| HS Code | 171807 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.957 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Melting Point | 133 °C |
| Vicat Softening Temperature | 127 °C |
| Tensile Strength At Yield | 29 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1250 MPa |
| Notched Izod Impact Strength 23 C | 250 J/m |
| Environmental Stress Crack Resistance 10 Igepal F50 | >1000 h |
| Shore D Hardness | 65 |
| Water Absorption | <0.01% |
| Thermal Conductivity | 0.45 W/mK |
| Volume Resistivity | >10^16 ohm-cm |
| Dielectric Constant 1 Mhz | 2.3 |
As an accredited QAPCO HDPE LOTRÈNE TR-571 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | QAPCO HDPE LOTRÈNE TR-571 is supplied in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg/pallet). |
| Container Loading (20′ FCL) | QAPCO HDPE LOTRÈNE TR-571 is loaded in 20′ FCL containers as 25 kg bags, securely stowed for safe ocean transport. |
| Shipping | QAPCO HDPE LOTRÈNE TR-571 is a non-hazardous polyethylene resin, shipped as pellets in 25 kg PE bags, 1 MT jumbo bags, or bulk containers/trucks. Packaging is palletized and stretch-wrapped for transport. Store dry, ventilated, away from heat and direct sunlight; keep bags closed to prevent moisture. |
| Storage | Store QAPCO HDPE LOTRÈNE TR-571 in a cool, dry, well-ventilated warehouse, preferably in original sealed bags or containers. Protect from direct sunlight, rain, moisture, heat, and ignition sources. Keep away from strong oxidizers, oils, and contaminants. Stack pallets securely; use first-in, first-out rotation. Ensure good housekeeping and prevent static buildup. Avoid prolonged UV exposure. Do not store with food. |
| Shelf Life | Shelf life is 24 months from manufacture when stored unopened in original packaging in a cool, dry place away from direct sunlight. |
Lotrène TR-571 from QAPCO is a high molecular weight high density polyethylene whose downstream conversion is defined by a balance between high melt elasticity and controlled die swell. The grade is handled in extrusion blow moulding, heavy-gauge sheet extrusion, and high-strength blown film where sag resistance and environmental stress crack resistance dominate. Processing environments below treat the material as a rheological system, not as a universal HDPE drop-in. All numerical settings refer to production-scale equipment configurations reported in machine technical bulletins or to test methods listed in the text.
Extrusion blow moulding of UN-certified tight-head and open-top drums uses TR-571 as the main resin in formulations where the high load melt flow rate is controlled between 4.0 and 6.0 g/10 min under ISO 1133-1:2022 at 190 °C/21.6 kg. A single-station accumulator head machine with a 90 mm grooved-bush extruder and 24:1 L/D screw is set to a declining barrel profile of 190 °C, 210 °C, 220 °C, 215 °C, 205 °C; the adapter and die head remain at 210 °C. Melt temperature at the die entry is measured with an immersion probe and held within 215–225 °C; higher values reduce die head pressure but increase parison draw-down, while lower values raise pressure and cause sharkskin melt fracture at the die lip. For a 220 L L-ring tight-head drum, the parison die gap is set at 2.8–4.2 mm, target die swell is 35–50%, and the accumulator head is programmed with a 3 to 5% parison length overfeed at the bottom pinch zone to compensate for pre-blow sag. Blow pressure is set at 0.7–0.9 MPa, mold clamp force between 1,500 kN and 2,800 kN, and mold coolant inlet at 12–18 °C to avoid stress whitening at the pinch seam. The cycle time for a 220 L open-top drum runs from 160 s to 200 s; shorter cycles produce underfused pinch-off welds, while longer cycles generate inner-surface oxidation. Formulation is 100 parts TR-571, 2.25 parts of a 45% carbon black masterbatch in LDPE, 0.12 parts hindered phenolic antioxidant, 0.08 parts phosphite secondary stabiliser, and 0.25 parts HALS if the drum is exposed to outdoor weathering. Carbon black dispersion is inspected by ISO 18553:2002, with agglomerates greater than 0.5 mm² rejected because they initiate brittle failure in sidewall impact. Finished containers are qualified under UN 1H1 for tight-head and UN 1H2 for open-head designs; leakproofness is tested at 30 kPa internal air for tight-head types, hydraulic pressure is applied at 100 kPa for 30 min, stack load follows UN 6.1.5.3, and drop trials are performed after 24 h conditioning at -18 °C for Packing Group II. ESCR of pinch-off zones is checked under ASTM D1693-15 Condition B with 10% Igepal CO-630 at 50 °C; welds failing before 600 h indicate inadequate fusion temperature or excessive mold release. End products include 25 L jerrycans, 60 L open-head drums, 120 L cylindrical open-top containers, 220 L L-ring tight-head drums, and 1,000 L IBC inner bottles.
| Control parameter | Set range | Monitoring equipment |
|---|---|---|
| Melt temperature at die entry | 215–225 °C | Immersion thermocouple at head adapter |
| Accumulator die gap | 2.8–4.2 mm | Feeler gauge and linear transducer |
| Parison die swell | 35–50% | Cut-off mass vs parison length |
| Blow pressure | 0.7–0.9 MPa | Calibrated pressure transducer at blow pin |
| Mould coolant inlet | 12–18 °C | Chiller loop resistance temperature detector |
| Cycle time for 220 L open-top drum | 160–200 s | Machine PLC cycle timer |
In blown film extrusion of temporary enclosure liners, concrete curing sheets, and quarantine partitions, TR-571 is blended with 15–20 wt% of a C6-LLDPE to increase bubble symmetry and raise puncture resistance without sacrificing tensile yield. The melt is processed on a 250 mm spiral mandrel die with a 1.8 mm lip gap, 3.0:1 blow-up ratio, and frost line height at 10 to 12 die diameters. Extruder zones are profiled from 180 °C at the feed throat to 210 °C at the screen changer and 205 °C at the die; melt temperature is kept below 210 °C because higher levels reduce bubble tension and cause hunting at the nip rolls. Dual-lip air ring velocity is set between 5 and 7 m/s; insufficient lip air leads to gauge bands at the frost line, while excessive air chills the bubble at the die exit and produces visible shark-skin. The blend contains 85 wt% TR-571, 15 wt% C6-LLDPE MI 1.0 g/10 min, 0.8 wt% UV stabiliser masterbatch, and 0.2 wt% silica-filled slip/antiblock masterbatch. Film at 150 µm is produced at 180 kg/h; dart impact is tested under ISO 7765-1:2004 and Elmendorf tear under ASTM D1922-23 on machine and transverse direction samples. Compliance pathways vary with end use: concrete curing sheets require water retention measured by ASTM C156-23; temporary fumigation covers are evaluated for gas permeability under ASTM D3985-24; and structures intended for indirect food contact require organoleptic migration screening under EU 10/2011 with simulants assigned to the actual food type. This film is not considered a primary chemical packaging membrane unless a coextruded barrier layer is added, because the moisture vapour transmission rate of HDPE at 150 µm is higher than that of aluminium laminates. End products include 200 µm fumigation tarpaulins, 150 µm concrete cure covers, 250 µm temporary containment liners, and 100 µm dust partitions. Failure modes observed on production lines are bubble snaps in winds above 3 m/s and die lip drool from oxidative degradation; both are controlled by a low-pressure internal bubble stabiliser and chilled feed housing set at 35 °C.
Sheet extrusion and twin-sheet thermoforming of chemical containment bund liners and pallet dunnage use TR-571 as the structural layer where slow crystallisation permits lower internal stress in thick sections. A 120 mm single-screw extruder with 30:1 L/D, a melt pump, and a 1.2 m coat-hanger flat die is run at 220 °C, 228 °C, 230 °C, 225 °C from feed to die, with a screen pack of 80/120/80 mesh. The sheet is polished in a vertical three-roll stack with top roll at 85 °C, middle roll at 95 °C, and bottom roll at 80 °C; roll gaps are staged to deliver a 4.5 mm sheet at 180 kg/h. Closed-loop infrared edge heaters maintain sheet edges within ±2 °C of core temperature because cooler edges trim poorly and hotter edges feed thermoformer sag. Formulation uses 93.5 wt% TR-571, 4.0 wt% LLDPE, 2.0 wt% carbon black masterbatch, and 0.5 wt% stabiliser package. Twin-sheet forming on a rotary machine with 320 °C upper quartz heaters and 280 °C lower quartz heaters produces hollow pallet liners and sump forms with 6.5 mm wall thickness and welded perimeter flanges. The vacuum is staged 0.2 bar for pre-stretch, then 0.8 bar for full draw; core plug assist is maintained at 60 °C to prevent premature cooling. Chemical resistance is screened by ASTM D543-21 with 10% HCl and 30% NaOH for 30 days, and secondary containment duty is qualified under EPA 40 CFR 264.175 for 1,100 L tank bunds. Flammability of machine housing components made from the same sheet is classified by UL 94 HB. End products include 1.2 m × 1.2 m dunnage trays, 1.8 m × 0.9 m chemical pallet liners, 500 mm deep spill trays, and bund liner panels.
In open-head agrochemical and solid chemical packagings, the certification pressure is drop resistance after a -18 °C conditioning cycle. A 60 L open-head pail with a side handle is blown from TR-571 on a single-station shuttle machine with a 70 mm extruder and 600 kN clamp force; shot mass is 2.4 kg. Wall thickness distribution is specified as 2.2 mm at the sidewall and 2.8 mm at the corner radius, because drop cracks originate where the sidewall meets the base chime. The blow pin diameter is 48 mm, and the pin is equipped with a spreader die to force material into the handle pinch weld. Barrel temperatures are 195 °C, 215 °C, 225 °C, 220 °C, 210 °C; melt temperature is held at 225 °C. The mould is cooled with 10–15 °C water and cycle time is 85 s. Formulation adds 1.5 wt% carbon black masterbatch and 0.1 wt% calcium stearate; no odour-absorbing additive is used for seed treatment pails because any polar additive migrates to the surface and alters wettability. Drop testing follows UN 6.1.5.3 after 24 h of -18 °C storage; Packing Group II solid filling with a relative density of 1.2 is applied. Stack load is measured for 28 days at 40 °C with a load equivalent to 3 m stack height under the standard. Leakproofness is not required for open-head solid packages, but vacuum retention at -20 kPa is used as a production release test for pails with slip-lid closures. Outdoor storage of agrochemical solid containers is validated by ASTM D2565-23 Xenon-arc exposure for 500 h; colour retention and sidewall impact after exposure must remain within lot-specification limits. End products are 60 L seed treatment pails, 30 L veterinary mineral buckets, 45 L solid micronutrient tins, and 25 L UN solid packagings for copper oxychloride.
TR-571 is not qualified in the public domain as a PE100 pipe material under ISO 4437-2:2024. Hydrostatic design basis data, slow crack growth resistance, and rapid crack propagation performance are not reported in the QAPCO published technical file for this grade. Conversion of TR-571 into potable water pressure pipe or gas distribution pipe therefore cannot be validated without independent material reclassification. A pipe extrusion line may process the material because HDPE melt temperatures in the 200–220 °C range are accessible, but the finished pipe would lack the required 50-year design basis. Consequently, the realistic downstream scope for this grade excludes municipal pressure pipe, gas service pipe, and hot-water pressurised systems. Non-pressure conduit and corrugated drainage pipe are less demanding but still require stiffness and creep tests under EN 13476-2:2024; published data for these specific TR-571 configurations is limited. The operational boundary is meaningful because substituting a blow moulding grade into pipe extrusion typically causes excessive die swell and sag in large-diameter thick-wall sections, leading to wall thickness variation above ±10% of nominal. Processors considering non-pressure duct work should run a full lot qualification with melt flow stability checks per ISO 1133-1:2022, outer diameter control per ISO 3126:2005, and drop-weight impact per ISO 3127:2023.
Blow moulded float bodies and chemical dosing vessels made from TR-571 are processed on a 80 mm extruder with a 1.2 kg shot accumulator head for hollow technical parts. The die gap is varied during parison extrusion by a 20% wall-thickness program, from 3.5 mm at the bottom to 2.5 mm at the top, to produce uniform wall sections after forming. Melt temperature is maintained at 215 °C; cooling water inlet is 8–12 °C because thick float walls above 5 mm require low mould temperatures to shorten demould time. Formulation includes 0.5 wt% HALS at the top end of the recommended range and 2.0 wt% carbon black masterbatch for UV resistance. The components are not intended for permanent potable water contact; immersion testing is conducted under ASTM D543-21 in 10% NaCl and 5% sodium hypochlorite for 30 days. ESCR is measured with ASTM D1693-15 Condition A at 50 °C; articles with weld lines require 48 h notch aging before testing because residual orientation affects crack propagation. Water absorption is screened by ISO 62:2008, with maximum increase of 0.1% after 24 h at 23 °C. UV weathering is exposed under ASTM G154-23 cycle 1 for 1,000 h; retention of tensile elongation must remain above 70%. End products include 30 L marine floats, 150 mm chemical dosing floats, 80 L cleaning chemical dispenser bottles, and 45 L wastewater lift station floats. The material is incompatible with strong oxidisers at elevated temperature and with aromatic hydrocarbon solvents such as xylene; such service requires qualification of a different molecular design or barrier treatment.
Competitive QAPCO HDPE LOTRÈNE TR-571 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
QAPCO HDPE LOTRÈNE TR-571 is a high-molecular-weight high-density polyethylene film resin supplied in pellet form under the Lotrene trade name. The resin is manufactured by low-pressure ethylene polymerization and is stabilized with a primary antioxidant package; the base grade does not contain slip or antiblock agents unless specifically ordered. The product is intended for high-stalk blown film extrusion of thin-gauge packaging, including carrier bags, industrial liners, bin liners, and multiwall bag liners. The nominal melt flow rate is 0.65 g/10 min when measured according to ASTM D1238 at 190 °C and 2.16 kg load, and the nominal density is 0.957 g/cm³ according to ASTM D1505. These two values position the grade between lower-density LDPE film resins and lower-melt-flow HDPE blow-moulding grades: the higher density of 0.957 g/cm³ raises secant flexural modulus to approximately 1,100 MPa, while the moderate melt flow rate retains sufficient flow for thin annular dies. The resin is typically converted on single-screw extruders with grooved feed sections and barrier screws. Published data for the specific molecular weight distribution of this grade is limited; however, blown film grades in this density and melt flow range generally exhibit broad molecular weight distribution and shear-thinning behaviour that supports high-stalk bubble stability.
The melt flow rate of 0.65 g/10 min under ASTM D1238 does not by itself capture the shear-thinning response of the resin in a grooved-feed single-screw extruder, but it identifies a molecular weight range that balances die head pressure and bubble stability. On high-stalk blown film lines with 25:1–30:1 L/D barrier screws and an annular die gap of 0.8–1.2 mm, the resin is typically processed at melt temperatures from 190 °C to 210 °C. Operation below 190 °C raises melt pressure at the die and may produce sharkskin melt fracture on the outer bubble surface; operation above 210 °C lowers melt strength and destabilizes the high-stalk bubble. A deviation of more than ±5 °C around the centre of this window is a critical control point because it correlates with frost-line height oscillation and gauge variation across the collapsed film. The high-stalk process requires a neck height of 6–10 die diameters and a blow-up ratio between 3:1 and 5:1. These conditions impose high extensional strain on the melt at the freeze line; the resin’s high molecular weight fraction provides strain-hardening behaviour that delays bubble rupture. The strain-hardening response is affected by die land length, die gap, and melt temperature. Reducing the die gap below 0.8 mm increases wall shear stress and accelerates the onset of melt fracture; enlarging the die gap above 1.2 mm reduces shear and may produce gauge bands from poor melt homogenization. In addition, the resin’s density of 0.957 g/cm³ increases the crystalline fraction relative to LDPE, which raises the crystallization rate; the frost line must therefore be placed low enough to complete orientation before solidification but high enough to avoid blocking the collapsed film.
The following nominal values are used for incoming inspection and process benchmarking. They are determined on compression-moulded plaques or injection-moulded specimens, not on finished film.
| Property | Test method | Nominal value |
|---|---|---|
| Melt flow rate at 190 °C/2.16 kg | ASTM D1238 | 0.65 g/10 min |
| Density at 23 °C | ASTM D1505 | 0.957 g/cm³ |
| Tensile yield strength at 50 mm/min | ASTM D638 | 27 MPa |
| Elongation at break | ASTM D638 | > 800% |
| Flexural modulus, 1% secant | ASTM D790 | 1,100 MPa |
| Vicat softening point, 50 °C/h, 10 N | ASTM D1525 | 126 °C |
| Melting temperature by DSC | ASTM D3418 | 133 °C |
Values are nominal and will vary with specimen preparation, thermal history, and film gauge. The secant flexural modulus of 1,100 MPa measured under ASTM D790 is higher than that of LDPE film grades and provides the stiffness required for thin-gauge carrier bags. Tensile yield strength of 27 MPa under ASTM D638 indicates resistance to load-induced dimensional change, while elongation at break above 800% permits adequate deformation before rupture in side-seal and bottom-seal bag converting. The Vicat softening point of 126 °C under ASTM D1525 and the DSC melting temperature of 133 °C under ASTM D3418 are relevant for sealing operations, because heat-seal jaws must exceed the crystalline melting range without inducing excessive squeeze-out. Heat-seal initiation temperatures are usually 10–15 °C above the DSC peak, but published data for this specific film gauge is limited.
On a 90 mm grooved-feed single-screw extruder with a 30:1 L/D barrel and a 250 mm annular die, TR-571 is typically run with a die gap of 0.8–1.2 mm, a melt temperature of 195–205 °C at the die, and a blow-up ratio of 3:1–5:1. The high-stalk bubble is maintained with a neck height of 6–10 die diameters. Reducing the die gap below 0.8 mm raises shear rate and can initiate melt fracture; increasing the die gap above 1.2 mm reduces shear and may produce gauge bands. Batch-to-batch variance is controlled by the supplier within the nominal melt flow and density specification, but shifts in pellet temperature during transport into a hot silo can alter feed-zone conveying; plant operators compensate by adjusting screw speed rather than barrel temperature because melt-temperature changes affect bubble stability more than throughput. HDPE is not hygroscopic; pre-drying is not required except when pellet surface condensation occurs after storage at RH > 60%. The resin should not remain in the extruder at melt temperature above 220 °C for prolonged periods during shutdown, as oxidative chain scission may lower melt strength and increase gel formation. Screen-pack differential pressure should be monitored; a progressive increase at constant output is interpreted as gel or foreign matter accumulation on the filter media. The use of a gear melt pump between the extruder and die reduces pressure pulsation and helps maintain frost-line position when the screen pack loads.
Substitution of LDPE by TR-571 in a high-stiffness film structure changes the mechanical response at the same gauge. LDPE film grades typically exhibit a density near 0.922 g/cm³ under ASTM D1505, a tensile yield strength below 12 MPa under ASTM D638, and a secant modulus below 300 MPa under ASTM D790. TR-571 at 0.957 g/cm³ density raises tensile yield strength to 27 MPa and secant modulus to 1,100 MPa under the same test methods. The increase in modulus permits downgauging for a given bag stiffness, but it also lowers dart impact resistance and puncture resistance relative to LLDPE-rich blends. When converting from LDPE to TR-571, the frost line must be lowered or the bubble geometry adjusted because the higher melt density and crystallization rate shorten the available time for bubble stabilization. Compared with QAPCO HDPE blow-moulding grades with melt flow rates below 0.4 g/10 min, TR-571 has a higher melt flow rate tailored for thin annular film extrusion rather than parison hang strength and pinch-off weld integrity. Compared with LLDPE film grades, TR-571 produces higher modulus and lower elongation at break, and it is generally used in blends rather than as a puncture-resistant monolayer. Published data for the specific dart impact value of TR-571 film under ASTM D1709 is limited; the value is highly dependent on bubble geometry, gauge, and blending ratio with LLDPE. The higher density of TR-571 also reduces water vapour transmission rate relative to LDPE at equal thickness, which is a process outcome of increased crystallinity rather than a direct specification value.
Compliance depends on the final film construction, additives, and migration testing. The following standards and clauses are commonly referenced when the resin is used in packaging.
| Standard or clause | Scope | Application boundary |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers | Paragraph (c) covers high-density polyethylene; end-use migration testing is required for specific film |
| Commission Regulation (EU) No 10/2011 | Plastic food-contact materials | Overall migration limit of 10 mg/dm² applies to finished articles |
| EU Packaging Directive 94/62/EC | Packaging and packaging waste | Concentration limits for lead, cadmium, mercury, and hexavalent chromium |
| REACH Regulation (EC) No 1907/2006 | Chemical safety | Annex XVII restrictions on monomers and substances of very high concern |
| Directive 2011/65/EU | Restriction of hazardous substances | Relevant only where packaging is incorporated into electrical equipment |
Operational boundaries include minimizing residence time at temperatures above 220 °C, because prolonged exposure to oxygen can reduce molecular weight and generate carbonyl species. The resin should not be combined with strong oxidizing agents or stored in direct contact with aromatic hydrocarbons at elevated temperature. For food-contact decisions, converters must perform migration testing under the intended film thickness and polymer composition; the base resin certification alone does not establish compliance of the final article. If post-consumer recyclate is blended, the regulatory position changes and must be re-evaluated under the relevant national contact-sensitive packaging standard.