| HS Code | 449876 |
| Glass Fiber Content | 30% |
| Density | 1.53 g/cm³ |
| Tensile Strength | 145 MPa |
| Tensile Elongation | 2.5% |
| Flexural Modulus | 9,000 MPa |
| Flexural Strength | 210 MPa |
| Charpy Notched Impact Strength | 8 kJ/m² |
| Heat Deflection Temperature At 1 82 Mpa | 210 °C |
| Rockwell Hardness | M90 |
| Mold Shrinkage | 0.2-0.5% |
| Water Absorption 24h | 0.07% |
| Melting Point | 224 °C |
| Flammability Ul94 | HB |
| Hydrolysis Resistance | Improved |
As an accredited Polyplastics DURANEX® PBT+GF30%-Hydrolytic 330HR factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyplastics DURANEX® PBT+GF30%-Hydrolytic 330HR is supplied in foil-lined, moisture-barrier 25 kg bags, 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Polyplastics DURANEX® PBT+GF30%-Hydrolytic 330HR, palletized in moisture-protective bags, evenly distributed and secured for ocean shipment. |
| Shipping | Polyplastics DURANEX® PBT+GF30%-Hydrolytic 330HR ships as non-hazardous polymer pellets in original sealed moisture-barrier bags, boxes, or octabins. Keep dry and avoid heat, direct sunlight, and moisture. Store in a cool, dry, ventilated area. Transport per SDS/local regulations; no special UN hazard classification under normal conditions. |
| Storage | Store DURANEX® PBT+GF30%-Hydrolytic 330HR indoors in a cool, dry, well-ventilated area on pallets, away from direct sunlight, heat, ignition sources, moisture, and strong oxidizers. Keep original containers tightly closed to prevent contamination and moisture pickup. Avoid dust generation, protect bags from damage, use first-in, first-out rotation, and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Store in a cool, dry, well-ventilated area; shelf life is typically 12 months in unopened original packaging. |
Competitive Polyplastics DURANEX® PBT+GF30%-Hydrolytic 330HR prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyplastics DURANEX® PBT+GF30%-Hydrolytic 330HR is a 30% glass-fiber-reinforced polybutylene terephthalate injection-molding grade specified for components that must retain mechanical and electrical function after exposure to hot and humid environments. The resin combines a semicrystalline PBT matrix with a nominal glass fiber loading of 30% by mass and a hydrolytically stabilized end-group system. The product is used in automotive underhood connector bodies, sensor housings, and electrical enclosures where environmental test sequences such as USCAR-2 Class 3 and ISO 16750-4 damp heat cycles are applied during qualification. The grade is distinguished from standard PBT GF30 materials by reduced free carboxyl end-group concentration, which alters the rate of autocatalytic ester hydrolysis under moisture load.
In unmodified polybutylene terephthalate, chain scission at ester linkages is accelerated by carboxylic acid end groups that form during hydrolysis. The released protons protonate ester oxygen atoms and lower the activation barrier for further cleavage; the process becomes autocatalytic. DURANEX 330HR is formulated with a controlled acid end-group concentration and a stabilizer package that interrupts this feedback loop. The result is a lower rate of molecular weight loss, slower tensile strength decay, and reduced surface cracking after damp-heat exposure.
Comparative industrial evaluations commonly use 85 °C and 85 % relative humidity for 1000 h to 1500 h. Under these conditions, hydrolytically stabilized 30% glass-filled PBT grades typically retain more than 80 % of initial tensile strength, while unmodified PBT GF30 may fall below 50 %. Published data for this specific configuration is limited at exposure times beyond 2000 h; component-level testing under the final part geometry is required. The reduced carboxyl end-group concentration also lowers melt-phase hydrolysis during processing, provided that moisture control is maintained.
Residual moisture in the melt is the most common cause of batch rejection on production lines. When moisture reaches 0.04 % by mass, the vapor pressure at melt temperature produces silver streaks and brittle weld lines. Water in the melt also hydrolyzes ester groups during plastication; this damage is not visible at the surface and may pass a dry-as-molded mechanical test, then cause failure after 200 h to 500 h of damp-heat aging. Moisture analysis should therefore be performed on dried pellets at the hopper inlet, not only at the dryer outlet.
Before melt processing, the granulate must be dried to a residual moisture content below 0.02 % by mass. Desiccant-wheel hopper dryers with a dew point of −30 °C or lower are recommended; drying at 120 °C for 4 h to 6 h is typical for material from originally sealed packaging. If the resin has been exposed to ambient relative humidity above 60 % for more than 2 h, drying at 120 °C for 8 h to 12 h is required. Dried pellets should be conveyed in closed loaders or kept in a hopper heated to 80 °C or above; open hoppers in uncontrolled humidity can allow moisture regain in less than 30 min.
Barrel setpoints from 240 °C to 260 °C are standard for 30% glass-filled PBT. The nozzle may be held at 250 °C to 265 °C for thin-wall sections. Mold temperature should be controlled between 40 °C and 80 °C; for maximum dimensional stability under thermal shock protocols such as USCAR-2, a mold temperature near 80 °C promotes rapid crystallization and reduced post-mold warpage. Melt residence time above 280 °C must be limited to less than 5 min, because residual moisture plus high temperature accelerates ester hydrolysis and darkens the material.
Shot size should occupy 40 % to 70 % of barrel capacity to avoid excessive residence time and glass fiber attrition. A general-purpose screw with an L/D ratio of 18:1 to 22:1 and a hardened check ring is appropriate for reinforced material. Back pressure between 0.3 MPa and 0.7 MPa is used to homogenize fiber distribution without excessive frictional heat. Screw surface speeds above 0.3 m/s can reduce glass fiber length from a nominal 0.4 mm to below 0.2 mm, which lowers tensile and impact performance; injection speed should therefore be moderate for thick-section connector bodies.
At 250 °C and a shear rate of 1000 s⁻¹, 30% glass-filled PBT melts typically exhibit apparent viscosity in the range of 80 Pa·s to 150 Pa·s when measured by capillary rheometry according to ISO 11443. Melt-volume-flow-rate acceptance limits for DURANEX 330HR should be read from the lot certificate of analysis under ISO 1133-1:2022 at 250 °C/2.16 kg; generic values for standard GF30 PBT are not a substitute.
The supplier-datasheet envelope for DURANEX 330HR is summarized as follows. Lot-specific values vary with color concentrate, regrind content, and specimen preparation; certificate-of-analysis data should be used for production release.
| Glass fiber content | ISO 3451-1 | 30 ± 2 | % by mass |
| Density | ISO 1183-1 | 1.52–1.54 | g/cm³ |
| Water absorption, 23 °C/24 h | ISO 62 | 0.06–0.08 | % |
| Tensile strength | ISO 527-1/-2 | 135–145 | MPa |
| Tensile elongation at break | ISO 527-1/-2 | 2.2–2.8 | % |
| Flexural strength | ISO 178 | 195–215 | MPa |
| Flexural modulus | ISO 178 | 8.8–10.2 | GPa |
| Charpy notched impact strength | ISO 179-1/1eA | 7.0–9.5 | kJ/m² |
| Heat deflection temperature, 1.80 MPa | ISO 75-1/-2 | 198–208 | °C |
| Volume resistivity | IEC 60093 | 1 × 1015–1 × 1016 | Ω·cm |
| Comparative tracking index | IEC 60112 | 500–600 | V |
Mold design for glass-reinforced PBT requires short gate lands, full-round or trapezoidal runners, and vent depths of 0.01 mm to 0.02 mm. Inadequate venting causes diesel-effect burns at vent pins because volatile hydrolysis products can ignite under adiabatic compression. Subgates below 0.8 mm may increase fiber breakage and produce glass-fiber-rich surfaces at the gate. Observed production failure modes include brown streaks at knit lines, dull surface regions, and increased variance in terminal retention force when dry-as-molded moisture exceeds 0.03 %.
Incoming quality control should include moisture determination by ISO 15512 Method A or Karl Fischer titration, melt volume-flow rate by ISO 1133-1:2022, and glass content by ISO 3451-1. If MVR deviation exceeds ±10 % from the qualified lot, barrel temperatures, hold pressure, and injection speed should be revalidated before production release. Regrind content should not exceed 20 % without mechanical revalidation, because repeated plastication reduces glass fiber length and lowers damp-heat strength retention.
The principal difference between DURANEX 330HR and a standard 30% glass-filled PBT grade is the retention of tensile strength and surface integrity after damp-heat aging. Standard PBT GF30 may meet initial mechanical requirements but can lose substantial molecular weight in 85 °C/85 % relative humidity because carboxylic acid end groups accelerate chain scission. In contrast, the hydrolytically stabilized end-group system in 330HR reduces the concentration of catalytic acid end groups. The grade is therefore selected where terminal retention force, snap-fit load, or connector latch force must remain stable over vehicle service life.
Compared with unfilled PBT, the 30% glass reinforcement increases flexural modulus from approximately 2.5 GPa–3.0 GPa for unfilled PBT to 8.8 GPa–10.2 GPa and reduces isotropic mold shrinkage from 1.2 %–2.0 % to as low as 0.2 %–0.6 % in the flow direction. Actual shrinkage depends on gate location, wall thickness, and mold temperature.
Compared with impact-modified PBT GF30, 330HR may have a lower notched Charpy impact value, because elastomeric modifiers can reduce long-term hydrolytic retention. Compared with polyamide 66 GF30, PBT absorbs less moisture; PA66 GF30 can reach 2.0 %–2.5 % water uptake at saturation, whereas 30% glass-filled PBT typically saturates below 0.5 %. This difference gives PBT GF30 improved dimensional stability in humid service, but continuous exposure to pressurized water or water/glycol above 120 °C is outside the recommended service envelope for 330HR.
The material should not be compounded with amine-containing additives that can promote ester aminolysis. Prolonged contact with strong mineral acids at pH below 3, strong bases at pH above 10, or hot organic solvents such as methylene chloride should be avoided unless component chemical resistance is validated by immersion testing per ISO 175 or environmental stress cracking testing per ISO 22088-3. For applications requiring a flame-retardant V-0 rating at the same wall thickness, an appropriate flame-retardant DURANEX grade must be selected because 330HR is not inherently flame retardant.
Tight-tolerance connector housings for underhood sensors and electronic control units are specified with DURANEX 330HR when the part must pass thermal shock, terminal pull-out, and damp-heat aging protocols. The resin’s low post-mold shrinkage in the flow direction supports tight pin pitch and terminal insertion geometry. Sensor enclosures mounted near engine coolant circuits are evaluated with the material under USCAR-2 Class 3 and ISO 16750-4 exposure sequences; qualification programs typically include 1000 h of 85 °C/85 % relative humidity followed by tensile strength and dielectric withstanding voltage verification. Published data for this specific configuration is limited for continuous exposure beyond 2000 h; production release should therefore rely on component-level testing of molded parts from the production tool.