    Product Name Ravago HDPE RPEHDW
    Manufacturer Ravago
    Material Family High Density Polyethylene
    Grade Designation RPEHDW
    Form Pellets
    Color White
    Recycled Content Yes
    Density 0.950 g/cm3
    Melt Flow Rate 0.30 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 24 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 600%
    Flexural Modulus 1000 MPa
    Notched Izod Impact 100 J/m
    Heat Deflection Temperature At 0 45mpa 70°C
    Heat Deflection Temperature At 1 8mpa 50°C
    Vicat Softening Point 120°C
    Shore D Hardness 65
    Processing Method Blow molding, extrusion, injection molding

    As an accredited Ravago HDPE RPEHDW factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Ravago HDPE RPEHDW is typically supplied in 25 kg polyethylene bags, with 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) Ravago HDPE RPEHDW high-density polyethylene in 20′ FCL, palletized bags, securely stowed, optimized for safe ocean container shipping.
    Shipping Ravago HDPE RPEHDW is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg polyethylene bags, octabins, or bulk containers on pallets, via truck or rail. Store in a cool, dry, ventilated area away from direct sunlight, ignition sources, and moisture. Follow local transport and environmental regulations.
    Storage Store Ravago HDPE RPEHDW in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed, clean, and labeled. Protect from moisture, dust, and contamination. Stack pallets securely to prevent deformation. Follow first-in, first-out rotation and all local regulations and the manufacturer’s SDS.
    Shelf Life Ravago HDPE RPEHDW has no fixed shelf life; stable under normal storage. Keep dry, cool, out of direct sunlight, in original packaging.
    Application of Ravago HDPE RPEHDW

    What ESCR Thresholds and Parison Programming Parameters Govern Household Chemical Bottle Extrusion?

    In extrusion blow molding of rigid household chemical and agrochemical bottles, the Ravago HDPE RPEHDW grade is allocated only after lot screening against ISO 1133-1:2022 melt mass-flow rate at 190 °C/2.16 kg and density under ISO 1183-1:2019; typical high-molecular-weight HDPE bottle lots fall in the 0.25–0.60 g/10 min MFR and 0.945–0.957 g/cm³ density windows. The compound formulation is built from 95.0–99.5 wt% base HDPE, 1.5–3.0 wt% color masterbatch, and 0.05–0.20 wt% external processing lubricant; external post-consumer recyclate is introduced at 15–35 wt% only for non-food and non-UN packaging, while certified UN 3H1 and 3H2 jerrican stocks typically keep PCR at or below 10–20 wt% to maintain sidewall environmental stress crack resistance under ASTM D1693-21 Method B, 10% Igepal CO-630, 50 °C. Compliance for food-contact variants requires 21 CFR 177.1520 olefin polymer clearance and, where applicable, EU 10/2011 with overall migration below 10 mg/dm²; household chemical packaging additionally tracks REACH Annex XVII and the EU Packaging Directive 94/62/EC. Production-scale equipment for this application consists of continuous shuttle or accumulator-head blow molding machines with 24:1–30:1 L/D single-screw extruders, barrel temperatures profiled from 170 °C feed to 210 °C die head, and parison programming controlling wall thickness over 50–100 points. Die swell in practice ranges 35–70% depending on shear rate at the tooling land and is inversely related to parison hang time; a lot with a melt flow rate above 0.60 g/10 min typically produces visible parison sag on 1–5 L bottle tools and must be compensated by reduced melt temperature or faster mold close. Off-spec batch failure modes observed on production lines include pinch-off weld thinning at the mold parting line, die lines from degraded material at the spider leg, and buckling in sidewall compression tests when the blow-up ratio exceeds 3.5:1. End product types include 0.5–20 L detergent and bleach bottles, agrochemical and industrial cleaner containers, institutional floor-chemical packaging, and UN-certified jerricans for dangerous goods.

    Injection moulded tamper-evident closures and dispensing fitments from HDPE require a narrower melt-viscosity envelope than blow molding; the RPEHDW lot that measures 0.5–1.5 g/10 min under ISO 1133-1:2022 may be used at 40–70 wt% with a controlled-flow HDPE or LLDPE modifier to bring the melt flow into the 4–8 g/10 min range required by high-cavitation closure tooling. The closure compound is formulated with 96.5–99.0 wt% HDPE base, 1.5–3.0 wt% color masterbatch, 0.10–0.40 wt% erucamide slip, and 0.05–0.15 wt% nucleating agent when cycle-time reduction below 7 s is targeted; side-gated or hot-runner molds of 24–96 cavities are filled on 250–650 t toggle-clamp injection molding machines with melt temperatures of 200–240 °C and chilled mold water at 8–15 °C. The compliance framework for food-contact closures is 21 CFR 177.1520 and EU 10/2011 with overall migration 10 mg/dm²; packaging-specific compliance is governed by 94/62/EC and, for child-resistant or tamper-evident functionality, by ISO 8317:2015. Dimensional stability after demolding is validated through ISO 291:2008 conditioning and ISO 527-2:2012 tensile yield at 23 °C; short-shot analysis on multi-cavity molds shows that a 0.3 g/10 min upward shift in lot MFR increases cavity-to-cavity weight variation by up to 0.08 g on 38 mm closure geometries, which in turn alters child-resistant engagement torque. Published data for this specific RPEHDW grade on high-cavitation closure tools is limited; trials with 500 kg batch sizes are recommended to establish inter-lot coefficient of variation under ISO/IEC 17025:2017 quality control. End product types include 28 mm and 38 mm tamper-evident caps, dispensing spouts for detergents, pharmaceutical overcap fitments, and sauce-bottle closures.

    Thermoformed HDPE Sheet for Industrial Dunnage and Reusable Logistics Trays

    Extruded HDPE sheet for industrial dunnage and reusable logistics trays uses the RPEHDW grade when the supplier certificate shows density 0.945–0.962 g/cm³ by ISO 1183-1:2019 and a broad molecular weight distribution inferred from melt flow ratio; the sheet compound is mixed from 98.5–99.8 wt% HDPE, 0.10–0.35 phr primary hindered-phenol antioxidant, 0.05–0.20 phr secondary phosphite stabilizer, and 0.2–0.5 wt% carbon black or 0.3–0.8 wt% UV stabilizer masterbatch when the part remains outdoors. In-plant regrind of thermoforming skeletons is incorporated at 20–50 wt%; higher regrind fractions increase sheet gel count and reduce hot-tensile strength at the thermoforming window, measured by ISO 527-3:2018 on 2.0 mm sheet. Sheet extrusion lines for this application employ 120–150 mm single-screw extruders with 30:1 L/D barrier screws, screen changers with 80–120 mesh packs, melt pumps, and flexible-lip dies with 1.2–6.0 mm adjustable gaps; melt temperatures are held at 185–210 °C and the three-roll stack operates at 70–90 °C. Thermoforming of the sheet is performed on plug-assisted vacuum or pressure formers at sheet surface temperatures of 165–178 °C, with mold temperatures of 50–70 °C; the forming window narrows to ±4 °C when the sheet contains more than 50 wt% regrind. Compliance documentation includes ASTM D638-22 tensile properties, ASTM D790-17 flexural modulus, ASTM D543-21 chemical resistance where battery acid or cutting fluids contact the tray, and EU 94/62/EC. End product types include 1200 × 800 mm pooling trays, automotive engine-component dunnage, returnable logistics bases, and industrial material-handling trays.

    For non-pressure drainage and cable conduit extrusion, HDPE is accepted only when the finished pipe meets EN 13476-3 for corrugated polypropylene and polyethylene drainage systems, ASTM F2306-23 for corrugated polyethylene drainage pipe, AASHTO M294-22 for culvert pipe, and NEMA TC-7 for high-density polyethylene electrical conduit. The compound formulation uses 100 parts HDPE base with a 5.0–6.5 wt% addition of 40% carbon black masterbatch, giving a finished-pipe carbon black content of 2.0–2.5 wt% for UV resistance under ASTM D3350-22 cell classification; a melt mass-flow rate of 0.30–0.70 g/10 min by ISO 1133-1:2022 and density 0.945–0.962 g/cm³ are required to maintain crush resistance and ring stiffness. Production lines are configured as 65–90 mm grooved-feed single-screw extruders, 30:1–36:1 L/D, melting at 180–215 °C and feeding a corrugator with moving mold blocks 100–1200 mm in diameter; internal cooling air and external water sprays set the corrugation wall at 0.8–2.5 mm thickness. The corrugator speed, melt strength from the resin lot, and the vacuum-forming pressure of 0.02–0.08 MPa must be balanced; a resin lot with low molecular weight causes thinning at the corrugation valleys and can drop the 3% ring stiffness below the class limit. The compliance checklist for buried applications is shown in the table below. End product types include 100–1200 mm agricultural drainage lines, highway culverts, stormwater retention laterals, and 32–200 mm high-density polyethylene power and telecommunication conduit.

    Application segmentStandard referenceKey assessed parameter
    Non-pressure corrugated drainageEN 13476-3Ring stiffness class
    Highway culvert pipeAASHTO M294-22Pipe stiffness and impact
    PE electrical conduitNEMA TC-7Crush and impact resistance
    Outdoor UV classificationASTM D3350-22Carbon black content and dispersion

    When HDPE Blown Film Replaces LDPE in High-Stiffness Retail Bag Applications

    When HDPE blown film is down-gauged to 10–25 µm for retail bag applications, the processor selects a high-molecular-weight HDPE with melt index of 0.50–1.20 g/10 min under ISO 1133-1:2022 and density 0.950–0.965 g/cm³; the film compound commonly blends 60–80 wt% HDPE with 20–40 wt% LLDPE to raise Elmendorf tear and puncture resistance, with 1.0–3.0 phr slip/antiblock masterbatch and 2.0–4.0 phr white masterbatch added per 100 parts resin blend. High-stalk HDPE blown film lines with 50–70 mm extruders, 24:1–30:1 L/D barrier screws, and 1.2–2.0 mm die gaps run at blow-up ratios of 3.5:1–4.5:1 and frost line heights of 450–750 mm; melt temperatures are held at 180–220 °C, and bubble stability is maintained by chilled air from an internal bubble cooling system at 8–15 °C. The orientation balance between machine direction and transverse direction is controlled by the stalk geometry: a high BUR above 4.0:1 increases transverse direction shrinkage and can cause print registration drift on 500 mm wide bags. Standards for the application include ASTM D882-18 for film tensile, ISO 6383-2:2010 for tear, ASTM D1709-22 for dart drop, and ASTM D4976-23 for polyethylene film materials; food-contact printed bags require 21 CFR 177.1520 and EU 10/2011. Published data for this specific RPEHDW grade in high-stalk film extrusion is limited, so a 250 kg scouting run is recommended to establish the lot-dependent frost line sensitivity. End product types include 10–25 µm T-shirt grocery bags, produce bags, garment cover film, and retail carry-out sacks.

    Structural Foam Injection Moulding of HDPE Pallets and Returnable Transit Packaging

    Structural foam injection moulding of HDPE pallets and returnable transit packaging using the RPEHDW grade requires a resin melt flow rate between 4–10 g/10 min under ISO 1133-1:2022 or a blend with controlled-flow HDPE to reach this window; the formulation consists of 100 parts HDPE base, 1.0–2.0 phr chemical blowing agent masterbatch based on sodium bicarbonate-citric acid, 2.0–3.0 phr color/UV masterbatch, and optionally 0.10–0.30 phr nucleating agent. The process runs on low-pressure structural foam injection machines with 1000–3500 t clamp force, 120–170 mm screw diameter, melt temperature 200–230 °C, and injection speed 90–180 mm/s; the mold is filled under nitrogen gas counterpressure of 0.10–0.60 MPa to control cell size and skin thickness. Density reduction ranges 10–30% compared with solid HDPE, with an observable processing conflict: above 0.45 phr chemical blowing agent, the unnotched tensile strength measured under ISO 527-2:2012 drops below acceptable pallet load-deflection limits, while below 0.15 phr the foam cell structure collapses in sections thicker than 25 mm. Compliance standards for the pallet application are ISO 8611-1:2021 for static and dynamic loading, ISO 8611-2:2021 for racking tests, and ASTM D638-22 for solid skin tensile tests; logistics packaging must also satisfy 94/62/EC and REACH. The table below summarises the performance evaluation matrix. End product types include 1200 × 1000 mm export pallets, 600 × 400 mm quarter pallets, collapsible bulk containers, and returnable automotive packaging bases.

    Evaluation parameterStandardConditionRelevance
    Static load capacityISO 8611-1:202123 °C, 24 hWarehouse stacking
    Racking strengthISO 8611-2:20211000 kgEdge racking
    Skin tensile modulusISO 527-2:201223 °CCorner impact resistance
    Free Quote

    Competitive Ravago HDPE RPEHDW prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Ravago HDPE RPEHDW is a high-density polyethylene grade supplied in pellet form for extrusion processes in which long-term hydrostatic integrity, slow crack growth resistance, and stable melt processing at low shear rates are the primary selection criteria. The designation RPEHDW identifies the compound within the Ravago HDPE portfolio but does not encode density, melt index, comonomer type, or additive package; those values appear only on the lot-specific certificate of analysis. As with all polyolefin compounds, material acceptance against a specification should be based on supplier-measured values and not on generic HDPE class data.

    Material Identity and Classification Basis

    Polyethylene pipe compounds are classified under ASTM D3350 by thermal, mechanical, and slow crack growth performance. The density value measured by ISO 1183-1 or ASTM D1505 establishes the density cell; HDPE pipe resins frequently fall between 0.945 g/cm³ and 0.955 g/cm³, but the exact cell assignment depends on the current ASTM D3350 density cell boundaries. Melt index cell assignment under ISO 1133-1:2022 at 190 °C and 5.0 kg load depends on lot-specific melt flow rate; pipe extrusion grades typically fall below 1.0 g/10 min. The molecular architecture of the polyethylene is more important than density alone. A bimodal resin with a high-molecular-weight fraction contributes to tie-molecule density, while the low-molecular-weight fraction maintains processability. Under ISO 12162, a material classified as PE100 has an MRS of 10 MPa; PE80 has 8.0 MPa. If RPEHDW is supplied as a PE100-type compound, its minimum required strength is 10 MPa and its hydrostatic design basis is based on 50-year extrapolation per ISO 9080.

    Dilute-solution or gel-permeation chromatography of bimodal pipe HDPE typically shows a broad molecular weight distribution with a high-molecular-weight shoulder. The low-molecular-weight tail contributes to extruder processing below 230 °C, while the high-molecular-weight fraction provides tie molecules that bridge lamellae. The comonomer content in the high-molecular-weight fraction, usually 1-butene or 1-hexene, controls the density and slow crack growth balance more than total short-chain branching. These architectural features cannot be inferred from density and melt flow rate alone; they appear in rheological measurements such as viscosity ratio, shear thinning index, and die swell. For RPEHDW, lot-to-lot variation in these parameters should be monitored because a shift in high-molecular-weight content can alter pipe wall thickness control without changing the lot’s standard density or melt flow rate.

    For thick-wall pipe extrusion, RPEHDW is processed on a single-screw extruder with a grooved feed section and an L/D ratio between 30:1 and 36:1. Barrel set points from 180 °C to 220 °C are common, with the melt temperature kept below 230 °C to prevent thermo-oxidative chain scission. A barrier screw with Maddock mixing elements provides shear homogenization without excessive temperature rise. Screen packs at 80/120/80 mesh remove contaminants; a rise in melt pressure of more than 5 bar/h at constant screw speed generally indicates screen blinding or gel accumulation. Melt pressure at the breaker plate in production-scale lines frequently falls between 100 bar and 250 bar depending on die restriction and output. Die head temperature is held within ±3 °C of the setpoint to limit pipe diameter variation. Surface moisture on pellets at ambient relative humidity above 60 % may require hopper-air drying at 70–80 °C for 2–3 h, although HDPE absorbs negligible internal water.

    How Does RPEHDW Behave Under Low-Shear Long-Term Hydrostatic Loading?

    Long-term failure in pressurized HDPE pipe is governed by slow crack growth, not short-term tensile yield. Under ISO 9080, creep rupture data are generated at multiple temperatures and stresses and extrapolated to 50 years; the lower confidence limit at 20 °C defines the minimum required strength. For a PE100 classification under ISO 12162, the lower confidence limit must be at least 10 MPa. The notched pipe test per ISO 13479 is used to screen slow crack growth resistance at 80 °C and a hoop stress near 4.0 MPa; PE100 compounds typically exceed 500 h to failure under these conditions, while lower-performance PE80 materials may fail earlier. Oxidative induction time measured at 200 °C by ISO 11357-6 is used as a stabilization indicator; pipe-grade HDPE usually requires an OIT above 20 min, although the actual lot value depends on the antioxidant package and regrind history.

    At the molecular level, tie-molecule density and lamellar distribution determine resistance to slow crack propagation. A bimodal ethylene/1-butene or ethylene/1-hexene copolymer architecture improves stress-cracking resistance relative to a unimodal homopolymer HDPE, even when both have the same density. This is the principal difference between RPEHDW-type pipe compounds and general-purpose blow moulding or bottle grades, which may have similar density but lower long-term hydrostatic strength and higher melt flow rate. Published data for this specific configuration is limited; therefore end users should request hydrostatic design basis documentation and notched pipe test reports from Ravago rather than relying only on generic PE100 literature.

    Injection moulding of thick-walled HDPE fittings from a pipe-grade resin with low melt flow rate requires higher injection pressure and longer holding time than a standard injection moulding HDPE with melt flow rate between 4 and 20 g/10 min. Mould temperature between 20 °C and 60 °C, gate diameter above 3 mm, and holding pressure of 600–900 bar are typical starting points to avoid sink marks and weld-line failure. Shot-to-shot variation in cushion position below 2 mm is a practical control limit on production lines to maintain part weight stability with higher-viscosity HDPE.

    HDPE pipe compounds are stabilized with a phenolic/phosphite system and sometimes a hindered amine light stabilizer when outdoor storage is specified. At processing temperatures above 230 °C, the primary antioxidant can deplete rapidly; this is measured by OIT retention after multiple extrusion passes. Regrind addition up to 20 wt% is common in non-pressure applications, but for potable water pressure pipe the permitted regrind level is defined by the pipe manufacturer’s quality plan and by EN 12201 or ISO 4427 requirements. Batch-to-batch variance in residual volatile matter should be kept low because volatiles can create microbubbles at the die exit and reduce weld strength in butt fusion. Published data for this specific configuration is limited.

    When HDPE Pipe Grades Are Compared by Slow Crack Growth Resistance

    When RPEHDW is compared with a unimodal PE80 pipe compound, short-term tensile yield stress may be similar in the range of 22–25 MPa, but failure time under constant internal pressure at 80 °C can differ by an order of magnitude because of differences in tie-molecule density and slow crack growth kinetics. Compared with high-flow HDPE for injection moulding, RPEHDW typically has a lower melt flow rate, a higher elongational viscosity at parison-forming strain rates, and a narrower processing window. Compared with recycled-content HDPE extrusion grades, the product is expected to contain lower volatile matter and less crosslinked gel, although the exact values must be confirmed by lot-specific testing. If the product is supplied with a PE100 MRS classification, it should not be used interchangeably with PE80 because the long-term hydrostatic design stress, wall thickness calculations, and fusion joining parameters are different under ISO 4427 and EN 12201.

    Potable water contact compliance for HDPE requires batch testing against EN 12201 or NSF/ANSI/CAN 61 when the product is used in drinking water distribution. The base polymer falls under 21 CFR 177.1520 as an olefin polymer, but the finished pipe or fitting is the article requiring end-use compliance. For the European Union market, REACH 1907/2006 registration and possibly EU 10/2011 migration testing apply for food contact; for potable water, national approvals such as KTW-BWGL or WRAS are separate from the resin datasheet. RoHS 2011/65/EU heavy metal restrictions apply to electrical conduits rather than buried pipe, but if the product is used in electrical conduit, the formulation must be certified for lead, cadmium, mercury, and hexavalent chromium below the applicable thresholds.

    Interpreting Lot-Specific Datasheet Values Against HDPE Pipe Requirements

    The table below summarises representative property windows for HDPE pipe extrusion compounds within the same MRS class. It is not the product datasheet for RPEHDW; lot-specific values must be obtained from the supplier’s certificate of analysis because reactor technology, comonomer type, antioxidant masterbatch, and pelletization history all shift the results.

    PropertyTest methodRepresentative screening window
    DensityISO 1183-1 / ASTM D15050.945–0.955 g/cm³
    Melt flow rateISO 1133-1:2022 at 190 °C / 5.0 kg0.2–0.7 g/10 min
    Tensile stress at yieldASTM D638-14 / ISO 527-222–25 MPa
    Tensile elongation at breakISO 527-2>600 %
    Flexural modulusISO 178800–1100 MPa
    Notched Charpy impact at 23 °CISO 179-1/1eA>20 kJ/m²
    Oxidative induction time at 200 °CISO 11357-6>20 min
    Minimum required strengthISO 12162 / ISO 908010 MPa if PE100
    Pennsylvania notch test at 2.4 MPa, 80 °CASTM F1473>500 h for PE100-type pipe compounds

    The second table lists regulatory interfaces that apply to the finished pipe or fitting rather than the resin itself. Compliance statements should be issued for the final article because resin compliance does not automatically transfer to the fabricated part.

    StandardScopeTypical requirement relevant to finished HDPE pipe or fitting
    ISO 4427-1Plastics piping systems for water supplyMRS 10 MPa for PE100; lower confidence limit at 50 years
    EN 12201-1Pressure pipe for water supplyMaterial classification PE100; OIT >20 min at 200 °C
    ASTM D3350Polyethylene material classificationLot-specific cell class; pipe grades often meet higher slow crack growth cell classification
    NSF/ANSI/CAN 61Drinking water system componentsEnd-use product certification; no resin-only certification
    FDA 21 CFR 177.1520Olefin polymers in food contactBase resin compliance for intended use; article testing may apply
    EU 10/2011Plastics in food contactOverall migration limit 10 mg/dm²
    REACH 1907/2006Chemical safetySVHC declaration; no intentional SVHC above 0.1 wt% per article
    RoHS 2011/65/EUElectrical/electronic equipmentApplicable only for conduit; lead 0.1 wt%, cadmium 0.01 wt%, mercury 0.1 wt%, hexavalent chromium 0.1 wt%

    In butt-fusion joining of RPEHDW pipe, heater plate surface temperature is typically set at 200–220 °C, with bead-up pressure around 0.15 MPa and fusion force calculated to produce a double-bead width matching the pipe wall thickness. Site welds on thick-wall HDPE require cooling to ambient temperature under restraint before removal from the fusion machine; premature removal causes residual stress at the fusion zone. The material should not be joined with solvent cements or adhesives, and contact with strong oxidizers such as concentrated nitric acid above 40 °C may accelerate environmental stress cracking depending on service stress and exposure duration.