| HS Code | 942420 |
| Density | 0.918–0.922 g/cm³ |
| Melt Flow Rate | 2.0 g/10 min (190°C, 2.16 kg) |
| Tensile Strength At Yield | ≥10 MPa |
| Tensile Strength At Break | ≥20 MPa |
| Elongation At Break | ≥500% |
| Dart Impact Strength | ≥60 g |
| Tear Strength Md | ≥60 kN/m |
| Tear Strength Td | ≥80 kN/m |
| Haze | ≤12% |
| Gloss | ≥50% |
| Melting Point | 120–125°C |
| Vicat Softening Point | ≥90°C |
| Brittleness Temperature | ≤-70°C |
| Crystallinity | 40–50% |
As an accredited Pucheng Clean Energy LLDPE 7042 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Pucheng Clean Energy LLDPE 7042 is packaged in 25 kg PP woven bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | Pucheng Clean Energy LLDPE 7042 is loaded into a 20′ FCL container, securely stacked and wrapped for safe ocean transport. |
| Shipping | Pucheng Clean Energy LLDPE 7042 is shipped as non-hazardous polymer pellets, typically in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and wrapped. No special hazard class. Transport in clean, dry containers or trucks; protect from moisture, sunlight, and heat. Standard 20' container loads approximately 17–20 metric tons. |
| Storage | Store Pucheng Clean Energy LLDPE 7042 in a cool, dry, well-ventilated warehouse away from direct sunlight, rain, moisture, heat, and ignition sources. Keep bags or containers tightly sealed and palletized off the floor. Avoid prolonged stacking or heavy loads. Separate from strong oxidizers and incompatible materials. Maintain clean handling areas and follow local regulations and supplier recommendations. |
| Shelf Life | Shelf life is typically 12 months in unopened original packaging, stored dry, cool, ventilated, away from direct sunlight and contaminants. |
Blown film conversion of Pucheng Clean Energy LLDPE 7042 places the butene comonomer fraction under simultaneous shear and extensional deformation. The resin is characterised by a melt flow index of 2.0 g/10 min at 190 °C/2.16 kg according to ASTM D1238-20, and a density of 0.919 g/cm³ per ASTM D1505-18. These values establish a processing window that favours bubble stability at blow-up ratios between 2.0:1 and 3.0:1 on single-screw blown film lines with L/D 30:1 to L/D 32:1 barrier screws, dual-lip air rings, and die gaps from 1.8 mm to 2.2 mm. Melt temperature is maintained between 180 °C and 210 °C, while the frost line is held at 4 to 8 die diameters above the die exit to balance transverse and machine direction orientation. Bubble instability and edge flutter appear when output exceeds the cooling capacity of the air ring, particularly on dies above 300 mm diameter, and the resulting gauge variance is measurable as thickness variation beyond ±6 % on high-speed lines. For heavy-duty sack film and agricultural liner applications, the formulation normally uses 100 wt% LLDPE 7042, or a dry blend with 20 wt% to 40 wt% LDPE to improve bubble stability and reduce blocking, plus slip masterbatch at 1 wt% to 3 wt%, antiblock masterbatch at 2 wt% to 5 wt%, and processing aid at 200 ppm to 800 ppm. Dart impact of butene-based LLDPE can be lower than hexene-copolymer LLDPE at comparable density, so puncture-critical grades should be verified under ASTM D1709-16a before final film qualification. Regulatory compliance for food-contact blown film includes FDA 21 CFR 177.1520, EU Regulation 10/2011, REACH EC 1907/2006, and RoHS Directive 2011/65/EU. The terminal product spectrum includes heavy-duty shipping sacks, industrial liners, agricultural silage covers, construction vapour retarder film, and carrier film for lamination.
| Standard / Regulation | Relevant provision or test method | Typical limit or condition |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers, paragraph (c) | Conforms for food-contact use under Conditions of Use D–G |
| EU Regulation 10/2011 | Overall migration per EN 1186 series | ≤ 10 mg/dm² |
| REACH EC 1907/2006 | SVHC content declaration | ≤ 0.1 wt% |
| RoHS Directive 2011/65/EU | Pb, Hg, Cd, Cr(VI), phthalates | ≤ 0.1 wt% per restricted substance |
In cast stretch film production, Pucheng Clean Energy LLDPE 7042 is co-extruded or blended with metallocene-catalysed LLDPE to raise tensile strength and puncture resistance while retaining the drawdown necessary for thin gauge film. The melt flow index of 2.0 g/10 min imposes higher extruder head pressure than cast film grades with 3.5 g/10 min to 5.0 g/10 min, so screw speed and die pressure must be monitored on lines with extruders of L/D 30:1 to L/D 36:1, barrier screws with Maddock mixing sections, flat dies from 2,000 mm to 4,500 mm effective width, and die gaps from 0.5 mm to 0.9 mm. Melt temperature at the die is held at 220 °C to 250 °C, and chill roll temperature is set at 25 °C to 35 °C to stabilise web flatness. Formulation addition ratios for machine pallet wrap include 70 wt% to 90 wt% LLDPE 7042, 10 wt% to 30 wt% metallocene LLDPE, tackifier at 0.5 wt% to 3.0 wt%, and antioxidant masterbatch at 0.5 wt% to 1.5 wt%. At line speeds above 600 m/min, draw resonance and web edge tear are observed if chill roll surface temperature deviates by more than ±3 °C or if the air knife position is not matched to the melt curtain. Tensile properties are measured on 25 mm wide strips according to ASTM D882-18 or ISO 527-3:2018, and puncture resistance is assessed per ASTM D5748-19. Compliance for industrial stretch film is assessed under REACH EC 1907/2006 and RoHS Directive 2011/65/EU; food-contact stretch film also requires EU Regulation 10/2011 overall migration testing. Terminal articles include hand-applied pallet wrap, machine pallet wrap, pre-stretched film, agricultural bale wrap, and bundling film.
Thin-wall injection moulding of Pucheng Clean Energy LLDPE 7042 is carried out in food-contact containers, overcaps, and storage articles where part wall thickness lies between 0.6 mm and 2.5 mm. The melt flow index of 2.0 g/10 min is lower than that of high-flow polypropylene or injection-grade HDPE, so the process requires injection pressures from 80 MPa to 120 MPa and larger gate dimensions to avoid jetting and surface flow marks. Barrel temperature profiles range from 190 °C to 230 °C, mould temperature from 10 °C to 40 °C, and clamping force is estimated from projected area using 2.0 kN/cm² to 4.0 kN/cm². Formulation addition ratios include 100 wt% LLDPE 7042, or a blend with 20 wt% to 30 wt% HDPE to increase top-load rigidity, plus colour masterbatch at 1 wt% to 3 wt% and slip/antiblock masterbatch at 1 wt% to 2 wt% where demoulding or nesting performance is critical. Mould shrinkage is controlled between 1.5 % and 2.5 %, and the value is higher in thick sections because the butene comonomer disrupts crystallinity. Compliance for food-contact injection moulded parts is established under FDA 21 CFR 177.1520, EU Regulation 10/2011, and GB 4806.7-2016 for food-contact plastic articles supplied into the PRC market. Mechanical verification uses ASTM D638-14 tensile testing, ASTM D790-17 flexural modulus, and ASTM D256-23 Izod impact testing. Terminal product types include thin-wall freezer containers, dairy tubs, non-carbonated beverage cup lids, overcap closures for cans, industrial buckets, and storage bins.
Because Pucheng Clean Energy LLDPE 7042 has a molecular weight distribution and comonomer profile compatible with polyolefin carriers, twin-screw compounders use it as a carrier resin in colour and additive masterbatches destined for film, extrusion coating, and injection moulding. In a conventional 40 wt% pigment black masterbatch, LLDPE 7042 may constitute 50 wt% to 55 wt% of the total formula, with low-molecular-weight polyethylene wax at 5 wt% to 8 wt% and antioxidant at 0.2 wt% to 0.5 wt%. The carrier is compounded on a co-rotating twin-screw extruder with L/D 40:1 to L/D 48:1, screw speed from 600 rpm to 800 rpm, and specific mechanical energy input of 0.15 kWh/kg to 0.25 kWh/kg. Pelletising uses a strand bath or die-face cutter with pellet temperature maintained below 60 °C to prevent regrind sticking. The regulatory framework for masterbatch carriers is supplier-level conformance to REACH EC 1907/2006, heavy-metal limits under RoHS Directive 2011/65/EU, and, where the final article is food-contact, FDA 21 CFR 177.1520 or EU Regulation 10/2011 applies to the total formulation and not solely to the carrier resin. Terminal outputs include mono-pigment colour masterbatches, antioxidant/UV stabiliser masterbatches, slip/antiblock concentrates, and filler masterbatches used at 2 wt% to 8 wt% let-down ratios in downstream polyolefin processing.
The extrusion of drip irrigation laterals from Pucheng Clean Energy LLDPE 7042 differs from blown film in that long-term hydrostatic strength, environmental stress cracking resistance, and carbon black dispersion determine field performance. Pipe extrusion is performed on a single-screw extruder with L/D 30:1 to L/D 33:1, a grooved feed throat, and a pin-and-die arrangement for emitter insertion. Melt temperatures are held between 200 °C and 230 °C, and vacuum calibration controls outside diameter to ±0.2 mm at line speeds of 30 m/min to 80 m/min. The compound typically consists of 100 parts by weight LLDPE 7042, carbon black masterbatch at 5 wt% to 7 wt% to achieve final carbon black content of 2.0 wt% to 2.5 wt%, hindered amine light stabiliser at 0.3 wt% to 0.6 wt%, and process aid at 0.05 wt% to 0.2 wt%. Dispersion is assessed by ISO 18553, and finished laterals are qualified under ISO 9261:2004 for emitters and emitting pipe, with pipe dimensional and pressure requirements referenced from ISO 8779:2020. Published hydrostatic design basis data for this specific resin grade is limited under ISO 9080; long-term pressure testing is therefore required before qualification for municipal water mains or high-pressure irrigation networks. LLDPE 7042 is not a UV-stabilised grade, so outdoor service requires the specified carbon black and hindered amine stabiliser system; unpigmented pipe exposed to sunlight should be considered non-conforming for long-term UV exposure. Terminal product types include drip irrigation laterals, micro-irrigation tubes, emitter pipes, and greenhouse irrigation lines.
Competitive Pucheng Clean Energy LLDPE 7042 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Pucheng Clean Energy LLDPE 7042 is a butene-comonomer linear low density polyethylene pellet resin intended primarily for blown-film extrusion. The grade is produced by Pucheng Clean Energy Chemical Co., Ltd. and supplied with certificate-of-analysis data for melt mass-flow rate and base density. Nominal melt mass-flow rate is 2.0 g/10 min when measured at 190°C under 2.16 kg using ISO 1133-1:2022 or ASTM D1238. Nominal density is specified between 0.918 g/cm³ and 0.922 g/cm³ at 23°C by ISO 1183-1:2019 or ASTM D1505. The resin is obtained through low-pressure α-olefin copolymerization; the butene comonomer introduces short-chain branching on a predominantly linear backbone. This architecture separates 7042 from high-pressure LDPE in melt elasticity, and from metallocene LLDPE in molecular weight distribution and processing behavior.
| Parameter | Method | Typical or nominal value | Conversion relevance |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, ASTM D1238 | 1.9–2.1 g/10 min at 190°C, 2.16 kg | Controls melt viscosity, draw-down, and extruder load |
| Density | ISO 1183-1:2019, ASTM D1505 | 0.918–0.922 g/cm³ at 23°C | Sets film modulus, barrier, and yield stress |
| Tensile, dart impact, haze | ISO 527-3, ASTM D882, ASTM D1709, ASTM D1003 | Producer lot certificate and converter film-line data required; public grade-specific data limited | Property balance depends on die gap, blow-up ratio, frost-line height, and additives |
On monolayer blown-film lines, 7042 is commonly run with die gaps of 1.8–2.5 mm, blow-up ratios of 2.0–2.5:1, and melt temperatures of 190–220°C. Frost-line height is normally held at 4–8 die diameters. These settings are not universal; they represent a start-up envelope for standard LLDPE screw and air-ring combinations. Because butene LLDPE has less long-chain branching than autoclave LDPE, the bubble is more sensitive to air-ring turbulence and winder tension variations. A dual-lip air ring is preferred over a single-lip design to maintain a stable freeze line at low stalk height. Extruders with barrier screws and Maddock mixing sections reduce localized melt-temperature excursions. On grooved-feed extruders, melt pressure should be monitored before the screen changer; pressure instability above approximately 25 MPa can propagate into bubble oscillation.
Melt-pressure variations in production often arise when screen packs are heavily loaded or when the barrel temperature profile is too low in the transition zone. Converters using 45–90 mm extruders with L/D 25:1–30:1 should establish the maximum stable screw speed by measuring film gauge uniformity rather than by relying solely on melt temperature. Blending with 10–30 wt% LDPE is a common correction for bubble instability, but the blend reduces dart impact and increases film modulus. The exact ratio is adjusted on the line with reference to ASTM D1709 dart impact, ASTM D1922 tear, and ISO 527-3 tensile data from produced film.
A single melt index value cannot predict film-line energy input because the shear-thinning index of butene LLDPE is typically shallower than that of LDPE. For process modeling, capillary viscosity measurements under ISO 11443 should be used at 190°C, 210°C, and 230°C across shear rates of 101–104 s−1. Melt strength should be evaluated by Rheotens or equivalent extensional rheometry if cast-film or high-stalk blown-film operation is planned. Published data for this grade’s extensional viscosity is limited; therefore, this measurement is an equipment-specific qualification rather than a datasheet parameter.
The response to shear heating in high-output blown-film lines is meaningful because excessive melt temperature increases oxidation risk and lowers bubble strength. When a barrel temperature profile is set to 180°C in the feed zone, 200°C in the compression zone, and 210°C in the metering zone, shear heating may raise the actual melt temperature above the set point. This difference should be checked with an immersion probe at the die exit. If the measured melt temperature exceeds 230°C, screw speed should be reduced or the screw configuration changed. Additive packages containing phenolic antioxidants may be consumed faster under such thermal stress; residual protection cannot be assumed without oxidative induction time testing.
Surface melt fracture can appear as a regular sharkskin pattern on the film surface when the die shear stress exceeds the critical stress of the resin. For butene LLDPE, the onset of sharkskin depends on die gap, die land length, and melt temperature; it is not solely determined by melt index. Converters reduce melt fracture by increasing die gap, raising melt temperature in the die, or adding 5–15 wt% LDPE. Die-lip build-up occurs when oxidized material accumulates at the die exit; the condition is managed by periodic purge with LDPE or a commercial purging compound and by avoiding excessive melt temperature above 230°C. The grade may exhibit higher die-lip build-up than metallocene grades because of a broader molecular weight distribution and lot-dependent extractables, but this behavior varies with antioxidant package and storage age.
In three-layer coextrusion with polyamide or EVOH, 7042 is used as a sealant or outer skin. Interlayer adhesion between nonpolar 7042 and polar barrier resins requires a maleic anhydride-grafted tie resin. The tie layer thickness is usually 10–15% of total film thickness, but the exact thickness is set by adhesion testing under ASTM F904. Seal initiation temperature of formulated film should be determined by ASTM F2029 rather than predicted from base density. Typical seal initiation for butene LLDPE of this class is often observed in the range of 100–110°C; lot-specific distribution of comonomer can shift this range by several degrees.
At equivalent density and melt index, octene-based LLDPE produces higher dart impact resistance and Elmendorf tear than butene-based 7042. The explanation lies in tie-molecule concentration: octene branches are more effective than butene branches at creating load-bearing tie chains between lamellae. In comparative film studies using 25 µm blown film, octene grades may exhibit dart impact values 1.3–2.0 times higher than butene grades when tested under ASTM D1709 Method A; exact differences depend on molecular weight, processing orientation, and film additives. Metallocene LLDPE has a narrower molecular weight distribution and lower seal initiation temperature, but it is more sensitive to melt fracture and die-lip build-up. 7042 has a broader processing window and lower melt-pressure sensitivity than many metallocene grades, at the cost of higher haze and lower impact.
This trade-off is relevant when converting machines lack high-speed air rings or internal bubble cooling. In such equipment, 7042 may provide acceptable film gauge control where a fast-crystallizing metallocene grade would produce melt-fracture defects or unstable frost-line movement. Conversely, in premium stretch-film lines where clarity and impact are dominant, 7042 is used as a blend partner rather than the sole resin. Typical blend ratios with metallocene LLDPE range from 30:70 to 70:30 by weight, but the ratio must be adjusted because film-line orientation at blow-up ratios above 2.5:1 can reduce machine-direction tear in butene-rich blends.
Because producer datasheets for this specific grade often omit tensile and dart impact values, converters should generate baseline film data at a fixed set of conditions. A laboratory blown-film line with 25 mm die diameter, 1.8 mm die gap, 2.5:1 blow-up ratio, and 200°C melt temperature is commonly used. Film specimens are conditioned at 23°C and 50% RH for 40 h before testing. Tensile properties are measured under ISO 527-3 at 500 mm/min; dart impact under ASTM D1709 Method A; and Elmendorf tear under ASTM D1922. The resulting data are specific to the film-making conditions and should only be compared against other resins produced on the same line.
The base resin should not be assumed to contain slip, antiblock, or processing stabilizers beyond those needed for pellet handling. High-speed packaging operations commonly add silica antiblock to achieve coefficient of friction below 0.30 under ISO 8295. Slip addition requires care because erucamide migration can occur over hours to days after extrusion; film tested immediately after winding may show higher coefficient of friction than film tested after 24 h. Print adhesion and heat-seal strength should be re-qualified after slip masterbatch addition because surface bloom can reduce seal strength under ASTM F88. Agricultural film exposed to more than 100 kLy per year requires compounded HALS and UV absorber packages because the base grade is not UV-stabilized.
Food-contact status must be confirmed against the specific lot. Relevant standards include GB 4806.6-2016, GB 9685-2016, EU 10/2011, and FDA 21 CFR 177.1520. A converter seeking food-contact approval should obtain migration test reports from the producer or an independent laboratory for the finished film structure, because the presence of tie resins, masterbatches, and regrind changes the compliance assessment. The resin should be stored at 20–30°C and protected from direct sunlight. Cold pellets stored below dew point can carry surface moisture into the feed throat; while 7042 does not usually require drying, surface condensation at high humidity above 60% RH should be avoided to prevent feed-zone slip and minor melt-pressure fluctuation.
Hexane extractables and low-molecular-weight oligomers are relevant for food-contact and pharmaceutical packaging. The base resin may have a specified hexane extractable limit under FDA 21 CFR 177.1520, but the limit should be confirmed from the certificate of analysis or migration report. For nonfood industrial liners, extractables are less critical, but they can affect print adhesion and seal strength. Converters using regrind should limit addition to 10–20 wt% of the layer unless the finished film is validated for higher recycled content, because each heat cycle reduces the antioxidant package and increases gel formation.
In cast-film conversion, the melt curtain is unsupported between the flat die and the chill roll. The molecular structure of 7042, with limited long-chain branching, can exhibit draw resonance at high line speeds when the melt curtain is drawn too aggressively. Cast-film converters generally operate with a die gap between 0.3 mm and 0.8 mm, melt temperature near 220–250°C, and an air gap of 10–20 cm. When draw resonance appears, the corrective sequence is to reduce line speed, raise melt temperature within the permitted envelope, or lower the draw ratio. If these changes do not stabilize the web, blending with a low-MFI LDPE or a long-chain-branched LLDPE increases extensional strain hardening. Published data for neat 7042 in high-speed cast film is limited; therefore, the maximum line speed must be established by trial with chill-roll temperature profiling and thickness mapping.
In coextruded structures, changes of more than 10% in the 7042 layer ratio should trigger re-qualification of heat-seal strength and interlayer adhesion because adjacent layers change the thermal history of the sealant skin. The product is therefore qualified against a specific film structure and set of conversion parameters, not as a standalone replacement for LDPE, C8 LLDPE, or metallocene LLDPE without line-specific verification.