| HS Code | 260564 |
| Glass Fiber Reinforcement | 30% |
| Flame Retardancy | UL94 V-0 at 0.75 mm |
| Halogen Free Flame Retardant | Yes |
| Density | 1.59 g/cm³ |
| Water Absorption | 0.2% |
| Mold Shrinkage Md | 0.3% |
| Mold Shrinkage Td | 0.9% |
| Tensile Strength | 125 MPa |
| Tensile Elongation At Break | 2.0% |
| Flexural Modulus | 9000 MPa |
| Charpy Notched Impact Strength | 6 kJ/m² |
| Deflection Temperature Under Load 1 82 Mpa | 200 °C |
| Volume Resistivity | 1×10^16 Ω·cm |
| Dielectric Strength | 20 kV/mm |
| Arc Resistance | 120 s |
As an accredited Polyplastics DURANEX® PBT+GF30%-FR-NF CN7030 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Polyplastics DURANEX® PBT+GF30%-FR-NF CN7030 is supplied in 25 kg moisture-proof bags, 40 bags (1,000 kg) per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading for Polyplastics DURANEX® PBT+GF30%-FR-NF CN7030: standard export palletized bags, shrink-wrapped and secured inside container for ocean transport. |
| Shipping | Polyplastics DURANEX® PBT+GF30%-FR-NF CN7030 is shipped as non-hazardous thermoplastic pellets, typically in sealed moisture-barrier bags or cartons. Transport and store in dry, ventilated conditions away from direct sunlight, heat, and humidity. Keep packaging intact. No special dangerous-goods classification is normally required for transport. |
| Storage | Store DURANEX® PBT+GF30%-FR-NF CN7030 in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep original containers closed and undamaged to prevent contamination and moisture pickup. Avoid dust, static, and prolonged UV exposure. Use clean handling equipment and FIFO. Dry according to supplier recommendations before processing if required. |
| Shelf Life | Store in original sealed packaging, dry, at ≤30°C, out of sunlight; typical shelf life: 24 months from manufacture. |
Competitive Polyplastics DURANEX® PBT+GF30%-FR-NF CN7030 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The designation Polyplastics DURANEX® PBT+GF30%-FR-NF CN7030 identifies a glass-fiber-reinforced polybutylene terephthalate compound in which short glass fiber is incorporated at 30 wt%, a flame-retardant additive package delivers a UL94 V-0 classification, and the NF suffix is commonly associated with a non-fogging/low-emission variant intended for enclosed cabin environments. The base polymer is a semi-crystalline aromatic polyester produced from 1,4-butanediol and terephthalic acid. The glass-fiber phase raises tensile strength and flexural modulus while reducing elongation at break to 2.0–2.5%; the flame-retardant system shifts the combustion response from HB to V-0 at thicknesses as low as 0.75 mm. The low-fogging modification addresses volatile condensation in automotive interior glazing and lighting assemblies, where standard FR packages may leave an opaque film after thermal cycling.
| Property | Typical value | Test method |
|---|---|---|
| Density | 1.50 g/cm³ | ISO 1183-1 |
| Tensile strength at break | 125 MPa | ISO 527-2/5 |
| Flexural modulus | 8800 MPa | ISO 178 |
| Notched Izod impact at 23°C | 7.0 kJ/m² | ISO 180/1A |
| Heat deflection temperature at 1.8 MPa | 200°C | ISO 75-2/Af |
| Flammability | V-0 at 0.75 mm | UL 94 |
| Comparative tracking index | 300 V | IEC 60112 |
| Dielectric strength | 20 kV/mm | IEC 60243-1 |
In this substitution, the primary changes are in shrinkage anisotropy and weld-line integrity. Unfilled PBT exhibits near-isotropic mold shrinkage of 1.5–2.0%; CN7030 exhibits flow-direction shrinkage of 0.3–0.5% and transverse shrinkage of 0.8–1.0%, creating a higher warpage potential on flat covers unless gate location and cooling layout are rebalanced. Production-scale molding lines use sequential valve-gate hot runners with round flow channels ≥2.5 mm to prevent fiber-rich freeze-off. In connectors with multiple pin cores, the melt front splits and recombines; at the weld lines, the glass fibers orient parallel to the interface, reducing local tensile strength by 30–40% relative to bulk values. Part design should therefore place knit lines away from snap-fit retention features or increase local wall thickness to 2.0 mm minimum around the weld area.
Pre-drying is mandatory before melt processing. Moisture level above 0.02% in PBT produces hydrolytic chain scission at barrel temperatures above 250°C, lowering intrinsic viscosity and causing silver streaks, splay, and drop in tensile strength at break. Desiccant dryer with dew point of -40°C and inlet air at 120°C for 4–6 h is required; closed-loop vacuum conveying from dryer to feed throat prevents regain. Barrel profile across a 40:1 L/D injection screw is set 240–270°C from feed to nozzle, with nozzle at 260°C. Melt residence time above 270°C should not exceed 10 min; the flame-retardant package decomposes at excessive shear or temperature, causing mold plate-out, corrosion of unplated tool surfaces, and loss of UL94 V-0. Screw back pressure of 0.3–0.7 MPa is maintained to disperse glass bundles without excessive fiber breakage; fiber length in molded parts is typically 250–400 µm after processing, whereas pellet fiber length before processing is 3–4 mm. Injection speed in the 100–200 mm/s screw-advance range is used for thin-wall sections; hold pressure is set at 50–70 MPa hydraulic and held until gate freeze. Mold temperature is maintained at 40–80°C, with 60°C preferred to balance crystallization rate and cycle time. Because the glass fibers orient in the flow direction, the mold shrinkage is anisotropic: 0.3–0.5% flow-direction versus 0.8–1.0% transverse. Cooling fixtures may be required after ejection if flatness tolerance is below 0.2 mm on parts longer than 100 mm.
At the same nominal glass loading, non-FR PBT-GF30 has no UL94 V-0 classification and is used where flammability is not specified. Halogenated PBT-GF30 FR usually achieves V-0 at 0.75 mm but at higher density from brominated aromatic compounds and antimony synergist; its comparative tracking index is often 200–250 V, and mold deposits can form on tool surfaces after 8–12 h production runs. CN7030’s low-fogging package, when NF is interpreted as non-fogging, is intended to reduce volatile organic emissions and surface condensation, but the exact additive composition is supplier-confidential; published data for this specific configuration is limited. The mechanical property band is similar to other PBT-GF30 products: tensile strength near 125 MPa and flexural modulus near 8800 MPa under ISO 527-2 and ISO 178.
| Material class | Density | Flexural modulus | UL94 | Moisture absorption | Processing implication |
|---|---|---|---|---|---|
| Unfilled PBT | 1.31 g/cm³ | 2.6 GPa | HB | 0.08% | Near-isotropic shrinkage, low modulus |
| PBT-GF30 non-FR | 1.53 g/cm³ | 8.5 GPa | HB | 0.07% | Higher strength, no combustion classification |
| Halogenated PBT-GF30 FR | 1.65 g/cm³ | 9.0 GPa | V-0 at 0.75 mm | 0.10% | Higher density, lower CTI, mold plate-out tendency |
| CN7030 low-fogging FR | 1.50 g/cm³ | 8.8 GPa | V-0 at 0.75 mm | 0.10% | Low emission, anisotropic shrinkage |
Electrical performance is dominated by the semi-crystalline polyester matrix and glass-fiber content. Volume resistivity is typically 1 × 10¹⁶ Ω·cm under IEC 62631-3-1; dielectric strength measured on 3.0 mm plaques is commonly 20 kV/mm under IEC 60243-1. The comparative tracking index is reported around 300 V under IEC 60112, which places the material in a middle tracking-resistance class; designs for high-humidity, high-voltage applications require surface creepage distances per IEC 60664-1 pollution degree 3. Glass fibers intersecting the surface can reduce dielectric breakdown strength by creating local field concentrations, so molded surfaces exposed to voltages above 600 V are typically designed with a 0.5 mm minimum resin-rich skin maintained by moderate injection speed and higher mold temperature. In connector bodies, the toughness of unfilled PBT is not retained; snap-fit deflection angles should not exceed 1.0° unless long-term creep testing under ISO 899-2 supports the design.
Although PBT absorbs less moisture than polyamide 66, extended exposure to hot water/glycol at temperatures above 85°C causes gradual hydrolysis. In automotive underhood connectors, parts exposed to ethylene glycol/water at 125°C for 1000 h typically lose 20–40% of initial tensile strength; published data for this specific configuration is limited. Molded parts specified for continuous hot-moisture service should use minimum wall thickness 1.5 mm, avoid direct contact with copper ions, and be validated by pressure-cooker exposure at 121°C and 100% RH or by the device manufacturer’s coolant compatibility protocol. Hydrolysis is pH-sensitive; continuous service is recommended only within pH 4–9 because acidic or alkaline conditions accelerate chain scission.
Compliance statements for CN7030 are material-specific and color-dependent. The grade is typically listed under the UL Yellow Card with category designations QMFZ2 or QMFZ8; the current certification number must be verified for each production color and thickness. Under European Union directives, the supplier publishes REACH SVHC and RoHS 2011/65/EU Annex II declarations; because flame-retardant packages may contain antimony or brominated species in some variants, halogen-free claims require separate written confirmation. For automotive interior use, fogging behavior is evaluated per DIN 75201-B, where low-fogging grades target condensate below 2 mg; this value is test-specific and is not a permanent material property. Parts intended for food-contact or medical use are outside the standard DURANEX CN7030 specification and require a separate review.
For mold-filling simulation, process engineers input CN7030 data as a fiber-filled semicrystalline thermoplastic with Carreau-WLF viscosity coefficients and PVT data from the supplier. Predicted pressure drop for a 2.0 mm wall connector housing at 260°C is typically 40–80 MPa depending on flow length; actual injection pressure on a 1000 kN clamp machine is adjusted from short-shot studies. Rib thickness should not exceed 60% of adjacent wall to avoid sink marks; bosses should be cored and gusseted. Weld-line location is controlled by gate sequencing; when two flow fronts meet, local tensile strength is reduced by 30–40%, so knit lines should not intersect snap-fit hooks or ultrasonic welding beads. If ultrasonic welding is used, glass fiber at the weld interface may be displaced and produce a resin-rich bond line; weld amplitude should be reduced and energy director height increased to 0.5–0.7 mm.