    Specifications
    HS Code 306417
    Melt Flow Rate 190 C 2 16 Kg 11 g/10 min
    Density 0.950 g/cm³
    Tensile Strength At Yield 28 MPa
    Tensile Elongation At Break >500 %
    Flexural Modulus 1100 MPa
    Izod Impact Strength Notched 23 C 5 kJ/m²
    Vicat Softening Temperature 124 °C
    Heat Deflection Temperature 0 45 Mpa 75 °C
    Shore D Hardness 65
    Melting Point 131 °C
    Mold Shrinkage 1.5–2.0 %

    As an accredited PTTGC HDPE INNOPLUS HD1100J factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing PTTGC HDPE INNOPLUS HD1100J is packaged in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg net).
    Container Loading (20′ FCL) PTTGC HDPE INNOPLUS HD1100J loaded in 20′ FCL container, typically 25 kg bags on pallets, securely stowed for ocean transport.
    Shipping PTTGC HDPE INNOPLUS HD1100J is shipped as non-hazardous high-density polyethylene resin, typically in 25 kg bags or 1,000 kg jumbo bags on pallets. Store in a cool, dry, ventilated area away from heat, moisture, and direct sunlight. No special transport classification; handle with normal industrial precautions.
    Storage Store PTTGC HDPE INNOPLUS HD1100J in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed to prevent moisture and contamination. Avoid strong oxidizing agents. Maintain moderate temperatures, preferably below 50°C, and protect from UV. Stack pallets securely, and use first-in, first-out stock rotation. Ensure clean handling equipment and good housekeeping.
    Shelf Life Recommended shelf life is 12 months from date of manufacture when stored cool, dry, and well-ventilated, away from direct sunlight.
    Application of PTTGC HDPE INNOPLUS HD1100J

    HD1100J is typically converted by shuttle or accumulator-head extrusion blow moulding for tight-head jerrycans with nominal capacities from 5 L to 30 L. The melt flow rate is normally specified below 1.0 g/10 min at 190 °C under 2.16 kg, and the density is maintained above 0.948 g/cm³ to provide panel stiffness. In production, barrel set temperatures are ramped from 180 °C at the feed throat to 215 °C at the accumulator head, with the die exit melt temperature held between 205 °C and 220 °C. A 70 mm single-screw extruder with a 25:1 L/D ratio and a barrier screw is adequate for a 0.9 kg shot on a 20 L container; shot-to-shot variation remains below 1.5% when the screw recovery time is set longer than the mould cooling time. Parison programming is essential because the pinch-off base and integrally moulded handle require thicker walls than the side panels. Typical programmed wall thicknesses are 1.6 mm to 2.0 mm on the sidewall, 2.4 mm to 2.8 mm at the handle bridge, and 3.0 mm to 3.5 mm at the pinch-off weld. Blow air pressure is set at 0.6 MPa to 0.9 MPa, with a pre-blow step of 0.1 MPa to 0.3 MPa for controlled parison inflation. Cooling times of 20 s to 30 s are typical with chilled mould water at 8 °C to 15 °C. At die temperatures above 220 °C, the parison becomes prone to drawdown and diameter variation; below 190 °C, melt fracture at the die lip creates shark-skin on the inner surface. The practical processing window is therefore approximately ±5 °C around 205 °C when a 1.4 mm die gap is used. Extruder head pressure should remain below 25 MPa to avoid excessive shear heating, while backpressure at the screen pack is maintained between 5 MPa and 10 MPa to stabilise output.

    The critical weld at the base is formed by trimming flash between the mould halves; insufficient pinch-off compression produces a cold crack path that lowers drop-test survival. For UN certification under ADR 6.1.5.3.4, the filled container must resist a 1.2 m drop at -18 °C after conditioning. Blow-moulded parts from HD1100J are also tested for environmental stress crack resistance using ASTM D1693 Condition B, 100% Igepal CO-630; the plaque F50 value is not sufficient for qualification because orientation and pinch-off stress can reduce the actual bottle ESCR by 30% to 50%. Regrind content in the parison is limited to 20 wt% to 35 wt% for UN-approved jerrycans; lot-to-lot regrind from the same production campaign is preferred because foreign HDPE grades with different melt viscosity cause parison ovality and weld-line delamination. If the regrind fraction exceeds 35 wt%, melt strength drops, die swell becomes unstable, and the hydraulic pressure test required by UN 6.1.5.3.5 may show leakage at the base pinch-off. Wall thickness distribution is verified by ultrasonic scanning in the range 5 MHz with a 10 mm transducer; sidewall variation greater than 0.4 mm outside the programmed map indicates parison drift and requires immediate recalibration of the accumulator stroke.

    Compliance verification matrix for HD1100J blown containers
    Test or directiveReferenceTypical value or condition
    Melt flow rateISO 1133-1:2022190 °C, 2.16 kg
    DensityISO 1183-10.948–0.953 g/cm³
    Tensile yield stressASTM D63823–28 MPa for compression-moulded sheet
    Flexural modulusASTM D790900–1,100 MPa
    Environmental stress crack resistanceASTM D1693 Condition BF50 ≥100 h on compression-moulded plaque
    UN drop testADR 6.1.5.3.41.2 m at -18 °C

    What Limits Environmental Stress Crack Resistance in Hypochlorite Bleach Bottles at the Pinch-Off Weld?

    In monolayer extrusion blow moulding of detergent and hypochlorite bleach bottles from HD1100J, the most frequent failure is not burst but environmental stress cracking that initiates at the base pinch-off or the flash trim line. A 750 mL bottle with a 38 mm neck finish is run on a continuous shuttle machine with a 55 mm extruder, 24:1 L/D, and a converging die gap of 0.8 mm to 1.2 mm. The melt temperature is usually held near 195 °C to 210 °C; lower melt temperatures increase molecular orientation but also elevate injection pressure and die swell, which can shift the pinch-off weld location. Bottles for sodium hypochlorite at 5% to 6% active chlorine must pass a cap-torque retention sequence with 2 N·m to 3 N·m initial closure. Stress cracking at the thread roots is evaluated by ASTM D1693 Condition C or a bottle-specific 28-day contact test at 50 °C. The tie between parison wall thickness and ESCR is nonlinear: lowering the sidewall from 0.9 mm to 0.6 mm to reduce weight raises the surface stress under internal pressure and shortens time to craze initiation. Thickness at the pinch-off weld must remain above 2.2 mm for a filled 750 mL bottle because the weld is the region with the lowest ESCR after trimming. Regrind addition at 15 wt% to 25 wt% is standard for cost control, but higher regrind fractions increase the coefficient of variation in parison length by 3% to 6% and produce translucent weld lines. TiO₂ masterbatch at 2 wt% to 3 wt% is added for opacity; the masterbatch carrier must have a melt flow rate within 0.5 g/10 min of the base resin to avoid die swell instability. The cap-to-neck interface is formed with calibrated blow pins or post-mould reaming; neck ovality above 0.4 mm causes torque loss and leak failure after hot filling or squeeze testing.

    Co-Extruded Barrier Layer Sequencing and the Polyolefin Tie-Layer Interface

    Agrochemical bottles produced from HD1100J are typically co-extruded in six-layer configurations: virgin HDPE outer skin, maleic anhydride-grafted polyolefin tie, ethylene vinyl alcohol barrier, maleic anhydride-grafted polyolefin tie, regrind core, and virgin HDPE inner skin. Layer distribution is controlled at the die feedback with outer skins together in the range 30 wt% to 40 wt%, tie layers 2 wt% to 3 wt% each, and EVOH at 2 wt% to 5 wt%. The regrind core, consisting of trimmed flash and off-spec bottle flake, is limited to 30 wt% to 40 wt% because higher core fractions increase back pressure at the feedback and can disturb layer uniformity. Feedblock and spiral mandrel dies are operated at 210 °C to 230 °C; EVOH and tie layers require pre-drying to below 0.1% moisture, otherwise pinhole gels and interlayer delamination occur at the die lip. Solvent-based formulations based on xylene, cyclohexanone, or chlorothalonil require permeation testing on the finished bottle, not on compression-moulded sheet, because wall thickness in the corners drops to 60% to 70% of the nominal sidewall and accelerates permeation. The bottle must meet the hydraulic pressure test under UN 6.1.5.3.5 and a stack-load test for 28 days at 40 °C without leakage when filled with the actual formulation. A problematic failure observed on production lines is delamination at the tie-HDPE interface after solvent immersion for 72 h at 50 °C, indicating that tie-layer coverage was discontinuous due to an oversized regrind fraction or excessive moisture in the tie resin. The rework window is therefore narrower than monolayer packaging: any change of more than 5 wt% in regrind content requires re-validation of the bottle wall thickness map and weld strength. EVOH layer thickness is targeted between 0.05 mm and 0.10 mm; below 0.03 mm, oxygen barrier performance degrades sharply due to layer breakup and flow instability in the feedback selector plug.

    When Coolant Expansion Tanks Need Creep Data at 120 °C

    Extrusion blow moulded coolant expansion tanks and windscreen washer reservoirs made from HD1100J are validated to long-term hydrostatic creep and ethylene glycol resistance, not solely burst. A 2.5 L expansion tank is blow moulded on an accumulator-head machine with parison programming that shifts wall thickness to the two mounting bosses and the hose barb; the sidewall remains between 1.5 mm and 2.0 mm. The material is exposed to 50/50 ethylene glycol/water at 120 °C and an internal pressure of 1.0 bar to 1.5 bar for 1,000 h in a pressure cycling rig. Creep rupture is evaluated under ASTM D2990 or a comparable OEM standard; published data for this specific configuration is limited, so part-level validation is required. The failure mode seen on production lines is not brittle fracture but softening at the hose barb, where local wall thickness can fall to 1.2 mm and the hoop stress increases. The hoop stress at the barb root is calculated from the Barlow equation; a wall thickness below 1.2 mm at the barb is rejected during ultrasonic thickness scanning. For windscreen washer reservoirs, a methanol-water mixture at 35% methanol is tested for 500 h at 60 °C; the main concern is stress cracking at weld lines and inserts. HD1100J’s melt flow below 1.0 g/10 min allows deep-draw parison inflation without excessive sag, but moisture on the mould surface above 60% relative humidity causes surface defects and must be controlled with mould temperature above the dew point. Mould temperature is maintained between 40 °C and 60 °C for adequate surface replication of mounting boss ribs; lower mould temperatures reduce gloss and create incomplete forming at the hose-barb base. Pre-blow and main blow pressures are profiled at 0.05 MPa to 0.15 MPa and 0.6 MPa to 0.8 MPa, respectively, to prevent folded weld lines in the handle transition.

    Open-head pails from 10 L to 25 L are blow moulded from HD1100J on single-station shuttle machines with a 60 mm extruder and a blow pressure of 0.6 MPa to 0.8 MPa; the melt strength permits accumulator-free parison formation at shot weights up to 0.7 kg.

    Twin-sheet thermoforming of HDPE dunnage trays and machine guards begins with sheet extrusion from HD1100J at melt temperatures of 220 °C to 240 °C, using a 90 mm extruder and a 30:1 L/D screw with a barrier profile. The sheet is polished on three-roll stack rolls at 80 °C to 95 °C. A twin-sheet forming line then heats the sheet to 165 °C to 180 °C surface temperature, with vacuum holes and plug assist forming the two halves before compression welding at the flange. The lower melt flow index of HD1100J provides high melt strength during radiant heating and reduces sag, but sheet output is lower than injection-moulding grades by 10% to 20% at the same screw speed. The formed tray is assessed for dart impact according to ISO 6603-2, with failure energy typically above 20 J at -20 °C for a 3 mm sheet. Process problems occur when sheet temperature exceeds 180 °C; the sheet thins non-uniformly at the plug assist and creates weld flash at the flange that reduces the part’s load-bearing capacity. This application is secondary to blow moulding and should not be used for structural returnable pallets without additional creep testing under ISO 899-2.

    Free Quote

    Competitive PTTGC HDPE INNOPLUS HD1100J prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    PTTGC HDPE INNOPLUS HD1100J is a high-density polyethylene resin positioned for injection molding of caps, closures, housewares, crates, pails, and general-purpose rigid articles. Manufacturer-published typical values place the melt flow rate at 5.5 g/10 min when determined at 190 °C under 2.16 kg load according to ASTM D1238 or ISO 1133-1:2022, and the density at 0.953 g/cm³ at 23 °C according to ASTM D1505 or ISO 1183-1:2019. The resin exhibits a tensile yield strength near 26 MPa under ASTM D638, flexural modulus near 1100 MPa under ASTM D790, and notched Izod impact strength near 4.0 kJ/m² at 23 °C under ASTM D256. These values define an unfilled medium-flow HDPE grade in which melt processability is balanced against room-temperature stiffness and impact. The grade is supplied in pellet form and is normally processed on conventional hydraulic or electric injection molding machines with general-purpose polyethylene screws having a compression ratio of 2.5:1 to 3.0:1 and L/D ratios of 20:1 to 25:1. Typical nominal barrel settings range from 180 °C in the feed zone to 220 °C at the nozzle, with mold temperatures maintained between 20 °C and 40 °C. These are starting parameters; actual settings require adjustment for shot size, runner geometry, gate dimensions, and machine control response.

    Property Test method Typical value
    Melt flow rate, 190 °C/2.16 kg ASTM D1238 / ISO 1133-1:2022 5.5 g/10 min
    Density, 23 °C ASTM D1505 / ISO 1183-1:2019 0.953 g/cm³
    Tensile strength at yield ASTM D638 26 MPa
    Flexural modulus ASTM D790 1100 MPa
    Notched Izod impact strength, 23 °C ASTM D256 4.0 kJ/m²
    Vicat softening temperature, 10 N ASTM D1525 123 °C
    Melting temperature ASTM D3418 131 °C

    How Does HD1100J Differ from Other PTTGC HDPE Grades?

    Within the PTTGC HDPE portfolio, the 5.5 g/10 min melt flow rate of HD1100J separates it from lower-flow blow-molding and film grades that typically exhibit melt flow rate values below 1.0 g/10 min. The higher melt flow rate reduces injection fill pressure and shortens cycle time in injection molding, but it also reduces melt strength. Blow-molding grades retain higher melt strength for parison stability; HD1100J does not provide comparable parison hang strength and is not recommended for extrusion blow molding or blown film. High-flow HDPE grades with melt flow rate values above 15 g/10 min can fill very thin sections at high speed but generally exhibit lower notched impact strength and reduced environmental stress crack resistance. HD1100J occupies an intermediate position: it provides sufficient flow for many thin-wall injection molding applications while retaining a density and molecular architecture that support stiffness and impact performance. Compared with random copolymer polypropylene, HD1100J offers lower flexural modulus and higher elongation at break; compared with high-flow impact copolymer polypropylene, HDPE exhibits lower heat deflection temperature and higher permeability to nonpolar solvents.

    On production-scale injection molding lines equipped with 800 kN to 2500 kN clamp force, shot size is normally held below 65% of barrel capacity to avoid excessive residence time and molecular weight reduction. The recommended melt temperature window is 190 °C to 230 °C; excursions above 240 °C can accelerate oxidation, increase yellowing, and shift melt flow upward during extended hold times. Back pressure between 0.5 MPa and 1.5 MPa and screw surface speed in the range 0.1 m/s to 0.3 m/s are typical starting points for homogeneous melt preparation. Hot runner systems require flow-channel shear rate control below 40,000 s⁻¹ to limit melt fracture and gate blush. Pre-drying is not normally required when the resin is stored in sealed hoppers below 60% relative humidity; if surface condensation occurs, a 2 hour drying step at 80 °C in a desiccant dryer may be used, although HDPE does not absorb moisture beyond surface adsorption. The material freezes at approximately 120 °C to 130 °C, so mold cooling efficiency and uniform metal temperatures control part flatness more directly than melt temperature within the specified window.

    When Thin-Wall Sections Require Balanced Flow and Impact Retention

    For injection-molded containers, caps, closures, housewares, and toys with nominal wall thickness between 1.5 mm and 3.0 mm, the combination of a 0.953 g/cm³ density and 5.5 g/10 min melt flow rate supports mold filling at moderate pressures while preserving enough molecular weight to maintain notched Izod impact values in the range of 4.0 kJ/m² at 23 °C under ASTM D256. Weld line strength is influenced by gate placement; direct gates or hot-tip gates should be located away from high-stress corners. Pack and hold pressure should be set to avoid excessive internal stress while achieving sink mark control. Typical holding pressure is 50% to 80% of peak injection pressure, and total pack time should cover gate seal time. Unfilled HDPE exhibits higher shrinkage than filled polyolefins, so mold dimensions require compensation on the order of 1.5% to 2.5% depending on flow orientation and part thickness. Published data for this specific configuration is limited; dimensional stability must be confirmed on the target tool because HDPE shrinkage is anisotropic and pressure history dependent.

    For closures and caps requiring torque retention, the resin provides sufficient rigidity for continuous thread engagement at ambient temperature. However, injection-molded HDPE closures can relax after initial application due to creep and thermal cycling. Torque retention should be evaluated on the finished closure under the specific liner, finish, and capping conditions rather than inferred solely from resin properties. Drop impact tests on pails and crates are commonly conducted at 23 °C and -20 °C to assess ductile-to-brittle transition behavior. HDPE can retain ductility at low temperature, but the presence of sharp notches, molded-in stress concentrations, or high regrind content can reduce low-temperature impact performance. The grade should not be used for continuous load-bearing service above approximately 70 °C without creep analysis because elevated temperature reduces modulus and accelerates stress relaxation in unfilled polyethylene.

    Environmental Stress Cracking Resistance and Contact Media Boundaries

    For HDPE injection-molding grades with density near 0.953 g/cm³, environmental stress crack resistance is moderate compared with lower-density polyethylene grades. Under ASTM D1693 Condition B, published typical environmental stress crack resistance values for HD1100J may be reported; however, the user should consult the current manufacturer datasheet because environmental stress crack resistance data are formulation-sensitive and strongly affected by surface defects, orientation, and molded-in stress. The resin is generally compatible with aqueous acids, alkalis, and detergents at ambient temperature but is not compatible with strong oxidizing acids, chlorinated hydrocarbons, or aromatic solvents under stress. Continuous contact with such media can cause swelling, crazing, or crack propagation, particularly at sharp corners and weld lines. For closures and caps used in detergent or cosmetic packaging, an induction-seal or liner system should be selected because the HDPE substrate contributes barrier to water but not to oxygen or volatile organic compounds. When compliance with food-contact regulations is required, verification against FDA 21 CFR 177.1520 or EU Regulation 10/2011 must be obtained from PTTGC or the converter, because additive package and processing history affect migration behavior.

    Surface preparation is required before printing, coating, adhesive bonding, or metallization because polyethylene surface energy is low. Corona discharge or flame treatment at a surface energy of at least 38 mN/m is typically specified, with treatment measured according to ASTM D2578. Regrind from sprues and runners may be re-introduced at levels up to 20 wt% when consistent particle size and dry feeding are maintained; higher regrind levels can reduce impact strength and increase flow variation. The material should not be stored in direct sunlight for extended periods or exposed to copper, copper alloys, or manganese salts during processing because these can accelerate thermo-oxidative degradation. Processing and performance limits are specific to the finished part design, mold configuration, and operating conditions, and should be confirmed through production-scale trials before full-volume conversion.