Qapco Hdpe LotrÈne 50100

QAPCO HDPE LOTRÈNE 50100

    • Product Name: QAPCO HDPE LOTRÈNE 50100
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 117935
    Density 0.950 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Strength At Yield 26 MPa
    Tensile Elongation At Break >600%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 20 kJ/m²
    Shore D Hardness 60
    Vicat Softening Temperature 126 °C
    Melting Temperature 131 °C
    Environmental Stress Crack Resistance >1000 h
    Water Absorption <0.01%
    Mold Shrinkage 1.5–3.0%
    Processing Temperature 180–220 °C
    Thermal Conductivity 0.42 W/m·K
    Dielectric Strength 20 kV/mm

    As an accredited QAPCO HDPE LOTRÈNE 50100 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing QAPCO HDPE LOTRÈNE 50100 is packaged in 25 kg polyethylene bags, palletized and shrink-wrapped for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL container loading: QAPCO HDPE LOTRÈNE 50100 in 25 kg bags, palletized, securely stowed, total 20 MT.
    Shipping QAPCO HDPE LOTRÈNE 50100 is a non-hazardous high-density polyethylene resin in pellet form. Ship in dry, covered containers or trucks, using sealed 25 kg bags or 1,000 kg jumbo bags on pallets. Protect from moisture, sunlight, and contamination. No special dangerous goods documentation required.
    Storage Store QAPCO HDPE LOTRÈNE 50100 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizing agents. Keep original bags sealed and palletized off the floor to prevent moisture, dust, and contamination. Avoid prolonged outdoor exposure. Maintain clean, dry conditions and use first-in, first-out stock rotation. Do not stack excessively; protect packaging from damage.
    Shelf Life Typical shelf life is 24 months when stored cool, dry, sealed in original packaging, away from direct sunlight and heat.
    Application of QAPCO HDPE LOTRÈNE 50100

    High-cavitation stack-mould conversion of Lotrène 50100 in thin-wall dairy container production imposes a melt-temperature ceiling that is set less by barrel set points than by shear heating generated during screw recovery and hot-runner manifold flow. Lotrène 50100 is handled as a pre-stabilized high-density polyethylene injection-moulding grade with a nominal melt flow rate of 10 g/10 min at 190 °C under 2.16 kg load (ISO 1133-1:2022; ASTM D1238-23) and a nominal density of 0.950 g/cm³ at 23 °C (ISO 1183-1:2019; ASTM D792-20). In tubs with sidewall thickness between 0.45 mm and 0.80 mm, the controlled flow length of the 10 g/10 min grade permits filling of multi-gated stack tools without moving the melt temperature into oxidative degradation territory. Compliance in this segment is anchored to EU Regulation (EU) No 10/2011 Annex I overall migration, where final articles must not exceed 10 mg/dm² of food-contact surface under the simulant and time-temperature conditions assigned to the intended food type, and to FDA 21 CFR §177.1520(c) for olefin polymers used in food-contact articles, with final article responsibility resting on the converter. Typical dairy-container formulations let down a titanium dioxide white masterbatch at 2.0–3.5 wt%, a slip/antiblock masterbatch at 0.3–0.8 wt%, and a fluoropolymer-free processing aid at 0.1–0.3 wt% only when high-speed stack operation produces surface sharkskin or mould-release sticking. The downstream process is injection moulding on accumulator-assisted hydraulic or all-electric stack-turn systems with clamp force normally between 400 t and 600 t, hot-runner valve-gate manifolds, and injection velocities above 150 mm/s at the screw tip to prevent premature freeze-off. Barrel set points are held from 200 °C at the feed throat to 220 °C at the nozzle, while mould surface temperature is controlled at 10–25 °C. Terminal products include margarine and spread tubs from 250 g to 1 kg, dairy snap-lid bases, delicatessen containers, and single-serve portion cups. The operational boundary is thermal: sustained product contact above 60 °C is not recommended without dimensional stability tests because HDPE sidewall deflection increases rapidly as the softening point is approached.

    What Limits Injection Velocity When Moulding Tamper-Evident Closure Bores?

    In closure conversion lines relying on Lotrène 50100, the main process limit is usually encountered not at the screw recovery stage but at the gate, bore surface, and tamper-evident band during sequenced core retraction. Closure-grade HDPE must balance flowability against torque retention, cap integrity, and organoleptic neutrality. Compliance anchors for this application include FDA 21 CFR §177.1520 for food-contact olefin polymers and EU Regulation (EU) No 10/2011 for final article migration testing; where the closure is used for edible oil, dairy, or UHT milk, sensory panel passes are normally specified because low-molecular-weight oxidation products can migrate into the package headspace. Formulation practice in tamper-evident closure production typically deploys a 5% active erucamide masterbatch at 1.0–3.0 wt% to achieve a final erucamide concentration of 0.05–0.15 wt%. Overdosing above 0.25 wt% final erucamide can produce excessive migration to the closure surface, leading to ejection slip and torque scatter on filling lines. Colour masterbatch is held at 0.5–1.0 wt% only where coloured closures are manufactured; natural caps are run without pigment. The production process is high-cavitation injection moulding in tools of 48 to 96 cavities with valve-gated hot runners. Barrel set points range from 190 °C at the rear zone to 230 °C at the nozzle, with actual melt temperature controlled at 210–225 °C, mould surface temperature at 15–30 °C, holding pressure at 30–45 MPa, and total cycle time between 8 s and 12 s. Injection velocity is profiled so that the flow front does not exceed a speed that causes bore surface fold-back or gate blush; when tamper-evident band cores are retracted, decompression is sequenced 0.2 s before ejection to reduce tearing of the band thinned section. Terminal products include single-piece tamper-evident screw closures from 25 mm to 45 mm for edible oil, sauces, dairy beverages, and UHT milk. Residence time above 230 °C must be kept below 10 min because longer exposure shifts molecular-weight distribution toward the low-molecular-weight fraction and increases taste-and-odour failure risk.

    Large-Cavity Crate and Logistics Tray Flow-Length Limits, Regrind Fractions, and Impact Retention

    Large-cavity crate and logistics-tray tooling exposes Lotrène 50100 to flow paths that can exceed 300:1 length-to-wall-thickness ratio at rib intersections, creating orientation gradients that reduce impact strength at weld lines. The material is processed on hydraulic toggle or two-platen machines with sufficient shot capacity for multi-kg parts. Compliance for this non-food returnable packaging segment is anchored to EU Packaging Directive 94/62/EC Article 11, which restricts the sum of lead, cadmium, mercury, and hexavalent chromium to 100 mg/kg by weight in packaging or packaging components, and to REACH 1907/2006 for SVHC screening of the final article. Typical formulation practice allows in-house regrind incorporation at 10–30 wt%, provided the regrind is dry, free of label adhesive, and produced from the same Lotrène 50100 feedstock. For outdoor crates and field bins, a hindered amine light stabilizer masterbatch is added at 0.5–1.5 wt%. Where sub-zero impact retention is required, 5–10 wt% of a linear low-density polyethylene is introduced as a cold-temperature impact modifier. The downstream process is injection moulding with melt temperature between 210 °C and 240 °C, mould surface temperature at 15–30 °C, hydraulic holding pressure at 40–70 MPa, and sidewall thickness from 2.0 mm to 4.0 mm. Multi-stage injection speed profiling is used to avoid jetting at the gate: first-stage velocity is reduced to fill the gate area without turbulence before the second-stage velocity fills the base and rib network. Terminal products include returnable transit crates, pallet-top frames, automotive dunnage trays, and agricultural field bins. Published data for this specific configuration is limited when regrind exceeds 30 wt%; therefore, notched impact tests on moulded parts are required before increasing the regrind fraction.

    Compliance verification matrix for Lotrène 50100 downstream conversion routes
    Conversion routeRegulatory anchorCritical endpoint or test obligation
    Thin-wall dairy and delicatessen containersEU Regulation (EU) No 10/2011; FDA 21 CFR §177.1520Overall migration ≤ 10 mg/dm²; food-type simulant assignment to final article
    Closure systemsFDA 21 CFR §177.1520; EU Regulation (EU) No 10/2011Organoleptic threshold; additive-specific migration limits per Annex I listing
    Returnable logistics cratesEU Packaging Directive 94/62/EC Article 11; REACH 1907/2006Heavy metals sum ≤ 100 mg/kg; SVHC screening
    Industrial pailsADR/RID 6.1.5.2; UN type code 1H2/3H2Design-type drop, stack, leakproofness on exact compound
    Municipal wheeled-bin accessoriesEN 840-1:2017; ISO 4892-2:2013Weathering and mechanical durability verification on finished accessory

    For domestic storage containers moulded from Lotrène 50100, the processing envelope differs from thin-wall dairy tubs because consumers apply repeated freeze-thaw cycling, lid-body engagement forces, and occasional warm washing. The material is converted into containers that require dimensional stability, deep-draw geometry, and consistent lid sealing. Compliance anchors for this segment include FDA 21 CFR §177.1520 for olefin polymers in food-contact applications, EU Regulation (EU) No 10/2011 for final article migration, and GB 4806.7-2016 for food-contact plastic articles sold into the Chinese market. Formulation ratios are moderate: colour masterbatch is added at 1.5–3.0 wt%, silicone-based mould-release masterbatch at 0.2–0.5 wt% for deep-draw demoulding, and a nucleating agent masterbatch at 0.05–0.15 wt% where thicker bases would otherwise develop sink marks. The production process is single-face injection moulding with melt temperature controlled at 200–215 °C, mould temperature at 15–25 °C, pack pressure at 35–55 MPa, and vent depth maintained between 0.02 mm and 0.03 mm to prevent burn marks at the base corner. In-mould labelling is used for decorated freezer boxes and kitchen containers, which requires the label bond to survive freeze-thaw cycling. Terminal products include freezer boxes, cereal canisters, water pitcher bases, and kitchen drawer organisers. The operational boundary is clear: these containers are not intended for high-moisture microwave reheating or hot-fill above 60 °C; distortion becomes measurable as wall temperature approaches 80 °C, and dimensional verification is required before any hot-wash dishwasher claim.

    When Open-Head Pails Are Specified for UN-Certified Dangerous Goods Packaging

    Open-head pail tooling with deep-draw cores and lid-sealing lands exposes Lotrène 50100 to long residence times and high packing pressures, especially in thick-wall handle-lug areas. Where pails are certified for dangerous goods transport, the design-type testing follows ADR/RID 6.1.5.2 for plastics packagings, and the final article is typically marked with UN type code 1H2 or 3H2. Certification is a function of the complete pail, including the closure, handle, gasket, and colour masterbatch; it is not an intrinsic pellet-level property. Formulation practice for industrial pails uses UV/colour masterbatch at 2.0–4.0 wt%, clean in-house regrind at 10–20 wt%, and an anti-static masterbatch at 1.0–2.0 wt% only when solvent-based paint or ink filling requires static dissipation. The downstream process is injection moulding of 5 L to 20 L pails with melt temperature between 200 °C and 230 °C, mould temperature at 15–25 °C, holding pressure at 40–70 MPa, wall thickness between 1.8 mm and 3.0 mm, and cooling time from 18 s to 28 s. Hydraulic core pulls are used for handle lugs, and the gate location is placed opposite the lug to prevent weld-line alignment through the handle formation. Terminal product types include 5 L, 10 L, and 20 L open-head pails, paint containers, ink buckets, and joint-compound pails. Drop test, stack test, and leakproofness must be conducted on the exact production compound because changing pigment masterbatch supplier, regrind level, or handle geometry can alter crack-initiation resistance and void the UN design type.

    Municipal Waste-Container Hinge and Axle Bracket Moulding With Carbon-Black Masterbatch

    In municipal waste-container accessory moulding, Lotrène 50100 sees long residence times in large shot-weight tools, and carbon-black masterbatch loadings above 1.0 wt% increase heat absorption during barrel residence. Compliance for wheeled-bin accessories is anchored to EN 840-1:2017 for mobile waste and recycling containers, which covers dimensional, mechanical, and outdoor durability requirements, and to ISO 4892-2:2013 for accelerated weathering verification of pigmented polyethylene. Formulation typically includes carbon-black masterbatch at 1.0–2.0 wt%, clean regrind at 10–25 wt%, and a hindered amine stabilizer masterbatch at 0.2–0.5 wt% for long-term outdoor exposure where surface cracking must be minimised. The production process is thick-wall structural injection moulding with melt temperature from 210 °C to 235 °C, mould surface temperature from 15 °C to 30 °C, pack pressure between 45 MPa and 65 MPa, and cycle time from 45 s to 70 s depending on rib depth. Clamping force on structural moulds commonly ranges from 800 t to 1,200 t to counteract projected area and rib-induced pressure drop. Terminal products include wheeled-bin hinges, axle brackets, caster mounts, and lid clips. The primary operational boundary is residence time: at melt temperatures above 220 °C, total barrel residence should remain below 8 min to prevent oxidative chain scission and the resulting loss of hinge impact strength after outdoor exposure.

    Free Quote

    Competitive QAPCO HDPE LOTRÈNE 50100 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    QAPCO HDPE LOTRÈNE 50100 is a high-density polyethylene injection-moulding grade supplied by Qatar Petrochemical Company (QAPCO). Published datasheet values identify the grade by a nominal density of 0.950 g/cm³ and a melt flow rate of 10 g/10 min when measured at 190 °C under a 2.16 kg load according to ISO 1133-1:2022 and ASTM D1238. The grade belongs to the medium-flow segment of HDPE injection resins, positioned between fractional-melt HDPE used for thick-walled industrial containers and high-flow HDPE used for large multicavity housewares. LOTRÈNE 50100 is specified for thin-wall packaging components, caps and closures, crates, storage containers, toys, and general injection-moulded articles that require a balance of stiffness, impact resistance, and processability.

    In field operation, the resin is processed on single-flight general-purpose injection screws with an L/D ratio of 20:1 to 24:1. Barrel temperature settings from 200 °C to 250 °C are common, with the feed zone held at 170 °C to 195 °C to avoid premature melting and bridging. The low moisture uptake of HDPE means routine drying is not required; however, surface condensation can appear when pellets stored below 15 °C are transferred into a humid hall with relative humidity above 60%. Under those conditions, pre-drying at 80 °C for 2 h prevents splay and internal porosity.

    What limits the processing window for LOTRÈNE 50100 in thin-wall injection moulding?

    The lower temperature boundary is governed by short-shot formation and gate freeze, not by melting point alone. In thin-wall moulds with flow-length-to-thickness ratios above 120:1, melt temperatures below 190 °C can lead to incomplete filling at the last cavity positions and visible flow lines at the weld region. The upper processing limit is controlled by thermal-oxidative chain scission. At melt temperatures above 260 °C and residence times beyond approximately 8 min, published degradation mechanisms for HDPE indicate increased formation of carbonyl species, viscosity loss, and yellowing. Injection moulders therefore limit melt cushion to 3 mm to 6 mm, hold screw recovery speed between 40 rpm and 80 rpm, and avoid excessive back pressure to prevent frictional heating beyond the set barrel profile.

    Holding pressure and gate seal are critical for controlling sink marks and dimensional consistency. On machines of 800 kN to 1,600 kN clamp force, hydraulic injection pressures at transfer of 80 MPa to 120 MPa are typical, with holding pressures between 40 MPa and 70 MPa applied for 5 s to 12 s. The use of a short holding time can produce gate freeze at low part mass, leading to sink marks; excessive holding pressure can overpack the cavity and increase moulded-in stress. Mould temperature is normally maintained at 20 °C to 45 °C. Lower temperatures shorten cycle time but increase residual stress and warpage; higher temperatures improve surface gloss and shrinkage uniformity at the cost of longer cooling. For a 2 mm wall section, cooling time in a water-cooled mould is typically 8 s to 15 s.

    At shear rates from 1,000 s⁻¹ to 10,000 s⁻¹, the melt shows pseudoplastic behaviour. Mould-filling simulation of LOTRÈNE 50100 typically uses a Cross-WLF viscosity model; a power-law index below 0.5 in this region reflects the shear-thinning response common to medium-MFR HDPE. The viscosity loss at high shear permits filling of thin sections at lower transfer pressure than a linear viscosity assumption would indicate, but high injection velocities above 100 mm/s in cold-runner tools with small gates can promote jetting. Careful gate placement and a melt temperature at the upper end of the 200 °C to 250 °C window reduce the visual and mechanical defects associated with high-shear flow.

    Weld-line strength in multicavity and multi-gate tools is controlled by melt temperature, packing pressure, and melt-front contamination. At a melt temperature below 200 °C, interpenetration at the weld region is incomplete, reducing elongation at break in the welded area. A holding pressure above 50 MPa and gate sequencing can move the weld line to a lower-stress location. The grade does not require corona treatment or gas injection; mechanical failures in thin-wall crates are often initiated at weld lines, so shell-element mould-filling analysis is used to locate the weld-line position before tool manufacture.

    Specification Data and Test Methods

    The following property values are published typical lot averages and must be checked against the certificate of analysis for the specific production batch.

    PropertyValueTest Method
    Melt flow rate, 190 °C/2.16 kg10 g/10 minISO 1133-1:2022 / ASTM D1238
    Density0.950 g/cm³ISO 1183-1:2019 / ASTM D792
    Tensile strength at yield, 50 mm/min26 MPaISO 527-2 / ASTM D638
    Elongation at break, 50 mm/min>200%ISO 527-2 / ASTM D638
    Flexural modulus, 2 mm/min1000 MPaISO 178 / ASTM D790
    Vicat softening temperature, A50122 °CISO 306 / ASTM D1525
    Hardness Shore D62ISO 868 / ASTM D2240

    The 0.950 g/cm³ density and 10 g/10 min melt flow rate define the product’s position in the HDPE injection-grade range. The flexural modulus of 1000 MPa provides load-bearing stiffness for crates and boxes, while the MFR allows multicavity filling at moderate injection pressure. However, the same crystallinity that provides stiffness also reduces environmental stress-crack resistance compared with medium-density or higher-molecular-weight HDPE grades. Articles exposed to wetting agents, oils, or continuous stress should be tested under ASTM D1693 or ISO 22088-2; published data for LOTRÈNE 50100 in this specific ESCR configuration is limited.

    In closure manufacturing, the grade is processed on high-cavitation moulds with valve-gate hot runners. The melt flow rate of 10 g/10 min reduces pressure loss through the hot-runner drop, but the low melt strength requires balanced runner lay-outs. If the central sprue-to-gate distance is long, differential packing can occur between inner and outer cavities. On a 24-cavity hot-runner tool with 2.0 g shot weight and 800 kN clamp force, cycle times of 5 s to 9 s are reported for similar medium-flow HDPE grades; no guarantee applies to LOTRÈNE 50100 in a different tool configuration.

    When compared with LDPE injection grades, LOTRÈNE 50100 provides higher tensile yield strength and flexural modulus due to its higher density and crystallinity. LDPE grades with similar MFR may show better environmental stress-crack resistance and lower warpage in large flat parts. Against polypropylene homopolymer, LOTRÈNE 50100 exhibits lower heat deflection under load but better low-temperature toughness. The choice between HDPE and PP for caps and closures is therefore driven by liner compatibility, hinge life, and seal stress relaxation rather than viscosity alone. LOTRÈNE 50100 is not intended for applications requiring the high continuous-use temperature of polypropylene or the clarity of clarified polypropylene random copolymers.

    When LOTRÈNE 50100 replaces a lower-melt-index HDPE in existing tooling

    Existing tools designed for fractional-melt or blow-moulding HDPE may require reduced injection speed and lower holding pressure to avoid flash. The viscosity of LOTRÈNE 50100 is lower at typical shear rates, so fill is easier, but the same property decreases the margin against parting-line flash if clamp force is insufficient. A clamp force margin of at least 15% above the projected cavity pressure is used to prevent mould opening. Gate size should be checked against the viscosity: a gate diameter below 0.8 mm can cause shear heating and gate wear, while a gate above 1.5 mm can slow gate seal and increase cycle time. Shrinkage difference must also be addressed. The density of 0.950 g/cm³ results in mould shrinkage typically in the range of 1.5% to 2.5%; lower-melt-index HDPE may be supplied with different shrinkage values, so printed dimensional tolerances should be recalculated.

    Blending LOTRÈNE 50100 with lower-MFR HDPE at varied ratios can shift the effective MFR and impact performance, but the resulting properties do not follow a linear mixing rule. A 20 wt% addition of a fractional-melt HDPE typically reduces the MFR more than predicted by a mass-weighted average because the high-molecular-weight component increases melt elasticity and die swell. This is relevant for colour-compounded variants where a pigment masterbatch let-down of 2% to 4% is used. The masterbatch carrier resin must be compatible with HDPE; use of low-density or acid-modified carriers can alter surface gloss and weld-line strength.

    Dimensional control depends on packing consistency, mould temperature uniformity, and part geometry. Mould shrinkage for LOTRÈNE 50100 is typically specified in the range 1.5% to 2.5%, although the final value changes with wall thickness and gate location. Differential cooling between top and bottom plates can generate warpage in flat lids exceeding 0.4 mm for a 250 mm × 150 mm × 2 mm moulding. Cooling channels should be sized so that the temperature difference between any two cavity surfaces does not exceed 5 °C; otherwise, residual stress and post-ejection deflection become difficult to correct without a longer cycle.

    Regrind from sprues and reject parts can be reintroduced. The particle size and thermal history affect the melt: regrind levels above 20% can reduce the effective MFR and impact strength because the recycled fraction has already undergone one heat history. Gravimetric dosing of regrind is preferred over volumetric blending to control bulk density variations.

    Compliance statements are issue-specific and must be obtained from QAPCO for the final article. The matrix below lists commonly applied frameworks for HDPE injection-moulding food-contact and industrial parts.

    FrameworkStandard or RegulationStatus / Condition
    US food-contact resin21 CFR 177.1520Olefin polymers section; subject to end-use migration and additive restrictions
    EU food-contactRegulation (EU) No 10/2011Overall migration limit 10 mg/dm² for food simulants
    REACHRegulation (EC) No 1907/2006Monomer and additives registered; compliance declaration required for final article
    RoHSDirective 2011/65/EULead, mercury, cadmium, hexavalent chromium, PBB, and PBDE below threshold values for unpigmented HDPE; final article must be verified

    LOTRÈNE 50100 is not designated for pressure pipe, blown film, rotational moulding, or extrusion blow moulding. Continuous immersion in strong oxidising acids, chlorinated solvents, or high-purity oxygen at elevated temperature can accelerate thermo-oxidative degradation. Outdoor service requires an adequate UV stabiliser package; unpigmented HDPE is not sufficiently resistant to ultraviolet exposure for long-term exterior use. No claim is established for medical or pharmaceutical use beyond the specific regulatory assessments provided by the manufacturer.

    Top