Pttgc Hdpe Innoplus Hd2308j

PTTGC HDPE INNOPLUS HD2308J

    • Product Name: PTTGC HDPE INNOPLUS HD2308J
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 603325
    Density 0.953 g/cm³
    Melt Mass Flow Rate 190c 2 16kg 0.80 g/10 min
    Tensile Strength At Yield 26 MPa
    Tensile Elongation At Break 800%
    Flexural Modulus 1100 MPa
    Notched Izod Impact Strength 23c 15 kJ/m²
    Vicat Softening Temperature 125 °C
    Melting Temperature 133 °C
    Hardness Shore D 65
    Environmental Stress Crack Resistance >1000 h

    As an accredited PTTGC HDPE INNOPLUS HD2308J factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing PTTGC HDPE INNOPLUS HD2308J is supplied in 25 kg polyethylene bags or 1,000 kg jumbo bags, 40 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with PTTGC HDPE INNOPLUS HD2308J resin in 25 kg bags, palletized, shrink-wrapped, and secured for ocean transport.
    Shipping PTTGC HDPE INNOPLUS HD2308J is shipped as non-hazardous high-density polyethylene resin pellets, typically in 25 kg PE bags on pallets, stretch-wrapped. Transport in clean, dry trucks or containers; keep packages sealed and store cool, dry, away from direct sunlight, moisture, heat, and contamination.
    Storage Store PTTGC HDPE INNOPLUS HD2308J in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags/containers sealed, clean, and palletized; prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Observe good housekeeping and safe stacking to prevent bag damage. No special temperature control is required under normal conditions.
    Shelf Life Shelf life is 24 months from manufacture when stored dry, cool, well-ventilated, away from direct sunlight and contaminants.
    Application of PTTGC HDPE INNOPLUS HD2308J
    Extrusion blow moulding of 200 L tight-head L-ring drums from HD2308J uses accumulator-head machines with screw diameter 80–120 mm, grooved feed sections, and barrier profiles at 25–30 L/D. The granulate is dried to 0.01 wt% residual moisture at 80°C for 2–3 h only when storage RH exceeds 60%; otherwise surface moisture on regrind flake is the main volatile source. Melt temperature at the die face is held between 190°C and 210°C, with the accumulator head and die zones no more than 10°C above that window to limit thermal degradation at stagnant boundary layers. Parison programming across 50–150 points controls wall thickness after swell to 2.0–3.5 mm, with the top chime and L-ring zones receiving 15–20% additional material because these sections carry stacking loads under 49 CFR 178.606. Blow air enters at 0.6–1.0 MPa; mould coolant is run at 10–25°C; a 200 L drum cycles in 120–160 s depending on accumulator shot size and cooling water temperature.The pinch-off weld at the top and bottom is the primary qualification boundary. In-production burst testing of welded chime areas under 49 CFR 178.605 hydrostatic pressure reveals that insufficient melt temperature at the pinch-off produces a brittle interface with low transverse elongation measured by notched tensile testing under ASTM D638-14. Conversely, melt temperatures above 210°C create a visibly darker weld with lower molecular orientation and higher parison sag, causing wall thinning at the lower chime. The practical control point is infrared weld-surface temperature measured immediately after mould opening; stable lines hold 135–155°C at the pinch-off before the part is ejected. When the grade carries 20–35% post-industrial regrind from rejected drums, the melt-flow drift under ISO 1133-1:2022 should not exceed ±10% of the virgin value or the accumulator shot weight control loses repeatability. For hydrocarbon-containing liquids the relevant stress crack requirement is ASTM D1693-15 Condition B in 10% Igepal CO-630 at 50°C; blow-moulded HDPE drums in this class are typically specified with an F50 greater than 600 h, but final UN qualification must be run on the finished closure assembly because cap torque and gasket compression alter hoop stress at the neck.
    Process variableLower windowUpper windowFailure mode outside range
    Melt temperature at die190°C210°CLow: cold welds and die-lip freeze. High: parison drawdown and centreline thinning.
    Die gap1.8 mm3.0 mmLow: excessive shear and melt fracture. High: uncontrolled swell and post-mould warpage.
    Blow pressure0.6 MPa1.0 MPaLow: poor engraving transfer and under-fill at pinch-off. High: flash splitting and localised stress concentration.
    Mould temperature10°C25°CLow: high residual stress and ESCR loss. High: extended cycle and dimensional instability.
    The ranges in the table are not intrinsic material limits; they reflect the intersection of tooling geometry, accumulator-head temperature gradients, and blown-part cosmetics on production-scale drum lines.

    Does Automotive Fuel Tank Production Permit Wall-Thickness Reduction Without Sulfonation?

    In monolayer automotive fuel tank tooling, parison sag between die face and mould cavity is controlled less by barrel setpoint than by die-head flow distribution and the high-load melt strength characteristic of low-sag HDPE grades. HD2308J is processed on 3D blow-moulding stations with six or more extruder positions when a barrier layer is required; in monolayer fuel tanks the accumulator shot size is typically 15–40 kg, depending on tank capacity from 40 L to 80 L. Wall thickness is profiled in 8–15 mm increments by parison programming, with nominal wall after swell between 2.5 mm and 5.0 mm. Blow-moulding is performed at 0.8–1.2 MPa blow pressure and mould temperatures of 15–30°C. Under service conditions the tank must pass ECE R34.01 fire resistance, slosh and low-temperature impact testing, but the limiting chemical property is hydrocarbon permeation.A monolayer HDPE tank wall has gasoline permeation several orders of magnitude above the evaporative emission limits in US EPA 40 CFR Part 1060 and CARB LEV III. Two plant-level routes are therefore used: in-mould surface sulfonation or post-mould fluorination. Sulfonation with SO₃ gas at 40–60°C for 3–8 s produces a cross-linked surface layer typically 10–30 μm deep, reducing fuel permeation by 90–99% compared with untreated HDPE. Process incompatibilities include silicone-based mould release, which masks sulfonation locally and causes high permeation bands around the parting line; barium-based heat stabilisers migrating to the surface also interfere with sulfonation uniformity. In six-layer coextrusion, the structure is typically HDPE skin/regrind/adhesive/EVOH/adhesive/regrind/HDPE skin, with EVOH occupying 2.5–3.5% of total wall thickness. The HDPE layers carry the mechanical load and process stability; the EVOH layer provides permeation resistance only if the adhesive layer remains continuous and the tank is not crushed through pinch-off zones.Published data for HD2308J in a six-layer fuel tank without post-treatment is limited; the grade supports the skin and regrind layers rather than the barrier function. Fuel tank validation therefore requires full assembly-level permeation testing under the applicable legislative test procedure, not a material data sheet comparison. The filler neck weld and moulded-in insert bosses are crack initiation sites; ESCR measured under ASTM D1693-15 Condition B is used as a screening parameter, with an F50 value above 600 h considered necessary but not sufficient for tank certification.When the packaging is exposed to ester-based crop protection formulations, environmental stress cracking resistance becomes the controlling property because the bottle wall is simultaneously under hoop stress from internal hydraulic head and partially swollen by the solvent system. Blow-moulded 1 L to 25 L F-style jugs in HD2308J are produced on shuttle machines with single or dual parison heads. For this package class, average wall thickness is 0.8–1.8 mm, which gives a high surface-area-to-volume ratio and makes any wall-thickness variation in the label panel immediately visible as panel deformation after contact with esters or ketones. The material is not selected for solvent resistance in the chemical compatibility sense; it is selected because the high molecular weight and low-sag characteristics permit blow moulders to maintain uniform wall distribution and avoid thin spots that would otherwise fail under drop testing at 1.2 m per 49 CFR 178.603. Bottle qualification for agricultural formulations includes ASTM D1693-15 Condition B exposure to a 10% Igepal solution and compatibility immersion under ASTM D543-14. A practical batch-release test is closure torque retention after 14 days at 40°C; torque loss greater than 25% indicates neck swelling or stress relaxation. The most common plant-floor defect is neck-area stress cracking caused by insufficient cooling of the threaded finish; the corrective action is to increase blow-air duration and reduce demould temperature to below 70°C.

    IBC Inner Bottle Fabrication and Layer Homogeneity at Reduced Wall Thickness

    The 1,000 L–1,250 L intermediate bulk container inner bottle converts from extrusion blow moulding on long-stroke accumulator machines with 400–600 mm head tooling. Using HD2308J, shot sizes range from 20 kg to 35 kg, and the parison wall is programmed to achieve 3.0–6.0 mm after swell, with the bottom chime and top fill opening receiving the heaviest sections. A single-wall bottle is used for water-based products and dilute acids; for oxygen-sensitive or low-viscosity flammable liquids, a fluorinated or coextruded structure is used, with the HDPE layer still forming the load-bearing wall. On production lines running 20–35% clean in-house regrind, the melt-flow variation under ISO 1133-1:2022 should be held to ±10% to avoid oscillation in the parison programmer. The main process failure is internal pinhole formation at the top ring where the parison weld line is compressed during mould closing; this defect is not visible to inline vision systems and causes UN 31A/Y leakproofness failures when the bottle is filled to 98% capacity. For chemical resistance screening, the finished inner bottle is subjected to ASTM D1693-15 Condition B and ASTM D543-14 immersion using the intended product concentrate; any change in ESCR F50 greater than 20% after immersion indicates that the formulation is attacking the polymer morphology rather than merely wetting the surface.In off-highway hydraulic oil reservoirs, blow-moulded from HD2308J on shuttle machines with clamp force from 500 kN to 2,000 kN, the primary process challenge is maintaining boss flatness for pump suction and return fittings. These reservoirs operate at 60–80°C in service and are subjected to cyclic internal pressure below 0.2 MPa. Because the tank wall also acts as a noise radiator, blow moulders adjust wall thickness to 4.0–7.0 mm to shift panel resonance away from hydraulic pump pulsation frequencies. Moulded-in threaded inserts must be supported by raised bosses with 2.0–3.0 mm additional local wall thickness; otherwise insert torque-out values fall below the machine builder's requirement. The grade's high-melt-strength behaviour allows a 50–100 mm diameter parison to be run without excessive sag, but barrel temperature should not exceed 210°C or the material begins to degrade at the stagnant accumulator corners. Completed reservoirs are tested for pinholes with 0.03–0.05 MPa air under water and for oil compatibility by ASTM D543-14 immersion at 70°C for 168 h; mass increase above 1.5% indicates excessive absorption into the hydraulic fluid grade.

    When Chlorinated Solvent Vapour Pressure Exceeds 0.1 MPa at 40°C

    Small 500 mL–5 L HDPE containers for chlorinated solvents require a combination of low-temperature impact resistance, neck finish stability under vapour pressure, and low weight-loss permeation. HD2308J is blow-moulded on multi-cavity shuttle equipment with 2–8 parisons, at wall thicknesses of 0.6–1.2 mm and cycle times of 15–30 s. Packaged methylene chloride or perchloroethylene produces internal pressure that can exceed 0.1 MPa at 40°C; the neck finish must therefore be designed with a buttress thread or tamper-evident overcap that resists back-off. Permeation weight loss is measured gravimetrically after 28 days at 40°C under the closure-specific procedure used by the filling line; published data for this specific HD2308J formulation is limited, so each container assembly is qualified individually. Fluorination is frequently applied to the outer surface to reduce solvent permeation, but the treatment must be completed before fitting labels or overcap liners because surface-active processing aids can migrate from the label adhesive and interfere with fluorination uniformity. Organoleptic masking agents should be avoided if the container is later fluorinated or sulfonated; such additives tend to bloom to the surface and create localised high-permeation zones. Containers for oxidising solvents are tested for stress cracking under ASTM D1693-15 Condition B, while chemical compatibility is evaluated by ASTM D543-14 immersion at 40°C for 14 days; any loss of tensile elongation measured under ASTM D638-14 greater than 25% after exposure is grounds for rejection of the container design.
    Free Quote

    Competitive PTTGC HDPE INNOPLUS HD2308J prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    PTTGC HDPE INNOPLUS HD2308J is a high-density polyethylene extrusion blow molding resin supplied by PTT Global Chemical Public Company Limited. The grade is intended for rigid containers in the approximate capacity range of 0.5 L to 5.0 L, particularly household chemical, agrochemical, and personal care packaging requiring resistance to stress-cracking agents and stable parison formation. Typical datasheet release values associated with the material include a density of 0.953 g/cm³ when tested under ASTM D1505, a melt flow rate of 0.30 g/10 min at 190 °C with a 2.16 kg load per ASTM D1238, a tensile yield strength of 27 MPa per ASTM D638 at 50 mm/min, a flexural modulus of 1,150 MPa per ASTM D790, a Vicat softening temperature of 126 °C per ASTM D1525 under 10 N, and an environmental stress-cracking resistance F50 time greater than 600 h in 100% Igepal CO-630 per ASTM D1693A. These values are typical release data rather than specification limits, and finished-article performance must be confirmed on production tooling because cooling rate, screw work history, and wall-thickness distribution influence final crystallinity and stress-crack response.

    Property Test Standard Typical Datasheet Value
    Melt flow rate (190 °C, 2.16 kg) ASTM D1238 / ISO 1133-1:2022 0.30 g/10 min
    Density ASTM D1505 / ISO 1183-1:2019 0.953 g/cm³
    Tensile yield strength ASTM D638-14, 50 mm/min 27 MPa
    Flexural modulus ASTM D790-17 1,150 MPa
    Environmental stress-crack resistance F50 ASTM D1693-15b, condition A, 100% Igepal CO-630 >600 h
    Vicat softening temperature ASTM D1525-17e1, 10 N 126 °C

    Why Is Environmental Stress-Cracking Resistance the Primary Selection Criterion?

    The dominant long-term failure mode in rigid polyethylene containers for surfactant-based formulations is not tensile yield but slow crack propagation at stress concentrators, especially the pinch-off tail, handle flash edges, and base corners. Under ASTM D1693A conditions, a notched bent specimen is held in a constant-strain jig at 50 °C in 100% Igepal CO-630 to accelerate this mechanism. General-purpose unimodal high-density blow molding grades in the same melt flow class frequently show F50 values below 200 h, whereas published release data for HD2308J exceed 600 h. The distinction is significant when containers are filled with formulations containing 10%–30% nonionic surfactant, hypochlorite-based bleach, or alcohol-containing personal care liquids. In such systems, crack initiation in low-tie-chain regions can occur within weeks if the resin lacks adequate stress-crack resistance.

    Resistance to slow crack growth is not controlled solely by density. At 0.953 g/cm³, the grade retains sufficient crystalline stiffness for top-load performance while avoiding the known stress-crack collapse that often appears in high-density polyethylene above approximately 0.958 g/cm³. The measured flexural modulus of 1,150 MPa indicates that the material maintains bottle wall rigidity without shifting density into the regime where tie-chain concentration is compromised. For this reason, the grade is differentiated from higher-density HDPE blow molding resins that provide slightly greater stiffness but markedly lower ESCR.

    The melt flow rate of 0.30 g/10 min further indicates a high average molecular weight relative to commodity blow molding grades with values of 0.45–0.60 g/10 min. This contributes to parison melt strength and slow crack resistance. However, it also raises melt pressure and reduces shear flow length. Process selection therefore requires an extruder with sufficient torque margin and a die head rated for the resulting pressure under continuous operation.

    In extrusion blow molding, HD2308J is typically processed on single-station or shuttle machines using a grooved-feed extruder with an L/D ratio of 24:1 to 30:1 and a barrier screw having a compression ratio of 2.5:1 to 3.0:1. Barrel temperature setpoints are commonly established from 175 °C at the feed zone to 210 °C in the metering section, with the die head maintained between 205 °C and 215 °C. Melt temperature at the die entry should remain below 215 °C for extended runs. Sustained operation above 225 °C accelerates oxidative chain scission, reduces ESCR, and destabilizes parison length. On shuttle machines with 60 mm screw diameters and output rates near 25 kg/h, stable parison formation is observed when the temperature difference across the head is less than 5 °C. Larger gradients can produce nonuniform die swell and localized wall-thickness variation.

    Mold temperatures are typically controlled between 10 °C and 25 °C with turbulent-flow cooling channels. Lower mold temperatures shorten cycle time but increase frozen-in stress at the pinch-off and may reduce ESCR in the final article. Blow-air pressure in 1 L tooling is generally set between 0.6 MPa and 0.8 MPa. Pre-blow delay is adjusted to prevent parison sag while allowing sufficient melt distribution in the pinch-off zone. Pre-blow delays above 1.5 s can produce wall thinning in the upper load-bearing sections of handleware containers.

    When Substitution into Existing High-Density Blow Molding Tooling Requires Adjustments

    A mold originally optimized for a high-density polyethylene with melt flow rate near 0.45 g/10 min and density 0.955 g/cm³ may require revised parison programming when converted to HD2308J. The grade exhibits higher melt strength and longer parison hang time, which supports larger part weights but also increases die swell relative to a conventional chromium-catalyzed blow molding resin. In practice, maintaining the same target part weight on existing tooling may require a die bushing diameter reduction of 2%–4% or an adjustment of the parison programmer offset by 5%–10%. Failure to compensate can generate excess top flash, uneven sidewall thickness, and inadequate pinch-off compression.

    Mold close speed should also be evaluated. Because the grade retains higher melt viscosity at blow molding temperatures, a slower clamp closing speed may be required to allow uniform flash compression at the parting line. Pinch-off flash above 0.3 mm thickness has been associated with delamination in the parting-line region after drop impact. In container drop tests conducted under ASTM D2463-15, failures are most frequently observed at the bottom pinch-off and handle attachment points when mold close forces are insufficient to produce a sharply defined flash boundary.

    The product is not optimized for injection molding, capillary film extrusion, or rotational molding. Its low melt flow and high shear viscosity at 190 °C result in excessive pressure loss in small injection gates and poor thin-wall mold filling. These limiting characteristics define the operational boundary: the material is suitable for extrusion blow molding of rigid containers, while injection molded closures and films should be produced from grades designed for those processes.

    Mechanical Property Retention After Five Extrusion Passes

    Post-industrial flash and defective containers can be reclaimed and reintroduced into the extruder when the target application permits regrind use. The retention of mechanical properties after repeated extrusion is governed by stabilizer consumption and thermo-oxidative chain scission. In general high-density polyethylene regrind evaluations, five passes on a 45 mm extruder at melt temperatures between 190 °C and 210 °C may reduce environmental stress-crack resistance by 15%–25% relative to virgin material. The magnitude depends on screw speed, temperature overshoot, and residence-time distribution. Because HD2308J contains an antioxidant stabilization package intended for multiple extrusion cycles, occasional regrind use is not excluded, but extended five-pass recycling should be validated for stress-crack-sensitive end uses.

    Clean in-house regrind can be blended at levels up to 20 wt% without automatically invalidating food-contact status when the virgin resin complies with 21 CFR 177.1520 and the regrind is derived solely from food-contact articles produced in a controlled closed-loop process. Above 20 wt%, melt flow rate drift and ESCR loss become more pronounced, and the resulting containers should be requalified under the relevant test standards. If stored bags or regrind exceed 0.08 wt% moisture, pre-drying at 80 °C for 2 h is recommended. At higher humidity, surface moisture can generate pinholes and internal bubbles in pinch-off zones during the blow cycle.

    Compliance Status for Food, Pharmaceutical, and Industrial Packaging

    Regulatory or Test Domain Standard or Jurisdiction Typical Documentation Status
    Olefin polymers for food contact FDA 21 CFR 177.1520 Compliance statement available from the resin supplier; finished article testing remains the responsibility of the converter.
    European food contact plastics EU Regulation (EU) No 10/2011 Overall migration and specific migration require validation on the final molded article; resin documentation alone is not sufficient.
    REACH substances of very high concern REACH Regulation (EC) No 1907/2006 Supplier documentation indicates no SVHC above 0.1 wt% in the supplied substance.
    RoHS restricted substances Directive 2011/65/EU Lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE are documented below maximum concentration values.

    Chemical compatibility with aggressive hydrocarbons, ketones, and solvent-based formulations must be confirmed by immersion testing under ASTM D543 or an equivalent test protocol. Published long-term storage data for HD2308J in full commercial containers are limited for polar solvent systems; accelerated testing on production bottles is required before commercialization. The grade is not intended for direct contact with strongly oxidizing liquids above ambient temperature unless the finished article has been specifically validated under the intended use conditions.

    Top