Sabic Hdpe Cc453

SABIC HDPE CC453

    VTB
    Specifications
    HS Code 769028
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.953 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 4.5 g/10 min
    Tensile Modulus 1200 MPa
    Tensile Stress At Yield 28 MPa
    Tensile Strain At Yield 9%
    Tensile Strain At Break >500%
    Flexural Modulus 1300 MPa
    Notched Izod Impact Strength 23 C 8 kJ/m²
    Notched Izod Impact Strength 30 C 4 kJ/m²
    Vicat Softening Temperature 128 °C
    Heat Deflection Temperature 0 45 Mpa 75 °C
    Melting Temperature 133 °C
    Crystallization Temperature 115 °C
    Shore D Hardness 65
    Water Absorption <0.01%
    Environmental Stress Cracking Resistance >1000 h

    As an accredited SABIC HDPE CC453 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC HDPE CC453 is packaged in 25 kg polyethylene bags on pallets, or 1,000 kg jumbo bags.
    Container Loading (20′ FCL) SABIC HDPE CC453 pellets in 25 kg bags, palletized and loaded into a 20′ FCL container; typically approximately 20 MT net.
    Shipping SABIC HDPE CC453 is a non-hazardous high-density polyethylene resin supplied as solid pellets. It is typically shipped in 25 kg bags, jumbo bags, or octabins. Not classified as dangerous goods for transport; no UN number or hazard class required. Store dry, away from heat and sunlight.
    Storage Store SABIC HDPE CC453 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging sealed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Store away from acids, bases, and incompatible materials. Ensure appropriate ventilation and spill containment. Maintain good housekeeping; use first-in, first-out stock rotation.
    Shelf Life SABIC HDPE CC453 shelf life is 24 months when stored in original, unopened packaging, dry, cool, and protected from sunlight.
    Application of SABIC HDPE CC453

    In high-cavitation closure injection moulding, SABIC HDPE CC453 is processed at melt temperatures of 210–230 °C and mould temperatures of 10–20 °C. The grade is a high-flow high-density polyethylene with a melt flow rate of 45 g/10 min when tested under ISO 1133-1 at 190 °C and 2.16 kg, and a density of 0.953 g/cm³ under ISO 1183-1. Published datasheet values place tensile yield stress in the range of 26–30 MPa under ISO 527-2 and flexural modulus in the range of 1200–1400 MPa under ISO 178. In beverage closure shells with wall sections ranging from 0.45 mm to 0.80 mm, the low melt viscosity permits filling at injection speeds of 180–350 mm/s through valve-gated hot-runner systems with 48, 64, or 96 cavities. The hot-runner manifold and nozzle-tip setpoints are normally held within ±2 °C of the barrel front-zone temperature to prevent sequential filling and uneven cap weight. Hold pressure is applied in the range of 60–80 MPa hydraulic pressure for 0.8–1.5 s, followed by cooling of 3–6 s. Demoulding must be sequenced with the cap inner-diameter stabilisation required by PCO 1881 or PCO 1810 bottle-neck finishes; premature ejection produces ovality at the tamper-evident band and thread starts. Compliance for food-contact closure production is assessed under EU 10/2011 and FDA 21 CFR 177.1520. Organoleptic panels for bottled water and dairy products are nevertheless mandatory because the low molecular weight fraction in high-flow HDPE can generate off-notes when hot-runner residence time is extended beyond 10 min. The cut-off of the tamper-evident band and the slit-bridge geometry must be validated by finished-cap torque retention testing on capping heads running at production speeds of 600–1200 bottles/min; torque loss greater than 15% after 24 h indicates thread-root stress relaxation or dimensional drift in the undercuts.

    Regulation or standardRelevant provisionTypical limit or condition
    EU Regulation (EC) No 1935/2004Framework for food contact materialsNo transfer of constituents in quantities endangering human health
    EU 10/2011Plastics intended for food contactOverall migration limit 10 mg/dm² for plastic articles; specific migration limits for additives
    FDA 21 CFR 177.1520Olefin polymers for food contactCompliance with intended conditions of use A–H; no specific migration limit stated for homopolymer HDPE
    REACH Regulation (EC) No 1907/2006SVHC candidate listSVHC content 0.1% w/w per article
    RoHS Directive 2011/65/EUElectrical and electronic equipment materialsLead 1000 ppm, cadmium 100 ppm, mercury 1000 ppm, hexavalent chromium 1000 ppm

    What Governs Mould-Filling Pressure in Thin-Walled Dairy and Spread Containers?

    For thin-walled dairy and spread containers with sidewall thickness from 0.35 mm to 0.55 mm, flow length-to-wall-thickness ratios frequently exceed 200:1. Under these conditions, fill pressure is controlled primarily by the solidification rate at the frozen layer and by the melt flow rate of the high-density polyethylene. SABIC HDPE CC453, with an MFR of 45 g/10 min under ISO 1133-1, reduces injection pressure requirements relative to lower-flow HDPE grades, allowing filling of round tubs with rim diameters up to 180 mm at melt temperatures of 220–235 °C and injection speeds of 250–400 mm/s. Mould temperature is normally set at 10–20 °C to freeze surface gloss and maintain ejection rigidity. The feeding system requires a cold or hot runner with a gate diameter of 0.8–1.5 mm for centre-gated lids or side-gated tubs; undersized gates create jetting and surface flow marks that are unacceptable on dairy sidewalls. For fatty dairy products the specific migration limit for overall migration under EU 10/2011 is 10 mg/dm². The article must also comply with FDA 21 CFR 177.1520 for olefin polymers under the intended conditions of use; high-temperature washing of re-usable containers may require conditions of use A or C, whereas single-use dairy spread tubs may be evaluated under conditions of use E. Because the high melt flow rate of this grade reduces low-temperature impact resistance relative to blow-moulding HDPE grades, containers intended for freezer storage at −18 °C must be subjected to instrumented falling-dart impact testing under ISO 6603-2 or ASTM D3763 at the design wall thickness. Published data for this specific grade under frozen dairy distribution conditions is limited, so full-scale drop testing from 1.2 m at −18 °C is recommended before design freeze.

    When Hot-Runner Residence Time Exceeds 10 Minutes in Multi-Cavity Closure Tools

    In hot-runner closure tools with 96 or 128 cavities, melt residence time in the manifold cannot be ignored because SABIC HDPE CC453 is an injection-moulding grade with a melt flow rate of 45 g/10 min and a narrow molecular weight distribution. The residence time in minutes should be estimated from manifold volume, melt density, shot weight per cavity, and cycle time. A practical check is: residence time (min) = (manifold volume in cm³ × 0.75 g/cm³ / total shot weight in g) × (cycle time in s / 60). Residence times above 10–12 min at melt temperatures of 220–230 °C produce a progressive shift in the molecular weight distribution toward lower molecular weight species, leading to reduced thread-root ESCR, cap yellowing, and generation of volatile carbonyl compounds associated with off-notes in sensitive food packaging. Barrel and hot-runner setpoints should not exceed 245 °C for extended runs; zone temperatures above this threshold accelerate thermo-oxidative degradation and can shift the effective MFR outside the specification window, causing flash in thin-wall closure tools. The failure mode in production is often a slow drift in cap weight: as the material degrades, melt viscosity drops, and the same shot volume delivers lower part mass because leakage past check rings and nozzle seats increases. Holding pressure should be adjusted only after verifying that non-return valve clearance is below 0.05 mm and that nozzle contact force is stable. If the tool is stopped for more than 5 min, the hot-runner manifold should be set to a purge temperature at least 20 °C below the processing setpoint, and the first 10–20 shots should be discarded. No pre-drying is required under normal storage conditions below 60% relative humidity; however, condensation on cold granulate introduced into the feed throat can produce splay in thin-walled lids. The grade should not be compounded with peroxide masterbatches or pro-oxidant additives without full validation because oxidative chain scission in a high-flow HDPE matrix shifts the melt flow rate upward and reduces cap thread load-at-break in a non-linear manner.

    Dispensing Closures and Overcaps for Personal Care: Hinge Fatigue After Filling-Line Torque

    Flip-top dispensing closures and over-caps for personal care bottles are produced in single-face or two-plate tools where hinge flexural endurance and thread torque retention are more critical than top-load. SABIC HDPE CC453 is processed at melt temperatures of 215–235 °C and mould temperatures of 12–22 °C. The hinge is normally gated with a sub-gate or hot-tip gate of 0.8–1.2 mm diameter to orient melt flow across the hinge; hinge thickness between 0.25 mm and 0.45 mm requires flexural fatigue testing after moulding, typically 100,000 cycles at an angle of 180° under laboratory conditions. High-flow HDPE reduces injection pressure for long gas channels, but the low viscosity narrows the packing window: overpacking beyond 70 MPa hydraulic pressure creates hinge brittleness, while underpacking causes sink marks around boss features and thread minor diameters. Both failures are detectable by measuring closure thread diameter against PCO or custom neck finish drawings and by tensile hinge tests using a universal testing machine at 50 mm/min. For personal care applications involving surfactants, the closure must be conditioned with representative formulations because ESCR in HDPE is sensitive to nonylphenol ethoxylates and certain ester-based fragrances; evaluation under ASTM D1693, condition B, or a finished-part ESCR protocol is required. Published data for this specific grade under all surfactant classes is limited, so qualification should use a design-specific environmental stress crack test before mould validation. If the closure is coloured, pigments and carrier resins must be checked against REACH SVHC content limits below 0.1% w/w and the RoHS lead limit of 1000 ppm for the final article. The over-cap may be assembled onto a PP inner closure, and the difference in shrinkage between HDPE and PP must be accounted for in the retaining bead interference; a dimensional tolerance of ±0.1 mm on the bead diameter is commonly required to prevent either assembly cracking or rotational slip.

    When moulding stackable storage containers and houseware lids from SABIC HDPE CC453, the high melt flow rate allows filling of long, thin lid sections down to 0.6 mm in tools with up to 8 cavities, but differential shrinkage between the lid centre and the rim produces out-of-flatness greater than 1.5 mm if the packing phase is not profiled. Holding pressure should be applied in two stages: a first stage at 60–70 MPa for the first 0.5 s, followed by a second stage at 35–45 MPa for an additional 2–4 s. Cooling time is set by the lid centre temperature reaching 75 °C or below before ejection. For containers intended for repeated dishwasher exposure at 65–75 °C, the long-term detergent ESCR of the grade must be evaluated in a finished-part test; high-flow HDPE grades typically exhibit lower ESCR than bimodal blow-moulding grades, so stress concentrations at gate vestiges and stack lugs must be minimised by using generous radii of at least 0.5 mm. Stacking tolerance for lids and bases should be held to ±0.2 mm across the sealing diameter; post-mould shrinkage of HDPE can continue for 24–48 h after demoulding, so dimensional audits should use samples conditioned for 48 h at 23 °C and 50% relative humidity under ISO 291. The material is not recommended for microwave use or for continuous service above 80 °C without load-bearing inserts, because the heat deflection temperature under 0.45 MPa according to ISO 75-2 normally falls below this threshold for high-density polyethylene. If outdoor storage is contemplated, UV stabilisation must be added by the compounder; the natural grade does not contain a UV package.

    Thread ESCR After Accelerated Ageing in Mineral Water and Carbonated Beverage Sealing

    For still and carbonated beverage closure applications, the critical failure mode is environmental stress cracking at the thread root and sealing ring after capping torque and carbonation pressure are applied. The closure material must combine an MFR high enough for thin-wall filling with a sufficiently high ESCR to survive contact stress from the bottle finish. SABIC HDPE CC453 has an MFR of 45 g/10 min under ISO 1133-1, which places it in the high-flow HDPE category. ESCR decreases with increasing MFR in Ziegler-Natta HDPE; therefore, closure designers using this grade for carbonated soft drink PCO 1881 or PCO 1810 finishes should not rely solely on resin datasheet values. Finished-part testing should follow internal cap ESCR protocols, often involving application of 1.5–2.5 N·m torque to a filled bottle conditioned at 40 °C and 50% relative humidity for 14 days. Failure criteria include visible crazing, torque loss greater than 15%, or pressure loss greater than 0.1 bar over 24 h. The closure must also comply with EU 10/2011 and FDA 21 CFR 177.1520; sensory evaluation for bottled water should be performed because high-flow HDPE grades can contribute off-taste when overheated in hot runners. If the application requires carbonation retention at 4 °C for six months, the use of CC453 may be restricted to short-neck finishes with reduced hoop stress; long-term published data for this specific configuration is limited.

    Free Quote

    Competitive SABIC HDPE CC453 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC HDPE CC453 is a high-density polyethylene resin developed for injection-moulded and compression-moulded closures, particularly one-piece carbonated soft drink caps, still water closures, and dairy caps. The grade occupies an intermediate position between low-flow blow-moulding resins and high-flow thin-wall packaging grades. Its nominal melt flow rate is 5.0 g/10 min at 190 °C/2.16 kg and its density is 953 kg/m³. The narrow molecular weight distribution reduces shot-to-shot mass variation in high-cavitation stack tools, limits cap warpage after demoulding, and improves gate-vestige consistency in valve-gated hot-runner systems. In comparison with general-purpose high-density polyethylene extrusion grades, SABIC HDPE CC453 is not intended for film, pipe, or sheet extrusion; its melt rheology and additive package are configured for thin-wall closure geometries and high-speed moulding.

    What specifications and test methods define SABIC HDPE CC453 in closure production?

    The property set is defined by standardised test methods. The table below lists typical values from the current SABIC technical data sheet; exact lot-to-lot limits are governed by the certificate of analysis.

    PropertyTest methodUnitTypical value
    Melt flow rateISO 1133-1:2022g/10 min5.0
    DensityISO 1183-1:2019kg/m³953
    Tensile stress at yieldISO 527-2:2012MPa27
    Tensile modulusISO 527-2:2012MPa1100
    Flexural modulusISO 178:2019MPa1200
    Vicat softening point A50ISO 306:2022°C127
    HardnessISO 868:2003Shore D63

    The melt flow rate of 5.0 g/10 min is lower than high-flow closure grades in the 10–20 g/10 min range. This lower flow character increases melt pressure on identical tooling by approximately 5 % to 10 %, but it contributes to higher melt strength at the gate and reduces jetting in edge-gate closure designs. A single apparent viscosity value is not sufficient for mould-filling simulation; capillary rheometry data over shear rates from 10 s⁻¹ to 10⁴ s⁻¹ should be used. The density of 953 kg/m³ places the grade in the stiff, highly crystalline region of the HDPE density range, which supports top-load performance and dimensional stability but reduces low-temperature impact relative to lower-density copolymers.

    Rheological and failure-resistance thresholds in cap and closure tooling

    The shear viscosity of SABIC HDPE CC453 should be characterised by capillary rheometry in accordance with ISO 11443:2021 at 190 °C, 230 °C, and 250 °C. In closure injection moulding, apparent shear rates at the gate commonly reach 10⁵ s⁻¹ to 10⁶ s⁻¹, while shear rates along the flow path are typically 10² s⁻¹ to 10⁴ s⁻¹. At these rates, the melt is strongly shear-thinning; mould-filling simulations should use a temperature-dependent Cross-WLF or Carreau model rather than a Newtonian approximation. Gate diameter should be matched to flow length so that shear stress at the gate remains below the critical melt fracture threshold. For thin-wall beverage closures, gate diameters in the range of 0.6 mm to 0.9 mm are common, but the exact value must be derived from flow length, wall thickness, and available injection pressure.

    Thermal analysis of the grade under ISO 11357-3:2018 shows a crystallisation exotherm typical of high-density polyethylene; the peak crystallisation temperature is approximately 118 °C at a cooling rate of 10 °C/min. Mould temperatures from 10 °C to 20 °C provide rapid skin-layer solidification, which improves roundness and reduces cap ovality in stack moulds. Higher mould temperatures extend cycle time without a proportional improvement in top-load strength. In closures with wall thicknesses below 0.5 mm, cooling time is often limited by gate freeze-off and part ejection stiffness rather than by bulk crystallisation.

    Residual moulded-in stress is a key variable in environmental stress crack resistance. Closure samples tested under ASTM D1693 Condition B may show large scatter if flow-induced orientation or gate-vestige strain is not controlled. Annealing at 40–50 °C for 1–2 h is sometimes used to separate material resistance from processing history. The grade is formulated to reduce low-molecular-weight tail chains that act as craze initiation sites, but the actual ESCR result on a closure depends on tool cooling uniformity, injection speed, and packing pressure. Published data for specific closure geometries is limited; qualification should be performed on production tooling under intended beverage contact conditions.

    On production-scale lines using 48- to 96-cavity stack moulds, SABIC HDPE CC453 is normally processed at melt temperatures from 220 °C to 250 °C. Mould temperatures are typically kept between 10 °C and 20 °C using chilled water. A general-purpose polyolefin screw with an L/D ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3:1 is adequate. High-shear barrier screws can generate unnecessary viscous heating at elevated screw speeds and should be avoided unless dispersion of a specific masterbatch is required. Shot size should be between 40 % and 70 % of barrel capacity to limit residence time. The resin is not hygroscopic; pre-drying is unnecessary when storage relative humidity remains below 60 %. If surface condensation appears after outdoor storage, a short air-purge at 60 °C is sufficient. Processors have observed that valve-gated hot-runner systems require minimum tip temperatures of approximately 220 °C to avoid stringing and cold-slug formation; below this value, gate-vestige tear may increase. Overheating above 270 °C or prolonged residence at high melt temperature accelerates chain scission and may generate odour-active degradation species that affect closure organoleptic performance.

    When carbonated soft drink seal integrity demands elevated stress-crack resistance

    Carbonated soft drink closures must maintain sealing force after carbonation pressure cycles, top-load stacking, and torque removal events. SABIC HDPE CC453 is formulated to provide higher environmental stress crack resistance than general-purpose HDPE bottle-cap grades. The stress-cracking mechanism in polyethylene involves craze initiation at surface micro-defects under hoop stress, followed by fibril rupture in the presence of secondary seal lubricants or beverage-derived stress-cracking agents. The resin’s narrow molecular weight distribution and controlled short-chain branching reduce the concentration of low-molecular-weight tail chains that act as craze initiators. However, ESCR results should always be verified by ASTM D1693 Condition B testing on moulded plaques or closures because laboratory results are sensitive to moulded-in stress and cooling history.

    Compared with a high-flow HDPE closure grade having a melt flow rate near 20 g/10 min, SABIC HDPE CC453 trades some melt fluidity for improved stress-crack resistance and dimensional stability. This makes it suitable for carbonated soft drink closures where cap ovality and seal leakage are more costly than a marginal increase in cycle time. Relative to SABIC HDPE CC254, a higher-flow grade in the same family, CC453 is positioned for applications requiring lower warpage and higher resistance to slow crack growth. It differs from polypropylene closure resins in melting point, modulus, and sealing mechanics: polypropylene offers higher heat resistance for hot-fill or pasteurisation, while HDPE CC453 offers lower processing temperature and better low-temperature impact behaviour. The grade should not be used for extrusion blow moulding because its lower melt strength under parison extension is insufficient for sag resistance in continuous-extrusion shuttle or rotary blow moulding machines. Unlike bimodal HDPE pipe resins designed for long-term hydrostatic pressure resistance, SABIC HDPE CC453 does not carry a PE100 or PE4710 pressure rating and is not intended for pressurised pipe service.

    Regulatory compliance for the virgin grade is documented by the resin supplier. Food-contact eligibility follows FDA 21 CFR 177.1520 for olefin polymers under conditions of use A through H, and EU Regulation 10/2011 for plastic food-contact materials, subject to migration limits for the specific closure design. REACH documentation confirms that the resin does not contain substances of very high concern above 0.1 % w/w per supplier declarations. RoHS Directive 2011/65/EU compliance applies to heavy metal restrictions.

    Regulatory instrumentScopeStatus
    FDA 21 CFR 177.1520Olefin polymers in food contactApplicable to virgin resin
    EU 10/2011Plastic materials in food contactCompliant subject to migration testing
    REACHSVHC screeningNo SVHC > 0.1 % w/w
    RoHS 2011/65/EUHeavy metal restrictionsCompliant

    Compliance statements apply only to unmodified virgin SABIC HDPE CC453. The addition of recycled content, external lubricants, colour concentrates, or oxygen-scavenging masterbatches may change the regulatory status, organoleptic profile, and stress-crack resistance. The grade should not be exposed to strong oxidising agents, solvent-based cleaning fluids, or repeated hot-fill conditions above 85 °C unless the closure design has been specifically validated. Direct contact with high-peroxide sanitising solutions used in some aseptic filling lines can accelerate environmental stress cracking; peroxide concentration and contact temperature must be controlled and validated on the specific closure geometry. Masterbatch let-down ratios above 3 % should be evaluated for effect on ESCR and impact strength because particulate inclusions can act as local stress concentrators in thin-wall sections.

    Top