the inverse trend; F00952 provides the strongest melt and widest processing window at high blow-up ratios, while F04660 may exhibit thinner stable bubble walls at high output but reduced melt strength.

    Table 2 — Comparative grade-level data for SABIC HDPE film resins
    GradeMelt flow rateDensityTest method
    F009520.09 g/10 min0.952 g/cm³ISO 1133-1 / ISO 1183
    F015520.15 g/10 min0.952 g/cm³ISO 1133-1 / ISO 1183
    F046600.60 g/10 min0.946 g/cm³ISO 1133-1 / ISO 1183

    The density equal to 0.952 g/cm³ for both F00952 and F01552 means that short-term stiffness properties are closer than the melt flow difference would suggest. F04660 at 0.946 g/cm³ has a lower crystallinity and therefore lower tensile modulus; this places F01552 as a replacement candidate when converter specifications require stiffness retention without moving to a lower-MFR resin with higher head pressure. However, film impact and tear properties are not fixed by density and melt flow rate alone. They depend on film gauge, die geometry, blow-up ratio, and frost-line height. Converter trials should measure dart impact under ASTM D1709 or ISO 7765-1 and tear strength under ASTM D1922 on the actual line configuration.

    Compared with metallocene-catalyzed HDPE film grades of similar density, F01552 may have a different molecular weight distribution and shear-thinning response. This can yield different die swell and melt strength behavior; die gap compensations may be required when replacing a metallocene grade. Published data for this specific comparison is limited and should be verified by a controlled pilot run.

    Processing trials on high-density blown-film extrusion lines normally set barrel temperatures in the feed, compression, and metering zones from 160 °C to 220 °C, with the die and adapter held at 190 °C to 210 °C. Melt temperature measured directly at the die exit should remain between 180 °C and 220 °C. A grooved-feed single-screw extruder of 45 mm to 65 mm diameter and 25:1 to 30:1 L/D is suitable. Die gaps from 1.2 mm to 2.0 mm and blow-up ratios from 3:1 to 5:1 are common for film thicknesses between 10 µm and 50 µm. Field observations from production lines indicate that a frost-line height of 4 to 8 die diameters usually gives a stable bubble; lower frost-line heights can increase film blocking, while higher frost-line heights can alter orientation balance.

    Pressure at the die entry typically ranges from 200 bar to 400 bar depending on output rate, melt temperature, screen-pack condition, and die diameter. Published data for this specific configuration is limited because pressure values are line-dependent; treat the range as an industrial reference, not a grade guarantee. Pressure spikes above ±25 bar from the normal setpoint usually indicate screen-pack fouling, feed-bridge melting irregularities, or a worn screw. Melt fracture at the die lip is observed when melt temperature is below 180 °C or when the die gap is too small. Bubble flutter at high blow-up ratios may occur if the cooling-air ring is unbalanced or if the air temperature varies by more than 5 °C across the bubble circumference.

    Rheologically, F01552 displays shear-thinning behavior typical of linear HDPE. Capillary rheometry at 190 °C shows an apparent shear viscosity that decreases with increasing shear rate; converters requiring exact flow curves should request the manufacturer’s viscosity-shear rate data or measure under ISO 11443. Lot-to-lot variation in melt flow rate is generally controlled within narrow limits, but pellet-to-pellet heterogeneity can be introduced by poor silo blending. A homogenous silo discharge is recommended before film extrusion.

    Virgin pellets do not require predrying when stored in sealed containers. If cold resin is transferred from outdoor storage into a conditioned hall, condensation can form on pellet surfaces; in that case hopper drying at 60 °C to 70 °C for 1 h to 2 h is sufficient. Avoid melt temperatures above 240 °C for prolonged periods because thermal-oxidative chain scission accelerates, the melt flow rate drifts upward, and gel formation can increase. A purge with low-density polyethylene or a commercial purging compound is recommended after color or additive changes to avoid cross-contamination. Do not introduce polypropylene, polyamide, or polyester fines into the system; molten contaminants of these polymers do not homogenize with HDPE and can form visible gels, holes, or film-splitting defects.

    Post-industrial regrind addition up to 20% is common in blown-film operations. At regrind levels above 30%, converters should monitor melt flow rate under ISO 1133-1 and check film appearance for gel defects because repeated heat history can shift the molecular weight distribution and reduce film toughness.

    When F01552 replaces lower-density HDPE grades in high-stiffness packaging

    The density of 0.952 g/cm³ gives F01552 a higher tensile modulus than many 0.946 g/cm³ HDPE film grades. This property is relevant for T-shirt carrier bags, bakery bags, industrial liners, and overwrap structures where stiffness and stacking strength limit converter economics. On form-fill-seal lines, the higher crystallinity shifts heat-seal initiation to a higher temperature; seal temperature, jaw pressure, and dwell time should be re-established by measuring seal strength under ASTM F88 on the actual laminate or monolayer structure. Differential scanning calorimetry under ISO 11357-3 can map the melting peak and define the sealing window. The resin is not the preferred choice where transparency is the dominant requirement; lower-density and metallocene-catalyzed ethylene polymers usually have lower haze and higher clarity under ASTM D1003.

    The grade is not formulated as an outdoor weatherable product. If the film will be exposed to UV for more than short indoor handling, a UV-stabilization masterbatch compatible with HDPE must be added and outdoor performance tested under ISO 4892-2 or ASTM D4329. The base resin does not provide long-term resistance to strong oxidizing acids or aromatic hydrocarbons; chemical compatibility should be verified for each liquid or packaged product. For food-contact applications, the converter must obtain the current grade-specific compliance statement. The base resin is commonly supplied with regulatory data referencing FDA 21 CFR 177.1520 and European Union 10/2011, but final migration and organoleptic testing remain the responsibility of the package manufacturer.

    F01552 is not intended for high-pressure pipe extrusion or long-term hydrostatic pressure applications requiring ISO 9080 design curves. It is also not recommended for injection molding or rotational molding where melt flow rates above 4 g/10 min are typically required. Use with high levels of conductive carbon black, hygroscopic fillers, or incompatible polymer scraps should be preceded by separate dispersion and melt-flow stability trials.

    Top