Polyplastics Duranex Pbt Gf30 Fr Lw 751sa

Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA

    • Product Name: Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 286567
    Polymer Base PBT
    Glass Fiber Content 30%
    Flame Retardant Yes
    Low Warpage Yes
    Density 1.65 g/cm³
    Water Absorption 24 H 0.2%
    Tensile Strength 130 MPa
    Elongation At Break 2.0%
    Flexural Modulus 9,000 MPa
    Charpy Notched Impact Strength 6 kJ/m²
    Hdt At 1 82 Mpa 205 °C
    Ul94 Flammability Rating V-0 (0.75 mm)
    Molding Shrinkage 0.3–0.7%
    Volume Resistivity >1×10^16 Ω·cm
    Dielectric Strength 20 kV/mm

    As an accredited Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA is packaged in 25 kg moisture-resistant bags, palletized for industrial storage and transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized, shrink-wrapped 25 kg bags of Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA, securely stowed for ocean freight.
    Shipping Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA is shipped as a non-hazardous solid in sealed moisture-barrier bags or containers. Store in a cool, dry, ventilated area away from direct sunlight, heat, and ignition sources. Handle carefully to avoid package damage, keep dry, and follow first-in/first-out inventory practices.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep original containers tightly closed and clearly labeled. Avoid dust generation, static discharge, open flames, and smoking. Separate from incompatible chemicals, oxidizers, and foodstuffs. Protect from humidity and water; dry before processing if required. Follow local regulations and the supplier’s safety data sheet.
    Shelf Life Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA typically has a two-year shelf life when stored unopened in original packaging under cool, dry conditions.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyplastics DURANEX® PBT+GF30%-FR-LW 751SA is a flame-retarded, 30% glass-fiber-reinforced polybutylene terephthalate injection-moulding compound. The designation identifies the PBT matrix, 30 wt% short-glass-fiber reinforcement, a flame-retardant package, and a low-warpage modification that alters differential shrinkage between flow and transverse directions. The compound is supplied as cylindrical pellets for conventional reciprocating-screw moulding and is specified for electrical insulation components requiring a UL 94 V-0 classification at wall thicknesses down to 0.75 mm. Its combination of stiffness, dimensional stability, and flame retardancy separates it from unfilled PBT and from standard PBT GF30 FR grades that show pronounced moulded-in bow and twist. Typical density measured by ISO 1183-1 is in the range of 1.65 g/cm³ to 1.68 g/cm³.

    How Does the 30% Glass Fiber Reinforcement Alter Mechanical Response in Thin-Wall Sections?

    Under tensile loading at 23°C, the 30% short-glass-fiber reinforcement raises tensile strength and flexural modulus relative to unfilled PBT, but the response is anisotropic because glass fibers orient in the flow field. Supplier-documented typical values for DURANEX 751SA include a tensile strength at break of 120 MPa to 125 MPa when tested according to ISO 527-2, a flexural modulus near 9,000 MPa according to ISO 178, and a Charpy notched impact strength of approximately 7 kJ/m² according to ISO 179-1/1eA. The heat deflection temperature under a 1.8 MPa load is typically 195°C to 200°C when measured by ISO 75-2/A. Weld lines generated downstream of pin cores and stiffening ribs can exhibit tensile strength losses of 30% to 50% relative to flow-direction values, a limitation common to short-glass-fiber PBT systems. Thin-wall connector housings below 1.0 mm should therefore be simulated with fiber-orientation tensors rather than designed from isotropic datasheet values. The critical fiber length for stress transfer in PBT is estimated at 0.2 mm to 0.3 mm using shear-lag analysis; fibers below this length act as fillers rather than reinforcing elements, which is one reason barrel residence time and screw recovery must be controlled during melt production.

    Prior to injection moulding, the granulate must be dried in a desiccant dryer at 120°C for 4 h to 6 h until residual moisture is below 0.02% by weight, measured by ISO 15512 method B. Hydrolytic degradation of PBT accelerates above 250°C when moisture is present; the result is melt viscosity reduction, loss of tensile strength, and surface silver streaking. Barrel temperature settings are typically maintained between 250°C and 270°C from feed throat to nozzle, with the nozzle held near 260°C. A mould temperature of 60°C to 100°C is used; lower temperatures reduce cycle time but produce insufficient crystallinity and increase post-moulding warpage, while temperatures above 100°C may extend gate seal time without proportional dimensional benefit. On production-scale multi-cavity connector tools, cavity-to-cavity fill imbalance is a frequent observation; this imbalance creates differential crystallinity and measurable dimensional scatter, particularly in long, thin-walled components with side gates. Runner systems for DURANEX 751SA should use full-round or trapezoidal runners with diameters not smaller than 3 mm. Gate thickness should be 60% to 80% of the part wall thickness to avoid premature freeze and excessive pressure drop. For multi-cavity tools, geometrically balanced runners are required because artificial balancing of glass-filled PBT with differing melt residence times can generate different fiber orientation and warpage. Screw recovery should limit glass fiber attrition: surface speeds below 0.3 m/s and back pressures of 0.3 MPa to 0.7 MPa are common on reciprocating-screw machines with L/D ratios of 20:1 to 24:1.

    Flame Retardant Mechanisms and Electrical Tracking Resistance in Connector Housings

    The flame-retardant behaviour of this grade is evaluated through UL 94 vertical burn testing at 0.75 mm, where DURANEX 751SA carries a V-0 classification. The flame-retardant system acts primarily in the condensed phase by promoting char formation and suppressing dripping; this is distinct from purely gas-phase flame retardants that may leave thin sections susceptible to afterglow. Electrical tracking resistance is assessed by the comparative tracking index method of IEC 60112; typical values for this grade fall in the 250 V class. This is sufficient for many appliance and industrial-control components but is not equivalent to high-CTI polymers such as certain non-glass-filled, mineral-filled FR grades. Dielectric strength tested at 2.0 mm thickness according to IEC 60243-1 is typically 20 kV/mm; the value is affected by moisture absorption, so pre-conditioning at 23°C and 50% relative humidity should follow ISO 291. For parts subject to glow-wire end-product testing under IEC 60695-2-11, the PBT matrix plus glass reinforcement may pass 750°C glow-wire ignition tests when part thickness and terminal spacing are favourable; however, published data for this specific configuration is limited, and end-product testing is mandatory because the glass-fiber content influences ignition point and char geometry.

    Test method or standardMeasured propertyTypical value or classification
    UL 94Flammability at 0.75 mmV-0
    IEC 60112Comparative tracking index250 V
    IEC 60695-2-12Glow-wire flammability index at 750°CEnd-product dependent
    ISO 527-2Tensile strength at break120–125 MPa
    ISO 75-2/AHeat deflection temperature at 1.8 MPa195–200°C
    IEC 60243-1Dielectric strength, 2.0 mm thickness20 kV/mm

    Low-warpage behaviour in this grade is not an additive afterthought but a formulation response to differential shrinkage between the flow and transverse directions in glass-fiber-reinforced PBT. Mould shrinkage measured according to ISO 294-4 is typically around 0.4% in the flow direction and 0.9% in the transverse direction; this inequality remains, but the low-warpage package reduces its practical effect in flat multi-pin connector bodies. The greater transverse shrinkage is caused by the orientation of glass fibers along flow, which constrains flow-direction contraction. When unfilled PBT is replaced by DURANEX 751SA, the absolute shrinkage is lower and the modulus is higher, but the part design must still account for anisotropic thermal expansion; coefficients of linear thermal expansion of roughly 3 × 10⁻⁵ K⁻¹ in the flow direction and 7 × 10⁻⁵ K⁻¹ in the transverse direction are typical of 30% glass-filled PBT systems. Post-moulding annealing at 150°C for 2 h can further relax residual stress, but it adds cost and may reduce impact toughness slightly. Because the low-warpage modification does not eliminate glass-fiber orientation, designers of flat rectangular connectors should avoid rapid wall-thickness transitions and isolated thick bosses that create non-uniform packing and post-moulding distortion.

    When Dimensional Stability Under Thermal Cycling Dictates Part Design

    When a part design is transferred from an unfilled PBT or from a standard PBT GF30 FR grade, the comparison must account for more than the UL 94 classification. Compared with unfilled PBT, DURANEX 751SA provides a heat deflection temperature under 1.8 MPa of approximately 195°C to 200°C, whereas unfilled PBT may exhibit values near 60°C under the same load. The flexural modulus is roughly three to four times greater because the glass-fiber network suppresses long-range chain mobility. Compared with a non-low-warpage PBT GF30 FR compound, the dimensional stability advantage appears primarily in reduced post-moulding bow and twist in flat parts, not in the absolute shrinkage values. The trade-off is usually notch sensitivity: the Charpy notched impact strength of this class is in the range of 6 kJ/m² to 8 kJ/m², so snap-fit arms and latching features require generous radii and should avoid direct gate-to-weld-line loading. In humid-service comparisons against PA66 GF30 FR alternatives, PBT absorbs significantly less moisture—typically below 0.1% at 23°C and 50% relative humidity according to ISO 62, versus 1.2% or more for PA66—so electrical characteristics and dimensions remain more stable in condensing environments. The 30% glass-fiber content raises the short-term tensile modulus to approximately 9,000 MPa (ISO 527-2), which is used in finite-element terminal-retention calculations; long-term creep should be validated by ISO 899-2 because creep of the PBT matrix at elevated temperatures remains a governing deformation mode.

    In electric vehicle charging infrastructure and industrial connector applications, the material is typically specified against the end-product standard rather than only the raw-material datasheet. For EV charging inlet and coupler components, compliance is assessed through IEC 62196-1 and IEC 62196-3 tests, including ball-pressure heat resistance and glow-wire end-product testing; DURANEX 751SA with UL 94 V-0 at 0.75 mm supplies the necessary ignition resistance when the moulded part is accepted at the specified thickness. In miniature circuit-breaker housings and relay bases, insulation resistance and dimensional stability are evaluated under IEC 60077 or IEC 61984. The 30% glass-fiber content raises the short-term tensile modulus to approximately 9,000 MPa (ISO 527-2), which supports terminal retention analyses; long-term retention must be confirmed by terminal withdrawal force testing per IEC 60512-16-20. The material's CTI value of 250 V imposes design constraints for high-voltage creepage distances under IEC 60664-1. For photovoltaic junction boxes, long-term UV exposure is managed by enclosure design or coating because PBT is not inherently UV-stable; published data for this specific grade in outdoor PV service is limited, so weathering qualification must follow IEC 61215-2 and UL 746C f1 conditions rather than an assumption of UV resistance.

    Controlling Barrel Residence Time and Screw Recovery During Injection Moulding

    On a conventional reciprocating-screw injection moulding machine with a three-zone general-purpose screw of L/D 20:1 to 24:1, the melt should be processed within a barrel temperature envelope of 250°C to 270°C. Holding the melt at 270°C for more than 5 min accelerates β-hydrogen abstraction in PBT and produces tetrahydrofuran, acetaldehyde, and carboxyl end groups; visible degradation appears as yellowing, gas bubbles, and reduced melt viscosity. Screw recovery should be sequenced to avoid extended residence time: shot size should use 50% to 70% of barrel capacity, and cycle interruption beyond 5 min requires purging with a low-viscosity PBT or a commercial purging compound. Back pressure in the 0.3 MPa to 0.7 MPa range improves melt homogeneity, but excessive back pressure increases fiber breakage. Screw surface speed should remain below 0.3 m/s to limit glass-fiber attrition; fiber length reduction below the critical length of approximately 0.2 mm to 0.3 mm lowers tensile strength and notched impact performance.

    Processing parameterUnitRecommended range
    Desiccant drying temperature°C120
    Drying timeh4–6
    Maximum residual moisturewt%<0.02
    Barrel temperature, feed to nozzle°C250–270
    Mould temperature°C60–100
    Back pressureMPa0.3–0.7
    Screw surface speedm/s<0.3
    Shot size as barrel capacity%50–70
    Top