| HS Code | 363029 |
| Manufacturer | Polyplastics |
| Product Name | DURANEX® PBT+GF40% 3400 |
| Grade | 3400 |
| Base Polymer | Polybutylene terephthalate (PBT) |
| Reinforcement | Glass fiber 40% |
| Processing Method | Injection molding |
| Density | 1.62 g/cm³ |
| Water Absorption 24h | 0.10% |
| Tensile Strength | 140 MPa |
| Tensile Elongation At Break | 2.5% |
| Flexural Strength | 210 MPa |
| Flexural Modulus | 11500 MPa |
| Charpy Notched Impact Strength | 9 kJ/m² |
| Hdt At 1 82 Mpa | 210 °C |
| Melting Point | 224 °C |
| Mold Shrinkage Md | 0.2% |
| Mold Shrinkage Td | 0.8% |
| Flammability Ul94 | HB |
| Volume Resistivity | 1×10^16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Dielectric Constant 1 Mhz | 3.5 |
As an accredited Polyplastics DURANEX® PBT+GF40% 3400 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyplastics DURANEX® PBT+GF40% 3400 is packaged in sealed 25 kg moisture-proof bags for industrial handling and storage. |
| Container Loading (20′ FCL) | Polyplastics DURANEX® PBT+GF40% 3400 is palletized and securely loaded into a dry 20′ FCL container for safe transport. |
| Shipping | Polyplastics DURANEX® PBT+GF40% 3400 is a non-hazardous glass-fiber-reinforced PBT thermoplastic resin. It is shipped as pellets in sealed bags or containers and is not regulated as dangerous goods for transport (no UN number, hazard class, or packing group). Keep dry and protect from moisture, heat, and contamination. |
| Storage | Store DURANEX® PBT+GF40% 3400 in original sealed packaging in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and moisture. Keep containers closed to prevent contamination and moisture pickup. Avoid prolonged high humidity; dry pellets per supplier recommendations before processing. Store separately from strong oxidizers and follow local regulations and the SDS. |
| Shelf Life | Shelf life: typically 12 months when stored cool, dry, and away from direct sunlight in original unopened packaging. |
Competitive Polyplastics DURANEX® PBT+GF40% 3400 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DURANEX® 3400 is a 40 wt% short glass fiber–reinforced polybutylene terephthalate injection-molding compound manufactured by Polyplastics Co., Ltd. The grade is specified for rigid precision components that require higher flexural modulus and lower creep than unfilled PBT or 30 wt% glass-fiber PBT within the same product family. Representative property data are determined under ISO 1183, ISO 527-1/2, ISO 178, ISO 179/1eA, ISO 75-1/2, and IEC 60093. The following matrix reports typical values, not production release limits; specimens are conditioned at 23 °C and 50 % relative humidity according to ISO 291.
| Property | Test method | DURANEX® 3400 typical value |
|---|---|---|
| Density | ISO 1183 | 1.63 g/cm³ |
| Tensile stress at break | ISO 527-1/2 | 130 MPa |
| Tensile elongation at break | ISO 527-1/2 | 2.3 % |
| Flexural strength | ISO 178 | 210 MPa |
| Flexural modulus | ISO 178 | 12,600 MPa |
| Charpy notched impact strength | ISO 179/1eA | 10 kJ/m² |
| Heat deflection temperature, 1.80 MPa | ISO 75-1/2 | 205 °C |
| Volume resistivity | IEC 60093 | 1016 Ω·cm |
| Comparative tracking index | IEC 60112 | 250 V |
| Water absorption, 24 h immersion | ISO 62 | 0.2 % |
The reinforcement content is the primary differentiator within the DURANEX portfolio. Compared with unfilled PBT, the 40 wt% glass fiber increases density from approximately 1.31 g/cm³ to 1.63 g/cm³ under ISO 1183 and raises flexural modulus by more than a factor of four under ISO 178. Compared with 30 wt% glass-fiber DURANEX® 3300, the 3400 grade yields higher tensile and flexural stiffness but lower elongation and a different weld-line strength profile. These differences affect gate selection, wall-thickness targets, and post-mold dimensional correction.
At 40 wt% reinforcement, the fiber skeleton becomes load-bearing under tensile and flexural deformation. The measured tensile stress at break of approximately 130 MPa under ISO 527-1/2 is accompanied by a tensile elongation at break of only 2.3 %; localized yielding in the matrix is constrained by the fibers. The flexural modulus of 12,600 MPa under ISO 178 reduces short-term deflection in structural ribs and supports higher screw torque retention than unfilled PBT. However, high fiber packing reduces the volume fraction of ductile matrix available for energy dissipation. Charpy notched impact strength of 10 kJ/m² under ISO 179/1eA should therefore be treated as a notch-sensitive value; sharp corners, knit lines, and molded-in gate stresses can produce lower energy absorption in the finished part than in standard test specimens.
Pre-drying of DURANEX® 3400 is carried out in a desiccant dryer at 120 °C for 4–6 h to reach a residual moisture content below 0.02 %. The measurement is made by Karl Fischer titration or a calibrated volumetric moisture analyzer. Residual moisture above this limit hydrolyzes the ester linkages in the PBT backbone at melt temperature, producing silver streaks, reduced tensile strength, and batch-to-batch part brittleness. When bags have been exposed to humid air for more than 8 h, a hopper dryer without a desiccant bed is insufficient because PBT does not release moisture rapidly at hopper-air temperature.
Injection molding is performed with a reciprocating screw machine using barrel temperature settings from 250 °C to 270 °C and a mold temperature from 60 °C to 100 °C. A high-cavitation tool for electrical connectors benefits from the upper end of the mold-temperature range because slower cooling reduces anisotropic stress and improves dimensional repeatability. The 40 wt% glass content increases melt viscosity; injection pressure and clamp force must be estimated from the flow-length-to-wall-thickness ratio of the cavity rather than from unreinforced PBT data. A general-purpose screw with an L/D ratio between 20:1 and 25:1 and a compression ratio of 2.5:1 to 3.5:1 is specified to maintain stable melt quality.
The upper limit is governed by residence time and local shear heating. Melt temperature above 270 °C accelerates PBT decomposition and generates volatile byproducts that appear as surface blemishes and gas-emission odor. Production-scale twin-screw compounding of glass-reinforced PBT uses vented barrels and controlled screw cooling to avoid barrel-temperature overshoot; injection molding of the finished compound does not include a devolatilization section, so any thermal degradation occurring in the barrel remains in the melt. Hot-runner systems must avoid dead spots because stagnant material can exceed a residence time of 10 min and produce black specks. Hardened check rings and bimetallic screw flights are specified to reduce wear from glass fiber and to prevent cushion instability. When a molding cell is shut down for more than 15 min, the barrel should be purged and the screw should not be left rotating against a closed nozzle.
Glass fiber orientation induces anisotropic shrinkage. Under ISO 294-4, typical mold shrinkage values for DURANEX® 3400 are 0.2 % to 0.5 % in the flow direction and 0.4 % to 0.8 % transverse to flow, with the actual range dependent on gate geometry, wall thickness, and mold temperature. Multi-cavity tools with naturally balanced runners reduce cavity-to-cavity fill-pressure variation; imbalance in a four-cavity connector mold can generate cavity-to-cavity weight differences above 2 % and dimensional scatter outside ±0.05 mm. For this reason, flow simulation is performed before final steel cutting, and short-shot studies verify that all cavities fill within 5 % of one another by weight. High gate-freeze times and adequate holding pressure minimize sink marks over ribs; inadequate packing pressure causes voiding along the fiber bundles in thick sections.
Electrical and electronic components are specified with DURANEX® 3400 for dielectric strength, volume resistivity, and dimensional stability under terminal insertion. Volume resistivity of 1016 Ω·cm under IEC 60093 supports use as a dry-service insulating body, but the glass fiber surface can provide a hygroscopic path that lowers insulation resistance in humid environments. Parts intended for 85 °C and 85 % relative humidity service should be evaluated under IEC 60068-2-78 with leakage-current limits established by the end-use product standard. The comparative tracking index of 250 V under IEC 60112 is typical of glass-filled PBT; designs requiring CTI above 400 V require a different base resin or an approved surface treatment. Thin-wall battery-insulator components also require verification of dielectric strength on molded parts, because fiber orientation at a weld line can reduce local breakdown voltage.
Heat deflection temperature of 205 °C at 1.80 MPa under ISO 75-1/2 is a short-term thermal deformation indicator. It does not establish continuous use temperature. For automotive under-hood structures operating between 140 °C and 160 °C, qualification requires thermal aging data according to UL 746B relative thermal index or customer-specific heat-aging protocols. PBT matrix oxidation reduces elongation and increases brittleness at the surface after long-term exposure; the 40 wt% glass reinforcement does not prevent oxidative embrittlement. Published multi-year creep data for this specific grade are limited, so creep and stress-relaxation testing at the actual service temperature and stress state must be performed on molded plaques from production tooling.
Power-tool housings, motor brackets, and threaded-insert carriers use the high flexural modulus to reduce deflection under assembly torque. Axial pull-out of inserts is evaluated on molded bosses rather than on flat specimens because the glass fiber orientation around a cylindrical core is helical; the measured tensile strength of 130 MPa under ISO 527-1/2 is therefore not directly transferable to boss tear-out. When insert designs create excessive hoop stress, cracking can initiate at the boss inner surface, especially if mold temperature is below 60 °C or if the boss wall contains a weld line. Boss cracking is reduced by raising mold temperature to 80–100 °C and by using rounded insert knurling with a minimum wall thickness of 1.5 times the insert outer diameter for this glass-fiber level.
Chemical exposure limits include hydrolysis by hot aqueous acids and alkalis, stress-cracking by aromatic solvents, and oxidative embrittlement by engine oil at elevated temperature. The glass fiber itself is stable, but the PBT matrix remains vulnerable to hydrolysis in long-term contact with coolants and road salt. Compatibility with glycol-based coolants at 120 °C and with zinc chloride–based salt solutions should be verified by immersion testing under ISO 175 on stressed specimens. Avoid combination with amine-containing heat stabilizers or certain silicone-based mold releases that may interfere with weld-line strength; any additive package should be validated for melt stability and surface adhesion before production release.