Polyplastics Duranex Pbt Glass Bead Lw 727bm

Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM

    • Product Name: Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 514517
    Density 1.50 g/cm3
    Water Absorption 0.07 %
    Tensile Strength 55 MPa
    Elongation At Break 2.5 %
    Flexural Modulus 4500 MPa
    Flexural Strength 100 MPa
    Charpy Notched Impact Strength 3 kJ/m2
    Rockwell Hardness M85
    Deflection Temperature At 1 82 Mpa 90 °C
    Melting Point 224 °C
    Mold Shrinkage Md 0.8 %
    Mold Shrinkage Td 1.0 %
    Coefficient Of Linear Thermal Expansion 7e-5 /°C
    Volume Resistivity 1e16 ohm·cm
    Dielectric Constant 3.5
    Flammability HB

    As an accredited Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM is supplied in sealed 25 kg moisture-barrier bags, with 40 bags per pallet.
    Container Loading (20′ FCL) Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM loaded in a 20-foot FCL container, palletized, securely strapped, dry conditions, standard industrial packaging.
    Shipping Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM is shipped as non-hazardous PBT resin pellets in sealed moisture-barrier bags or 25 kg sacks, palletized and secured. Keep dry, cool, and protected from contamination. No UN hazard class; transport according to the SDS and local regulations.
    Storage Store DURANEX® PBT+Glass-Bead-LW 727BM in a cool, dry, well-ventilated area in original sealed packaging. Protect from direct sunlight, heat, moisture, dust, and contamination. Keep away from ignition sources and incompatible chemicals. Use first-in, first-out stock rotation. Avoid prolonged humid exposure; dry as recommended before processing. Follow the manufacturer’s SDS and keep containers clearly labeled.
    Shelf Life Shelf life is typically 12 months in unopened original packaging, stored dry below 30°C away from moisture and direct sunlight.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction
    Polyplastics DURANEX® PBT+Glass-Bead-LW 727BM is a glass-bead-reinforced polybutylene terephthalate compound formulated for injection-molded parts in which post-mold flatness, dimensional repeatability, and reduced shrinkage anisotropy are the primary acceptance criteria. The low-warpage additive system differentiates this grade from standard unfilled PBT and from short-glass-fiber-reinforced DURANEX products. The glass bead phase creates a quasi-isotropic filler architecture rather than the oriented high-aspect-ratio reinforcement produced by fiber-filled melts during cavity filling. Typical specification values for this grade are reported under ISO 1183 for density, ISO 527-1/-2 for tensile strength and elongation, ISO 178 for flexural modulus, ISO 179/1eA for Charpy notched impact, ISO 75-1/-2 for heat deflection temperature, ISO 294-4 for mold shrinkage, IEC 60112 for comparative tracking index, and UL 94 for flammability. Because pigment package, regrind ratio, and cavity pressure influence crystallinity and final dimensions, the current manufacturer’s datasheet should be used for release testing rather than generic PBT reference data. The filled system is positioned between unfilled PBT and short-glass-fiber PBT in mechanical performance. Glass-bead mass fractions for low-warpage PBT compounds of this type are commonly in the 15–30 wt% range; within that window, tensile strength and flexural modulus rise with filler loading while melt viscosity increases and impact resistance declines. The grade is therefore specified where dimensional control under thermal cycling matters more than maximum load-bearing stiffness.

    How Does Glass-Bead Reinforcement Alter Shrinkage Anisotropy in DURANEX 727BM?

    The critical processing distinction of 727BM is the reduction in direction-dependent mold shrinkage, rather than the absolute magnitude of shrinkage. In short-glass-fiber PBT, fiber orientation follows the melt-front velocity profile and cavity shear. Shrinkage in the flow direction is usually lower than shrinkage perpendicular to flow, producing internal stress and warpage in thin-wall housings. Glass beads are spherical and do not orient strongly under shear. As a result, specimens molded under ISO 294-4 show flow-direction and transverse-direction shrinkage values that are much closer than those of glass-fiber-reinforced grades of similar density. In production qualification this behavior is evaluated by molding a 60 mm × 60 mm plaque and calculating shrinkage anisotropy as the absolute difference between flow and transverse values. Because PBT crystallizes rapidly, final part dimensions are controlled by hold pressure, gate seal, and mold temperature more than by filler geometry alone. The glass-bead phase reduces orientation stress and minimizes distortion, but it does not compensate for insufficient packing. Short-shot pressure studies and gate-seal verification should be performed on the production tool, especially for parts with wall thickness below 1.0 mm, where flow-length-to-thickness ratios above 100:1 limit hold-pressure transmission from the cavity gate to the last fill point. Rheological behavior also differs from fiber-reinforced PBT. Spherical glass beads produce less interparticle entanglement than glass fiber, so melt viscosity increases less sharply with filler content. Under ISO 1133-1 at 250 °C and 5 kg, glass-bead-reinforced PBT melts typically show higher melt volume-flow rates than short-glass-fiber PBT at equivalent filler mass fraction. However, narrow gates below 0.6 mm may exhibit surface defects if bead size approaches gate dimension; gate sizing trials are recommended when switching from a fiber-filled grade to this low-warpage compound. Post-mold dimensional stability is also influenced by moisture absorption and thermal relaxation. Glass-bead PBT parts are conditioned at 23 °C and 50 % RH per ISO 291 before coordinate measuring machine audit. Published data for this specific configuration is limited; multi-cavity validation under production conditions remains necessary because cavity-to-cavity fill imbalance can generate more warpage than filler anisotropy alone. Field failures observed on production lines include gate halo, splay from inadequate drying, and warp reversal after hot storage or secondary painting. Gate halo typically indicates excessive barrel temperature or shear heating; corrective action is to lower the barrel profile by 5–8 °C and verify dryer dew point before adjusting injection speed. Warp reversal after painting is often a stress-relaxation response to solvent exposure or oven conditions, and it is addressed by checking mold-temperature uniformity and hold-pressure decay rather than by increasing filler content.

    Pre-Drying and Barrel Residence Constraints in DURANEX 727BM Molding

    Drying. PBT hydrolyzes at melt-processing temperatures when residual moisture is present, reducing molecular weight and producing surface splay, embrittlement, and lower Charpy impact. The material is predried in a desiccant dryer with a dew point below −30 °C. At 120 °C, sealed bags opened within one shift require 4–6 h to reach a moisture content below 0.02 % by Karl Fischer titration; bulk containers, regrind, or material exposed to ambient air above 60 % RH for more than 30 min may require 6–8 h. The drying hopper should be sized for actual hourly shot-weight consumption. An oversized hopper extends residence time and can cause thermal-oxidative yellowing even when the dew point is correct. Melt temperature profile. A conventional three-zone screw with a positive non-return valve is suitable. Rear-zone, center-zone, front-zone, and nozzle temperatures are typically set from 240 °C to 260 °C, with the nozzle held below 260 °C. Melt temperature should not exceed 270 °C. Above this boundary, hydrolysis and thermal degradation products generate acetaldehyde and reduce molecular weight. Total residence time at melt temperature is controlled below 8–10 min. In hot-runner systems, manifold and drop temperatures are set in the same range, and stagnation points are reviewed because glass-bead-filled melts can form dead spots in sharp corners. Back pressure and injection speed. A hydraulic back pressure of 2–5 bar is applied to maintain a stable melt cushion and adequate homogenization without excessive shear heating. Injection velocity is set at the mid-to-high range for thin-wall housings. Excessive shear can raise melt temperature locally and degrade the matrix. Holding pressure is determined by pressure-drop studies and gate-seal time. Typical cushion settings are 3–5 mm, and screw decompression below 3 mm avoids air entrapment, burn marks, and inconsistent shot weight. Mold temperature. The mold surface is maintained at 60–90 °C. Lower mold temperatures increase cooling rate, reduce crystallinity, and raise post-mold shrinkage. Higher mold temperatures improve crystallization and dimensional stability but increase cycle time. For parts with tight tolerances, mold-temperature variation across cavities should be controlled within ±5 °C. Uneven mold cooling can dominate warpage far more than the glass-bead anisotropy benefit itself. Production-scale equipment boundary. On injection molding machines with clamp force below 80 tonnes, thin-wall parts may require higher packing pressure to compensate for rapid gate freeze. On machines above 300 tonnes, melt residence time increases if shot weight is small relative to barrel capacity. The material is therefore best processed on a barrel sized so that shot weight is 40–70 % of rated capacity. Lower shot utilization increases thermal history and degrades mechanical properties; higher utilization may produce unmelted bead-rich zones at the melt front. In electrical connector and sensor-housing applications where comparative tracking index and flammability are release criteria, this material is tested under IEC 60112 and UL 94. The low-warpage glass-bead PBT is specified for multi-pin connectors, lamp sockets, and ECU housing covers because cavity pressure gradients, weld lines, and post-mold assembly stresses are less likely to produce visible distortion after thermal cycling. For enclosure-validated programs, dimensional change after 1,000 h at 85 °C and 85 % RH is often recorded according to customer-specific methods. Published data for this specific configuration is limited; validation should be performed on the production tool rather than extrapolated from laboratory plaques.
    Test PropertyStandardQualification Purpose
    DensityISO 1183Verify filler loading consistency and lot-to-lot compounding stability
    Tensile strength and elongationISO 527-1/-2Release mechanical performance after molding
    Flexural modulusISO 178Quantify stiffness for housing and bracket design
    Charpy notched impactISO 179/1eAAssess toughness and risk of brittle failure at weld lines
    Heat deflection temperatureISO 75-1/-2Confirm load-bearing capacity at elevated under-hood or lamp temperatures
    Mold shrinkageISO 294-4Control flow-direction and transverse-direction shrinkage difference
    Comparative tracking indexIEC 60112Evaluate surface leakage resistance in electrical housings
    FlammabilityUL 94Classify end-use minimum wall thickness for electrical enclosures
    The glass-bead reinforcement also reduces the tendency for sink marks in thick-to-thin transitions because the spherical fillers do not create the same oriented internal stress as fibers. However, gas-counterpressure molding, conformal cooling, and optimized gate placement remain more effective for sink control than filler substitution alone. For connectors with pin pitch below 1.27 mm, mold-flow analysis should incorporate experimentally measured viscosity data for this grade to predict weld-line location and glass-bead distribution near small features.

    When Low-Warpage Requirements Outweigh Maximum Tensile Modulus

    When a designer prioritizes flatness and dimensional repeatability over ultimate tensile modulus, 727BM is selected instead of short-glass-fiber DURANEX grades. The mechanical trade-off is measurable and systematic. A 30 wt% short-glass-fiber PBT may reach tensile modulus above 9,000 MPa under ISO 527-2, whereas low-warpage glass-bead grades of this class typically remain below 6,000 MPa. The spherical filler does not bridge fracture surfaces as effectively as high-aspect-ratio fiber. Notched Charpy impact values under ISO 179/1eA are therefore lower than comparable fiber-reinforced compounds. Snap-fit retention features and load-bearing bosses must be designed with lower strain if this material is substituted. Shrinkage comparisons also define the substitution boundary. Unfilled PBT mold shrinkage is typically 1.5–2.0 % under cold-mold conditions. Glass-fiber reinforcement reduces average shrinkage but increases anisotropy. Glass-bead-reinforced low-warpage grades produce shrinkage values closer to 1.0–1.5 % in both flow and transverse directions. When part tolerances are below 0.05 mm, the preference is for glass-bead PBT, with tooling dimensions adjusted from production shrinkage studies rather than from single-point datasheet values. Because the glass-bead surface-to-matrix interface controls stress transfer, adhesion package selection and bead surface treatment affect final performance. The material is not recommended for applications demanding tensile modulus above 8,000 MPa or Charpy notched impact above 6 kJ/m². In those cases, short-glass or long-glass fiber DURANEX grades should be evaluated under the same ISO 527-2 and ISO 179/1eA protocols. Conversely, where sheet-metal replacement requires curvature stability but not high stiffness, the low-warpage PBT may be acceptable if dynamic fatigue testing shows strain below the material’s proportional limit. The grade also differs from mineral-filled and mineral/glass-fiber hybrid PBT grades. Mineral fillers such as talc or mica can reduce warpage but increase density and can produce a rougher molded surface. Glass-bead reinforcement maintains lower abrasion in the gate and runner system and provides a more uniform surface appearance. In applications requiring both low warpage and higher modulus, a hybrid mineral/glass-fiber grade may be evaluated, but it will generally have higher density and lower melt flow than this glass-bead system. Contamination boundaries in manufacturing. The glass-bead PBT should not be combined with acetal, polyamide, or flame-retardant masterbatches without supplier approval. Contamination with 0.1 % acetal can generate formaldehyde and trigger rapid molecular-weight loss. Regrind is permissible in controlled proportions up to 20 wt% when sprues and runners are dried and kept clean. Machine operators confirm lot flow by melt volume-flow rate under ISO 1133-1 at 250 °C and 5 kg. If the measured MVR deviates more than ±10 % from the supplier’s reference value, the regrind fraction is reduced and the dryer settings are rechecked before further molding. In hot-oil mold systems or high-temperature tooling above 120 °C, the cycle time advantage of PBT is reduced and the material may approach its continuous-use thermal boundary. Long-term aging at 140 °C in air can embrittle the PBT matrix and should be validated under shear and vibration loads. The low-warpage glass-bead system does not eliminate oxidative degradation; it only changes the failure distribution by reducing warpage-driven stress concentration.
    Top