| HS Code | 535874 |
| Manufacturer | QAPCO |
| Grade | LOTRÈNE TR-168 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.20 g/10 min |
| Melt Flow Ratio 21 6 2 16 Kg | 100 |
| Tensile Strength At Yield | 26 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1200 MPa |
| Vicat Softening Temperature | 125 °C |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Notched Izod Impact Strength | 100 J/m |
| Hardness Shore D | 65 |
| Water Absorption | <0.01% |
As an accredited QAPCO HDPE LOTRÈNE TR-168 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | QAPCO HDPE LOTRÈNE TR-168: 25 kg polyethylene bags, palletized and stretch-wrapped; 1,375 kg per pallet. |
| Container Loading (20′ FCL) | QAPCO HDPE LOTRÈNE TR-168 in 20′ FCL: palletized, 25 kg bags, 55 bags/pallet, 18 pallets, 24.75 MT net. |
| Shipping | QAPCO HDPE LOTRÈNE TR-168 is shipped as a non-hazardous thermoplastic resin in 25 kg PE bags, palletized, stretch-wrapped, and labeled. Transport by truck or sea in dry containers; keep dry and away from heat, sunlight, and sharp objects. No dangerous goods requirements apply. |
| Storage | Store QAPCO HDPE LOTRÈNE TR-168 in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, flames, and oxidizing agents. Keep original bags or containers closed, off the floor, and protected from moisture, dust, and UV exposure. Avoid excessive stacking; follow first-in, first-out rotation. Maintain clean handling areas and prevent static accumulation. |
| Shelf Life | Shelf life typically 2 years from production date when stored unopened in original packaging, dry, cool, away from direct sunlight. |
QAPCO HDPE LOTRÈNE TR-168 is introduced into extrusion blow molding lines as a high-molecular-weight HDPE copolymer base resin for tight-head and open-head industrial drums. The resin is dry-blended with 1.0–2.0 wt% color masterbatch and, for outdoor service, a UV stabilizer masterbatch at 0.5–1.0 wt%. Production is performed on an accumulator-head blow molding machine with a screw diameter of 90–120 mm, an L/D ratio of 24:1–30:1, and a grooved feed section. Barrel temperatures are profiled from 180 °C in the feed zone to 210 °C in the accumulator head, while melt temperature is held at 200–220 °C. The die gap is set between 0.7 mm and 1.0 mm for a 220 L drum parison, and blow air pressure is maintained at 0.7–0.9 MPa. Mold clamping force is not less than 450 t for consistent pinch-off weld integrity. Process water at the mold is controlled at 10–20 °C; mold cooling below 10 °C produces surface microcracks in the pinch-off zone. Finished drums are tested for impact resistance and leakage under the UN Manual of Tests and Criteria, Part III, and are marked as UN 1A1 or UN 1A2 packagings when the wall thickness distribution remains within ±15 % of the design value. End products include 220 L tight-head drums for solvent transport, open-head drums for viscous chemical intermediates, and internally fluorinated drums for aggressive oxygenated solvents.
For containers above 120 L and for intermediate bulk container inner bottles, melt strength limitations require closed-loop parison programming. The accumulator head is equipped with a hydraulically actuated mandrel and a 30–64 point parison programmer that adjusts die gap during extrusion. Without programming, a parison length above 1.2 m produces top-wall thinning beyond ±20 % of nominal. The programmed profile compensates for extrudate swell and sag by opening the die gap at the top region and reducing the gap at the bottom pinch-off. TR-168 is processed at a melt temperature of 205–215 °C in this application; a melt temperature above 220 °C lowers sag time and increases wall-thickness variation. Accumulator head volume is selected at 1.5–2.0 times the shot weight to avoid flow lines and charge-to-charge temperature drift. Parison programming data are generated from ultrasonic or infrared wall-thickness scanning after trial runs. The end products are 1,000 L intermediate bulk container inner bottles and large open-top process vessels. Compliance is evaluated against ISO 16106:2018 and the relevant IMDG Code requirements for internally transported liquids.
Automotive fuel tank coextrusion blow molding uses TR-168 as the high-molecular-weight HDPE skin layers and as the carrier for regrind. The six-layer structure is composed of HDPE outer skin, maleic anhydride grafted LLDPE tie layer, EVOH barrier layer, tie layer, regrind layer, and HDPE inner skin. Layer distribution is typically 8–12 % outer HDPE, 2–3 % tie, 2–4 % EVOH, 30–40 % regrind, and the balance HDPE inner skin. Melt temperature for the HDPE layers is set at 220–230 °C; the EVOH layer is limited to 205–220 °C to avoid gel formation, and the tie layers are processed at 210–220 °C. The six-layer accumulator head is purged with HDPE at shutdown to prevent EVOH degradation. Fuel permeation is measured under 40 CFR 86.165 or ECE R34 Annex 5 depending on the final vehicle market; tank assemblies are also subjected to impact, internal pressure, and fire resistance tests required by the relevant vehicle type approval. The grade’s high molecular weight provides the required drop impact resistance at −40 °C, but the final fuel tank must be validated with the specific regrind content. End products include gasoline and diesel tanks for passenger vehicles, marine fuel tanks, and generator set reservoirs. Published fuel permeation values are product-specific; published data for this specific configuration is limited.
| Layer | Material | Layer distribution (wt%) | Melt temperature window (°C) |
|---|---|---|---|
| Outer skin | TR-168 HDPE | 8–12 | 220–230 |
| Tie layer | Maleated LLDPE | 2–3 | 210–220 |
| Barrier layer | EVOH | 2–4 | 205–220 |
| Tie layer | Maleated LLDPE | 2–3 | 210–220 |
| Regrind | Mixed fuel-tank regrind | 30–40 | 220–230 |
| Inner skin | TR-168 HDPE | Balance | 220–230 |
Jerry cans for agricultural chemicals and cleaning concentrates impose a narrower environmental stress crack resistance window than general packaging. The compound is based on 96.0–98.0 wt% TR-168 with 2.0–4.0 wt% pigment or carbon black masterbatch, and ESCR is evaluated per ASTM D1693-15 condition B in 100 % Igepal CO-630. A failure time below 100 h on the notched specimen indicates that the selected pigment masterbatch carrier is incompatible with the base resin and must be replaced. Blow molding is performed at a melt temperature of 205–215 °C on shuttle or long-stroke machines with a clamp force of 40–120 t for 20–30 L containers. The neck finish is molded in the same blowing step, and dimensional stability of the closure thread is checked by torque testing at 3.5–5.0 N·m for standard 63 mm closures. The finished containers are drop-tested at 0.8–1.2 m after conditioning at −18 °C and must show no seam leakage. End products include 20 L and 25 L jerry cans for crop protection chemicals, liquid detergents, and automotive antifreeze. Compliance for dangerous goods packaging is documented under the UN Manual of Tests and Criteria and, where applicable, ADR 2023.
TR-168 is processed into heavy-gauge HDPE sheet for thermoformed industrial dunnage and automotive protective panels. The extruder is a single-screw machine with a screw diameter of 100–150 mm, an L/D of 30:1–33:1, and a barrier screw with a grooved feed section. Melt temperature is maintained at 210–230 °C. The flat die width is 2.0–2.5 m, and the melt is polished in a vertical three-roll stack with roll temperatures of 80–100 °C. Sheet thickness ranges from 3 mm to 10 mm. Cooling uniformity is critical; differential roll temperature above 5 °C across the sheet width causes warpage after trimming. Formed parts are tested for notched Charpy impact per ISO 179-1:2010 at 23 °C and −30 °C, tensile properties per ISO 527-2:2012, and puncture resistance per ASTM D3763-18. The end products are reusable material handling trays, rack protection panels, and automotive transit dunnage. The formulation includes 2.0–3.0 wt% antistatic masterbatch only where explosion-proof storage of electronic components is required; antistatic loading above 3.0 wt% reduces melt strength and causes sheet sag in the roll stack.
For outdoor water storage tanks and agricultural spray tanks, the compounded resin must contain a final carbon black content of 2.0–2.5 wt% to achieve ultraviolet resistance. A 50 wt% carbon black masterbatch in a compatible HDPE carrier is dry-blended with TR-168 at 4.0–5.0 wt% letdown. The blend is processed on an accumulator-head blow molding line with a melt temperature of 200–220 °C. Carbon black dispersion is checked on pressed film per ISO 18553:2002; undispersed agglomerates above rating 3 act as stress concentrators in the tank base and can initiate environmental stress cracks after outdoor exposure. The cooling cycle for 500 L tanks requires mold temperature between 15 °C and 25 °C; cooling time is set to 180–300 s depending on wall section. The tank wall is inspected at the pinch-off zone for thinning below ±15 % of the sidewall thickness. Compliance for potable water contact is not automatic; the final pigmented compound must be tested under EU 10/2011 for specific migration and, for North American use, under 21 CFR 177.1520 when potable water approval is claimed. End products include vertical water storage tanks, agricultural sprayer tanks, and rainwater harvesting vessels.
| Ingredient | Function | Letdown loading (wt%) | Final parameter |
|---|---|---|---|
| TR-168 | Base resin | 95.0–96.0 | Balance |
| Carbon black masterbatch 50 % | UV stabilisation | 4.0–5.0 | Final CB 2.0–2.5 wt% |
| Antioxidant/processing aid masterbatch | Melt stability | 0.5–1.0 | OIT ≥ 20 min at 200 °C |
Large blow molded containers for liquid food concentrates and food ingredients are produced from TR-168 only when the final pigmented compound meets the extraction limits in 21 CFR 177.1520(c) and the overall migration limit in EU 10/2011. The melt is processed at 205–215 °C on accumulator-head machines; no external lubricants are applied to the die head. Color masterbatch is restricted to 1.0–2.0 wt%, and only food-grade pigment carriers with documented compliance are used. The blow mold is operated with a clamp force sufficient to produce a flat pinch-off weld, because residual weld flash in the interior must not create crevices that retain product. Finished containers are subjected to leak testing at 20–30 kPa internal air pressure and are stacked under load for 24 h at 40 °C to verify top-load resistance. End products include 200 L drums for liquid food concentrates, 50 L bag-in-box outer containers, and bulk aseptic package shells. No direct food-contact status can be assumed for the base resin alone; compliance belongs to the fully compounded and finished article.
Competitive QAPCO HDPE LOTRÈNE TR-168 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
QAPCO HDPE LOTRÈNE TR-168 is a high-density polyethylene resin positioned within the LOTRÈNE polyolefin family supplied by Qatar Petrochemical Company (QAPCO). The designation identifies a specific density, melt-flow, and additive position for conversion processes in which melt strength and film stiffness are controlling variables. Classification as high-density polyethylene follows ASTM D883-23, which places HDPE at a density of 0.940 g/cm³ or greater. Density is measured under ISO 1183-1:2019, and melt mass-flow rate is determined under ISO 1133-1:2022, Procedure A, at 190 °C and 2.16 kg. The certified lot-specific interval for TR-168 is supplied through the QAPCO certificate of analysis and the technical datasheet rather than a single consolidated public datasheet.
The material is normally supplied in pellet form, stabilised for thermal processing, and intended for blown film applications where a high-density linear backbone improves stiffness, downgauging, and moisture barrier. Because published product-specific data for TR-168 is limited, engineering specifications should be validated against the lot-level certificate of analysis. The absence of a public unified datasheet is a procurement constraint, not a basis for inference from unrelated HDPE grades.
The property envelope is defined by the standard test methodology used for high-density polyethylene film resins. Product-specific values are lot-dependent and are not reproduced here where they are not publicly available. The following checklist establishes the measurement basis for incoming inspection, process capability studies, and compliance documentation.
| Property | Standard designation | Measurement configuration | Engineering relevance |
|---|---|---|---|
| Density | ISO 1183-1:2019 | Immersion or density gradient column at 23 °C | Crystallinity, modulus, barrier |
| Melt mass-flow rate | ISO 1133-1:2022 | Procedure A at 190 °C/2.16 kg | Extruder pressure, bubble stability |
| Tensile properties | ISO 527-2:2012 | Type 1B specimen at 50 mm/min | Film stiffness, yield point |
| Elmendorf tear | ASTM D1922-23 | Pendulum tear, nicked specimen | Machine/transverse tear balance |
| Dart impact | ASTM D1709-24 | Method A or B falling dart | Puncture resistance |
| Environmental stress crack resistance | ASTM D1693-15 | Condition B, 10% Igepal, 50 °C | Chemical contact durability |
| Vicat softening temperature | ISO 306:2022 | A50 method, 10 N, 50 °C/h | Temperature resistance |
The property profile of TR-168 is therefore verified through methods that are standard for HDPE film resins, but the numerical acceptance limits must be obtained from QAPCO. Published data for this specific configuration is limited, and laboratory testing of the received lot is required for critical packaging qualifications.
On production-scale blown film lines, HDPE resins in the LOTRÈNE TR-168 density class are frequently processed on grooved-feed extruders with screw diameters from 60 mm to 90 mm and L/D ratios of 30:1 to 33:1. Melt temperature at the die is maintained between 190 °C and 220 °C; excursions above 230 °C accelerate thermo-oxidative chain scission unless the stabilisation package is sufficient for the residence time involved. Die gaps from 1.2 mm to 1.8 mm are used to generate the shear stress necessary for homogenisation of a high-density melt. TR-168 is not inherently hygroscopic, but if storage humidity exceeds 60% RH, surface condensation can create pinholes in the bubble. In such cases, predrying at 70 °C to 80 °C for 2 h to 3 h is applied using desiccant or hot-air drying equipment. These settings are class-level starting points; lot-specific optimisation for TR-168 is required because of the limited public data.
High-stalk blown film equipment is the relevant conversion environment for HDPE grades of this class. The bubble is intentionally raised to 8 to 10 die diameters above the die, allowing the melt to orient before it reaches the frost line. Blow-up ratios between 4:1 and 6:1 are characteristic for HDPE film production. Ratios below this range produce anisotropic tear propagation, which is quantified by ASTM D1922-23 as a difference between machine-direction and transverse-direction tear resistance. Neck stability is sensitive to melt-temperature uniformity, die-lip condition, and extrusion pressure. Die-lip deposits are observed on low-melt-index HDPE lines when the die lip temperature drops below the melt temperature or when low die gaps are run for extended periods. Fluoropolymer process aids at addition levels of 0.05 wt% to 0.10 wt% are sometimes used to suppress deposit formation; compatibility with the QAPCO stabilisation package should be confirmed before use.
LOTRÈNE TR-168 is not interchangeable with QAPCO LDPE grades such as the FE-series products. The structural distinction is chain architecture: LDPE produced by free-radical polymerisation contains long-chain branching, whereas HDPE produced by low-pressure or slurry processes is predominantly linear. The linear backbone increases density and crystallinity, which raises tensile modulus and reduces permeability for a fixed gauge. In comparison with QAPCO high-flow HDPE injection grades, TR-168 is not designed for thin-wall mould filling. The lower melt-flow position of TR-168 provides bubble stability in blown film but would produce excessive injection pressure in moulds with wall sections below 1.0 mm. For injection applications, a QAPCO high-flow HDPE grade should be selected instead. Compared with LLDPE, the HDPE class generally shows lower dart impact but higher stiffness and moisture barrier; the exact balance for TR-168 must be measured under ASTM D1709-24 and ASTM E96/E96M-24.
For food-contact packaging, the resin must be evaluated under the applicable regulatory framework. QAPCO should provide the product regulatory statement for TR-168 before commercial use. Polyethylene of this class is assessed under 21 CFR 177.1520 for US food-contact applications when the polymer is listed and migration testing supports the intended use temperature. For European Union supply, documentation is generally provided according to Regulation (EC) No 1935/2004 and EU Regulation 10/2011. The grade is not automatically RoHS-compliant; a supplier declaration is required to confirm absence of the restricted substances listed in Directive 2011/65/EU, Annex II. Additives, colourants, or processing aids added downstream are not covered by the base resin regulatory statement and must be assessed separately.
| Parameter | HDPE class (TR-168) | LDPE class | LLDPE class | Standard designation |
|---|---|---|---|---|
| Density | ≥ 0.940 g/cm³ | 0.910–0.930 g/cm³ | 0.912–0.940 g/cm³ | ASTM D883-23/ISO 1183-1:2019 |
| Chain architecture | Predominantly linear | Long-chain branched | Linear with short-chain branches | Not applicable |
| Tensile modulus trend | Higher | Lower | Intermediate | ISO 527-2:2012 |
| Moisture barrier trend | Higher | Lower | Intermediate | ASTM E96/E96M-24 |
When LOTRÈNE TR-168 is evaluated as a replacement for conventional LDPE in thin-gauge sack extrusion, the line must be rebalanced because the linear HDPE backbone changes extensional flow, drawdown, and tear anisotropy. Tensile modulus measured under ISO 527-2:2012 may increase, allowing a gauge reduction if stiffness is the limiting criterion. However, dart impact measured under ASTM D1709-24 often decreases in HDPE relative to LDPE at the same gauge. Downgauging must therefore be validated by sack drop testing and field performance, not by tensile modulus alone. Seal initiation is also shifted upward because HDPE has a higher crystalline melting endotherm than LDPE; differential scanning calorimetry under ISO 11357-3:2018 is used to measure the melting profile. Seal strength must be checked under ASTM F88/F88M-23 after jaw temperature is raised. Published data for this specific TR-168 replacement configuration is limited, so full-scale sack production trials with tare weight, seal strength, and tear balance measurements are required before commercial changeover.
Operational boundaries follow the limitations common to high-density polyethylene film resins. Melt temperature should not remain above 230 °C to 240 °C during extended idle periods because chain scission and vinyl group formation reduce mechanical properties. Direct contact with strong oxidising acids, chlorinated solvents, or mineral oils should be evaluated for environmental stress cracking under ASTM D1693-15. Regrind levels must be validated with QAPCO technical service because acceptable regrind percentage depends on film gauge, gel count, and end-use specification. High levels of amine-based additives should be avoided unless compatibility with the base stabilisation package is confirmed; antagonism in long-term thermal ageing can occur. The resin must be stored away from direct sunlight and ultraviolet radiation because unstabilised high-density polyethylene undergoes rapid photodegradation. No compliance or performance statement in this document replaces the QAPCO certificate of analysis for LOTRÈNE TR-168.