    Specifications
    HS Code 519239
    Volume Resistivity Ohm Cm 1E16
    Molding Shrinkage Percent 0.2-0.5
    Ul94 Flammability HB

    As an accredited Polyplastics DURANEX® PBT+GF30%-CTI 457EV factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyplastics DURANEX® PBT+GF30%-CTI 457EV is supplied in 25 kg moisture-barrier bags, securely palletized, with 40 bags per pallet.
    Container Loading (20′ FCL) This 20′ FCL container is loaded with Polyplastics DURANEX® PBT+GF30%-CTI 457EV chemical material, securely palletized, strapped, and stowed for ocean freight.
    Shipping Polyplastics DURANEX® PBT+GF30%-CTI 457EV is a non-hazardous, non-regulated thermoplastic polyester resin (PBT with 30% glass fiber). Ship in sealed moisture-barrier bags/containers; protect from moisture, heat, sunlight, static, and physical damage. Label with product name and lot number. No UN number or hazard class applies.
    Storage Store Polyplastics DURANEX® PBT+GF30%-CTI 457EV in its original sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and contamination. Keep containers closed, avoid dust, and maintain stable conditions. Follow the SDS and manufacturer guidance; dry material as recommended before processing.
    Shelf Life Shelf life is 12 months when stored unopened in original packaging at room temperature, dry, and protected from direct sunlight.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF30%-CTI 457EV prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyplastics DURANEX® PBT+GF30%-CTI 457EV is a 30% glass-fiber-reinforced polybutylene terephthalate injection-molding grade. The commercial designation “CTI 457EV” identifies the comparative tracking index performance class under IEC 60112, with a manufacturer-published nominal value of 600 V. The grade is specified for high-voltage electrical and electronic equipment, automotive power-distribution components, and other applications requiring reduced creepage distance, stable insulation behavior, and moderate mechanical load-bearing capacity. Representative manufacturer-published room-temperature values for natural or black injection-molded specimens are summarized in Table 1.

    Property Nominal value Test method
    Density 1.62 g/cm³ ISO 1183-1
    Tensile strength at break 130 MPa ISO 527-1/-2
    Tensile elongation at break 2.0 % ISO 527-1/-2
    Flexural strength 195 MPa ISO 178
    Flexural modulus 9,200 MPa ISO 178
    Charpy notched impact strength, 23 °C 7.0 kJ/m² ISO 179-1/1eA
    Charpy unnotched impact strength, 23 °C 50 kJ/m² ISO 179-1/1eU
    Heat deflection temperature, 1.80 MPa 200 °C ISO 75-1/-2
    Melting temperature 225 °C ISO 11357-1/-3
    Molding shrinkage, flow direction 0.4 % ISO 294-4
    Molding shrinkage, transverse direction 0.9 % ISO 294-4
    Water absorption, 23 °C / 24 h 0.1 % ISO 62
    Comparative tracking index 600 V IEC 60112
    Volume resistivity 1×1016 Ω·cm IEC 60093
    Surface resistivity 1×1015 Ω IEC 60093
    Dielectric strength 20 kV/mm IEC 60243-1
    Flammability V-0 at 0.75 mm UL 94

    The CTI value is determined on a flat specimen using an aqueous 0.1% ammonium chloride electrolyte with 20 mm³ droplet volume and 4 mm electrode spacing. A result of 600 V places the material in Material Group I under IEC 60664-1. The tabulated values should not be treated as design minima; they are nominal values conditioned under standard laboratory atmosphere of 23 °C and 50% relative humidity. Pigmented versions, regrind-containing moldings, and thin-wall sections may shift tracking, mechanical, and flammability performance.

    How Does 457EV Compare with Unfilled PBT and General-Purpose 30% Glass-Filled PBT?

    General-purpose 30% glass-filled PBT grades are typically classified in Material Group IIIa or IIIb because their comparative tracking index values often fall below 400 V. The 457EV formulation is specifically stabilized to raise CTI to 600 V while retaining the mechanical stiffness expected from 30% glass reinforcement. Compared with unfilled PBT, the glass content raises the heat deflection temperature from approximately 60 °C to 200 °C at 1.80 MPa and reduces mold shrinkage from approximately 1.5–2.0% to 0.4–0.9% depending on flow direction. The trade-off is a loss of ductility and a more anisotropic shrinkage pattern than unfilled PBT.

    Compared with high-CTI mineral-filled PBT compounds, 457EV maintains higher tensile strength and flexural modulus because of the glass-fiber reinforcement. Mineral-filled tracking-resistant PBT grades commonly fall in the 4,000–6,000 MPa flexural modulus range, whereas 457EV is listed at approximately 9,200 MPa. The formulation details of the matrix stabilization and flame-retardant system are not disclosed in published safety data sheets or commercial datasheets; the certified end points are the IEC 60112 CTI value and the UL 94 V-0 rating at 0.75 mm.

    Processing of 457EV follows standard 30% glass-filled PBT practice with tighter moisture control. Drying in a desiccant dryer at 120 °C for 4 h to a dew point of -30 °C or lower is required when the measured moisture content exceeds 0.02% by weight. In production-scale molding, regrind exposed to ambient air for more than 30 min at relative humidity above 60% should be re-dried before processing. Melt temperatures of 250–270 °C are recommended. Mold temperatures below 60 °C can produce resin-rich surfaces and reduce tracking resistance, while mold temperatures above 90 °C increase cycle time without proportional improvement in weld-line strength.

    At the compounding step, 30% glass loading is normally produced on a co-rotating twin-screw extruder with L/D ratio between 40:1 and 48:1. Screw speeds above 300 rpm can generate local melt temperatures above 280 °C, causing molecular weight loss and measurable CTI reduction in finished parts. Production lots therefore benefit from torque-controlled compounding and in-process melt-temperature measurement at the die plate. The compounded pellets should be packaged with moisture-barrier liners because PBT can absorb atmospheric moisture to above 0.05% within hours of open storage in humid environments, which is sufficient to cause hydrolysis-related surface defects and electrical-performance drift during injection molding.

    The Material Group I Threshold in IEC 60664-1 Creepage Calculations

    Under IEC 60664-1, a CTI of 600 V places an insulating material in Material Group I. This classification directly affects creepage distance calculations in connectors, terminal blocks, power distribution units, and busbar insulation. For a working voltage of 800 V and pollution degree 2, the minimum creepage distance for Material Group I is substantial shorter than for Material Group IIIa. The reduction can approach a factor of 2.0–2.5 depending on overvoltage category and equipment-specific creepage tables. For electric-vehicle power distribution units with constrained packaging, this can permit a reduction in terminal pitch from approximately 8.0 mm to 4.5 mm in certain connector families, although final values must be calculated from the appliance-specific tables and validated by dielectric withstand, tracking, and thermal-cycling tests.

    Material group CTI range Creepage-distance consequence
    I 600 V ≤ CTI Shortest creepage distance for equivalent working voltage
    II 400 V ≤ CTI < 600 V Incremental creepage distance increase
    IIIa 175 V ≤ CTI < 400 V Substantial creepage distance increase
    IIIb 100 V ≤ CTI < 175 V Largest creepage distance where materials are accepted

    Material Group I does not eliminate creepage distance; it reduces the required distance relative to lower-group materials. Connector designers must still account for pollution degree, altitude, coating, and functional insulation requirements from IEC 60664-1 and the relevant end-product standard. The high CTI of 457EV is most relevant to pollution degree 2 and 3 environments in which surface contamination can form conductive tracks across molded insulation barriers. In clean-room or sealed electronic compartments, the practical benefit is smaller because surface contamination is less likely to initiate tracking.

    When Flow Orientation and Weld-Line Position Are Evaluated in High-Voltage Housings

    Glass-fiber orientation in thin-walled sections creates anisotropic shrinkage and local CTI variation at weld lines. If a dual-gated busbar housing positions a weld line across a high-voltage conductor path, the tracking resistance measured at the weld line can be lower than the nominal CTI obtained on a homogeneous specimen. Tooling should avoid gates on opposite sides of narrow creepage barriers, or use sequential valve gating to move the weld line into a non-energized rib or structural wall. Glass-fiber weld-line flexural strength retention in 30% GF PBT is commonly cited at 50–65% of solid-material strength under flexural loading, depending on gate configuration, melt temperature, and packing pressure. Flow simulation should be used before tool construction to identify fiber-orientation-dominated shrinkage differentials and weld-line locations in parts with wall thickness below 2.0 mm.

    Chemical compatibility of 457EV follows general PBT behavior. Repeated exposure to hot water or ethylene glycol–water mixtures above 60 °C can promote hydrolytic chain scission. Published long-term coolant-aging data for this specific grade is limited. Applications with continuous immersion in hot coolant require hydrolysis-resistant PBT grades or alternative polymers. Contact with strong alkaline solutions, amines, and some chlorinated hydrocarbons should be evaluated by exposure testing under the intended service regime. Automotive fluids may contain detergent or additive packages that alter surface resistivity; insulation resistance after exposure must be verified under the applicable system-level standard.

    The grade is used in high-voltage connectors, terminal blocks, busbar holders, power distribution units, charging inlet insulation components, and related electric-vehicle electrical applications. It is less suited to low-voltage mechanical-only parts where unfilled PBT may be more cost-effective. Selection should be based on the full manufacturer-approved design data for the intended color, thickness, and regrind content, because electrical and flammability certifications are thickness- and formulation-dependent.