Polyplastics Duranex Pbt Gf30 Lw Hydrolytic 733ld

Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD

    • Product Name: Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 433548
    Grade DURANEX 733LD
    Polymertype PBT
    Fillertype Glass fiber
    Fillercontent Percent 30
    Lowwarpage Yes
    Hydrolysisresistant Yes
    Density G Cm3 1.53
    Tensilestrength Mpa 135
    Tensileelongation Percent 2.5
    Flexuralmodulus Mpa 9000
    Flexuralstrength Mpa 200
    Charpyimpact Kj M2 45
    Charpynotchedimpact Kj M2 9
    Hdt 1 82mpa C 207
    Meltingpoint C 224
    Waterabsorption Percent 0.1
    Moldshrinkage Percent 0.3-0.7
    Ul94flammability HB
    Volumeresistivity Ohm Cm 1E16
    Dielectricstrength Kv Mm 17
    Processingmethod Injection molding
    Dryingtemperature C 120
    Dryingtime H 3
    Melttemperature C 250-270
    Moldtemperature C 60-80

    As an accredited Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: 25 kg moisture-proof, foil-lined bags on pallets, securely sealed and labeled for Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD.
    Container Loading (20′ FCL) 20′ FCL container loading of Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD, securely palletized and shrink-wrapped for safe ocean transport.
    Shipping Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD is shipped as non-hazardous plastic pellets in sealed moisture-barrier bags, cartons, and pallets. Keep cool and dry, protected from humidity and direct sunlight. It is not classified as dangerous goods for transport; no special handling is required.
    Storage Store DURANEX® PBT+GF30%-LW-Hydrolytic 733LD in a cool, dry, well-ventilated warehouse, sealed in original moisture-barrier packaging. Protect from direct sunlight, heat, moisture, and ignition sources; avoid strong oxidizers, acids, and bases. Keep containers clean, labeled, and closed. Use first-in/first-out. Do not store outdoors or near foodstuffs. If moisture exposure occurs, dry per supplier recommendations before processing.
    Shelf Life Shelf life is approximately 24 months when stored dry in original sealed packaging below 30°C, away from sunlight.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyplastics DURANEX® PBT+GF30%-LW-Hydrolytic 733LD is a 30 wt% glass-fiber-reinforced polybutylene terephthalate injection molding grade formulated with low-warpage and hydrolytic stabilization architecture. The product designation encodes the following: DURANEX is the Polyplastics PBT family; PBT+GF30% indicates a nominal 30% glass fiber mass fraction; LW identifies low-warpage behavior; and Hydrolytic 733LD identifies the hydrolysis-resistant grade number. The resin is supplied in pellet form and is processed by injection molding. Compared with unfilled PBT, the 30% glass fiber increases tensile modulus, reduces mold shrinkage, raises melt viscosity, and decreases notched impact toughness. Compared with standard PBT-GF30, the 733LD formulation is intended for parts in which hot-wet exposure, thermal cycling, and dimensional stability are simultaneous requirements, such as automotive connector housings, relay bases, sensor bodies, and underhood enclosures.

    Polybutylene terephthalate is a semi-crystalline polyester with a melting peak in the region of 220°C to 230°C and a glass transition temperature below 60°C. The addition of 30% glass fiber increases heat deflection temperature and reduces mold shrinkage, but the ester linkages in the PBT backbone are susceptible to hydrolytic chain scission. Water at melt temperature attacks these ester bonds and reduces molecular weight. The grade therefore requires closed-loop desiccant drying at 120°C to 130°C for 4 h to 6 h, with a drying-air dew point of −30°C or lower. The target moisture content before processing is below 0.02%. At plant-floor relative humidity above 60%, open contact with ambient air should be limited to less than 30 min at the press hopper. If the material is not dried to this level, the result can be splay, surface delamination, loss of tensile elongation, and premature loss of hydrolysis resistance in the molded part.

    What narrows the processing window for a hydrolysis-stabilized low-warpage PBT-GF30?

    The processing window is narrower than that of an unmodified PBT-GF30 because the low-warpage effect and the hydrolytic stabilizer depend on melt temperature, shear history, and residence time. Low-warpage behavior is sensitive to final glass fiber length distribution and orientation. Excessive screw speed or back pressure can reduce fiber length and lower tensile modulus; insufficient back pressure can produce glass-fiber agglomerates and non-uniform filler distribution. Typical melt temperature settings for this class are 250°C to 270°C, and mold surface temperatures are typically 60°C to 80°C. The barrel residence time at 260°C should not exceed 5 min. A general-purpose reciprocating screw with an L/D ratio of 20:1 to 24:1 and a compression ratio of 2.0:1 to 2.5:1 is typical. The feed throat should be water-cooled and maintained below 60°C to prevent bridging of glass-filled pellets.

    Back pressure is normally set between 0.3 MPa and 0.7 MPa; screw speed is typically limited to 100 rpm to 200 rpm. The shot volume should occupy 50% to 80% of barrel capacity. Small shot volumes increase residence time and thermal degradation risk; large shot volumes may exceed plasticating capacity and produce unmelt. The nozzle and hot-runner system should be free of dead spots where material can stagnate. Hot-runner manifold temperatures should be kept within 250°C to 265°C, and local heating above 270°C should be avoided because the stabilizer can degrade and carbonized particles can form. Gate depth for thin-walled connector bodies is often 0.8 mm to 1.2 mm for edge gates, but final dimensions should be confirmed by mold-filling simulation. Glass fiber is abrasive; screw, barrel, check ring, and tool surfaces in gate and vent areas should be hardened or coated. Mold vent depth for glass-reinforced PBT is typically 0.01 mm to 0.03 mm.

    The selection of mold temperature within the 60°C to 80°C range is not purely cosmetic. Lower mold temperatures shorten cycle time but can reduce crystallinity at the surface and increase residual stress in the glass-filled skin layer. Higher mold temperatures improve crystallization and wetting of glass fibers, but they may extend cooling time and increase out-of-plane warpage if cooling is non-uniform. For thin-walled connector bodies, mold filling at the upper end of the range is sometimes used to prevent premature freeze-off at the gate. The final choice should be based on short-shot studies and pressure-loss measurements from mold-filling simulation.

    Spiral flow length for PBT-GF30 at 260°C injection temperature and 70°C mold surface is generally lower than unfilled PBT. The addition of 30% glass fiber increases viscosity, especially at low shear rates. The low-warpage filler system may further reduce melt fluidity relative to a standard fiber-only grade. For thin sections below 1.0 mm, wall thickness strongly limits flow length, and injection pressure should be evaluated to avoid short shots. Published data for this specific configuration is limited; actual flow-length data should be generated on a spiral mold or through mold-filling analysis.

    In underhood electrical distribution systems, the primary degradation load is not a single mechanical property but the combined effect of 85°C to 125°C air, 85% relative humidity, thermal shock, glycol spray, and terminal insertion stress. Connector housings molded from 733LD must retain latch deflection, terminal retention force, and creep resistance after such exposure. Hydrolytic stabilization is relevant because terminal insertion leaves micro-strains and molded-in stress concentrations that accelerate moisture uptake and crack initiation. If the PBT matrix loses molecular weight through ester hydrolysis, the glass-filled material becomes more notch-sensitive and can crack at latch roots or terminal insertion points. Evaluation therefore includes hot-wet aging followed by tensile property measurement on ISO 527-2:2012 type 1A specimens and notched impact measurement using ISO 179-1:2010. Electrical properties such as volume resistivity and dielectric strength can be monitored after aging according to IEC 60093 and IEC 60243-1.

    Hot-wet property retention and the divergence from unmodified PBT-GF30

    Standard PBT-GF30 without a hydrolysis-resistant package tends to embrittle in hot-water or glycol aging because hydrolysis generates carboxylic acid end groups that autocatalyze further cleavage of the ester backbone. The 733LD formulation is designed to delay this autocatalytic cycle. The supplier does not disclose the exact additive composition, but the stabilization approach generally involves reducing free carboxylic acid end-group concentration and adding acid-scavenging or chain-extending species. Published data for this specific configuration is limited; designers should request lot-specific hydrolysis curves from Polyplastics. In comparative evaluations under 95°C water or 50/50 ethylene glycol/water immersion, unstabilized PBT-GF30 can show pronounced tensile strength and elongation loss after 500 h to 1000 h, while a hydrolysis-stabilized PBT-GF30 is expected to retain a higher fraction of initial properties. The actual retention for 733LD depends on part thickness, glass orientation, and residual stress from molding.

    PBT itself absorbs less moisture than polyamide 66. At equilibrium, PA66-GF30 can absorb 1.5% to 2.5% water by mass, whereas PBT-GF30 generally remains below 0.3%. This lower moisture regain helps preserve dimensional and electrical performance in humid environments, but hydrolysis rate in hot-water contact is controlled more by acid end-group concentration than by equilibrium water content. The 733LD hydrolytic stabilization package therefore targets chemical degradation rather than moisture absorption alone. Low-warpage behavior does not imply isotropic mechanical strength. Weld lines in glass-reinforced PBT are zones of fiber orientation parallel to the melt front and can exhibit local tensile strength well below the bulk value. Gate placement should position weld lines away from latch roots and terminal retention features. Multiple gates can improve filling balance and warpage control but create additional weld lines. The low-warpage package narrows the shrinkage differential between flow and cross-flow directions, but it does not eliminate weld-line weakness.

    Property categoryTest standardCharacteristic of 733LD versus unmodified PBT-GF30Design consequence
    Tensile strengthISO 527-2Comparable class range; possible slight offset due to stabilizer and low-warpage additivesStatic load-bearing calculations remain close to standard PBT-GF30
    Tensile modulusISO 527-2Within PBT-GF30 classSnap-fit and deflection behavior follow glass-reinforced PBT design rules
    Notched Charpy impactISO 179-1/1eALower than unfilled PBT; glass-filled notch sensitivity appliesAvoid sharp notches and molded-in stress risers
    Mold shrinkage anisotropyISO 294-4Reduced flow/cross-flow differential compared with standard PBT-GF30Improved part flatness and dimensional stability in thin-wall housings
    Heat deflection temperatureISO 75-2Comparable to PBT-GF30Short-term heat resistance suitable for underhood enclosures
    Hydrolytic stabilityCustomer-specific hot-wet protocolsImproved retention in hot water or glycol versus unmodified PBT-GF30Extended connector latch and terminal retention under humid aging

    Differences from other low-warpage approaches are significant. Low-warpage can also be achieved by blending PBT with polycarbonate or PET, which reduces crystallinity and changes shrinkage behavior. Such blends may show reduced chemical resistance, lower heat deflection, or slower crystallization. The 733LD grade remains within the PBT family, so it retains fast crystallization, solvent resistance, and low moisture regain. Compared with PA66-GF30, 733LD offers lower water absorption and better dimensional stability in humid conditions, but a lower continuous-use temperature ceiling. Compared with standard DURANEX PBT-GF30 grades without hydrolysis protection, 733LD is selected when the connector must survive high-humidity thermal cycling, coolant spray, or hot-water exposure.

    In service, PBT can undergo secondary crystallization at temperatures above 80°C. If dimensional checks are performed immediately after ejection, additional shrinkage can occur during underhood service. Post-mold annealing at 120°C for 2 h is sometimes used to stabilize crystalline structure before final inspection. The glass fiber phase also reduces creep and stress relaxation compared with unfilled PBT, but snap-fit latch designs still require creep modulus data generated under ISO 899-1 at the target service temperature. The low-warpage/hydrolytic package does not remove the viscoelastic response of the PBT matrix.

    Chemical exposure limits remain important. Hydrolytic stabilization improves hot-wet resistance but does not confer universal chemical resistance. Prolonged exposure to strong alkaline solutions, steam above 121°C, or concentrated oxidizing acids can degrade PBT. Contact with automotive brake fluid beyond short-term splashes should be validated. Molding residues of polycarbonate, polyamide, or acetal should be purged thoroughly because polyester matrices can undergo transesterification or incompatible phase separation when mixed with dissimilar polymers. Regrind usage for glass-reinforced PBT is typically limited to 20% to 30% of the feed stream; molded parts that have been exposed to hot-wet service or strong chemical media should not be reground into material intended for hydrolysis-stability-critical components.

    For automotive use, regulatory assessment is usually conducted under REACH, RoHS, and applicable UL 94 flammability categories. Electrical connectors may also be tested according to IEC 60112 for comparative tracking index and IEC 60695-2-10 for glow-wire ignition. The exact flammability rating and comparative tracking index for 733LD should be taken from the supplier’s technical datasheet, because transfer of generic PBT-GF30 ratings can misrepresent the specific stabilizer and filler package. Tool design should be supported by mold-filling simulation, and mold shrinkage values should be verified using ISO 294-4 plaques or a representative tool.