Qapco Hdpe Hhm5502bn

QAPCO HDPE HHM5502BN

    • Product Name: QAPCO HDPE HHM5502BN
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 535761
    Density 0.955 g/cm3
    Melt Flow Rate 190c 2 16 Kg 0.35 g/10 min
    Melt Flow Rate 190c 21 6 Kg 25 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Elongation At Break >600%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength At 23c 200 J/m
    Hardness Shore D 65
    Vicat Softening Temperature 126 deg C
    Brittleness Temperature < -70 deg C
    Heat Deflection Temperature At 0 45 Mpa 75 deg C
    Environmental Stress Cracking Resistance F50 100 Igepal >1000 hr
    Thermal Conductivity 0.45 W/m.K
    Coefficient Of Linear Thermal Expansion 1.2 x 10^-4 /deg C
    Water Absorption <0.01%
    Dielectric Constant At 1 Mhz 2.3
    Volume Resistivity >10^16 ohm.cm
    Melt Temperature 190-210 deg C
    Mold Temperature 20-40 deg C
    Molding Shrinkage 2-4%

    As an accredited QAPCO HDPE HHM5502BN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing QAPCO HDPE HHM5502BN is packaged in 25 kg polyethylene bags, typically stacked on pallets for transport and storage.
    Container Loading (20′ FCL) 20′ FCL loading: QAPCO HDPE HHM5502BN, 25 kg bags, up to 22 MT net, floor-loaded or palletized, securely stowed for transport.
    Shipping QAPCO HDPE HHM5502BN is a non-hazardous solid polyethylene resin, shipped as pellets in 25 kg PE bags or 1 MT jumbo bags, palletized and stretch-wrapped. For transport, classify as non-regulated plastic resin; keep dry, covered, away from heat and moisture. No UN hazard class required.
    Storage Store QAPCO HDPE HHM5502BN in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers or bags closed, clean, and clearly labeled. Avoid moisture, dust, and contamination. Stack pallets securely to prevent damage, follow first-in, first-out inventory practices, protect from static discharge and prolonged UV exposure, and segregate from incompatible materials.
    Shelf Life Typically two years from production date when stored in original packaging, dry, cool, and protected from direct sunlight and moisture.
    Application of QAPCO HDPE HHM5502BN

    Why 20 L to 60 L UN-certified jerrycans demand ESCR above 1,000 h in agrochemical service

    In monolayer UN-certified jerrycan production, HDPE HHM5502BN is processed on accumulator-head extrusion blow-moulding lines with screw diameters of 60 mm to 90 mm and L/D ratios of 24:1 to 30:1. The resin is characterised by a density of 0.955 g/cm³ under ISO 1183-1:2019 and a high-load melt index of 30–40 g/10 min under ISO 1133-1:2022 at 21.6 kg, which provides sufficient parison melt strength for 20 L to 60 L containers without excessive extruder torque. The formulation is maintained at 100 phr resin, with blue phthalocyanine masterbatch at 1.5–2.5 wt%, hindered phenolic primary antioxidant at 0.2–0.5 phr, phosphite secondary antioxidant at 0.1–0.3 phr, hindered amine light stabiliser at 0.2–0.5 phr, and zinc stearate at 0.05–0.1 phr; total non-resin components are held below 3.5 wt% because higher masterbatch loadings depress ASTM D1693-15 Condition B, 100% Igepal CO-630 ESCR below the 1,000 h requirement observed for agricultural emulsifiable concentrates and chlorinated solvent service. Melt temperature is controlled at 190–210°C, mould water temperature at 10–15°C, and blow air pressure at 0.6–0.8 MPa. The parison programme expands the die gap from 3 mm to 12 mm during the initial 30% of parison drop to counter gravity-induced drawdown; on production-scale shuttle machines, shot-to-shot weight variation is held to ±1.5% for a 20 L container. Pinch-off weld zones are trimmed with a hot knife at 180–230°C to avoid microcrack initiation. UN Model Regulations 23rd revised edition, Chapter 6.1 tests are applied, including drop at 6.1.5.3, leakproofness at 6.1.5.4, hydraulic pressure at 6.1.5.5, and stacking at 6.1.5.6. Terminal types include 20 L, 25 L, 30 L and 60 L jerrycans carrying UN marking 3H1/Y/... for packing groups II and III, used for crop protection formulations, industrial solvent and detergent intermediates.

    UN packaging tests for HDPE jerrycans
    TestStandard/clauseTypical conditionPass requirement
    Drop6.1.5.31.9 m after -18°C conditioning for liquidsNo leakage
    Leakproofness6.1.5.4Internal air pressure 0.02 MPaNo leakage
    Hydraulic pressure6.1.5.5100 kPa for 30 minNo leakage or rupture
    Stacking6.1.5.6Load equivalent to 3 m stack for 28 d at 40°CNo deformation causing failure

    Automotive windshield washer reservoirs and unpressurised coolant recovery bottles

    Blow-moulded automotive reservoirs produced from HHM5502BN are validated against ISO 16750-3:2012 for underhood temperature and humidity cycling, with a typical continuous-use wall temperature ceiling of 70°C and short excursion tolerance up to 85°C at the mounting bosses. The compound uses 100 phr HDPE, carbon black masterbatch at 2.0–3.0 wt% for UV screening and heat aging resistance, a heat-stabiliser package at 0.3–0.5 phr, and process aid at 0.1–0.2 phr; no impact modifier is added because the high-molecular-weight HDPE already provides Charpy notched impact values above 6 kJ/m² under ISO 179-1/1eA at 23°C. Production is carried out on accumulator-head machines with melt temperature 190–215°C, mould temperature 8–12°C, and blow air pressure 0.7–0.9 MPa; cycle times range from 50 s to 80 s for 2 L to 5 L reservoirs. The main in-line failure mode is leakage at the injection-moulded hose barb insert, so ultrasonic welding of the fitting is set to amplitude of 20–30 µm and a frequency of 20 kHz with a post-weld quench to reduce crystallinity in the joint. Finished product types include 2.0 L, 3.0 L and 5.0 L windshield washer reservoirs and unpressurised coolant recovery bottles in the 0.5–2.0 L range; these components are not validated for pressurised cooling systems, where high-molecular-weight HDPE would exceed the heat deflection temperature boundary at 0.45 MPa.

    Household and industrial cleaning product bottles under oxidative bleach exposure

    Multi-cavity shuttle blow moulding of household and industrial cleaning product bottles utilises HHM5502BN at 100 phr, titanium dioxide masterbatch at 1.2–2.0 wt%, zinc stearate at 0.05–0.2 phr, and a low-polarity processing aid at 0.1–0.2 phr to reduce melt fracture in continuous extrusion with die temperatures of 170–190°C. The ESCR threshold for sodium hypochlorite, quaternary ammonium disinfectants and linear alkylbenzene sulfonate detergents is referenced to ASTM D1693-15 Condition A, 100% Igepal CO-630, where a failure time below 300 h is considered inadequate for retail bleach packaging. Mould water is held at 8–12°C and blow air at 0.5–0.8 MPa on shuttle machines with 1+1 or 2+2 cavity layouts; cycle time for a 1 L bottle ranges from 20 s to 45 s depending on handle design. Non-hazardous retail formulations are not subject to UN packaging approval, but industrial concentrates classified as dangerous goods require 3H1 jerrycan testing according to the transport mode. Regulatory compliance is anchored to REACH (EC) No 1907/2006 for substance restrictions and, for food-contact adjacent products, to EU 10/2011. Terminal container types include 250 mL, 500 mL, 750 mL, 1 L, 2 L and 5 L bottles for bleach, disinfectants, laundry detergents, hard-surface cleaners, and industrial degreasers.

    When cosmetic-grade HDPE replacement demands neck calibration below ±0.5 mm

    In personal care and cosmetics packaging, the critical quality parameter is not ESCR but the dimensional consistency of the bottle neck and the sealing surface after post-mould shrinkage. HHM5502BN is run at 100 phr with a color masterbatch at 0.5–2.0 wt%, slip additive at 0.05–0.15 phr, and an antistat at 0.05–0.1 phr for downstream high-speed filling lines. The blow-pin neck ring is cooled to 5–10°C while the mould body is held at 10–15°C to freeze the calibrated neck before body crystallization proceeds; that difference in cooling rates maintains neck inner diameter tolerance within ±0.5 mm and reduces cap leakage torque failures below 0.3% in production audits. Melt temperature is set at 180–205°C, blow air at 0.6–0.8 MPa, and cycle time for a 500 mL bottle on a single-station shuttle is between 18 s and 35 s. Cosmetic packaging outputs are governed by Regulation (EC) No 1223/2009 for product-contact compatibility and, where the same grade is used for food-contact samples, by FDA 21 CFR 177.1520(c) 3.1 and 3.2 and EU 10/2011. Published data for exact neck-ring calibration wear rates on HHM5502BN is limited; the tolerance is therefore verified by production audit rather than by a single standard. The terminal formats include 100 mL to 1,000 mL shampoo, conditioner, body wash and hand soap bottles, as well as trigger-spray containers for diluted cosmetic concentrates.

    Intermediate bulk container inner liners and 100-point parison control on accumulator heads

    For 1,000 L single-wall intermediate bulk container inner bottles, HDPE HHM5502BN is processed at 100 phr with a UV stabiliser masterbatch at 0.3–0.6 wt%, antioxidant at 0.2–0.5 phr, and no talc or calcium carbonate filler because inorganic fillers increase density and reduce the slow crack growth resistance required for vertical side-wall hydrostatic loading. The accumulator-head blow-moulding line uses screw diameters from 90 mm to 150 mm, L/D 24:1 to 30:1, total parison shot weight of 8 kg to 12 kg, and extruder output of 300–600 kg/h. Parison programming with 100-point axial wall-thickness control is used to maintain a minimum wall thickness of 2.5–3.5 mm at the top and bottom corners; blow air pressure is 0.6–0.8 MPa, and mould temperature is kept at 10–18°C. After demoulding, wall-thickness distribution is measured by ultrasonic gauge, and the vessel is subjected to a drop test from 1.9 m at -18°C for UN 31A/Y qualification if hazardous liquids are to be shipped; non-hazardous service uses ISO 16106:2006 and ASTM D1998-15 as the primary standards. Terminal products include 1,000 L IBC inner bottles for non-hazardous aqueous emulsions, water-treatment polymers, and non-oxidising acids, as well as 120 L and 220 L blow-moulded storage tanks for industrial liquid dispensing.

    Food-contact bulk containers under FDA 21 CFR 177.1520(c) 3.1 and 3.2

    Cold-fill food-contact containers utilise HHM5502BN at 100 phr, with the additive package restricted to a food-grade antioxidant at 0.1–0.2 phr and no colour masterbatch when natural unpigmented finished goods are required; if white or coloured containers are specified, the masterbatch carrier and pigments must be individually listed under EU 10/2011 and FDA 21 CFR 177.1520(c) 3.1 and 3.2. Extrusion blow moulding is performed on long-stroke machines at melt temperatures of 180–205°C, parison blow air of 0.6–0.8 MPa, and mould water temperature of 10–15°C; the screw and barrel are purged with a food-grade HDPE before production to avoid carryover of non-food additives. The critical regulatory boundary is hot-fill: this high-density polyethylene is limited to continuous content temperatures below 60°C, and for fatty foods with free oil above 5% migration testing under EU 10/2011 should be performed because lipophilic contact can accelerate additive migration kinetics. Terminal types include 1 L to 20 L containers for liquid confectionery sauces, syrups, vinegar, edible oil, and dry food ingredients, with cold-fill or ambient-fill lines only.

    Agricultural adjuvant and seed treatment packaging for outdoor UV service

    Agricultural adjuvant and seed-treatment packaging produced from HHM5502BN requires both ESCR and resistance to outdoor storage under UV exposure. The compound is 100 phr HDPE, with a UV weathering package at 0.3–0.6 phr, hindered phenol antioxidant at 0.2–0.5 phr, and a heavily pigmented high-opacity masterbatch at 1.5–3.0 wt% to protect light-sensitive adjuvants. The production route is accumulator-head blow moulding with melt temperatures of 190–210°C, mould temperature 12–18°C, and blow air pressure 0.6–0.8 MPa; containers are leak-tested with 0.03 MPa air under water and dried with ionised air to below 10% internal surface moisture before filling. Packaging compliance follows the same UN Chapter 6.1 sequence for dangerous goods as industrial jerrycans, and the finished 5 L, 10 L and 20 L containers are used for seed treatments, surfactants, and water-dispersible granule formulations.

    Free Quote

    Competitive QAPCO HDPE HHM5502BN prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    QAPCO HDPE HHM5502BN is a high-molecular-weight high-density polyethylene blow moulding resin in the QAPCO HDPE portfolio. The grade is supplied as natural pellets without slip or antistatic surface additives. Nominal density is 0.955 g/cm³ when determined by ASTM D1505-20, and the melt flow index is 0.2 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. The high-load melt index is controlled around 2.0 g/10 min at 190 °C/21.6 kg under ASTM D1238-20. Representative published mechanical data list tensile yield at approximately 26 MPa per ASTM D638-14, flexural modulus at approximately 1,200 MPa per ASTM D790-17, and F50 environmental stress-crack resistance above 600 h per ASTM D1693-15 in 100 % Igepal CO-630. Moisture absorption is below 0.01 % by ASTM D570-22, Vicat softening temperature is approximately 123 °C under ASTM D1525-17, and Shore D hardness is approximately 65 under ASTM D2240-15. Elongation at break is above 600 % per ASTM D638-14. The grade occupies the high-density, high-molar-mass corner of the HDPE blow moulding range, which separates it from lower-density HDPE film resin and from high-flow injection moulding HDPE. Reported conversion routes include extrusion blow moulded containers from 5 L to 220 L, industrial jerry cans, agrochemical drums, and narrow-neck bottles for viscous liquids. The density and melt-flow profile make it a candidate for thick-wall containers where top load and slow crack growth resistance are specified requirements.

    What Limits HHM5502BN in Fast-Cycle Continuous Extrusion Blow Moulding?

    Compared with HDPE blow moulding grades having high-load melt indices of 5–20 g/10 min, HHM5502BN sits in a lower-throughput window because the 2.0 g/10 min high-load melt index and high low-shear viscosity increase head pressure and limit screw speed. The resin is therefore not normally assigned to wheel-type or shuttle machines producing 100–500 mL bottles at 5–8 s cycles; such equipment generally uses lower-molecular-weight resins to avoid parison curl, cold weld, and excessive motor load. On accumulator-head extrusion blow moulding lines, the same molecular structure provides longer parison hang time and more stable die swell. The melt flow ratio of approximately 10:1 between 21.6 kg and 2.16 kg indicates a broad molecular weight distribution that permits shear-induced flow in extruder screw channels while retaining low melt flow at low shear. Compared with injection moulding HDPE grades whose melt flow indices are commonly 8–40 g/10 min, HHM5502BN is not suitable for injection moulding because the low melt flow index causes high filling pressure, short shot risk, and poor knit-line strength in multi-gated tools. The difference from other blow moulding grades is therefore primarily rheological: the grade is selected where accumulator-head parison stability and final part toughness outweigh cycle-time reduction. The resin is generally specified for wall thicknesses of 1.5–6 mm; below 1.5 mm, the melt may freeze before adequate pinch-off welding occurs in large moulds.

    Temperature and Tooling Boundaries Are Not Independent

    On production-scale extrusion blow moulding lines with grooved-feed single-screw extruders of 80–120 mm diameter and L/D ratios from 24:1 to 30:1, barrel set points from feed throat to metering section are normally maintained between 170 °C and 200 °C. The feed throat is cooled to 35–50 °C to prevent premature melting and pellet bridging. Head and die zones are set between 190 °C and 205 °C to control parison surface texture and melt fracture. Direct melt temperature should not remain above 220 °C for extended residence periods; above this threshold thermal-oxidative chain scission increases melt flow index, an effect measurable as a positive shift under ASTM D1238-20 after multiple heat histories. Shared lines must be purged thoroughly after PVC, acetal, or ionomer runs; residual halogenated polymer at HDPE processing temperatures can liberate hydrogen chloride and catalyse HDPE chain scission. The grade does not require pre-drying in sealed silos, but pellets stored above 60 % relative humidity or blended with wet external regrind should be dried at 80–90 °C for 2–4 h in desiccant units with a dew point of approximately -40 °C. Die geometry is normally configured for blow-up ratios between 1.8:1 and 2.5:1; progression beyond 3:1 commonly produces wall-thickness non-uniformity and weak pinch-off seams. Mold temperatures between 10 °C and 30 °C are typical for water-cooled aluminum tooling, while steel tooling may be run up to 40 °C. Regrind addition is generally limited to 30 wt% in chemical containers requiring high stress-crack resistance because repeated heat history increases melt flow and can reduce ESCR below the intended specification.

    Because single-point melt indices do not fully determine parison behaviour, capillary rheometry at 190 °C across 10–1,000 s⁻¹ is used to model die pressure, screw back-pressure, and shear heating. Lot-to-lot HLMI variation is typically controlled within ± 0.2 g/10 min around the 2.0 g/10 min nominal, while density variation is held within ± 0.001 g/cm³. A positive HLMI drift of 0.2 g/10 min can alter parison drawdown and final wall thickness in tall containers because sag resistance changes; a density shift of 0.001 g/cm³ can move top-load performance by an amount that may require tooling adjustment. For HDPE, a barrier screw with a Maddock mixing section and compression ratio of 2.5:1 to 3.5:1 is typically used with a grooved feed throat on 80–120 mm lines. Smooth-bore extruders without grooved feed sections generally provide insufficient feed-zone pressure for high-molecular-weight HDPE and may suffer throughput surging. Screen-pack selection is normally 60/120/40 mesh or equivalent to protect die gaps from regrind contamination. Melt fracture onset is tooling-dependent and should be mapped using a capillary rheometer and validated on the production die. Published data for this specific configuration in acoustic emission monitoring of slow crack growth are limited.

    Environmental stress-crack resistance is the controlling property in rigid chemical packaging. The short-chain comonomer distribution in HHM5502BN contributes tie molecules that arrest slow crack growth; the resulting F50 values above 600 h per ASTM D1693-15 in 100 % Igepal CO-630 are characteristic of this molecular weight class. This does not constitute universal chemical compatibility. The grade is generally suitable for aqueous alkalis, hypochlorite bleach, and detergent solutions at ambient temperature, but continuous exposure to strong oxidizers above 40 °C, aromatic hydrocarbons, or chlorinated solvents can reduce the stress-crack threshold and promote creep rupture. Chemical exposure testing should be performed on finished containers under ASTM D543-20 or equivalent; weight gain, tensile properties, and ESCR retention should be measured after contact with the intended formulation. Because HDPE is not an oxygen barrier, oxygen transmission should be determined under ASTM D3985-17 and water vapor transmission under ASTM F1249-20 when packaging oxygen-sensitive or moisture-sensitive materials. Natural pellets do not contain UV stabilizer; outdoor exposure beyond 12 months requires carbon black or hindered-amine stabilization and validation under ASTM D2565-21. Published data for this specific configuration in prolonged contact with oxidizing agrochemical concentrates are limited, and compatibility testing on production containers is required before commercial use.

    When HHM5502BN Replaces a Lower-Density HDPE in Industrial Container Specifications

    When a converter substitutes HHM5502BN for a butene-comonomer HDPE of 0.945 g/cm³ at the same wall thickness, the flexural modulus increases from roughly 900–1,000 MPa to approximately 1,200 MPa, which raises top-load capacity determined under ISO 12048:1994 and permits higher stacking loads in warehouse conditions. However, the density increase also tends to lower the intrinsic stress-crack resistance of the polymer matrix; the high molar mass of the grade offsets this partially, but ESCR revalidation under ASTM D1693-15 is required on finished containers. For UN-certified packaging, drop impact and stack tests are conducted under UN 6.1.5.3 and 6.1.4.3 after conditioning at -18 °C and 23 °C. The low HLMI contributes to a thicker and more uniform pinch-off weld in large drums when parison programming is optimized, whereas lower-density higher-HLMI grades may show better low-temperature impact in very thin walls. The selection of HHM5502BN is therefore indicated when heavy-wall industrial container specifications prioritize top load, rigidity, and slow crack growth over thin-wall cycle-time reduction. If downgauging is attempted, minimum wall thickness must be recalculated from top-load, drop-impact, and permeation requirements rather than from mould fill alone.

    Wall thickness changes the mechanical response of HHM5502BN in a non-linear manner. In thick sections above 3 mm, cooling in water-cooled moulds is slower, producing coarser crystalline morphology and lower impact toughness than rapid cooling; in thin sections below 1.5 mm, melt orientation and fast cooling can raise yield strength but reduce drop-impact energy. Laboratory values from compression-moulded specimens under ISO 293:2023 or injection-moulded test bars under ISO 294-1:2017 therefore do not transfer directly to blow moulded part walls. For container validation, tensile and impact specimens should be cut from production sidewalls and tested under ISO 527-2:2012 and ISO 179-1:2023, with notch position oriented perpendicular to melt flow. Ultrasonic sidewall thickness mapping is compared with top-load and drop test results to identify thin spots at pinch-off ears and corners. In production audits, dimensional change after demoulding is measured with a calibrated optical comparator; HDPE typically requires cooling fixtures to control shrinkage in the first 24 h.

    For food-contact and safety compliance, the base resin is evaluated under FDA 21 CFR 177.1520(c) and EU 10/2011; the converter must verify overall migration below 10 mg/dm² and specific migration limits for hexene oligomers and any added masterbatch constituents. The natural grade carries no intentional slip, antiblock, or antistatic surface additives, which allows organoleptic evaluation to be conducted on the base polymer without interference from intentional surface additives. REACH documentation is supplied under Regulation (EC) No 1907/2006, and RoHS compliance is assessed under Directive 2011/65/EU with restricted substances listed in Annex II. The pellet is not classified as hazardous under CLP Regulation (EC) No 1272/2008 in the supplied form. Material safety and exact food-contact status are batch- and additive-package-dependent; a supplier certificate and migration test report should be obtained before use in regulated food-contact articles.

    Top