    Specifications
    HS Code 719513
    Density 0.952 g/cm³
    Melt Flow Index 190 C 2 16 Kg 0.09 g/10 min
    Melting Point 130–135 °C
    Crystallinity 70–80%
    Tensile Strength At Yield 24–25 MPa
    Elongation At Break >600%
    Flexural Modulus 1100–1200 MPa
    Vicat Softening Temperature 125 °C
    Escr F50 100 Igepal >1000 h
    Notched Izod Impact Strength 300–350 J/m
    Shore D Hardness 65
    Water Absorption <0.01%
    Thermal Conductivity 0.45 W/m·K
    Volume Resistivity >10^16 Ω·cm

    As an accredited Reliance Industries HDPE E52009 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Reliance Industries HDPE E52009 comes in 25 kg polyethylene bags, palletized and stretch-wrapped, with 40 bags (1,000 kg) per pallet.
    Container Loading (20′ FCL) 20′ FCL loading for Reliance HDPE E52009: 25 kg bags, approximately 17–18 MT net, securely stowed in standard dry container.
    Shipping Reliance Industries HDPE E52009 is typically shipped as a non-hazardous thermoplastic in 25 kg polyethylene bags, palletized and stretch-wrapped. It is transported in 20'/40' containers, trucks, or railcars under dry conditions. Store away from heat, moisture, and direct sunlight; keep packaging sealed during transit. Follow applicable transport regulations.
    Storage Store Reliance Industries HDPE E52009 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, ignition sources, and strong oxidizing agents. Keep original bags or containers tightly closed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and temperatures above 50 °C. Follow good housekeeping and local regulations; consult the SDS.
    Shelf Life Reliance Industries HDPE E52009 has a 24-month shelf life when stored in original packaging, cool, dry, away from direct sunlight.
    Application of Reliance Industries HDPE E52009

    Processing of Reliance Industries HDPE E52009 as a heavy-duty blown film begins with a nominal density of 0.952 g/cm³ and a melt flow rate of 0.9 g/10 min at 190°C/2.16 kg under ASTM D1238-20. This viscosity range produces the bubble stability required for film thicknesses between 50 µm and 150 µm, but it also transfers a significant portion of total energy input into shear heating across the screw. Barrel profiles on 24:1 to 30:1 L/D single-screw extruders are set from 180°C in the feed zone to 210°C in the metering zone, and die temperatures are held at 210°C to 220°C. Adapter and melt temperatures must remain below 240°C because oxidative chain scission in this grade becomes visible as pressure fluctuation and gel specks. The annular die gap is adjusted between 1.4 mm and 2.0 mm; blow-up ratio is normally set between 2.5:1 and 4.0:1 to balance machine-direction and transverse tensile strength. The frost line is placed at 6 to 10 die diameters above the air ring, and air temperature is maintained below 30°C to prevent bubble flutter at high line speeds. Pellets supplied without surface moisture can be fed directly; if storage relative humidity exceeds 60% and surface moisture exceeds 0.05% by weight, the material is pre-dried at 80°C for 2 h in a desiccant hopper dryer.

    Fabricated film from this grade is characterised under ASTM D882-18 for tensile properties and under ASTM D1709-22 for falling dart impact. The relationship between die-lip residence time and impact retention should be established through a designed experiment, because published data for E52009-specific dart values are limited. Heat sealing is performed at 160°C to 185°C using dwell times of 0.5 s to 1.2 s; seal-bar temperatures above 195°C induce film distortion and reduce seal strength. The film can be corona-treated to 40 mN/m to 45 mN/m for print and lamination, but treatment level decays rapidly if the film is stored for more than 30 days at 23°C.

    What limits parison sag in 20-litre extrusion blow moulding of E52009?

    In extrusion blow moulding of 20 L to 30 L industrial containers, the processing window is defined primarily by parison drawdown. E52009 has a melt flow rate of 0.9 g/10 min at 190°C/2.16 kg, which is high enough to avoid melt fracture in thin land areas but low enough to retain parison shape only if die temperature is controlled. Accumulator-head machines with diverging die gaps of 2.0 mm to 3.5 mm are preferred for shot weights above 1.5 kg. Die temperature is maintained at 195°C to 205°C; mould temperature is set at 20°C to 30°C for rapid solidification. Mandrel and bushing should be selected to deliver a parison wall thickness of 3.0 mm to 5.0 mm, and pinch-off flash is kept below 12% of shot weight to avoid overloading clamp tonnage in 100 t to 250 t presses. As the parison hang time increases beyond 10 s, diameter swell and local thinning become unacceptable; lowering melt temperature by 3°C to 5°C and shortening the die land by 0.5 mm to 1.0 mm restores wall-thickness uniformity within ±0.2 mm.

    Containers intended for dangerous goods are tested under UN 1H1 non-removable-head packagings; the drop impact at -18°C and hydraulic pressure retention at 100 kPa for 30 min are required according to packing group. Food-contact articles are verified against FDA 21 CFR 177.1520 and, for European markets, (EU) No 10/2011 with overall migration limited to 10 mg/dm². The final article must be tested after induction sealing because seal lacquers and closure liners can increase extractables beyond resin-level compliance.

    Microduct and cable-conduit conversion of E52009 is performed on a grooved-feed extruder with 24:1 to 30:1 L/D and a continuous screen changer fitted with 100 mesh to 150 mesh screens. This filtration train is required because incidental gel nuclei in HDPE with a density of 0.952 g/cm³ can survive melting and produce surface streaks on the inner wall. Barrel temperatures are maintained at 190°C in the compression zone and 215°C at the die head; the melt temperature at the breaker plate is not permitted to exceed 225°C. Vacuum sizing is performed at −0.2 bar to −0.4 bar with water temperatures of 15°C to 25°C. For 12 mm to 25 mm outer-diameter conduit, wall thickness is held between 1.0 mm and 1.8 mm. Crush resistance is measured according to ASTM D2412-21, and impact behaviour is checked through ISO 11173:2011. Carbon-black masterbatch is introduced at 6% to 8% by weight via side feeder after the melting zone; hopper dry-blending is avoided because it leads to stripe formation and variable weathering resistance.

    Geomembrane Flat-Die Extrusion and Textured-Surface Roll Stack Parameters

    Flat-die extrusion of E52009 into smooth or textured geomembrane sheet uses melt temperatures of 220°C to 235°C at the die lip and a die gap of 2.0 mm to 2.8 mm. A gear pump is placed between the screw and the die to reduce pressure surge to ±0.5 bar, which is necessary to hold sheet thickness to ±3% across a 2000 mm die. The three-roll calendering stack is normally operated at 70°C, 80°C, and 60°C from top to bottom. Embossed surfaces are formed with a patterned rubber or steel roll at 50°C to 70°C, and nip pressure is limited to 20 N/mm to 40 N/mm; higher pressure reduces thickness without improving peel strength and can generate transcrystallinity that lowers interfacial shear. Hot-wedge seams are evaluated under ASTM D6392-12 for peel and shear. Stress cracking resistance is determined under ASTM D5397-20 in 10% Igepal CO-630 at 50°C; project specifications must define minimum notched constant tensile load failure time because published E52009-specific values for textured geomembrane are limited.

    For geomembrane service in contact with potable water, certification is not automatic from resin data. Parallel testing under NSF/ANSI/CAN 61 is required for North American potable-water contact, while European applications may require migration testing under (EU) No 10/2011 or national regulations. The carbon-black loading for UV stabilisation in exposed geomembranes is maintained at 2% to 3% by weight with masterbatch, and dispersion is verified by pressure rise across the screen pack; an increase above 5 bar within 8 h indicates agglomeration.

    Coextrusion of E52009 as the structural skin layer in multi-layer barrier films is designed around its higher density and modulus relative to linear low-density polyethylene. The skin extruder is typically 24:1 to 28:1 L/D, set at 200°C to 215°C, and connected to a multi-layer die with adjustable inner and outer die gap. In a three-layer film with LLDPE skins or with an EVOH core, E52009 is used at 20% to 40% of total thickness to increase puncture resistance without raising heat-seal initiation temperature above 110°C. The die gap for the E52009 layer is kept at 1.0 mm to 1.4 mm to avoid melt instability at the layer interface. Adhesion to tie resin is checked before blending; if the tie resin contains amine-modified polyethylene or high levels of oleamide, interlayer streaks and delamination can appear because additives migrate to the interface. Films are evaluated for seal strength under ASTM F88/F88M-21 and for puncture under ASTM D5748-19. Published data for E52009 in this specific multi-layer layer distribution is limited, so pilot-line trials are required to determine the minimum skin-layer thickness before dart impact falls below the package specification.

    Application areaStandard or regulationTest mandateTypical acceptance boundary
    Industrial blow-moulded containersUN Model Regulations 1H1Drop impact at -18°C, hydraulic pressure 100 kPa/30 minNo leakage or rupture after impact; pressure retention for 30 min
    Food-contact finished articlesFDA 21 CFR 177.1520Olefin polymers for food contactResin compliance only; finished article must pass extraction testing
    Food-contact films(EU) No 10/2011Overall migration≤10 mg/dm²
    Heavy-duty sack filmASTM D1709-22Falling dart impactSet by package specification
    ConduitASTM D2412-21 / ISO 11173:2011Parallel-plate crush, impactPer project specification

    If the resin is reprocessed at 50% in-plant regrind for carry-out sacks

    When E52009 is reprocessed with in-plant regrind for heavy-duty carry-out sacks, the ratio of regrind is capped at 50% by weight unless melt flow rate and density are re-tested per ASTM D1238-20 and ASTM D1505-18 after every shift. Regrind from edge trim and start-up scrap contains additional oxidative history, which shifts the MFR upward and narrows the bubble stability window. The incoming blend is measured for melt flow rate; an upward shift of more than 0.2 g/10 min from the virgin baseline of 0.9 g/10 min indicates that the regrind fraction must be reduced or that the extrusion temperature must be lowered by 5°C to 8°C. Screen packs are set at 60/80/100 mesh to remove gel specks, and the die gap is widened by 0.2 mm to 0.3 mm to compensate for the higher elasticity of degraded chains. The resulting sacks are tested for cold drop impact at −10°C and for seal integrity under ASTM F88/F88M-21; because regrind reduces notched tensile impact more than it affects stiffness, the acceptance threshold must be derived from the specific fabrication line rather than from virgin-grade datasheet.

    Free Quote

    Competitive Reliance Industries HDPE E52009 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Reliance Industries HDPE E52009 is a high-density polyethylene blow moulding resin characterised by a nominal melt flow rate of 0.9 g/10 min at 190°C/2.16 kg and a nominal density of 0.952 g/cm³. The grade is supplied as pellets and is intended for continuous-extrusion and accumulator-head blow moulding of hollow containers, particularly narrow-neck bottles, industrial houseware, and small to medium jerry cans. Because the melt flow rate is below the typical injection moulding HDPE range of 4–8 g/10 min, the material is not designed for thin-wall injection moulding or high-speed spiral-flow filling. The density value places E52009 in the high-stiffness segment of the Reliance Industries HDPE portfolio; this separates it from lower-density blow moulding grades in the 0.945–0.950 g/cm³ range, which are often selected for very large containers where environmental stress crack resistance and low-temperature drop toughness outweigh top-load rigidity.

    Typical values from standard laboratory characterisation are summarised in the following table. These values are not specification limits and are not a substitute for lot-specific certificates of analysis.

    Property Test method Unit Typical value
    Melt flow rate at 190°C/2.16 kg ASTM D1238 g/10 min 0.9
    Density ASTM D1505 g/cm³ 0.952
    Tensile strength at yield ASTM D638 MPa 26
    Elongation at break ASTM D638 % 600
    Flexural modulus ASTM D790 MPa 950
    Notched Izod impact strength at 23°C ASTM D256 J/m 45
    Vicat softening point ASTM D1525 °C 125
    Environmental stress crack resistance, F50 ASTM D1693 h >600
    Hardness, Shore D ASTM D2240 — 64

    Specimen conditioning follows ASTM D618 at 23°C and 50% relative humidity. Tensile properties under ASTM D638 are generated with Type IV specimens at 50 mm/min. The notched Izod value of 45 J/m is a laboratory energy-loss measurement; it does not directly predict container drop performance because blow-moulded articles contain pinch-off zones, weld lines, and variable wall-thickness distribution. The environmental stress crack resistance value of >600 h under ASTM D1693 condition A is generated in 100% Igepal CO-630 at 50°C and should be used only as a comparative ranking indicator for surface-active agent exposure. Finished-container ESCR in actual packaged chemicals can differ substantially due to chemical concentration, storage temperature, and applied hoop stress.

    How Does the 0.9 g/10 min Melt Flow Rate Govern Parison Formation and Die Pressure?

    Parison formation on a blow moulding line is controlled by extruder output stability, melt temperature uniformity, die land length, and melt strength. A melt flow rate of 0.9 g/10 min is a single-point low-shear index; it does not define the extensional viscosity that resists sag after the parison exits the annular die. Nevertheless, the value is low enough to require adequate feed-zone heating and moderate screw speed. On a smooth-bore extruder with a length-to-diameter ratio of 20:1 to 30:1, the barrel profile for this MFR and density class is typically set from 170–190°C in the feed zone, 180–200°C in the compression zone, and 185–210°C in the metering zone. Head and die zones are commonly maintained at 190–210°C. Published machine-specific process data for E52009 across all extruder sizes is limited; these ranges are starting conditions and must be trimmed against parison weight, parison length, and part wall-thickness data.

    High-density polyethylene melts show pronounced shear thinning. As screw speed increases, apparent viscosity declines and viscous dissipation raises melt temperature. A screw speed increase without a compensating barrel adjustment can drive the melt above 220°C, where oxidative chain scission reduces melt strength, increases gel formation, and changes taste and odour in the finished package. The practical melt-temperature control window is narrow; a deviation of ±5°C is frequently observable as a change in parison length and container weight distribution. On accumulator-head machines, melt temperature should be measured at the head rather than inferred from barrel set points, because frictional heating can create a difference of 5–10°C between barrel zones and the actual melt.

    The annular die gap for this viscosity class is generally 1.0–1.8 mm, depending on parison diameter, target wall thickness, and blow-up ratio. An undersized die gap raises die pressure and can produce melt fracture at the die lips; an oversized die gap lowers back pressure and may reduce wall-thickness uniformity. Blow-up ratio is normally controlled between 2:1 and 3:1. Within that range, the parison expands into the mould without excessive sidewall thinning or corner stress concentration. Published data for parison sag and die pressure specific to E52009 is limited; therefore, line qualification on the actual moulding machine is required before production tooling is finalised.

    Accumulator-Head Temperature Profile, Screw Geometry, and Mould Cooling

    Accumulator-head blow moulding machines require a low-shear screw geometry that delivers homogeneous melt to the accumulator without excessive shear heating. For HDPE with a melt flow rate of 0.9 g/10 min, a barrier-free single-stage screw with a compression ratio of 2.5:1 to 3.5:1 is common. The feed depth should be matched to pellet bulk density and diameter. A grooved-feed extruder can improve throughput stability but also generates frictional heat and must be operated with tightly controlled barrel temperatures. Accumulator head zones should be maintained evenly; temperature differences greater than 5°C between zones can create preferential flow, parison curling, and visible wall-thickness variation in the moulded article.

    Pellets do not require deep drying, but surface moisture from condensation can produce porosity and surface splay. If the resin has been stored in an unheated warehouse and transferred to a warmer production floor at relative humidity above 60%, it should be dried for 2 h at 80°C in a desiccant hopper dryer. Trimmed flash and start-up scrap may be re-introduced up to 20 wt% provided the regrind is clean, dry, and handled through a closed loop. Contamination with polypropylene above 2 wt% reduces pinch-off weld strength and can cause delamination. Contamination with polyethylene terephthalate or polyamide creates unmelted inclusions that can block the die lips and produce surface tears during inflation.

    Mould cooling is the dominant cycle-time factor. Water-cooled aluminium or steel blow moulds are typically held at 10–30°C. Lower mould temperatures increase cycle rate but can raise frozen-in stress and cause surface defects, especially in thick sections. Blow air pressure is normally 0.6–0.9 MPa. Clamp force is set by the projected area of the flash and parison; on a 10–20 L jerry can mould, clamp tonnage is selected with a margin above the force generated by blow air. Insufficient clamping produces weak bottom pinch-off and flash tearing. The pinch-off insert should be hard chrome-plated and maintained with a clean compression edge to avoid rounded flash rather than proper melt displacement.

    Melt residence time at processing temperature should be kept below 15 min because repeated thermal cycling depletes stabiliser protection and lowers environmental stress crack resistance. The grade should not be processed above 230°C for extended runs, particularly when regrind is included. Liquid colorants or non-polyolefin carrier masterbatches may cause screw slip and inconsistent shot weight. If colouring is required, a polyethylene-based masterbatch at 2–3 wt% is preferred, with the dosage validated by measuring parison sag, part weight, and container drop performance.

    E52009 is used in small and medium blow-moulded containers in the 1–30 L range where high density contributes to top-load stiffness and chemical resistance. Finished containers intended for UN-certified carriage of dangerous goods must be tested under the applicable transport regime, such as ADR/RID/IMDG; the resin data sheet alone does not confer UN 3H1 certification. Food-contact compliance is not automatic. The grade may be evaluated under 21 CFR 177.1520 and EU 10/2011 for specific finished articles, but migration testing must be performed on the final package with its actual closure and gasket system. Chemical compatibility for aggressive fluids should be evaluated on finished containers by immersion testing according to ASTM D543 or equivalent end-use qualification.

    Relative to high-load melt index HDPE grades with melt flow rates from 0.2 to 0.4 g/10 min, E52009 has lower parison sag resistance and is less suited to very large containers above 60 L or parison lengths above 1 m. The higher density of 0.952 g/cm³ compared with 0.946–0.950 g/cm³ large-part grades provides greater flexural modulus and top-load stiffness but generally sacrifices some environmental stress crack resistance and low-temperature toughness. Processors switching from a lower-density grade should verify cold-drop performance and clamp force, not only melt pressure and cycle time. Unlike polyethylene pipe grades carrying an ISO 9080 hydrostatic classification, no long-term pressure-rating data for E52009 are available; the product is not intended for PE100 pressure pipe service and should not be substituted in pressure piping systems.

    The natural grade is not UV-stabilised. Outdoor service with prolonged sunlight exposure requires a UV stabiliser masterbatch selected for polyolefins and validated by accelerated weathering under ISO 4892-2 or equivalent. The oxidative induction time and long-term thermal stability of the final article depend on the additive package introduced by the converter. The material should not be blended with amine-based additives carried in incompatible carrier resins because phase separation can reduce parison melt strength and create surface defects. Hot-fill performance is determined by part design, wall thickness, and mould cooling history, not by Vicat softening point alone; containers filled above 60°C require elevated-temperature top-load testing on the finished article, such as compression testing under ASTM D2659. Drop impact of finished jerry cans and jugs should be evaluated under ASTM D2463 using conditioned specimens and the actual fill medium; the resin-level notched Izod value is not a substitute for container-level cold-drop performance.

    In comparison with high-flow HDPE injection moulding grades, the principal difference is melt flow path and cycle-time capability. E52009 is not intended for thin-wall parts with flow length-to-wall-thickness ratios above 200:1. Its melt flow characteristics are optimised for extrusion blow moulding rather than spiral-flow-dominated mould filling. The absence of product-specific parison sag data in public technical literature transfers process validation to the converter; production-scale validation should therefore include continuous monitoring of melt temperature, parison length, parison weight, and finished-part weight as the basis for lot-to-lot process adjustment.