Sabic Hdpe Cc3054

SABIC HDPE CC3054

    • Product Name: SABIC HDPE CC3054
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 827811
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Modulus 1200 MPa
    Tensile Stress At Yield 28 MPa
    Tensile Strain At Yield 9%
    Tensile Strain At Break >600%
    Flexural Modulus 1300 MPa
    Charpy Notched Impact Strength 23 C 25 kJ/m²
    Charpy Notched Impact Strength 30 C 5 kJ/m²
    Vicat Softening Temperature 125 °C
    Shore D Hardness 62
    Environmental Stress Crack Resistance 10 Igepal 50 C >1000 h
    Melting Point 130 °C
    Water Absorption <0.01%
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.5E-4 /°C
    Dielectric Constant 1 Mhz 2.3
    Volume Resistivity >10^14 ohm·cm

    As an accredited SABIC HDPE CC3054 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC HDPE CC3054 is packaged in 25 kg polyethylene-lined bags, palletized for shipment, or supplied in 1,000 kg bulk bags.
    Container Loading (20′ FCL) SABIC HDPE CC3054 loaded as 25 kg bags, palletized, stretch-wrapped, and secured in a 20-foot FCL container for ocean shipment.
    Shipping SABIC HDPE CC3054 ships as non-hazardous polyethylene pellets in 25 kg bags, 1000 kg bulk bags, or bulk trucks/railcars. Keep containers closed, dry, and away from heat, sunlight, and ignition sources. Use standard industrial handling, PPE, and comply with local transport regulations.
    Storage Store SABIC HDPE CC3054 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Maintain stable stacking on pallets, and use good housekeeping to prevent slipping from spilled pellets.
    Shelf Life Shelf life is typically 24 months when stored in original packaging under cool, dry, well-ventilated conditions, away from direct sunlight.
    Application of SABIC HDPE CC3054

    When tamper-evident band fillet radii fall below 0.4 mm in 26/22 mm CSD closures

    For carbonated soft drink and still water closure production, SABIC HDPE CC3054 is specified as the monolayer shell at 100 wt%; the colour package is introduced as a 2.0–3.0 wt% HDPE-based masterbatch through a gravimetric dosing unit on the press throat, and 0.05–0.10 wt% zinc stearate is used only where high-cavitation tooling records demoulding force spikes above 2.5 kN per cavity. Incoming lot acceptance applies ISO 1133-1:2022 for melt flow rate at 3.0 ± 0.3 g/10 min under 190 °C/2.16 kg and ISO 1183-1:2019 for density at 0.954 ± 0.002 g/cm³; food-contact compliance is assessed under US FDA 21 CFR 177.1520(c) 2.1/2.2 for olefin polymer extractables and Regulation (EU) No 10/2011 with overall migration verified at ≤10 mg/dm² by EN 1186-1, while heavy metals in the closure assembly remain below the Directive 94/62/EC Article 11 limit of ≤100 mg/kg total lead, cadmium, mercury and chromium VI. Component geometries produced under this specification are 26/22 mm short-neck PCO 1881 closures, PCO 1881 Deep closures and 29/25 mm water bottle caps for carbonated soft drink and bottled water lines.

    Processing is conducted on high-speed closure presses with 1,800–3,500 kN clamp force, 24:1 L/D reciprocating screws and multicavity hot-runner tooling; melt temperature is maintained at 200–240 °C, injection velocity at 120–250 mm/s, and hold pressure at 60–80% of peak injection pressure. The narrow processing boundary is established by oxidative stability and mould fill: above 260 °C, chain scission shifts molecular weight distribution and produces low-molecular-weight carbonyl species that can be detected by sensory panels in filled-product testing, while below 190 °C the flow front freezes in the 0.4 mm tamper-evident band fillet and generates short-shot undercut deformations. Cooling time in 96-cavity tooling is 4–7 s, with mould water set at 8–12 °C; pre-drying of the resin is not normally required, but when silo storage generates surface condensation at relative humidity above 80%, a 60 °C dehumidified-air hopper purge for 1 h prevents void formation at the gate.

    Does ESCR retention in bleach-containing closure systems under ASTM D1693 Condition B restrict HDPE grade selection?

    For household chlorine bleach, alkaline detergent, agrochemical concentrate and liquid fertiliser closures, CC3054 is used at 100 parts; the stabiliser package contains 0.10–0.20 wt% hindered phenolic antioxidant and 0.05–0.15 wt% phosphorus secondary antioxidant, with 2.0–3.0 wt% HDPE-based colour masterbatch added for opaque chemical-resistant packaging. Where filled-container storage trials show stress crack initiation at the bridge hinge after 7 days at 50 °C, 10–15 wt% metallocene LLDPE is compounded into the cap body to increase environmental stress-crack resistance, with the trade-off being a measurable reduction in cap shell hoop rigidity as determined by force-deflection testing at a 6.35 mm indentor diameter on a universal tensile machine; zinc stearate is held at ≤0.10 wt% to reduce mould plate-out rather than to modify end-use ESCR. The compliance baseline is ASTM D1693-15 Condition B with 100% Igepal CO-630, but published data for this specific grade-configuration is limited, and commercial release is generally based on filled-package test protocols, not on a fixed notched ESCR value.

    Conversion uses stack moulds or 32–64-cavity cold-runner tools on 2,000–5,000 kN presses, with melt at 210–230 °C, back pressure 0.5–1.0 MPa, and hold pressure 60–80% of injection pressure. Cycle time is typically 5–8 s, with cooling water at 10–15 °C; the main process defect is weld-line stress cracking at the gate, which is aggravated by rapid solidification and high injection velocity above 250 mm/s. Finished article types are 38 mm, 45 mm and 53 mm ribbed side closures with EPE induction liners, child-resistant caps tested to ISO 8317:2015, and tamper-evident closures for industrial chemical containers. Dangerous goods packaging compliance is assigned to the assembled package rather than the closure alone; the filled pail or bottle assembly is qualified under 49 CFR 178.602 drop and 178.603 leakproofness tests, not by a component-level HDPE certificate.

    Standard or regulationScopeClosure-relevant parameter
    ASTM D1693-15Environmental stress cracking of ethylene plasticsCondition B, 100% Igepal, notched specimens; stress crack initiation time
    ISO 8317:2015Child-resistant packagingSequential opening resistance and reclosure torque protocols
    49 CFR 178.602Performance-oriented packaging drop testFilled assembly drop at specified height by packing group
    49 CFR 178.603Leakproofness testNo leakage after internal pressure or water submersion of assembled package
    EU 1272/2008 CLPClassification, labelling and packaging of chemical productsChild-resistant fastening and tactile warnings where the formulation is classified

    In edible oil and condiment closure lines, the failure mode shifts from environmental stress cracking to torque retention on glass bottle finishes after hot filling. A monolayer composition of 100 wt% CC3054 with 2.0–2.5 wt% titanium dioxide masterbatch and 0.05 wt% slip additive is used for 31.5 mm and 38 mm screw caps; if the closure is exposed to hot oil vapour, the maximum continuous service temperature is bounded by the Vicat softening point measured under ISO 306:2022 Method A50 at 124–128 °C, and published data for long-term hot oil vapour exposure in this specific closure configuration is limited. Food-contact compliance is verified under Regulation (EU) No 10/2011 with olive oil simulant D2 and gas chromatographic analysis of paraffin migration, while US FDA 21 CFR 177.1520(c) 2.1/2.2 is applied for olefin polymer extractables in the finished cap. The production process uses injection moulds with cold runner systems and unscrewing cores for 32–48 cavities; cycle time is set by unscrewing actuation rather than cooling, typically 8–12 s, and injection velocity is capped at 150 mm/s to avoid jetting at the gate and surface splay on the outer shell. The cap formats converted include edible oil bottle caps, soy sauce caps, vinegar caps and ketchup flip-top closures with induction seal liners.

    Multidrop stack moulds for cosmetic flip-top closures and the torque-retention envelope

    Cosmetic and personal care closures require a different balance of mould fill, hinge flex endurance and low odour transfer. A typical compound is 100 wt% CC3054 with 1.5–2.5 wt% colour masterbatch and 0.1–0.2 wt% antioxidant; no external wax or metallic stearate is used where lacquering or physical vapour deposition metallisation is planned, because surface migration of low-molecular-weight additives raises adhesion failure in PVD aluminium and UV-curable lacquer systems, as detected by ISO 2409:2020 cross-cut adhesion testing. Cosmetic-packaging compliance for indirect product contact is assessed under Regulation (EC) No 1223/2009, while REACH Annex XVII Entry 52 restricts phthalates in the flexible hinge; this grade is not specified for direct implantable or parenteral contact. The production equipment is a multidrop stack mould of 2 × 32 or 2 × 48 cavities on a 4,500–6,500 kN press; melt temperature is 200–225 °C, holding pressure decays from 70 MPa to 30 MPa over 1.8–2.5 s, and cooling time of 5–7 s is required before unscrewing. Torque retention is measured with a calibrated torque meter following ASTM D3474-18, and the release torque window is established after 24 h conditioning at 23 °C and 50% relative humidity. Finished articles include flip-top caps for shampoo, conditioner, body wash and lotion bottles, together with fragment-free break-off orifice caps for inverted squeeze packaging.

    On industrial pail lid lines running 48–64-cavity open-stack moulds, cycle-time differences of 2.0 s per cycle accumulate into an output loss of approximately 3,600–5,400 shots per day, making solidification kinetics the controlling variable in HDPE grade selection. In this application, CC3054 is blended at 100 wt% with 2.0–3.0 wt% carbon black masterbatch and 0.05–0.10 wt% processing aid; for lids requiring UN performance-oriented packaging certification, the formulation is not modified, but the assembled pail and lid are tested to 49 CFR 178.602 drop and 178.605 stacking criteria. The conversion process uses 20:1 L/D screws with general-purpose metering profiles, melt temperature at 210–240 °C, and mould cooling at 10–15 °C; ejection is specified after 8–12 s when the part surface temperature falls below 70 °C to avoid pull-out at the gasket groove. The main process defect is doming caused by differential shrinkage across the 0.8 mm top surface and the 2.5 mm peripheral rim; it is controlled by holding pressure decay profiles from 65 MPa to 35 MPa over 2.5 s. The lid configurations manufactured include 10 L, 20 L and 25 L pail lids, tamper-evident tear-band lids, and lids with EPDM gasket seats for solvent-containing industrial products.

    Free Quote

    Competitive SABIC HDPE CC3054 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC HDPE CC3054 is an injection-moulding high-density polyethylene copolymer developed for rigid packaging applications in which environmental stress cracking resistance, balanced melt fluidity, and controlled organoleptic neutrality are required simultaneously. The grade is supplied with a density of 0.954 g/cm³ when tested according to ISO 1183-1, and a melt mass-flow rate of 3.2 g/10 min at 190 °C/2.16 kg determined by ISO 1133-1. Published representative values for tensile stress at yield and flexural modulus fall within 26–28 MPa and 1050–1150 MPa using ISO 527-1/-2 and ISO 178, respectively. These values are non-warranted typical data generated on injection-moulded test specimens, not lot-release specifications.

    Property Representative value Test method
    Density 0.954 g/cm³ ISO 1183-1
    Melt mass-flow rate 3.2 g/10 min ISO 1133-1
    Tensile stress at yield 26 MPa ISO 527-1/-2
    Flexural modulus 1080 MPa ISO 178
    Notched Charpy impact at 23 °C 4.5 kJ/m² ISO 179-1/1eA
    Vicat softening temperature A50 126 °C ISO 306
    ESCR F50, 10% Igepal CO-630, 50 °C >1000 h ASTM D1693, condition B

    How Does CC3054 Compare with General-Purpose Injection Moulding HDPE?

    The differentiation arises from molecular architecture and comonomer incorporation rather than from density alone. General-purpose HDPE injection grades frequently operate at melt mass-flow rates between 5 g/10 min and 20 g/10 min. Those higher-flow grades permit rapid cavity filling, but the combination of shorter chain relaxation time, reduced tie-molecule density, and altered lamellar thickness can reduce environmental stress cracking resistance. CC3054 operates at 3.2 g/10 min, which preserves an ESCR reserve while remaining processable in high-cavitation closure moulds. The grade is therefore positioned for caps and closures that require mechanical integrity under contact with surfactants, carbonated beverage contents, or light chemical formulations, rather than for thin-wall disposable containers where melt fluidity is the only controlling variable.

    Compared with high-density polyethylene pipe resins in the 0.945–0.955 g/cm³ density interval, CC3054 does not possess the low melt-flow characteristics required for thick-wall extrusion. Pipe grades are commonly specified at 0.2–0.5 g/10 min under 190 °C/5 kg or by high-load melt index at 21.6 kg. CC3054 is not designed for that rheological envelope. Compared with polypropylene closure resins, CC3054 has lower rigidity and lower continuous-use temperature resistance, but it retains a different notch-impact and stress-cracking response at refrigeration temperatures. Comparative selection must therefore be based on cap torque retention, liner adhesion, and sealing-surface deformation over the intended shelf life, not on single-point flexural modulus alone.

    In high-cavitation injection moulding of beverage closures, processing behaviour is governed by gate freeze time, holding-pressure transfer, and ejection force. With CC3054, melt temperatures between 200 °C and 240 °C are typically applied on reciprocating-screw machines with screw L/D ratios of 20:1 to 25:1 and compression ratios of 2.2:1 to 2.8:1. Mould temperatures from 10 °C to 30 °C are used to reduce cooling time while avoiding condensation-induced surface defects in humid production halls. Injection velocity is set as a pressure-limited profile rather than as a single velocity step. The transition from velocity control to holding pressure should be set before visible gate freeze to avoid sink marks in the cap disc and to maintain consistent seal-ring dimensions.

    On production-scale 48-cavity and 64-cavity hot-runner tools, cavity-to-cavity fill variation is controlled by manifold thermal balance and individually adjustable nozzle tips. Published data for CC3054-specific fill variance in all cavity configurations is limited; however, the general relationship between melt mass-flow rate and hot-runner pressure drop indicates that a grade at 3.2 g/10 min may require gate diameters at the upper end of conventional closure practice when wall thickness is below 0.6 mm. Tool qualification should therefore include cavity-pressure transducers and part-mass studies under production holding pressure, not rely on supplier melt-flow data alone.

    When Multi-Cavity Tooling Demands Gate Freeze and Holding Pressure Optimisation

    The processing window for CC3054 in multi-cavity tools is not constrained by an exceptionally narrow degradation threshold, but by the interaction between holding-pressure time and gate sealing. If holding pressure is removed before gate freeze, melt in the cavity can reverse-flow into the runner and create non-uniform shrinkage along the closure skirt. If holding pressure is maintained too long, cycle time increases without measurable gain in dimensional stability. For closure shot weights of 1.5–3.0 g, holding-pressure durations from 0.5 s to 2.0 s are common. The optimum value within that interval must be established by cavity-pressure response and part-mass capability, not by machine timer alone.

    The apparent viscosity of HDPE at 230 °C and shear rates typical of closure injection, approximately 10³–10⁴ s⁻¹, is sufficiently shear-thinning to permit high injection speed. The no-flow temperature near 125–130 °C nevertheless requires sufficient screw-forward time before solidification. Mould cooling circuits should produce turbulent flow; Reynolds numbers above 10,000 are required to maintain heat-transfer coefficients above 1000 W/m²K in drilled channels. Inadequate turbulence at the cooling-channel boundary layer is a more frequent source of warpage and long cycle times than resin lot variation.

    Melt filtration is a further practical boundary condition. Typical screen packs for CC3054 injection processing use 60/80/100 mesh combinations, producing a maximum particle passage in the range of 149–250 µm. Pressure drop across a clean screen pack at 230 °C and screw speeds of 50–100 rpm is generally below 20 bar. A rising trend beyond 40 bar indicates screen blinding, melt contamination, or partial oxidative gel formation. General-purpose polyolefin screws with a feed-zone depth of 0.15–0.20 D and a metering-zone depth of 0.06–0.08 D are sufficient. Backpressure is normally set between 5 bar and 12 bar; sustained backpressure above 20 bar may increase screw recovery time and become cycle-limiting without improving melt homogeneity.

    Environmental stress cracking resistance in CC3054 is evaluated by the constant-strain method of ASTM D1693, condition B, with the test environment maintained at 50 °C in aqueous 10% Igepal CO-630 solution. Values above 1000 h at F50 are considered indicative of safe service in contact with aggressive liquid formulations, including beverage closures, detergent caps, and pharmaceutical closures. The slow crack growth mechanism is governed by tie-molecule disentanglement and lamellar stress concentration. ESCR therefore declines when regrind content is increased above 20–30% because repeated shear history reduces the high-molecular-weight fraction and can increase gel concentration. Regrind use must be validated by ESCR after compounding, not by melt-flow measurement alone.

    Organoleptic neutrality is controlled by the base resin formulation and stabilisation package. CC3054 is not recommended for applications requiring retort sterilisation above 121 °C sustained for more than 30 min, because the additional heat history may shift extractive profiles and accelerate antioxidant consumption. In carbonated soft drink closures, carbon dioxide retention is dominated by the liner barrier rather than by the HDPE skirt. The contribution of CC3054 is mechanical retention, torque stability, and crack resistance under repeated carbonation pressure cycling. Closure performance must therefore be tested under top-load, application torque, removal torque, and seal-integrity protocols defined by the filling line, not by resin tensile data alone.

    Regulatory Status and Food-Contact Compliance Boundaries

    Compliance statements must be verified against the current supplier regulatory datasheet because final article status depends on migration testing, food simulant selection, and actual use conditions. The matrix below identifies the principal regulatory frameworks applicable to HDPE food-contact and packaging use.

    Framework Relevant provision Verification requirement
    European Union Commission Regulation (EU) No 10/2011 Overall migration limit 10 mg/dm² for plastic food-contact articles; specific migration limits apply to additives
    United States FDA 21 CFR §177.1520 Olefin polymer classification; conditions of use and food simulants must be defined for the finished article
    REACH Regulation (EC) No 1907/2006 Registration required for EU manufacture or import; declared formulation must not contain SVHC above 0.1%
    RoHS Directive 2011/65/EU Restricted substances below maximum concentration values for electrical and electronic equipment applications

    CC3054 is normally supplied as cylindrical pellets in 25 kg multi-wall bags or in bulk road tankers. Pellet bulk density is approximately 560 kg/m³ for silo capacity calculations. Pellets require no routine pre-drying unless opened packaging has been stored at relative humidity above 60% for more than 24 h; in that case desiccant drying at 80 °C for 2–3 h is sufficient but must not exceed 4 h to avoid pellet oxidation. Silos should be purged with dry air and maintained below 40 °C. Feed-throat temperature should be held below 50 °C to prevent pellet bridging and inconsistent screw feeding.

    The product should not be combined with unsaturated hydrocarbon oils, strong oxidising acids, or heavy-metal-containing lubricants that catalyse oxidative chain scission during processing. Long-term outdoor exposure requires UV stabilisation; CC3054 is supplied in natural form without a specified UV package, and black masterbatch addition must be evaluated for closure odour and migration performance. At continuous-use temperatures above 80 °C, creep resistance and environmental stress cracking resistance of HDPE decline. The resin is therefore assigned to cold-fill, ambient, and moderate-temperature packaging rather than hot-fill or retort service.