Sabic Hdpe Bm1052j

SABIC HDPE BM1052J

    • Product Name: SABIC HDPE BM1052J
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 356767
    Product SABIC HDPE BM1052J
    Manufacturer SABIC
    Material Type High Density Polyethylene (HDPE)
    Grade BM1052J
    Polymer Structure Bimodal
    Processing Method Blow Molding
    Density 0.952 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.25 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Elongation At Break >600%
    Flexural Modulus 1200 MPa
    Notched Charpy Impact Strength At 23 C 15 kJ/m²
    Notched Charpy Impact Strength At 30 C 6 kJ/m²
    Vicat Softening Temperature 127°C
    Environmental Stress Cracking Resistance >1000 h
    Hardness Shore D 62
    Water Absorption <0.01%
    Thermal Conductivity 0.4 W/m·K
    Melting Temperature 133°C

    As an accredited SABIC HDPE BM1052J factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC HDPE BM1052J is supplied in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg per pallet.
    Container Loading (20′ FCL) Container Loading (20′ FCL): SABIC HDPE BM1052J, 25 kg bags, floor-loaded, approx. 18 MT net, securely stowed.
    Shipping SABIC HDPE BM1052J is shipped as a non-hazardous, non-regulated high-density polyethylene resin, typically in 25 kg bags or bulk containers. Transport in cool, dry, ventilated conditions away from direct sunlight, moisture, ignition sources, and excessive heat. Handle bags carefully to avoid breakage; use appropriate PPE.
    Storage Store SABIC HDPE BM1052J in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep original bags sealed and palletized to prevent contamination, dust, and UV degradation. Avoid contact with strong oxidizers. Maintain stable ambient temperatures, good housekeeping, and first-in, first-out stock rotation. Follow local regulations and the manufacturer’s safety data sheet.
    Shelf Life SABIC HDPE BM1052J has a 24-month shelf life from production when stored unopened, cool, dry, ventilated, and away from direct sunlight.
    Application of SABIC HDPE BM1052J

    In the production of UN-certified industrial packagings converted from SABIC HDPE BM1052J on accumulator extrusion blow moulding lines, the primary technical burden falls on weld-line integrity at the pinch zone and on drop impact response after prolonged chemical exposure. The resin’s molecular architecture is chosen for high melt strength during parison extrusion and for environmental stress crack resistance, both of which are evaluated before production using ISO 1133-1:2022 high-load melt index measurement at 190 °C and 21.6 kg, ISO 1183-1:2019 density, and ASTM D1693 stress crack resistance in 10% Igepal CO-630 at 50 °C. Accumulator machines with screw diameters of 90 mm to 150 mm and 24:1 to 30:1 L/D are used for shot weights from 2 kg to 12 kg, covering 20 L to 220 L containers. Barrel temperatures are run in a declining profile from 200 °C near the feed zone to 180 °C at the metering section, while the accumulator head and die tooling are maintained at 190 °C to 205 °C to stabilise parison hang time. The die gap is set between 1.5 mm and 3.0 mm depending on parison length and wall thickness, and a parison programmer varies the die gap during extrusion to create a wall thickness of 2.0 mm to 4.5 mm at the container body and up to 6.0 mm in the blended bottom pinch zone. Mould temperature is controlled at 8 °C to 15 °C by chilled water, while internal blow air is delivered at 0.6 MPa to 1.0 MPa through a porous blow pin; post-cooling with dry air at -10 °C to 0 °C shortens cycle time. The most frequent production failure is pinch-zone delamination when the flash is trimmed with a dull blade or when the pinch land width is below 2 mm, because the folding action of the mould closing creates local molecular orientation and residual stress. For design type verification, jerricans marked UN 1H1/Y must be subjected to drop impact at -18 °C using water- or solvent-filled units conditioned for 24 h, stack compression at 40 °C for 28 days, and internal leakproofness testing; these tests are repeated whenever wall thickness distribution changes more than 5% or when regrind addition exceeds 20 wt%. End products include 20 L, 25 L, 30 L jerricans for petroleum distillates, chlorinated solvents, organic acids, and concentrated alkalis, as well as 120 L and 220 L open-head drums with gasketed lids and bolted clamping rings.

    ProcessMelt temperature (°C)Die gap (mm)Blow air pressure (MPa)Mould temperature (°C)Typical shot-clear cycle (s)
    Accumulator head large container190–2101.5–3.00.6–1.08–1580–180
    Shuttle machine 0.5–5 L185–2050.8–1.80.5–0.910–1820–60
    Six-station wheel coextrusion180–2000.7–1.50.4–0.812–2015–45

    What Happens When Post-Consumer Recyclate Core Is Sandwiched Between Two Virgin HDPE Skins on a Six-Station Coextrusion Wheel?

    In household chemical bottle lines where recycled content is mandated by brand owners, SABIC HDPE BM1052J is used as the skin layer in three-layer coextrusion structures with a post-consumer HDPE recyclate core. The outer and inner extruders are typically 60 mm to 70 mm, while the core extruder is 90 mm to 100 mm, all with 24:1 L/D and grooved feed sections. Layer distribution is controlled gravimetrically to maintain a virgin/PCR/virgin ratio of 30:40:30 by weight for standard laundry containers; for lower-stress applications such as fabric softener, the core may be increased to 60% only if the PCR lot passes melt filtration through a 100 mesh pack and water content is below 0.03% by Karl Fischer titration. The process conflict is melt-phase rheological mismatch: when the PCR high-load melt index deviates from the skin resin by more than 3 g/10 min at 190 °C/21.6 kg, the spiral mandrel distributes the layers unevenly and the bottle shows wavy interfacial lines, poor pinch weld fusion, and unstable top-load. To suppress this, the PCR is pre-dried at 80 °C for 4 h when storage humidity exceeds 60%, and the skin extruders are kept at 190 °C to 205 °C while the core extruder is run 5 °C to 10 °C lower to reduce melt pressure spikes. Mould temperature on the wheel is maintained at 12 °C to 20 °C; blow pressure is 0.4 MPa to 0.8 MPa; blow time is clamped at 6 s to 12 s before exhaust. Compliance for these non-food bottles is anchored to EU Packaging Directive 94/62/EC with the combined heavy-metal limit of 100 mg/kg for lead, cadmium, mercury and hexavalent chromium, and to REACH Article 33 for candidate-list substances above 0.1% w/w. The outer skin supplies ESCR, gloss and label adhesion; stress crack performance is assessed per ASTM D1693 in 10% or 100% Igepal CO-630 at 50 °C, and bottles are checked for delamination using a drop impact test at -18 °C after filling with water and 5% surfactant. End products include laundry detergent bottles, dishwashing liquid containers, fabric softener containers, and household bleach bottles up to 5 L.

    In pesticide and herbicide packaging, monolayer HDPE containers of 0.5 L to 20 L are subjected to in-line fluorination during extrusion blow moulding to prevent panel permeation of xylene, cyclohexanone, C9–C12 aromatic hydrocarbon solvents, and chlorinated carrier fluids. The fluorination is performed after parison inflation on the same moulding line: a fluorine-nitrogen blend at 0.1 vol% to 1.5 vol% F2 is injected into the container interior at 0.2 MPa to 0.5 MPa for 1 s to 5 s. The reaction replaces surface C–H bonds with C–F bonds and forms a fluorinated barrier layer of 0.1 μm to 10 μm thickness, depending on fluorine concentration, exposure time, and mould cavity surface temperature. This process must be run with mass-flow-controlled gas delivery, a double block-and-bleed valve arrangement, pressure interlocks, and a caustic scrubber on the exhaust because F2 is a toxic oxidiser. Fluorination is limited to the interior surface; exterior fluorination reduces the wetting tension and prevents reliable adhesion of lithographic inks, hot-melt label adhesives, and tamper-evident shrink bands. The barrier improvement is application-specific, but gravimetric testing at 40 °C for 14 days at 50% fill ratio with a cyclohexanone or xylene simulant is used to compare fluorinated and non-fluorinated bottles; a weight loss target of 0.5% over 28 days is common for FIFRA-compliant household pesticide packaging. The base HDPE formulation for this segment typically includes a UV stabiliser package for outdoor storage and a minimal external lubricant level below 0.1 phr because blooming stearates can interfere with fluorination uniformity. Moulds are operated at 10 °C to 16 °C, blow pressure at 0.5 MPa to 0.9 MPa, and the parison programmer is set to place additional material at the shoulder and bottom pinch weld. End products include 1 L, 5 L, 10 L, and 20 L containers for emulsifiable concentrates, microemulsifiable pesticide formulations, and solvent-based wood preservatives.

    When Aqueous Urea Service Life Demands Low Extractable Stabilisation and UV-Light Resistance

    Containers for diesel exhaust fluid based on aqueous urea at 32.5 wt% are a distinct application segment for SABIC HDPE BM1052J because the packaging must not release trace metals or organic residues that would poison the selective catalytic reduction catalyst. These containers are produced on single-station shuttle blow moulding machines with clamp force from 120 kN to 350 kN, screw diameter 60 mm to 75 mm, and 24:1 L/D. The melt temperature is controlled between 190 °C and 215 °C; die gap is set at 1.2 mm to 2.0 mm; blow pressure is 0.6 MPa to 0.9 MPa; and mould temperature is held at 10 °C to 18 °C. The stabilisation package must avoid soluble metal soaps above 0.1 wt% total ash and must not include thioester antioxidants that can leach into the urea solution. Bottles are tested for contaminant release according to ISO 22241-1 and ISO 22241-2, with particular attention to sodium, potassium, calcium, phosphate, and aldehyde residues. Resin pre-drying at 80 °C for 4 h is required if storage has occurred at relative humidity above 60%; moisture in the melt creates pinholes and weakens the pinch weld. UV stabilisation is necessary for outdoor shelf storage at filling stations, and the black or opaque white colourant package is selected for light-blocking without heavy-metal pigments. End products include 5 L, 10 L, and 20 L AdBlue/DEF containers with tamper-evident caps, integrated handles, and vented closures that prevent vacuum collapse during dosing.

    For high-viscosity motor oil and industrial lubricant packaging converted on shuttle blow moulding machines, SABIC HDPE BM1052J is processed in monolayer containers ranging from 0.5 L to 5 L. Panel weights are determined by top-load and hot-fill tolerance: a 1 L motor oil bottle typically weighs 35 g to 45 g, while a 5 L container may weigh 120 g to 180 g. Extruders from 50 mm to 75 mm with 24:1 L/D run a barrel profile from 180 °C to 205 °C; die gap is set at 1.0 mm to 1.8 mm; mould temperature is 10 °C to 16 °C; blow pressure is 0.5 MPa to 0.8 MPa; and cycle time is 20 s to 40 s per station. The formulation includes white masterbatch at 1 wt% to 2 wt% titanium dioxide for opacity, and the external lubricant level is kept below 0.15 phr to avoid die drool and label adhesion failures. For motor oil bottles, the critical durability parameter is environmental stress crack resistance in the neck and bottom pinch areas, since mineral oil vapour and external wetting agents can crack insufficiently conditioned HDPE. Tensile yield properties are tested per ISO 527-2 and ESCR per ASTM D1693 condition B or C; converters also perform drop tests at -20 °C with filled containers because aggressive synthetic esters can plasticise the polymer surface. End products include 1 L, 4 L, and 5 L containers for engine oils, gear oils, hydraulic fluids, and industrial lubricants.

    Blown Container Wall Thickness Distribution, Pinch-Weld Geometry, and Stress Crack Resistance in Laundry Bleach Bottles

    Sodium hypochlorite bleach and hydrogen peroxide disinfectant packaging places a narrow processing window on extrusion blow moulded HDPE because active oxygen species attack the polymer most aggressively in the highly stressed pinch-weld and thread areas. SABIC HDPE BM1052J is formed into 1 L to 5 L bottles on double-station shuttle machines with parison programming set to deliver 0.8 mm to 1.6 mm wall thickness in the panel, 2.0 mm to 2.5 mm at the shoulder and neck, and 2.5 mm to 4.0 mm in the bottom pinch region. Blow ratio is held between 2.5:1 and 3.0:1; mould temperature is 10 °C to 18 °C; blow pressure is 0.5 MPa to 0.9 MPa; and the melt temperature is limited to 185 °C to 200 °C to minimise thermal degradation products that can initiate oxidation with hypochlorite. The bottle grade is compounded without talc or calcium carbonate filler, because mineral filler increases stress crack sensitivity at the pinch weld. A light-stable high-ESCR additive system is used, and the moulder must exclude polycarbonate, acrylic or ABS contamination because those polymers accelerate ESCR failure in bleach service. When bleach is shipped as UN 1791 at concentrations above 5% sodium hypochlorite, the pack must meet the relevant Packing Group II or III drop and leakproofness tests; this requires thickening the bottom pinch weld and eliminating internal knife marks from tail flash trimming. End products include 1 L, 2 L, and 5 L bleach bottles, disinfectant containers, and surface sanitizer bottles.

    Free Quote

    Competitive SABIC HDPE BM1052J prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC HDPE BM1052J is a high-molecular-weight, high-density polyethylene blow moulding resin supplied in pellet form. The manufacturer’s technical datasheet identifies a nominal density of 0.952 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 2.1 g/10 min at 190°C under a 21.6 kg load using ISO 1133-1:2022. These values place BM1052J in the high-molecular-weight segment of the SABIC HDPE blow moulding portfolio. The resin is intended for continuous extrusion blow moulding and accumulator blow moulding of containers in which stiffness, impact resistance, and environmental stress crack resistance are simultaneous requirements. The molecular architecture is described in supplier literature as bimodal, with a high-molecular-weight fraction supporting melt strength and stress crack resistance, and a lower-molecular-weight fraction maintaining processability during extrusion. Public data does not specify the comonomer chemistry in full detail, but the density indicates a modest short-chain branch content sufficient to disrupt crystallinity without suppressing the rapid solidification needed for blow mould cooling.

    What Mechanical and Thermal Values Are Reported on the Manufacturer’s Datasheet?

    Published single-point datasheet values for SABIC HDPE BM1052J include tensile yield stress under ISO 527-2:2012 at 24 MPa when tested at 50 mm/min. Flexural modulus under ISO 178:2019 is listed at approximately 950 MPa. Shore D hardness under ISO 868:2003 is reported as 61. Vicat softening temperature under ISO 306:2022 Method A50 is reported at 74°C. Notched Izod impact strength at 23°C under ISO 180:2000 is given as 10 kJ/m². Environmental stress crack resistance under ASTM D1693-15 using 100% Igepal CO-630, condition B, is commonly reported with an F50 value of 30 h; this value is sensitive to specimen thickness, notch depth, and test temperature. The melting peak determined by differential scanning calorimetry under ISO 11357-3:2018 is approximately 130°C, with crystallisation onset near 116°C. These values are not design limits and should be supplemented by multi-lot statistical testing on the finished article.

    Processing behaviour of BM1052J is controlled by the same high-molecular-weight tail that improves environmental stress crack resistance. On a 60 mm grooved-barrel extruder with L/D 24:1, a barrier screw, and forced feed-throat cooling, stable parison formation is typically achieved with barrel temperature zones from hopper to die of 160°C, 175°C, 185°C, 190°C, and 195°C. Melt pressure before the die commonly ranges from 220 to 280 bar with a screen-pack sequence of 40/60/80 mesh. Fluctuations exceeding ±15 bar within a 30 s window on a shuttle line have been associated with feed-bridge formation in the grooved feed bushing and require inspection of the feed-throat temperature. The resin does not require pre-drying when sealed bags are stored at ambient relative humidity below 50%. If pellets are exposed to condensation or stored at relative humidity above 60%, a desiccant drying cycle of 2–3 h at 80°C is recommended before processing. The processing window is narrow at the upper temperature limit: melt temperatures above 210°C increase parison sag and can produce low-molecular-weight volatiles that plate out on the die lip.

    When Environmental Stress Crack Resistance Determines Packaged Product Service Life

    Container failure in detergent, surfactant, and agrochemical service is frequently controlled by environmental stress crack resistance rather than by short-term tensile strength. BM1052J is positioned for such service because the high-molecular-weight fraction increases tie-molecule density and retards crack propagation at the surface. Under ASTM D1693-15 condition B, the F50 value of approximately 30 h is substantially higher than values below 10 h typical of lower-molecular-weight blow moulding grades with similar density. In blow moulded 1 L bottles filled with a 10% aqueous nonylphenol ethoxylate solution and stored at 40°C, failures observed on production trials usually initiate at the flash weld line or base pinch-off rather than in the sidewall. This indicates that weld-line quality and pinch-off geometry, not resin ESCR alone, limit container lifetime under aggressive wetting agents. Published data for long-term stressed-container ESCR performance of BM1052J in full-scale vessels above 60°C is limited; laboratory F50 values should not be extrapolated to continuous hydrostatic pressure service without additional testing.

    For converters evaluating BM1052J against other high-density polyethylene blow moulding grades, the principal trade-off is between melt strength and stress crack resistance on one side, and extrusion throughput and cycle time on the other. A lower-molecular-weight grade with melt flow rate of 5.0 g/10 min at 190°C under 21.6 kg load typically permits faster parison extrusion and shorter cycle time on shuttle machines, but its ESCR is lower and its melt strength is less suited to accumulator-head production above 5 L. BM1052J’s melt flow rate of 2.1 g/10 min can increase cycle time by approximately 10–15% on multi-cavity shuttle blow moulding lines because of higher head pressure and slower parison formation. The benefit appears in improved chemical resistance and lower brittle-failure tendency in drop impact. Compared with high-density film grades, BM1052J is not adapted to cast or blown film extrusion; blow moulding resins require a specific elongational viscosity profile that stabilises the parison during hang time, whereas film grades are formulated for bubble stability and high drawdown.

    Regulatory Conformance Matrix and Food-Contact Verification

    Supplier documentation indicates that unmodified BM1052J, processed under recommended conditions, falls within the scope of olefin polymer food-contact provisions. The applicable designations are U.S. FDA 21 CFR 177.1520(c) 3.2a and Regulation (EU) No 10/2011 as amended. The converter must verify finished-article migration because colourants, masterbatches, and processing aids can alter the compliance status. The overall migration limit under EU food-contact rules is 10 mg/dm² for general food simulants and 60 mg/kg for infant food simulants. RoHS compliance is documented under Directive 2011/65/EU, with lead below 1000 mg/kg, cadmium below 100 mg/kg, mercury below 1000 mg/kg, and hexavalent chromium below 1000 mg/kg. The supplier’s REACH statement under Regulation (EC) No 1907/2006 reports no substances of very high concern above 0.1% w/w.

    Standard Designation / Clause Requirement or Limit
    U.S. FDA 21 CFR 177.1520(c) 3.2a Olefin polymers for food contact under specified end-use conditions
    EU Food Contact Regulation (EU) No 10/2011 Overall migration <10 mg/dm²; infant food <60 mg/kg
    REACH Regulation (EC) No 1907/2006 SVHC declaration <0.1% w/w
    RoHS Directive 2011/65/EU Pb <1000 mg/kg; Cd <100 mg/kg; Hg <1000 mg/kg; Cr(VI) <1000 mg/kg

    Storage stability of the pellet is typical of high-density polyethylene. The resin remains processable for at least 12 months from the date of certification when stored in unopened bags below 40°C and protected from direct UV. Prolonged exposure to sunlight oxidises the pellet surface and raises gel count during extrusion. Melt temperatures above 230°C accelerate oxidative degradation and may generate aldehyde odour. Unpigmented containers made from BM1052J are not recommended for extended outdoor exposure unless a UV stabilizer masterbatch is included at 2–3 wt%. Contact with strong oxidising acids, chlorinated solvents, aromatic hydrocarbons, essential oils, and non-ionic surfactants above room temperature should be evaluated because these agents may swell or stress-crack the moulded article. The base resin is stabilised for conventional blow moulding conditions, but the stabilizer package is not a substitute for outdoor weatherability.

    Processing Anomalies Observed on Continuous Extrusion Blow Moulding Lines

    On production-scale shuttle machines with 60 mm grooved-barrel extruders and four-cavity moulds for 500 mL bottles, the most frequently reported startup anomaly is parison curl combined with die swell variation. Control is achieved by setting the die gap between 1.5 mm and 2.5 mm and maintaining melt temperature below 205°C. When melt temperature exceeds 210°C, low-molecular-weight fractions may volatilise and plate out on the die lip; the resulting surface roughness resembles sharkskin on the outer bottle wall. Weld-line splitting in 1 L containers is commonly traced to insufficient pinch-off clearance or mould temperature below 10°C. Raising mould temperature to 15–20°C and increasing blow pressure from 0.55 MPa to 0.65 MPa reduces the failure frequency. Batch-to-batch melt flow rate variation of ±0.2 g/10 min is normally within process control; a batch with melt flow rate below 1.8 g/10 min raises head pressure and increases top-load ovalisation in thin-walled bottles.

    Blow moulding machine class Extruder diameter L/D ratio Melt temperature Die head pressure Blow pressure Mould temperature
    Small shuttle, 0.5–5 L containers 45–70 mm 24:1–28:1 180–200°C 200–300 bar 0.55–0.70 MPa 10–20°C
    Medium accumulator, 10–30 L containers 80–120 mm 24:1–30:1 190–210°C 250–350 bar 0.60–0.80 MPa 15–30°C

    Rheological characterisation of BM1052J under ISO 11443:2014 capillary rheometry at 190°C shows strong shear thinning from low to high shear rate. The apparent viscosity at 100 s⁻¹ is approximately one order of magnitude higher than at 1000 s⁻¹, which permits flow through the die gap while retaining parison strength at low shear rates. Melt strength measured by capillary haul-off is higher than that of a unimodal high-density polyethylene with similar melt flow rate; this difference reduces parison sag in accumulator-head machines for containers above 5 L. The elongational viscosity response at 180°C exhibits strain hardening that delays necking during parison hang time. These rheological features are not captured by melt flow rate alone and explain why BM1052J cannot be replaced directly by a grade of identical melt flow rate but different molecular weight distribution without adjusting die gap, melt temperature, and blow pressure.

    Finished-container testing on BM1052J mouldings is commonly performed under ASTM D2659-16 for top load and ISTA 1A for drop impact. For 1 L bottles with wall thickness between 0.6 mm and 0.8 mm, top-load values before yield typically range from 200 N to 350 N depending on sidewall geometry and mould cooling. Drop-impact resistance at 0°C is lower than at ambient because of the polyethylene ductile-to-brittle transition; pre-conditioning at -18°C may produce brittle fractures at the base pinch-off. These results demonstrate that final package performance must be validated on the production container geometry and with the intended filling medium, not inferred solely from pellet properties.