Polyplastics Duranex Pbt Gf30 Lw Fr 6300b

Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B

    • Product Name: Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 436722
    Polymer Type PBT
    Reinforcement 30% glass fiber
    Flame Retardant Yes
    Low Warp Characteristic Yes
    Density G Cm3 1.64
    Water Absorption 23c 24h Percent 0.20
    Mold Shrinkage Percent 0.2-0.6
    Tensile Strength Mpa 140
    Tensile Elongation Percent 2.0
    Flexural Modulus Mpa 9800
    Flexural Strength Mpa 210
    Charpy Notched Impact Kj M2 6
    Deflection Temperature 1 82mpa C 205
    Ul94 Flammability Rating V-0
    Dielectric Strength Kv Mm 20
    Volume Resistivity Ohm Cm 1e16
    Arc Resistance S 120
    Melting Point C 224
    Processing Method Injection molding

    As an accredited Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in sealed, moisture-barrier 25 kg net bags on pallets, ensuring stable storage and handling of Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B.
    Container Loading (20′ FCL) Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B is loaded in a 20′ FCL container with palletized bags, secured for export shipment.
    Shipping Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B is shipped as non-hazardous, moisture-sensitive thermoplastic pellets in sealed, PE-lined bags or containers. Protect from humidity, heat, and UV; store cool and dry. Not classified as dangerous goods for transport.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original packages tightly closed and palletized to prevent moisture pickup and contamination. Avoid contact with strong oxidizers. Maintain stable temperature and humidity, use first-in/first-out stock rotation, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Typically 12 months from manufacture when stored dry, below 30°C, in sealed original packaging; avoid moisture and direct sunlight.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyplastics DURANEX® PBT+GF30%-LW-FR 6300B is a 30 wt% glass-fibre-reinforced, flame-retardant low-warpage polybutylene terephthalate injection-moulding grade. The numerical model identifier is 6300B, and the suffix LW-FR denotes the low-warpage flame-retardant modification within the DURANEX® portfolio. The compound combines a semicrystalline PBT matrix, discontinuous glass fibre, a flame-retardant package, and low-warpage modifiers intended to reduce differential shrinkage and out-of-plane distortion in flat or thin-walled moulded components. The material is supplied as pellets and is normally specified for electrical and electronic parts where dimensional stability after moulding must coexist with a recognised flammability classification under UL 94. No design value should be taken from this document alone; the manufacturer’s current datasheet, UL Yellow Card, and certificate of analysis for the specific lot provide the mandatory property values. Typical use contexts include connector bodies, relay housings, sensor mounts, motor brush holders, and power-distribution enclosures. In each of these applications, mechanical stiffness, flame retardancy, and reduced warpage are required simultaneously, but moulding behaviour depends on gating, wall thickness, glass-fibre orientation, pigment package, regrind content, and mould temperature.

    The following test matrix identifies the minimum standard designations that should be requested when validating this 30 wt% glass-fibre-reinforced low-warpage flame-retardant PBT for a specific moulded part. Values are not supplied here because they depend on tool geometry, wall thickness, gating, pigment package, regrind content, and mould temperature. Melt volume-flow rate should be evaluated at the condition stated on the manufacturer’s datasheet, commonly 250 °C with a 2.16 kg nominal load unless otherwise specified.

    PropertyStandard designationTypical unit
    DensityISO 1183-1:2019g/cm³
    Melt volume-flow rateISO 1133-1:2022cm³/10 min
    Tensile stress at breakISO 527-2:2012MPa
    Tensile modulusISO 527-2:2012MPa
    Flexural strengthISO 178:2019MPa
    Flexural modulusISO 178:2019MPa
    Charpy notched impact strengthISO 179-1/1eA:2010kJ/m²
    Izod notched impact strengthISO 180/A:2000kJ/m²
    Heat deflection temperature at 1.80 MPaISO 75-2:2013°C
    Coefficient of linear thermal expansion, flow/transverseISO 11359-2:202110⁻⁶/K
    Moulding shrinkage, flow/transverseISO 294-4:2018%
    Water absorption at 23 °C and 50 % relative humidityISO 62:2008%
    Comparative tracking indexIEC 60112:2020V
    FlammabilityUL 94class/min thickness
    Glow-wire flammability indexIEC 60695-2-12:2021°C

    Which Compositional Levers Reduce Warpage Without Eliminating the Stiffness Contribution of Glass Fibre?

    In a conventional 30 wt% glass-fibre-reinforced polybutylene terephthalate, glass fibres orient preferentially along the flow direction during cavity filling. This creates a pronounced difference between flow-direction and transverse-direction shrinkage. The low-warpage modification used in 6300B is intended to compress that shrinkage differential, typically through a combination of filler morphology adjustment, nucleation, and base-resin modification. Under ISO 294-4:2018, shrinkage is reported separately in the flow and transverse directions. The difference between those two values is the primary numerical indicator of warpage potential for a given tool. A low-warpage grade should show a smaller flow-transverse shrinkage difference than a standard glass-fibre-reinforced flame-retardant PBT when moulded under identical conditions; however, the absolute values are gate-position dependent and cannot be transferred between cavities without mould-filling simulation using measured shrinkage data.

    Because the glass content is retained at 30 wt%, tensile stiffness remains in the glass-filled range rather than falling to the unfilled PBT level. For this product class, a 30 wt% glass-fibre-reinforced PBT commonly exhibits a tensile modulus between 9 000 MPa and 11 000 MPa under ISO 527-2:2012, while unfilled flame-retardant PBT is commonly between 2 500 MPa and 3 500 MPa. The low-warpage grade is expected to lie toward the lower portion of the glass-filled range because filler orientation and glass-length retention may be modified to achieve isotropic shrinkage. Published data for this specific 6300B configuration is limited and must be replaced by supplier release values before tool design. Crystallisation kinetics also influence warpage. PBT crystallises rapidly, and the low-warpage formulation may increase nucleation density, which reduces the fraction of post-mould crystallisation that can cause slow shrinkage and dimensional drift after demoulding.

    Drying is the first processing constraint. PBT hydrolyses at melt temperatures because water attacks the ester linkage, and this degradation is autocatalytic. Pellet moisture should be reduced below 0.02 % before injection moulding. A desiccant dryer set at 120 °C for 4–6 h with a dew point below -40 °C is the usual starting point. When ambient relative humidity exceeds 60 %, exposure of dried pellets to plant air should be limited to 30 min or less, and hopper purging with dry air is advisable. On a production-scale 40 mm to 80 mm three-zone screw with an L/D ratio of 20:1 to 25:1, glass-filled material creates higher screw-recovery torque than unfilled PBT. Back pressure of 2–6 bar and screw surface speed not exceeding 0.3 m/s are conventional starting points. Melt temperature should be measured by an air-shot probe and maintained at 250–270 °C. Mould temperature should be held at 60–100 °C depending on surface requirements and crystallinity. If mould temperature falls below 40 °C, insufficient crystallinity may produce post-mould shrinkage and warpage. If melt temperature remains above 270 °C for extended periods, polymer chain scission and flame-retardant package decomposition can occur, producing surface defects, plate-out on the mould, and loss of toughness.

    When Flame Retardancy Is Required at Reduced Wall Thickness in Electrical Housings

    Electrical connector housings, relay bases, and sensor enclosures increasingly require flame-retardant performance at wall thicknesses below 1.0 mm. At reduced wall thickness, the flame-retardant system does not necessarily behave identically to thicker sections because the thermal mass is lower and the flow-induced filler skin layers are different. Under UL 94, flammability classification is thickness-dependent. The UL Yellow Card for the grade specifies the minimum thickness at which a given classification is recognised. Designers should not extrapolate a 1.6 mm result to a 0.4 mm wall. For thin-wall connector housings, flammability must be verified at the actual minimum wall thickness, including weld lines and gate paths.

    Glow-wire requirements under IEC 60695-2-12:2021 may impose additional constraints. Electrical parts used in unattended appliances commonly require a glow-wire flammability index of 750 °C to 850 °C at a specified wall thickness; whether 6300B meets a particular value must be confirmed from the current manufacturer’s report. The comparative tracking index measured under IEC 60112:2020 is relevant for creepage distance calculations. A low-warpage filler system may reduce the tracking index relative to an unfilled flame-retardant PBT if the filler chemistry is not selected for high tracking resistance. The engineer should specify a tracking index threshold and request the lot value rather than assuming that a flame-retardant PBT automatically satisfies insulation coordination requirements.

    Property Trade-offs Against Unfilled Flame-Retardant PBT and Standard GF30 FR PBT

    Relative to an unfilled flame-retardant PBT, the 30 wt% glass reinforcement in 6300B raises tensile modulus and heat deflection temperature but reduces elongation at break and usually shortens flow length. The glass also suppresses the large shrinkage typical of unfilled PBT, but the low-warpage modification is required because plain glass reinforcement alone introduces anisotropic shrinkage. Relative to a standard 30 wt% glass-fibre-reinforced flame-retardant PBT, the low-warpage version trades a modest reduction in flow-direction stiffness and strength for improved dimensional stability and lower average warpage. Weld-line strength may also shift because low-warpage fillers alter the packing of glass fibres at knit lines. Compared with a PA66 GF30 flame-retardant grade, PBT typically exhibits lower water absorption under ISO 62:2008 and therefore better retention of dielectric properties in humid environments, but lower dry-heat deflection temperature under ISO 75-2:2013.

    Comparative parameterUnfilled FR PBTStandard GF30 FR PBTDURANEX® 6300B LW-FR
    Tensile modulus, ISO 527-2:20122 500–3 500 MPa9 000–11 000 MPa8 000–10 000 MPa representative class range
    Heat deflection temperature, 1.80 MPa, ISO 75-2:201355–70 °C200–220 °C190–210 °C representative class range
    Flow-transverse shrinkage difference, ISO 294-4:2018moderatepronouncedreduced by low-warpage modification
    Water absorption at 23 °C/50 % RH, ISO 62:20080.2 % class-typical0.1–0.2 % class-typicalsame class-typical range
    Flammability classificationV-0 at datasheet thicknessV-0 at datasheet thicknessV-0 at Yellow Card thickness