    Specifications
    HS Code 208024
    Material Type Polybutylene terephthalate (PBT)
    Reinforcement 30% glass fiber
    Density 1.60 g/cm³
    Water Absorption 23 C 24 H 0.10%
    Tensile Strength 120 MPa
    Tensile Elongation At Break 2.0%
    Flexural Modulus 9,000 MPa
    Flexural Strength 180 MPa
    Charpy Notched Impact Strength 23 C 6 kJ/m²
    Heat Deflection Temperature 1 82 Mpa 200°C
    Melting Point 224°C
    Comparative Tracking Index Cti 600 V
    Flammability Rating UL94 V-0
    Volume Resistivity 1×10^16 Ω·cm
    Dielectric Strength 20 kV/mm
    Molding Shrinkage 0.2–0.8%

    As an accredited Polyplastics DURANEX® PBT+GF30%-CTI CG7030 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyplastics DURANEX® PBT+GF30%-CTI CG7030 is packaged in 25 kg moisture-barrier bags, palletized and labeled for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL container loading of Polyplastics DURANEX® PBT+GF30%-CTI CG7030: palletized, moisture-proof bags, evenly distributed and securely lashed for export.
    Shipping Polyplastics DURANEX® PBT+GF30%-CTI CG7030 is shipped as non-hazardous, moisture-sensitive polybutylene terephthalate resin pellets in sealed moisture-barrier bags or containers, commonly 25 kg. It is not classified as dangerous goods for normal transport. Store in a cool, dry area and handle according to the SDS.
    Storage Store Polyplastics DURANEX® PBT+GF30%-CTI CG7030 in a cool, dry, well-ventilated warehouse in original sealed packaging. Keep away from direct sunlight, heat, ignition sources, moisture, dust, and strong oxidizers. Prevent contamination and prolonged UV exposure. Keep containers closed, use first-in-first-out rotation, avoid damaged bags, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Store sealed in a cool, dry place; typical shelf life is 12 months from manufacture under recommended conditions.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF30%-CTI CG7030 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DURANEX® PBT+GF30%-CTI CG7030 is a 30 wt% glass-fiber-reinforced polybutylene terephthalate injection-molding grade in which the matrix has been modified to raise the comparative tracking index while retaining the mechanical contribution of the glass phase. The manufacturer-published CTI is 600 V under IEC 60112:2003 solution A. Under IEC 60664-1:2020 insulation-coordination practice, this value supports material group I classification, whereas standard glass-filled PBT grades with 250–300 V CTI values fall in material group IIIa or IIIb. The product is encountered in molded electrical insulating components such as sealed connector housings, terminal blocks, power-module carriers, relay cases, and busbar supports where pollution degree 2 or 3 contamination is expected. The grade is not simply a standard 30 wt% glass-filled PBT with a higher filler level; the CTI response is supplied by an additive and matrix-stabilization system that changes the failure chemistry under surface electrical stress.

    Why Glass-Fiber Content Alone Does Not Define Tracking Resistance

    Comparative tracking index is a surface-failure metric. Under IEC 60112:2003, the test applies 50 drops of 0.1 % ammonium chloride solution at 30 s intervals between platinum electrodes, and the highest voltage at which a specimen survives without tracking is recorded. Unfilled PBT typically shows CTI above 500 V. Adding 30 wt% glass fiber to a general-purpose polyester lowers the value into the 250–300 V band because the fiber-matrix interface creates fine surface discontinuities, local electric-field concentrations, and paths for carbonized residue to propagate. In CG7030, the tracking-resistant matrix is formulated so that decomposition products under low-current arcing are less likely to form conductive char. The result is a 600 V CTI classification without moving to a higher-cost polymer family. However, CTI is not a substitute for dielectric strength or impulse-withstand data, and the value can shift downward if the part surface is heavily abraded, contaminated with mold-release agents, or compounded with color concentrates that introduce polar residues.

    Moisture control is the first processing constraint. PBT hydrolyzes above its melting temperature; a residual moisture content above 0.02 wt% produces molecular-weight reduction during the first 30 s of melt residence. The compound should be dried at 120 °C for 4–6 h in a desiccant hopper dryer with a dew point of -30 °C or lower. If the molding floor ambient relative humidity exceeds 60 %, shortened drying produces surface splay and inconsistent weld-line strength. General-purpose low-compression screws have been used on production lines; a compression ratio of 2.0–2.5 and a metering-zone length of at least 5 diameters limit fiber breakage. Barrel set temperatures are typically 240–270 °C, with a melt-temperature ceiling of 270 °C. Total residence time in the heated barrel should not exceed 5 min; longer times generate black specks and local CTI loss at the melt pool. Screw rotation speed is held between 50–100 rpm and back pressure between 0.5–1.0 MPa. Mold temperature is set at 60–100 °C. Higher mold temperatures reduce orientation stress and improve surface consolidation but lengthen cycle time; lower mold temperatures produce dull surfaces, higher visible weld lines, and greater in-flow/transverse shrinkage differences.

    Hot-runner systems present an additional thermal-history risk. Manifold temperatures above 270 °C have produced gate blush and surface splay on valve-gated tools even when pre-drying was correct. PBT-specific pressure-volume-temperature data should be used in mold simulation; generic polymer data underestimates specific volume at 250–270 °C and can cause short shots in connector walls below 0.8 mm. Vent depth for a glass-filled PBT is typically 0.01–0.02 mm; deeper vents flash due to low melt viscosity. Vent pins placed at weld lines prevent gas burns that locally depress tracking resistance. Batch-to-batch fiber-length variation after compounding is visible in notched Charpy results; shifts of ±1.5 kJ/m² around the nominal value are not unusual and do not by themselves indicate improper molding.

    Mold Filling Pressure, Gate Freeze Time, and Shrinkage Anisotropy

    For a 2 mm plaque mold, flow-direction mold shrinkage is typically 0.4–0.6 %, and transverse shrinkage is 0.9–1.3 %, measured on specimens prepared according to ISO 294-3 or ISO 294-4. This anisotropy occurs because glass fibers orient in the fill direction and constrain flow-direction contraction. The resulting difference must be compensated in tooling for rectangular connector housings and latch geometries; otherwise, post-molding warpage appears after moisture conditioning. Injection pressure measured at the nozzle is commonly 80–140 MPa, depending on flow length and gate size. Holding pressure is set at 60–80 % of injection pressure. Gate freeze time should be determined from the part mass plateau, not from machine timers; with edge gates of 1.0–1.5 mm thickness, gate freeze typically occurs within 3–6 s for a 2 mm wall. Weld-line tensile strength in glass-filled PBT falls to 40–60 % of the base value. For CG7030, weld lines arising from multi-gate filling should be positioned away from creepage surfaces because fiber-poor and matrix-rich local regions can alter tracking behavior. When part thickness exceeds 3 mm, cavity thermal uniformity is more critical than absolute mold temperature; thermal gradients above 10 °C across the cavity have produced measurable flatness variation in production runs.

    PropertyTest standardTypical value
    DensityISO 1183-11.59 g/cm³
    Tensile stress at breakISO 527-1/-2130 MPa
    Tensile elongation at breakISO 527-1/-22.5 %
    Flexural strengthISO 178210 MPa
    Flexural modulusISO 1789,000 MPa
    Charpy notched impactISO 179-1/1eA8.0 kJ/m²
    Heat deflection temperature at 1.8 MPaISO 75-1/-2200 °C
    Comparative tracking indexIEC 60112:2003600 V

    The values are representative datasheet values; they are not guaranteed specification limits and vary with specimen conditioning, tooling, and fiber orientation.

    Compared with general-purpose 30 wt% glass-filled PBT, DURANEX CG7030 differs primarily in contaminated-surface tracking resistance. Standard PBT-GF30 grades frequently show CTI values in the 250–300 V range and are therefore assigned to material group IIIa or IIIb under IEC 60664-1:2020. DURANEX CG7030 at 600 V moves the creepage design basis toward material group I. The mechanical profile remains close to standard PBT-GF30: the glass fiber supplies stiffness, while the CTI-enhancing package differentiates the surface failure mode. Compared with unfilled high-CTI PBT, the 30 wt% glass-fiber content raises flexural modulus from approximately 2,600 MPa to 9,000 MPa but also increases anisotropic shrinkage and warpage. Compared with PPS-based high-CTI grades, PBT processes at lower mold temperatures and lower barrel temperatures, but it has a lower continuous-use temperature and must be protected from hot moisture and alkaline environments. The material is therefore selected where the design needs glass-reinforced stiffness and creepage reduction simultaneously, not where the highest thermal or chemical resistance is the primary requirement.

    When CG7030 Replaces Standard PBT GF30 in Connector Housings

    If the part is a multi-pin connector housing under IEC 60664-1:2020 insulation coordination, the material group assigned to the insulator directly determines the minimum creepage distances for a given working voltage and pollution degree. A material with CTI 600 V is material group I; a material with CTI 250–399 V falls in material group IIIa. The dimensional benefit becomes relevant where working voltage exceeds 400 V and pollution degree 3 is specified, because the required creepage distance can be smaller for material group I than for lower CTI classes. Replacing a standard glass-filled PBT with CG7030 can permit closer pin pitch without changing part outline, provided clearance and solid-insulation requirements are independently satisfied. CTI alone does not cover transient overvoltages or bulk dielectric breakdown; impulse withstand voltage must still be verified under IEC 60664-1:2020. For high-voltage direct-current connectors above 800 V, published data for this specific formulation is limited, and field validation of creepage paths in the molded geometry is required.

    The material is supplied in moisture-barrier packaging. Once opened, pellets should be dried before molding, and open storage in humid plants should be limited. Moisture absorption after 24 h at 23 °C and 50 % RH for PBT-based compounds is approximately 0.2 %. Long-term exposure to hot water or steam above 80 °C, strong alkalis, or amine-containing additives can degrade the polyester matrix and reduce weld-line toughness. Compliance documentation from the material supplier should be obtained for EU REACH, RoHS Directive 2011/65/EU, and UL yellow-card recognition. Processing constraints and aging behavior must be evaluated by the end user because CTI and mechanical properties are influenced by fiber orientation, moisture, and molded-surface contamination.