    Specifications
    HS Code 491432
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Flame Retardancy UL94 V-0 (0.75 mm)
    Tensile Strength 135 MPa
    Tensile Elongation At Break 2.5%
    Flexural Modulus 9,500 MPa
    Flexural Strength 200 MPa
    Charpy Notched Impact Strength 8 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 200 °C
    Melting Point 225 °C
    Water Absorption 24 H 23 C 0.2%
    Molding Shrinkage Flow Direction 0.2–0.5%
    Volume Resistivity 1×10^16 Ω·cm
    Dielectric Strength 20 kV/mm

    As an accredited Polyplastics DURANEX® PBT+GF30%-FR 3316 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyplastics DURANEX® PBT+GF30%-FR 3316 is packaged in 25 kg moisture-proof bags, with 40 bags per pallet for secure transport.
    Container Loading (20′ FCL) Polyplastics DURANEX® PBT+GF30%-FR 3316 loaded in 20′ FCL: palletized original sealed bags, dry ventilated container, secured stowage; protect from moisture, heat, contamination.
    Shipping Polyplastics DURANEX® PBT+GF30%-FR 3316, a 30% glass-fiber-reinforced flame-retardant polybutylene terephthalate compound in pellet form, is not regulated for transport (non-hazardous). Ship in dry, sealed bags/containers, protected from moisture, contamination, and direct sunlight.
    Storage Store DURANEX® PBT+GF30%-FR 3316 in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, and open flames. Keep original containers sealed to prevent moisture absorption and contamination. Avoid dust generation and static discharge. Use proper PPE and follow the SDS. Do not store near incompatible chemicals. Rotate stock and inspect packaging for damage before use.
    Shelf Life Shelf life is approximately 24 months from manufacture when stored unopened in a dry, cool place in original packaging.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF30%-FR 3316 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyplastics DURANEX® PBT+GF30%-FR 3316 is a 30% by weight glass-fibre-reinforced flame-retardant polybutylene terephthalate injection-moulding compound specified for electrical/electronic housings, relay bases, connector bodies, and power-distribution components in which wall thicknesses below 1.0 mm must satisfy UL 94 V-0. The grade identifier 3316 places the product within the DURANEX PBT range as the 30% glass-reinforced flame-retardant variant. The glass loading raises the published flexural modulus to 9500 MPa under ISO 178 while reducing room-temperature tensile strain at break to approximately 2.1% under ISO 527-1/-2. Density is reported as 1.65 g/cm³ under ISO 1183. Relative to unreinforced flame-retardant PBT, the material offers higher creep resistance and lower thermal expansion; relative to 15% glass-reinforced FR PBT, it provides higher stiffness and reduced distortion in large-area thin-wall mouldings, at the cost of reduced flow length and lower weld-line integrity.

    The flame-retardant package is not labelled in all regional datasheets as halogen-free. When halogen-free compliance is required, lot-specific confirmation to IEC 61249-2-21 should be requested because brominated flame-retardant systems are common in this product class. Published data for this specific configuration is limited when comparing smoke density and mould deposit rates, so verification against the final assembly requirement is necessary.

    Typical physical, mechanical, thermal, and electrical values for DURANEX 3316
    PropertyTest standardTypical valueUnit
    DensityISO 11831.65g/cm³
    Tensile stress at breakISO 527-1/-2130MPa
    Tensile strain at breakISO 527-1/-22.1%
    Flexural modulusISO 1789500MPa
    Flexural strengthISO 178200MPa
    Charpy notched impact strength at 23 °CISO 179-1/1eA8.5kJ/m²
    Heat deflection temperature at 1.80 MPaISO 75-1/-2205°C
    Melting point by DSCISO 11357-1/-3225°C
    Comparative tracking indexIEC 60112250V
    Volume resistivityIEC 600931E13Ohm·m
    Flammability at 0.75 mm thicknessUL 94V-0—

    The values in the table are supplier-published typical data for engineering comparison, not guaranteed minimum specifications. Dimensional stability, fibre orientation, and flame-retardant concentration can shift at the cavity level depending on gate location, packing pressure, and wall-thickness distribution. Lot release should be checked against the current supplier certificate and the applicable UL Yellow Card for the minimum thickness class.

    What Limits Thin-Wall Flame Resistance in 30% Glass-Reinforced PBT?

    UL 94 V-0 at 0.75 mm depends on condensed-phase retention, stabilizer concentration, glass-fibre orientation, and mould venting. At 30% glass loading, the fibres increase heat transfer along the flow direction and can either accelerate re-ignition at weld lines or reduce dripping by reinforcing the char. Thin-wall sections below 0.4 mm may fall to V-1 or burn through; published data for this specific configuration is limited. The melting point is 225 °C under ISO 11357-1/-3 and the heat deflection temperature at 1.80 MPa is 205 °C under ISO 75-1/-2. Short-term load-bearing excursions above 205 °C are not recommended without additional metallic support, ribbing, or reduced applied stress.

    Weld-line regions in multi-cavity connector moulds represent the primary flame-resistance weak point because glass-fibre orientation is disrupted and the flame-retardant package may be locally depleted. Mould design using sequential valve gating or relocation of knit lines away from high-voltage conductor paths improves both mechanical integrity and burn-test consistency. Flame performance should be verified on actual production parts, not only on laboratory plaques, because cavity-induced orientation changes the wicking path and drip behaviour.

    Pre-Drying Thresholds, Hydrolytic Chain Scission, and Screw Residence-Time Boundaries

    Pre-drying is mandatory. The compound is supplied as pellets in moisture-resistant packaging, but exposure to ambient humidity above 60% RH will raise moisture content. Pre-dry in a dehumidifying hopper dryer at 120 °C for 4 h to 6 h to reduce moisture to less than 0.02 wt%. Moisture above 0.02 wt% hydrolyzes the ester linkages of the PBT backbone, reducing molecular weight, melt viscosity, and weld-line strength. The observed production failure is a drop in screw recovery torque and brittle fracture at the crimp insert, not only visible splay. A closed-loop dryer with a dew point below -20 °C is recommended during humid weather to prevent re-adsorption between drying and feeding.

    Residence time at melt temperature above 270 °C should not exceed 10 min in the barrel. At temperatures above 280 °C, visible black streaks and an acrid odour indicate decomposition of the flame-retardant package and PBT chain cleavage. When start-up delays exceed 15 min, the barrel should be purged with an unfilled PBT or a thermally stable purge compound. A shut-off nozzle is recommended to prevent drool and to minimise uncontrolled residence time in the front zone. Direct injection into the screw feed throat with excessive back pressure should be avoided because frictional heating can generate local melt temperatures above the barrel set point.

    For injection moulding, a general-purpose screw with 20:1 to 22:1 L/D and compression ratio of 2.5:1 to 3.0:1 is acceptable. Melt temperature should be controlled at 250 °C to 270 °C. Tool temperature should be held at 60 °C to 100 °C; 80 °C is preferred where post-mould dimensional stability and increased crystallinity are required, though it will extend cycle time. Injection velocity should be set in the 200 mm/s to 400 mm/s range for wall thickness below 1.0 mm. Holding pressure depends on gate geometry and projected area, but production tools typically require 60 MPa to 100 MPa hydraulic holding pressure to suppress sink marks and control post-shrinkage.

    When Comparative Tracking Index Falls Below 250 V in Polluted Environments

    Flame-retardant PBT compounds commonly exhibit lower comparative tracking resistance than non-flame-retardant grades. DURANEX 3316 is rated at 250 V under IEC 60112, solution A. In terminal blocks and connectors exposed to hygroscopic dust, oil mist, or soldering flux residue, surface contamination can create a conductive path. Creepage distances should be selected in accordance with IEC 60664-1 and a conformal coating or post-mould washing step considered when operating voltage exceeds 150 V in pollution degree 3 environments. Field failures from arcing often originate at sharp edge gates or screw bosses where local charge density is highest; design reviews should avoid pointed weld-line convergence in high-voltage regions. The CTI value should also be confirmed on actual moulded surfaces, not only on polished plaques, because mould release residues and glass-fibre bloom can lower the tracking resistance.

    Compared with non-flame-retardant 30% glass-reinforced PBT, DURANEX 3316 trades lower weld-line strength and reduced CTI for UL 94 V-0 at 0.75 mm. The additive package also increases melt viscosity at low shear and narrows the processing window. Moulders report a 5 °C to 10 °C reduction in the acceptable lower melt-temperature boundary before short shots occur in multi-cavity tools with 0.8 mm edge gates. Halogen-free flame-retardant grades may provide a higher CTI and lower smoke density, but typically require higher loadings of phosphorus-nitrogen synergists, producing more mould deposit build-up on vent surfaces. Deposit accumulation should be assessed on a 20:1 L/D reciprocating screw machine after 5000 cycles; published data for this specific configuration is limited.

    Typical usage includes automotive engine-compartment connectors, relay housings, industrial control enclosures, and power-distribution terminal blocks. The material is not recommended for infrared reflow soldering because the crystalline melting point is 225 °C; selective wave soldering with short contact times may be acceptable only if part geometry prevents deformation. Continuous exposure to hot water or steam above 60 °C should be avoided because ester hydrolysis accelerates with temperature and can reduce tensile strength over service life. Chemical resistance is adequate for aliphatic hydrocarbons, mineral oils, greases, and many detergent solutions at room temperature, but the compound is not suitable for prolonged contact with concentrated sulfuric acid, boiling strong alkali, or high-pressure steam.

    Compliance and electrical-safety verification matrix
    RequirementStandard or regulationTest condition / clauseTypical result
    FlammabilityUL 940.75 mm vertical burnV-0
    Comparative tracking indexIEC 60112Solution A250 V
    Heat deflection temperatureISO 75-1/-21.80 MPa flatwise205 °C
    DensityISO 118323 °C1.65 g/cm³
    RoHS restricted substancesDirective 2011/65/EU + (EU) 2015/863Supplier declaration requiredDeclared by supplier per lot
    Halogen-free verificationIEC 61249-2-21Not a default classificationLot-specific confirmation required

    Batch-to-batch variance in glass distribution and flame-retardant concentration is measurable in production. Suppliers control lot release against density and tensile stress under ISO 1183 and ISO 527-1/-2, but properties near the lower tolerance boundary should be verified with a three-lot validation before transfer to series production. Tool validation should include burn-test specimens from each cavity, not only a single plaque, because cavity-to-cavity variation in fibre orientation can change the effective flame class.