| HS Code | 888519 |
| Gradename | Reliance Industries HDPE M5018L |
| Manufacturer | Reliance Industries Limited |
| Polymertype | High Density Polyethylene (HDPE) |
| Density | 0.950 g/cm3 |
| Meltflowindex | 18 g/10 min at 190°C/2.16 kg |
| Tensilestrengthatyield | 28 MPa |
| Elongationatbreak | 100% |
| Flexuralmodulus | 1100 MPa |
| Vicatsofteningtemperature | 120 °C |
| Heatdeflectiontemperature | 75 °C at 0.45 MPa |
| Notchedizodimpactstrength | 30 J/m at 23°C |
| Shoredhardness | 65 |
| Moldingshrinkage | 1.5-2.5% |
| Meltingpoint | 130-135 °C |
| Processingtemperature | 180-230 °C |
| Moldtemperature | 20-60 °C |
As an accredited Reliance Industries HDPE M5018L factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Reliance Industries HDPE M5018L comes in 25 kg PP woven bags with inner PE liner, palletized and stretch-wrapped for transport. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Reliance Industries HDPE M5018L in 25 kg bags; loads ~25 MT loose or 20–22 MT palletized. |
| Shipping | Reliance Industries HDPE M5018L is typically shipped in 25 kg polyethylene bags, palletized and stretch-wrapped, or in bulk bags/containers. It is non-hazardous and not transport-regulated. Store sealed in a cool, dry, ventilated area away from direct sunlight, heat, moisture, and ignition sources. Always follow supplier SDS. |
| Storage | Store Reliance Industries HDPE M5018L in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep in tightly closed original bags or containers on pallets. Protect from moisture, dust, and physical damage. Avoid prolonged UV exposure. Follow local regulations and the safety data sheet. |
| Shelf Life | Reliance Industries HDPE M5018L has a 24-month shelf life when stored cool, dry, and well-ventilated, away from sunlight and heat. |
Reliance Industries HDPE M5018L is specified for high-speed injection molding of thin-wall food containers through a melt flow rate of 18 g/10 min at 190 °C/2.16 kg when tested in accordance with ASTM D1238 and a nominal density of 0.950 g/cm³ per ASTM D792. In 0.45 mm to 0.80 mm nominal wall dairy and deli tubs, the low melt viscosity allows filling of multicavity stack molds at flow-length-to-wall-thickness ratios of 250:1 to 350:1 without raising melt temperature above 230 °C, where oxidative degradation would initiate chain scission and reduce dart impact strength. Process settings on a reciprocating screw machine with a 20:1 to 25:1 L/D ratio and a compression ratio of 2.0:1 to 2.5:1 are maintained at barrel temperatures of 190 °C to 230 °C, nozzle temperature 190 °C to 215 °C, and mold cooling water temperatures of 10 °C to 30 °C. Injection velocities from 200 mm/s to 350 mm/s are used with hold pressure in the range of 40 MPa to 60 MPa; insufficient hold pressure below 35 MPa produces sink marks beneath stacking lugs, and excessive hold pressure above 65 MPa in thin sidewalls increases molded-in stress and warpage. The formulation ratio for colored dairy tubs is typically 1.5 wt% to 2.5 wt% titanium dioxide white concentrate combined with 0.5 wt% to 1.0 wt% slip/antiblock masterbatch; regrind from trimmed rims and reject tubs is limited to 20 wt% maximum and is dried to below 0.05% moisture by weight before blending. Food-contact compliance is assessed under FDA 21 CFR 177.1520(c) 3.2a and Commission Regulation (EU) No 10/2011 with overall migration limit of 10 mg/dm² or 60 mg/kg simulant, depending on surface-to-volume ratio. Terminal products are round and rectangular dairy tubs, deli containers, and portion cups with tear-off or snap-on lids, where consistent stack denesting force is controlled by sidewall taper and additive migration rather than by mold release spray.
In closure molding with M5018L, tamper-evident band sections are typically gated through a ring or multiple pin gates at the closure skirt, and the band wall is often specified at 0.35 mm to 0.55 mm. Because this zone freezes before the outer shell when the mold is run at 10 °C to 25 °C, the gate must have sufficient diameter—commonly 0.8 mm to 1.2 mm per cavity—to transmit pack pressure before gate freeze. If gate freeze time is below 0.5 s to 1.0 s, the band will exhibit incomplete filling or low tear strength; if the gate is too large, the gate vestige will remain above the closure inner surface beyond the specified 0.10 mm maximum protrusion and create seal interference. Melt temperature is held at 190 °C to 215 °C for non-carbonated dairy and condiment closures, with hold pressure from 45 MPa to 65 MPa and injection velocity from 120 mm/s to 220 mm/s. A color masterbatch is incorporated at 1.0 wt% to 2.0 wt%, and a slip masterbatch is dosed at 2 wt% to 3 wt% so that the final erucamide level does not exceed 0.10 wt% to 0.12 wt%; above this level, surface bloom can raise removal torque variation and reduce printing adhesion on the closure top. The grade is assessed under FDA 21 CFR 177.1520(c) 3.2a and (EU) No 10/2011 for dairy and condiment closure use, but it is not recommended for aggressive solvent-based contents or for carbonated beverage closures requiring high environmental stress crack resistance under ASTM D1693 Condition B. Terminal products are snap-on closures with breakaway tamper-evident bands for LDPE or HDPE bottles containing still liquids, milk, cream, sauces, and dry seasonings.
In injected housewares such as stackable storage totes and garage crates, M5018L is processed at melt temperatures up to 230 °C to fill ribs of 0.6 mm to 1.2 mm thickness attached to a nominal wall of 1.5 mm to 2.2 mm. The main dimensional conflict is differential shrinkage between the thick stacking boss and the adjacent thin web; after demolding, the boss region can shrink by 1.8% to 2.5% while the thin web stabilizes at 1.2% to 1.8%. Mold temperature is set from 15 °C to 35 °C, and cooling time is extended by 1.5 s to 2.5 s for each additional 0.5 mm of boss diameter beyond 5.0 mm to avoid sink and post-mold warpage. Tunnel gates of 1.0 mm to 1.5 mm diameter are located into thick sections, not into the thin ribs, because flow hesitation in the rib can produce cold-fracture weld lines at the rib base. Regrind of sprues and runners is reintroduced at 25 wt% to 30 wt% maximum, with granulate screened through a 3 mm mesh and dried to below 0.05% moisture to prevent hydrolysis of residual additives. Compliance for colored houseware articles is reviewed under EU REACH Annex XVII entries 23, 63 for cadmium and lead, and where articles may be handled by children, EN 71-3 migration limits for heavy metals apply. Terminal products are stackable storage totes, household crates, and garage organizers with molded-in handles and load-bearing stacking lugs.
For injection molded pails of 5 L to 20 L capacity intended for waterborne coatings and cleaning solutions, M5018L is processed with a melt temperature of 190 °C to 220 °C and mold temperature of 15 °C to 30 °C. Handle ears with wall sections of 4.0 mm to 6.0 mm are fed by tab or diaphragm gates of 2.0 mm to 3.0 mm, and pack pressure is held at 50 MPa to 65 MPa for 4 s to 6 s to prevent sink at the ear-to-wall junction. Outdoor-grade pails incorporate a UV stabilizer masterbatch at 0.5 wt% to 1.5 wt%, with carbon black concentrate at 2.0 wt% to 2.5 wt% where long-term exterior storage is required; regrind is kept at 20 wt% maximum. The high-flow grade reduces cycle time compared with lower-flow HDPE, but it is not suitable for pails holding strong surfactant solutions above 40 °C or aromatic hydrocarbon-based liquids because of environmental stress crack propagation under ASTM D1693 Condition A in 10% Igepal at 50 °C. Terminal products are industrial pails with tear-off lids and handle-grip ears for water-based adhesives, joint compounds, detergents, and non-hazardous cleaning solutions.
The following compliance matrix summarizes the main statutory and normative assessments encountered when M5018L is used in the listed downstream routes.
| Application route | Core regulatory standards and methods | Acceptance or measurement criterion |
|---|---|---|
| Thin-wall dairy containers | FDA 21 CFR 177.1520(c) 3.2a; EU No 10/2011 | Overall migration ≤ 10 mg/dm² or 60 mg/kg |
| Non-carbonated closures | FDA 21 CFR 177.1520(c) 3.2a; EU No 10/2011 | Erucamide retention ≤ 0.12 wt% to avoid bloom |
| Colored housewares | EU REACH Annex XVII entries 23, 63; EN 71-3 where relevant | Lead and cadmium migration limits per substance-specific migration |
| Industrial pails | ASTM D1693 Condition A | ESCR screening in 10% Igepal at 50 °C |
| Diagnostic labware | ISO 10993-5; USP <661>; ISO 11137-1 | Cytotoxicity grade 0–1; validated irradiation dose |
| Personal care dispensing plugs | EC 1223/2009; REACH Annex XVII | Orifice tolerance ±0.05 mm; heavy metal limits |
For non-implantable diagnostic housings and sample transport tubes, M5018L may be screened only after a documented extractables and leachables review because the grade is not supplied with USP Class VI certification as a default. If the application requires a tube with a 0.8 mm to 1.2 mm wall and a closed length of 80 mm to 120 mm, the high melt flow allows core pin deflection to be reduced through lower injection pressure, but the melt temperature should be limited to 180 °C to 210 °C to minimize low-molecular-weight oxidation products. Cleanroom molding is conducted under ISO 14644-1 Class 8 conditions, with HEPA-filtered cooling air and stainless steel tools. The formulation excludes regrind unless a two-step granulation and contamination-control validation is completed; antistatic masterbatch, if required, is evaluated at 0.5 wt% to 1.0 wt% but may alter extractables profiles. Dimensional stability is a hard boundary: autoclaving at 121 °C will distort HDPE because the continuous use temperature ceiling is below 90 °C; therefore, terminal sterilization is limited to ethylene oxide or gamma irradiation at validated doses, with dose mapping per ISO 11137-1. Cytotoxicity screening follows ISO 10993-5 and physicochemical testing follows USP <661>; for EU In Vitro Diagnostic Regulation (EU) 2017/746, published data for this specific configuration is limited and batch-specific migration testing is normally required. Terminal products are specimen transport vials, cuvette housings, and non-sterile laboratory containers where the olefinic base resin offers low water absorption and chemical inertness.
In dispensing plugs and flip-top overcaps with a 0.3 mm to 1.0 mm orifice, the melt flow of M5018L fills the micro-core pin feature without high injection pressure; however, because the melt viscosity is lower than that of a 2 g/10 min high-density polyethylene, any parting-line mismatch above 0.02 mm to 0.03 mm or uneven clamp force across a multicavity base produces visible orifice flash and a sharp edge at the dispensing outlet. Molds for this closure class are therefore fitted with hardened inserts, a mold fit tolerance of ±0.02 mm, and clamp force per cavity equivalent to 3 kN/cm² to 5 kN/cm² projected area to hold the parting line closed during injection velocities of 150 mm/s to 250 mm/s. Melt temperature is profiled from 190 °C at the rear zone to 210 °C at the nozzle; mold cooling is set at 15 °C to 25 °C. Formulation includes a silicone-based lubricant masterbatch at 0.3 wt% to 0.8 wt% and color concentrate at 1.0 wt% to 1.5 wt%; excessive lubricant above 1.0 wt% can cause delamination at the hinge and reduce fit retention on bottle necks. For personal care packaging, the closure must not affect the cosmetic product inside the bottle, and compliance is reviewed under European Regulation (EC) No 1223/2009 for the finished cosmetic article, while the plastic material itself is assessed under REACH with restrictions on lead, cadmium, and polycyclic aromatic hydrocarbons under Annex XVII. Terminal products are dispensing plugs for shampoo and lotion bottles, dishwashing liquid flip-tops, and overcap plugs where the orifice diameter is checked by optical comparator against a tolerance of ±0.05 mm.
Competitive Reliance Industries HDPE M5018L prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Reliance Industries HDPE M5018L is a high-flow high-density polyethylene injection-moulding grade. The material is specified by a nominal melt flow rate of 18 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022 and a nominal density of 0.950 g/cm³ according to ISO 1183-1:2019 or ASTM D1505. The grade is formulated for thin-wall moulded packaging, caps and closures, housewares, toys, and industrial containers in which cycle time and mouldability dominate product selection. Unlike high-molecular-weight film and blow-moulding HDPE grades, M5018L has a shorter average chain length and a narrow molecular weight distribution; this reduces melt viscosity and melt strength simultaneously. Consequently, the material fills thin sections at lower injection pressure than lower-flow HDPE, but it is unsuitable for extrusion blow moulding because parison stability cannot be maintained.
At 18 g/10 min, M5018L belongs to the high-flow segment of HDPE injection-moulding resins. On cold-runner tooling with rectangular edge gates, gate freeze time is shortened relative to HDPE grades with melt flow rates of 5 g/10 min or lower; this can shorten hold-pressure time but also creates a risk of sink marks when hold pressure is removed before the gate is sealed. Production-scale experience on a 120-tonne hydraulic injection moulding machine using a general-purpose screw of 20:1 L/D with a compression ratio of 2.8:1 indicates that barrel zone settings of 190 °C, 210 °C, and 220 °C with a nozzle temperature of 210 °C and mould temperatures of 20–40 °C provide an acceptable processing range for this melt-flow class. Peak injection pressure during filling of a 1.0 mm wall section is typically 15–25% lower than a 5 g/10 min HDPE under identical tool geometry, although exact values depend on gate diameter, runner length, and melt temperature. Published data for this specific configuration is limited; the above values are consistent with industrial practice for HDPE of this melt-flow class.
Because the non-Newtonian shear-thinning response at shear rates above 100 s⁻¹ reduces apparent viscosity sharply, screw-speed changes alter melt temperature and part weight more than in lower-flow HDPE grades. Processors should therefore verify shot weight after any screw speed adjustment greater than 10%. Low melt viscosity also requires controlled decompression after screw retraction to prevent drooling from an open nozzle; screw suck-back settings below 2 mm are often insufficient, while excessive decompression above 5 mm can introduce air streaks. Nozzle shut-off valves or negative pressure control are preferred for high-speed multi-cavity production.
Solid-state performance reflects the 0.950 g/cm³ base density. The following properties are typical values from manufacturer technical literature and are not specification limits.
| Property | Standard | Typical Value |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022 (190 °C/2.16 kg) | 18 g/10 min |
| Density | ISO 1183-1:2019 | 0.950 g/cm³ |
| Tensile yield stress | ISO 527-2/1A | 25 MPa |
| Tensile elongation at break | ISO 527-2/1A | 200% |
| Flexural modulus | ISO 178 | 850 MPa |
| Melting temperature | ISO 11357-3 | 130 °C |
| Vicat softening temperature | ISO 306/B50 | 121 °C |
The tensile and flexural values indicate a semi-rigid olefin with moderate crystallinity. A density of 0.950 g/cm³ places M5018L below the 0.960 g/cm³ grades used for rigid blow-moulded containers, translating into lower melt strength and slightly lower modulus. The lower density also improves resistance to warpage in flat, thin articles. Ductility remains adequate for snap-fit closures and container lids when part design avoids sharp notches; notched impact values are sensitive to gate location and should be checked on production parts. Because of the lower molecular weight relative to pipe grades, environmental stress crack resistance is limited. Exposure to polar hydrocarbons, surfactant-containing liquids, or high sustained stress can induce cracking earlier than high-molecular-weight HDPE grades. Environmental stress crack resistance is typically evaluated under ASTM D1693; M5018L values are expected to be low.
Where parison melt strength controls product quality, M5018L is displaced by lower-flow HDPE grades. The contrast with HDPE M60075, a nominal 0.75 g/10 min extrusion blow-moulding grade, illustrates the primary differentiation.
| Attribute | HDPE M5018L | HDPE M60075 |
|---|---|---|
| Melt flow rate (ISO 1133-1:2022) | 18 g/10 min | 0.75 g/10 min |
| Density (ISO 1183-1:2019) | 0.950 g/cm³ | 0.960 g/cm³ |
| Primary processing | Injection moulding | Extrusion blow moulding |
| Melt strength | Low, unsuitable for parison stability | Sufficient for bottle and jerrycan parisons |
| Typical product design | Thin walls, high flow length, short cycle time | Cylindrical containers requiring wall uniformity |
The melt flow rate difference of more than one order of magnitude reflects higher average molecular weight and greater entanglement density in M60075. Under identical cylinder temperatures, M5018L flows significantly farther, but the lower melt strength results in parison drawdown and poor wall-thickness control in extrusion blow moulding. Conversely, M60075 would require elevated melt temperature or high injection pressures in thin-wall injection moulding, increasing cycle time and energy consumption. The 0.950 g/cm³ density also gives M5018L slightly lower modulus and lower inherent barrier than the 0.960 g/cm³ grade, which can be relevant when designing containers for oxygen-sensitive or moisture-sensitive products.
Food-contact suitability is governed by regional regulatory frameworks. As a high-density polyethylene, M5018L is designed to be evaluated under FDA 21 CFR 177.1520 and EU Commission Regulation (EU) No 10/2011. Finished-article compliance depends on conversion conditions, colourants, and functional additives; overall migration and specific migration testing on the final container are required for food-contact end use. The material can be processed for consumer packaging when supported by REACH registration and RoHS declarations from the manufacturer. No intentionally added phthalates or heavy-metal-based pigments are present in the natural grade, but compounded colours must be qualified separately.
In multi-cavity thin-wall tools with wall sections below 1.2 mm, the low melt viscosity of M5018L permits lower melt temperature and lower injection velocity while preserving complete cavity filling. Cycle time is often governed by gate cooling; the high flow grade allows early transition from injection to hold pressure and a reduced screw buffer. On a 60 mm screw diameter machine, a cushion loss of 2–3 mm may be sufficient to generate short shots or cavity imbalance in tightly toleranced multi-cavity tools; therefore, screw cushion, hold-pressure time, and switch-over position should be recorded with ±1 mm resolution. If flashing occurs at the parting line, reducing nozzle temperature in 10 °C increments is preferred over exceeding rated clamp force.
Mould temperatures below 20 °C shorten cooling time but can freeze the gate before packing is complete, producing sink marks and warpage; temperatures above 40 °C extend cycle time and may reduce productivity. For hot-runner systems, gate freeze is influenced by the crystallisation temperature of HDPE, typically above 118 °C for this density class; process setup should therefore treat gate temperature as a physical boundary rather than as an arbitrary setpoint. Restricted-flow valve gates or sequential valve-gate systems should be adjusted to accommodate the quick decompression of the melt stream after injection.
Because M5018L is moisture-tolerant, drying is unnecessary for virgin material stored under dry ambient conditions. If surface condensation occurs after warehouse storage at relative humidity above 60%, pre-drying at 80 °C for 2 h in a desiccant dryer suppresses surface splay. The grade is not weatherable without stabilisation; outdoor exposure requires carbon black or a hindered amine light stabiliser masterbatch to prevent UV chain scission and tensile property loss. It is also not recommended for pressure-pipe applications requiring long-term hydrostatic strength under ISO 9080, nor for aggressive detergent packaging where environmental stress crack resistance is the limiting property. In those applications, grades with lower melt flow rate and higher molecular weight are required.