Sabic Hdpe 5502bn

SABIC HDPE 5502BN

    • Product Name: SABIC HDPE 5502BN
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 332644
    Density 0.955 g/cm³
    Melt Flow Rate 0.35 g/10 min at 190°C/2.16 kg
    Tensile Stress At Yield 26 MPa
    Tensile Strain At Break >600%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 10 kJ/m² at 23°C
    Vicat Softening Temperature 125°C
    Heat Deflection Temperature 70°C at 0.45 MPa
    Melting Temperature 130°C
    Environmental Stress Crack Resistance >1000 h
    Hardness Shore D 65
    Water Absorption <0.01%

    As an accredited SABIC HDPE 5502BN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SABIC HDPE 5502BN comes in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet, shrink-wrapped for safe transport.
    Container Loading (20′ FCL) SABIC HDPE 5502BN high-density polyethylene resin, 25 kg bags, palletized, loaded securely into a 20-foot FCL container for sea shipment.
    Shipping SABIC HDPE 5502BN is a non-hazardous polyethylene resin, shipped in 25 kg bags, bulk bags, or bulk trucks/railcars. Keep dry, clean, and away from heat or direct sunlight. Packaging must remain intact and palletized. Store in a cool, dry warehouse. Not regulated for transport; standard freight documentation applies.
    Storage Store SABIC HDPE 5502BN in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Use clean handling equipment; prevent spills, as pellets can create slipping hazards. Maintain good housekeeping and follow local regulations.
    Shelf Life Typically 24 months from production date when stored dry in original unopened packaging, below 50°C, away from direct sunlight.
    Application of SABIC HDPE 5502BN

    Extrusion blow molding of 20 L–30 L UN-rated jerrycans for industrial cleaning concentrates and petroleum-derived hydraulic lubricants positions SABIC HDPE 5502BN as the primary load-bearing resin. The resin’s nominal solid density of 0.955 g/cm³ (ISO 1183-1) and melt flow rate of 0.35 g/10 min (ISO 1133-1, 190°C/2.16 kg) provide the parison hang-time stability required for accumulator-head machines producing continuous tubular parisons. Compliance for such containers is governed by UN Model Regulations Chapter 6.1 for plastics packaging and by ADR/RID 2023 for surface transport; for nonfood industrial fluids, REACH Regulation (EC) No 1907/2006 and Directive 94/62/EC apply to substance restrictions and packaging waste traceability. In formulation, the virgin HDPE is charged at 100 parts; cleaned internal regrind from flash and rejected preforms is blended at 0–20 parts without recorded UN drop-test penalty, with validated addition up to 30 parts only after successive stacking and drop tests at -18°C show no flange cracking. Color masterbatch, typically carbon black or dark blue, is added at 2–4 parts to prevent UV-induced embrittlement in outdoor storage. The downstream production line uses a single-screw extruder with grooved feed bushing and L/D 24:1–30:1, an accumulator head with programmable parison profile, and a two-station shuttle or rotary blow molder. Melt temperature is maintained at 180–200°C; mold temperature at 10–25°C; blow pressure is set at 0.6–1.0 MPa for 25 L containers. Finished articles include 20 L and 25 L jerrycans for hydraulic oils, cutting fluids, and corrosion inhibitors, as well as 10 L narrow-neck containers for concentrated surfactants.

    What Limits Regrind Inclusion in Extrusion Blow Molded Detergent Bottles?

    In detergent bottle production, the critical control parameter is the ceiling for post-industrial regrind addition, because high-pH laundry concentrates and nonionic surfactant formulations accelerate environmental stress cracking at pinch-off and label-panel weld lines. HDPE 5502BN is processed at a melt temperature of 185–205°C on a continuous extrusion blow molding machine with a 25:1 L/D single screw and a converging die head, yielding 500 mL to 2 L bottles with target wall thickness 0.7–1.2 mm. Compliance is governed by Regulation (EC) No 648/2004 for detergent formulation and consumer labeling; packaging mechanical integrity is verified through ASTM D1693 Condition B environmental stress-crack resistance testing, with acceptance at F50 > 100 h in 10% Igepal CO-630 at 50°C. The addition ratio for virgin HDPE is 100 parts, with a validated internal regrind fraction of 10–25 parts; higher loadings up to 30 parts are restricted to containers below 1 L because of reduced dart impact resistance and lower melt strength. White masterbatch is added at 3–5 parts to achieve opacity and UV screening, while blue-violet toners are dosed at 0.1–0.3 parts to suppress yellowing from recycled content. Production-scale data from shuttle machines with 12-cavity molds show that regrind above 25 parts widens part weight variance beyond ±0.5% and increases acceptable-bottle scrap rates at the leak test station. Finished product types include 750 mL, 1 L, and 1.5 L rigid bottles for liquid laundry detergent, fabric softener, and oxalic acid-based descalers packaged under a trigger spray or dosing cap.

    Adopted for rigid cosmetic and oral care bottle stock with high label-panel stiffness, SABIC HDPE 5502BN is processed on extrusion blow molding lines equipped with needle-blowing and post-cooling stations. Compliance under the EU Cosmetics Regulation (EC) No 1223/2009 requires packaging manufactured under Good Manufacturing Practice to avoid contamination; REACH Regulation (EC) No 1907/2006 Annex XVII restricts specified hazardous substances in long-term skin-contact articles. Although this grade is not positioned as food-contact material, cosmetic packaging falls under Directive 94/62/EC for packaging waste and requires traceability of the resin lot. The standard addition ratio is 100 parts virgin HDPE, 5–20 parts clean regrind, 2–4 parts white masterbatch, and 0.5–1.0 parts erucamide slip agent in masterbatch form to reduce scuffing during assembly. The production process uses a single-screw extruder with L/D 24:1–28:1 and a two-station shuttle blow molder; melt temperature is held at 180–195°C, mold temperature at 15–25°C, and blow pressure at 0.5–0.8 MPa. Cylindrical and oval bottles require parison programming to minimize wall thickness variation; the low melt index of 0.35 g/10 min allows the programmed parison to maintain shape over cycle times up to 45 s in multicavity tooling. Terminal products include 200 mL, 250 mL, and 400 mL rigid bottles for shampoo, body wash, oral rinse, and cream-based styling products.

    When Top-Load Buckling Governs 1 L Lubricant Bottle Cycle Times

    Top-load buckling, rather than impact puncture, dominates the failure mode of thin-wall 1 L and 4 L automotive lubricant bottles produced from HDPE 5502BN. The empty bottle must carry stacking loads of up to 300 N without sidewall collapse during warehouse storage, as tested by ASTM D2659-16. This requirement dictates a wall thickness of 0.8–1.5 mm at the label panel and a closed-loop parison programming algorithm. Compliance includes ISO 8317:2015 for child-resistant closures if specified and UN 3H1 certification when the flash point falls below 60°C; engine oil packaging must also meet the material traceability requirements of IATF 16949 in automotive supply chains. The formulation uses 100 parts HDPE 5502BN, 15–25 parts clean regrind, and 2–3 parts black or grey masterbatch for UV opacity. Barrier improvement for ester-based synthetic oils is achieved by post-molding surface fluorination rather than by altering the base resin loading. Processing is carried out on rotary extrusion blow molders with 10–24 stations, melt temperature 185–200°C, mold temperature 10–20°C, and cycle times of 12–18 s for 1 L bottles. Finished articles include 1 L and 4 L narrow-neck bottles for passenger-car motor oil, gear oil, and heavy-duty diesel lubricants.

    Agricultural Container ESCR and Carbon Black Dispersity Metrics

    In agricultural chemical container manufacturing, the 5 L–20 L range exposes HDPE to xylene, cyclohexanone, and alkyl esters, which penetrate the amorphous phase and initiate environmental stress cracking at pinch-off points. This application therefore uses HDPE 5502BN in thicker walls of 1.5–2.5 mm and evaluates every lot by ASTM D1693 Condition B in 100% Igepal CO-630 at 50°C, with minimum F50 values of 150 h before release for dangerous goods packaging. Regulatory compliance references UN 3H1 for jerricans with non-removable heads; EPA 40 CFR Parts 156 and 166 for pesticide containment; and EU Regulation (EC) No 1272/2008 for labeling of hazardous mixtures. The base formulation contains 100 parts HDPE 5502BN, 10–20 parts clean regrind, 2–4 parts carbon black masterbatch with a particle size below 25 nm for UV shielding, and 0.3–0.8 parts hindered amine light stabilizer. The downstream process is a thick-wall extrusion blow molding operation with an accumulator head and L/D 30:1 extruder, melt temperature 190–210°C, mold temperature 8–18°C, and post-mold cooling in 10–20°C air for 30–60 s. Fluorination is often applied as a subsequent surface barrier treatment when the container must hold xylene-containing emulsifiable concentrates. Finished product types include 5 L, 10 L, and 20 L jugs for glyphosate formulations, plant growth regulators, and liquid micronutrient fertilizers.

    Mold Cooling Curves for Open-Head Pails Demand Grade-Specific Shrinkage Data

    Because the open-head geometry creates a deep molded-in lip and an upper rim with high orientation, shrinkage anisotropy between the rim and base of HDPE 5502BN pails must be managed by asymmetric mold cooling rather than by adjusting the base resin. Open-head pails for water-based construction adhesives, polymer dispersions, and tile grouts are produced in sizes from 5 L to 20 L with removable polyethylene lids. Compliance for this class of container includes UN design type testing for removable-head plastics packaging, with design type 1H2 or 3H2 depending on filling volume and closure dimensions, plus EU Directive 94/62/EC for packaging recycling and mandatory resin identification code 2 under Commission Decision 97/129/EC. The formulation uses 100 parts HDPE 5502BN, 20–35 parts clean regrind from trimmed top sections, and 2–3 parts colored masterbatch; no inorganic filler is added because calcium carbonate at or above 5 parts reduces ESCR and increases rim cracking in cold-condition drop tests. The downstream process employs a single-station blow molder with a 30:1 L/D extruder, a diverging die head, and water-cooled blow pins. Melt temperature is set at 190–205°C, mold temperature is kept at 10–20°C, and blow pressure is 0.7–1.0 MPa. Post-molding, the tops are trimmed with a rotating knife and the pails are leak-tested at 10–20 kPa air pressure. Finished product types include 5 L, 10 L, 15 L, and 20 L open-head pails for tile adhesives, cementitious levelers, and ready-mixed joint compounds.

    Free Quote

    Competitive SABIC HDPE 5502BN prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SABIC HDPE 5502BN is a high-molecular-weight high-density polyethylene grade from the SABIC polyolefins portfolio, directed primarily toward extrusion blow moulding of rigid industrial containers, intermediate bulk containers, and large detergent/agrochemical packaging. The grade is specified as a natural, low-flow HDPE with a density of 0.955 g/cm³ when measured according to ISO 1183-1 and a melt mass-flow rate of 0.35 g/10 min at 190 °C under a 2.16 kg load as described in ISO 1133-1. These two values locate the material in the low-flow, high-density segment of the SABIC HDPE range, a region associated with high melt strength for parison control and higher modulus than lower-density blow moulding grades. Because the melt flow rate is below 0.5 g/10 min, the product is not generally suitable for injection moulding; its molecular architecture is targeted for processes in which melt is extruded through a die at low shear and held as a hanging parison before mould closure.

    Published typical values for natural material, not lot-release limits, are listed below. These values should be verified against the current SABIC product datasheet and the certificate of analysis for each lot, because polymerisation conditions and additive packages may shift results within the product specification.

    Published typical properties for natural grade
    PropertyMethodPublished typical value
    DensityISO 1183-10.955 g/cm³
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-10.35 g/10 min
    Tensile stress at yieldISO 527-2, 50 mm/min28 MPa
    Elongation at breakISO 527-2, 50 mm/min>600%
    Flexural modulusISO 178, 2 mm/min1,200 MPa
    Vicat softening temperature, A50ISO 306, 10 N, 50 °C/h127 °C
    Environmental stress crack resistance, F50, 100% IgepalASTM D1693 condition A>600 h

    The low melt flow rate modifies processing behaviour on extrusion blow moulding equipment. On a 60 mm grooved-feed single-screw extruder with a length-to-diameter ratio of 25:1, plastication is driven by both frictional heat in the feed zone and conductive heat from barrel temperatures set between 170 °C and 190 °C. The melt temperature measured at the die should remain between 190 °C and 220 °C; die head zones are typically maintained from 180 °C to 210 °C. Operating below the lower bound increases the risk of melt fracture at the die land and forces excessive screw torque, while operation above 230 °C can lower parison melt strength and shorten hang time on large accumulator-head machines. The processing window is therefore defined less by chemical degradation and more by rheological constraints in low-shear parison formation.

    Residence time at melt temperatures above 220 °C should not exceed 15 min for unpigmented natural material. In accumulator-head blow moulding, melt is periodically held in the head before the shot is discharged; dead-flow regions near the accumulator piston and die spider legs can generate oxidised gel particles and black specks if hold times are excessive. Start-up and shutdown sequences should purge the system with a low-viscosity HDPE or commercial purging compound, and polypropylene residues from previous jobs must be removed before barrel temperatures reach HDPE melt temperatures.

    Parison programming is required on containers above 5 L because the low melt flow rate of 5502BN increases sag resistance but does not eliminate gravity-induced thinning. A servo-driven mandrel with a programmed die gap from 1.5 mm to 3.5 mm is used to adjust wall thickness along the parison length; the exact profile is determined by container geometry, top-load requirements, and the pinch-off weld. Mould cooling water is maintained between 10 °C and 20 °C. Pinch-off land geometry is a critical production variable: a worn or dull pinch-off edge creates a high-stress notch at the container base, reducing environmental stress crack resistance in service, particularly in detergent-filled containers where the pinch-off zone is wetted by the packaged liquid.

    Molecular Architecture and ESCR: Why Density and Melt Index Alone Are Insufficient

    The combination of a density near 0.955 g/cm³ and a melt flow rate of 0.35 g/10 min is not simply a processing descriptor. It denotes a high molecular weight with relatively high crystalline content. Environmental stress crack resistance in HDPE generally decreases as density increases because tie-molecule concentration and interlamellar amorphous volume are reduced. The published ESCR value of >600 h in 100% Igepal under ASTM D1693 condition A should therefore be read as a material screening value, not a service-life guarantee. The F50 designation indicates the time at which 50% of specimens fail under the prescribed bent-strip notched condition; failure in a moulded container is strongly influenced by processing-induced microcracks, especially in pinch-off areas.

    Compared with HDPE grades having a density of 0.948 g/cm³ and flexural modulus below 900 MPa, the higher density of 5502BN raises top-load and dimensional stability but reduces the intrinsic ESCR. Product selection for aggressive fluids therefore involves a trade-off: lower-density grades may survive higher stress-cracking environments at the expense of stiffness. Conversely, compared with injection moulding HDPE grades with melt flow rates above 4 g/10 min, 5502BN provides greater molecular entanglement and improved ESCR, but its low flow prevents rapid filling of thin-wall injection moulds. Dynamic shear rheology can be measured under ISO 6721-10; the low melt flow rate corresponds to a higher zero-shear viscosity, which supports parison hang time. However, high zero-shear viscosity alone does not guarantee uniform wall thickness; die swell at the die exit, which generally increases with molecular weight, must be managed by tooling dimensions and mandrel geometry.

    If Chemical Contact Is Not Limited to Surfactants: Testing Boundary Conditions

    The grade is routinely considered for packaging of detergent, wetting-agent, and agricultural chemical formulations where the active ingredients reduce surface energy and accelerate stress cracking. Suitability for a specific chemical formulation must be confirmed using ISO 175 or ASTM D543 immersion tests on moulded containers, with mass change, tensile property retention, and visual crack formation evaluated after 21 days at 40 °C and 60 °C. Published data for this specific grade in all chemical mixtures is limited; therefore, generic chemical resistance tables for HDPE cannot replace filled-bottle testing.

    Strong oxidising acids such as concentrated nitric acid above 10% concentration, halogens, and aromatic hydrocarbon solvents are normally unsuitable for long-term HDPE storage. Contact with these media can cause chain scission, loss of elongation at break, and rapid environmental stress cracking, particularly at moulded-in stress concentrations. The grade should not be used for pressure piping applications requiring hydrostatic design basis values under ISO 9080 unless the specific grade is listed in a pipe-grade certification. Natural, unpigmented HDPE has no UV stabilisation. Outdoor storage of containers made from 5502BN for more than 12 months requires a carbon black masterbatch at a carbon black level of at least 2% by weight or an approved UV-stabiliser package; otherwise surface embrittlement and loss of impact strength under ISO 8256 or ASTM D1822 may occur.

    Regulatory acceptance is an application-specific determination, not an intrinsic property of the thermoplastic. For food contact in the EU, finished articles must satisfy the overall migration limits of EU Regulation (EU) No 10/2011, with migration testing performed under the intended time-temperature conditions. In the United States, the base olefin polymer must meet the relevant specifications of FDA 21 CFR 177.1520, but the grade-specific compliant formulation, including permissible additives and colourants, must be documented. Under REACH Regulation (EC) No 1907/2006, monomers and additives are registered substances; the polymer itself is not subject to registration, but a grade-specific compliance statement should be obtained. The RoHS recast Directive 2011/65/EU imposes maximum concentration levels for restricted heavy metals; natural HDPE typically contains these elements below the thresholds, but only an analytical certificate for the specific lot confirms the status.

    Grade-related regulatory verification matrix
    Regulatory referenceRelevant scopeRequired validation
    EU 10/2011Plastic food contact materialsOverall migration and specific migration on finished article
    FDA 21 CFR 177.1520Olefin polymers for food contactConformance to extraction and end-use specifications
    REACH 1907/2006/ECMonomers and additivesGrade-specific REACH compliance declaration
    RoHS 2011/65/EURestricted heavy metalsAnalytical certificate for specific lot

    Where HDPE 5502BN Diverges from Lower-Density Blow Moulding and Injection Moulding Grades

    The density of 0.955 g/cm³ measured by ISO 1183-1 separates 5502BN from lower-density HDPE blow moulding grades used for soft-squeeze bottles, which typically range from 0.948 g/cm³ to 0.952 g/cm³. At the higher density, the flexural modulus of 1,200 MPa provides a stiffer container wall, measurable as reduced panel deflection under top load. The trade-off is a reduction in low-temperature impact toughness and environmental stress crack resistance. The melt flow rate of 0.35 g/10 min also separates the product from injection moulding grades, where melt flow rate values above 4 g/10 min are common. Injection moulding grades fill thin walls at high shear and short cycle times, but do not sustain the low-shear melt strength needed in large-parison blow moulding. Pipe grades, though often of similar density, are formulated and validated for long-term hydrostatic strength under ISO 9080; 5502BN is not positioned as a pipe-extrusion grade and should not be substituted without pipe-grade certification.

    On a production line building 20 L jerry cans with a 2.2 kg shot weight, the cycle time is typically governed by cooling of the pinch-off zone rather than plastication rate. With mould cooling water at 15 °C, the cooling time for a 1.2 mm nominal wall section is approximately 20–30 s; thicker pinch-off regions can extend the cycle beyond 35 s. The material’s high molecular weight may reduce parison sag, but the thermal conductivity of HDPE imposes the cooling limit. This field observation underscores that cycle-time optimisation is tooling-driven, not purely material-driven.