| HS Code | 623883 |
| Product Name | QAPCO LOTRÈNE HHM5502BN |
| Manufacturer | QAPCO (Qatar Petrochemical Company) |
| Material Type | High Density Polyethylene (HDPE) |
| Grade | HHM5502BN |
| Density | 0.955 g/cm³ |
| Melt Flow Rate | 0.35 g/10 min (190°C/21.6 kg) |
| Tensile Strength At Yield | 26 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1200 MPa |
| Charpy Notched Impact Strength At 23 C | 20 kJ/m² |
| Charpy Notched Impact Strength At 30 C | 8 kJ/m² |
| Vicat Softening Temperature | 126 °C |
| Melting Temperature | 132 °C |
| Environmental Stress Crack Resistance | >1000 h |
| Hardness Shore D | 65 |
| Thermal Conductivity | 0.4 W/m·K |
| Water Absorption | <0.01% |
As an accredited QAPCO HDPE LOTRÈNE HHM5502BN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | QAPCO LOTRÈNE HHM5502BN HDPE pellets are packaged in 25 kg polyethylene bags, typically 55 bags per pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): dry container loaded with 25 kg bags of QAPCO HDPE LOTRÈNE HHM5502BN, palletized, stretch-wrapped, and secured for ocean transport. |
| Shipping | QAPCO HDPE LOTRÈNE HHM5502BN is a non-hazardous solid polymer. It is typically shipped in 25 kg polyethylene bags, palletized and stretch-wrapped, via sea, road, or rail in clean, dry containers. Keep packages closed and dry. Store away from moisture, heat, direct sunlight, and ignition sources. No special dangerous goods handling required. |
| Storage | Store QAPCO LOTRÈNE HHM5502BN in original, closed packaging in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep pallets clean and off the floor to prevent moisture and contamination. Avoid prolonged UV exposure and incompatible oxidizers. Maintain ambient conditions; follow first-in/first-out stock rotation and protect from physical damage. |
| Shelf Life | Shelf life is typically 24 months when stored in original unopened packaging, dry, cool, ventilated conditions, away from direct sunlight. |
| Property | Test Method | BUR 3.5:1 | BUR 4.5:1 | BUR 5:1 |
|---|---|---|---|---|
| Dart Impact (F50), 12 µm film | ASTM D1709-16e1 | 220 g | 190 g | 160 g |
| Elmendorf Tear MD, 12 µm | ASTM D1922-15 | 14 g/µm | 11 g/µm | 9 g/µm |
| Elmendorf Tear TD, 12 µm | ASTM D1922-15 | 35 g/µm | 42 g/µm | 48 g/µm |
| Tensile Yield MD | ASTM D882-18 | 32 MPa | 29 MPa | 26 MPa |
| Tensile Yield TD | ASTM D882-18 | 28 MPa | 26 MPa | 24 MPa |
| Elongation at Break MD | ASTM D882-18 | 680% | 640% | 590% |
Competitive QAPCO HDPE LOTRÈNE HHM5502BN prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
QAPCO HDPE LOTRÈNE HHM5502BN is a black high-molecular-weight high-density polyethylene copolymer supplied as a pre-compounded extrusion blow-moulding grade. The material is designed for large technical containers and industrial packaging in which environmental stress-crack resistance, stiffness, and parison melt strength are the controlling process requirements. The grade is specified with a nominal melt flow index of 0.25–0.35 g/10 min at 190°C under 2.16 kg load when tested according to ISO 1133-1:2022, and a nominal density of 0.955–0.958 g/cm³ when tested according to ISO 1183-1:2019. These values place HHM5502BN in the high-molecular-weight HDPE blow-moulding family rather than in injection-moulding or film grades. The “BN” suffix denotes a black, stabilised pre-compound rather than a natural resin requiring downstream masterbatch addition.
The product is normally processed on extrusion blow-moulding machines with screw L/D ratios of 24:1–30:1. The black pre-compound form reduces the hopper-related dosing variability associated with natural HDPE plus carbon black masterbatch, but it also fixes the carbon black aggregate structure before the melt enters the extruder. Consequently, die swell and parison thickness distribution must be validated on the target tool rather than inferred from a natural-grade baseline. The property envelope below is based on published typical values; specification limits may be narrower on a certificate of analysis.
The molecular architecture of HHM5502BN is built around a bimodal molecular weight distribution. The high-molecular-weight fraction increases low-shear viscosity and melt strength, while the lower-molecular-weight fraction preserves high-shear processability and surface quality. This distribution produces a higher concentration of tie molecules than a unimodal grade of equivalent density, which translates into improved environmental stress-crack resistance and impact performance in thick-walled blow-moulded parts. At typical extrusion shear rates of 100–1000 s⁻¹, the material shear-thins sufficiently to prevent excessive screw torque and head pressure. The low-shear viscosity is nevertheless high enough to reduce parison sag on intermittent shuttle machines producing long, heavy parisons.
| Property | Test standard | Typical value |
|---|---|---|
| Melt flow index, 190°C/2.16 kg | ISO 1133-1:2022 | 0.25–0.35 g/10 min |
| Density, 23°C | ISO 1183-1:2019 | 0.955–0.958 g/cm³ |
| Tensile stress at yield, 50 mm/min | ISO 527-2/1A/50 | 28–31 MPa |
| Tensile elongation at break | ISO 527-2/1A/50 | >600% |
| Flexural modulus | ISO 178:2019 | 1500–1700 MPa |
| Charpy notched impact strength, 23°C | ISO 179-1/1eA:2023 | 18–25 kJ/m² |
| Vicat softening temperature, 10 N, 50°C/h | ISO 306:2022 | 126–130°C |
| Environmental stress-crack resistance, 100% Igepal, 50°C, F50 | ASTM D1693-15 | >600 h |
The combination of density and molecular weight distribution differentiates HHM5502BN from higher-melt-flow HDPE blow-moulding grades used for thin-walled bottles. A melt flow index below 0.35 g/10 min is appropriate for large parisons that must resist sag during mould closing. A density of 0.955–0.958 g/cm³ provides stacking stiffness for jerricans and pails, while remaining below the density range at which stress-crack resistance falls sharply. Increasing density toward 0.965 g/cm³ would raise top-load capability but typically reduces environmental stress-crack resistance in aggressive wetting agents. The reported ESCR value above 600 h under 100% Igepal at 50°C indicates suitability for containers holding surfactants, agricultural chemicals, and certain hydrocarbon-containing products, provided the finished part is tested in the specific chemical environment.
On an intermittent shuttle blow-moulding machine producing a 20–30 L tight-head jerrican, melt temperature measured at the die exit is usually controlled within 210–230°C. Cylinder zones are set from approximately 170°C at the feed throat to 210°C at the metering section, with head and die temperatures of 210–220°C. Extruders using 24:1–30:1 L/D screens and grooved feed bushings generate sufficient enthalpy without excessive back pressure; head pressures are typically held below 30 MPa. Die land length-to-gap ratios of 10:1–15:1 and die gaps of 1.5–2.5 mm are common. Under these conditions, die swell is observed in the 25–40% range, but the exact value depends on die geometry, melt temperature, shear rate, and pigment dispersion.
For a 25 L jerrican, mould clamping force is usually specified in the 150–300 kN range, depending on projected area, part depth, and blow pressure. Pre-blow pressure is typically 0.4–0.7 MPa, while final blow pressure is 0.8–1.2 MPa. Parison programming is used to compensate for wall-thickness distribution in the corner and pinch-off areas. A parison programming stroke of 20–35% from the accumulator is common, but the profile must be adjusted for each tool, because die swell and sag are coupled. Field experience on shuttle machines indicates that poor pinch-off welds and pinholes occur when the melt temperature drops below 190°C, especially at the flash parting line. Conversely, melt temperatures above 240°C can create visible carbon black agglomerates, brown streaks, or gels, particularly in extruders with dead spots or long residence time. The practical processing window is therefore approximately 20–30°C wide, which is a critical control parameter for converters using regrind or frequent colour changes.
Batch-to-batch melt flow shift should be considered when switching production lots. A shift of more than 0.05 g/10 min can change parison sag and wall distribution enough to require reprogramming of the parison profile or adjustment of the die gap. Suppliers of high-molecular-weight blow-moulding HDPE commonly control lot-to-lot melt flow variation within ±0.03 g/10 min, but the certificate of analysis should be reviewed for every silo or bulk truck receipt. If the material is blended with regrind, the regrind should be homogenised before addition. Regrind levels of 10–30 wt% are commonly used in non-food industrial containers, but black pre-compound regrind can shift viscosity and impact behaviour if fines or carbon black-rich dust are not controlled.
Moisture absorption is not normally an issue for HDPE under dry warehouse conditions. However, condensation on cold pellets moved into a humid processing hall with relative humidity above 60% can introduce surface moisture and produce splay or pinholes. Regrind moisture above 0.05% is also sufficient to cause surface defects. Pre-drying at 70–80°C for 2–3 h is recommended for wet pellets or regrind before blending. Contamination with polypropylene above 5 wt% is not recommended because phase-separated PP domains can reduce environmental stress-crack resistance and weld-line integrity. High levels of certain metal stearates can also increase die lip buildup and should be kept within supplier-approved limits.
Applications for HHM5502BN are concentrated in UN-certified industrial jerricans, open-head pails, and multilayer container structures. In a 20–25 L tight-head jerrican, the grade provides stiffness and stress-crack resistance required to contain hazardous liquids under ADR, RID, and IMDG packaging requirements. The container, not the polymer alone, is certified. Hydraulic internal pressure testing at 100 kPa and drop testing at -18°C are typically performed on the finished article according to Chapter 6.1 of the UN Recommendations on the Transport of Dangerous Goods. For automotive fuel tank applications, HHM5502BN may be used as the structural layer in coextruded six-layer systems with an EVOH barrier layer, where adhesion is controlled by tie resins. Published data for this specific configuration is limited, and permeation performance depends on layer thickness, barrier type, and surface sulfonation or fluorination.
The grade is not intended for injection moulding, film extrusion, or pressure pipe. High-viscosity blow-moulding HDPE of this class can shear heat excessively in injection moulding barrels and produce nozzle drool, gate blush, and weak weld lines. Film dies designed for LLDPE or LDPE cannot accommodate the melt strength and die pressure of HHM5502BN without excessive back pressure and sharkskin. Pressure-pipe applications require a pipe-grade HDPE with a hydrostatic design basis verified under ISO 9080 or ASTM D2837; HHM5502BN is not optimised for long-term hoop-stress performance in pressure service.
In conversion lines that previously used a natural blow-moulding HDPE plus carbon black masterbatch, substitution with HHM5502BN removes a letdown step. This changes melt homogeneity and die swell. A pre-compound is produced under controlled compounding conditions, typically in twin-screw extruders with L/D ratios of 36:1–48:1, to disperse carbon black below an agglomerate size that avoids visible specks and impact instability. A simple single-screw letdown of carbon black masterbatch at the hopper is more sensitive to dosing error and can create batch-to-batch colour and mechanical property drift. Commercial black HDPE blow-moulding compounds of this class typically contain 2.0–2.5 wt% carbon black with a primary particle size of 20–50 nm; the exact loading in HHM5502BN is supplier-controlled and should be confirmed on the certificate of analysis.
The fixed carbon black aggregate structure in a pre-compound means die swell and parison sag are more reproducible from lot to lot, but the processor loses the ability to fine-tune die swell by adjusting masterbatch level. When a tool is transferred from natural HDPE plus masterbatch to HHM5502BN, the die gap, parison profile, and cooling time should be revalidated because the melt elasticity of a compounded black grade can differ from a natural grade even when melt flow index and density are unchanged. Regrind of black parts can also accumulate carbon black locally if the blend feeder is not homogenised; using 10–30 wt% regrind is acceptable for most non-food industrial containers, but the blend ratio should be constant to avoid density and impact variations.
Black HDPE provides ultraviolet screening through carbon black. Accelerated weathering can be evaluated according to ISO 4892-2, but specific retained property data for HHM5502BN in a given part are not always published in the public datasheet. Such data should be obtained from QAPCO or qualified by the converter for the target service environment and wall thickness. Compliance with food-contact conditions may be supported by FDA 21 CFR 177.1520 for olefin polymers, but the black pre-compound must be confirmed by a written supplier declaration because carbon black and stabiliser selection may require end-use migration testing under EU Regulation (EU) No 10/2011. REACH compliance is assessed under Regulation (EC) No 1907/2006 and RoHS under Directive 2011/65/EU; the converter should verify that the grade is listed on the supplier’s current compliance declaration for the intended jurisdiction. Compared with natural HDPE plus external carbon black masterbatch, HHM5502BN reduces hopper letdown variation but requires stricter control of melt temperature and die swell validation. Compared with unimodal HDPE blow-moulding grades of equal density, the bimodal architecture provides higher environmental stress-crack resistance and reduced parison sag, but it requires higher melt temperatures and can generate higher die head pressure on small extruders.