| HS Code | 298809 |
| Density | 1.53 g/cm³ |
| Glassfibercontent | 30% |
| Tensilestrength | 135 MPa |
| Elongationatbreak | 2.5% |
| Flexuralmodulus | 9,000 MPa |
| Flexuralstrength | 200 MPa |
| Charpynotchedimpactstrength23c | 6.5 kJ/m² |
| Heatdeflectiontemperature182mpa | 210 °C |
| Ul94flammability | HB |
| Waterabsorption24h | 0.20% |
| Moldingshrinkage | 0.3-0.7% |
| Volumeresistivity | 1E16 Ω·cm |
| Dielectricstrength | 20 kV/mm |
| Arcresistance | 120 s |
| Meltingpoint | 224 °C |
| Coefficientoflinearthermalexpansion | 3E-5 /°C |
| Rockwellhardness | M90 |
As an accredited Polyplastics DURANEX® PBT+GF30% 3300 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically supplied in 25 kg moisture-barrier bags, 40 bags per pallet, giving 1,000 kg total per pallet. |
| Container Loading (20′ FCL) | Polyplastics DURANEX® PBT+GF30% 3300 is loaded dry, clean, palletized, and securely stowed in a 20-foot FCL container for shipment. |
| Shipping | Shipping description: Polyplastics DURANEX® PBT+GF30% 3300, non-hazardous glass-fiber-reinforced PBT resin pellets; not classified as dangerous goods for transport (no UN number). Ship in original sealed moisture-barrier packaging, keep dry at ambient temperature, avoid direct sunlight, and follow SDS/local regulations. |
| Storage | Store DURANEX® PBT+GF30% 3300 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original containers/pallets closed, clean, and labeled; protect bags from punctures and humidity. Avoid dust generation and prolonged high-temperature exposure. Rotate stock, follow the SDS and local regulations, and dry material per supplier recommendations before processing. |
| Shelf Life | Shelf Life: Stable under normal storage; no specific expiry; store cool, dry, sealed, away from heat, moisture, and sunlight. |
Competitive Polyplastics DURANEX® PBT+GF30% 3300 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Polyplastics DURANEX® PBT+GF30% 3300 is an injection-molding grade of polybutylene terephthalate reinforced with nominally 30% by mass glass fiber. Under ISO 1043-1, the grade is designated PBT-GF30. The compound is supplied as cylindrical pellets and is intended for melt processing on conventional reciprocating-screw injection molding machines with 18:1 to 22:1 L/D general-purpose screws. The glass-fiber network raises stiffness, strength, and heat deflection temperature compared with unfilled PBT, but it also introduces melt-flow anisotropy and weld-line strength reduction. Typical unfilled PBT density near 1.31 g/cm³ rises to approximately 1.53 g/cm³ for the 30% glass-filled grade because E-glass fiber density is approximately 2.54 g/cm³ to 2.60 g/cm³. The 30% mass fraction therefore corresponds to roughly 18% by volume reinforcement. The grade is used in connectors, relay housings, power tool housings, and under-hood automotive components requiring tensile stress above 130 MPa and heat deflection temperature above 200°C under 1.8 MPa load. Property claims in the following sections are tied to the test designations indicated; they are typical values from supplier literature, not batch-specific specifications.
Published processing guidance for reinforced PBT grades places melt temperature between 240°C and 270°C. The lower boundary is set by inadequate fiber wet-out and high melt viscosity; the upper boundary is set by thermal degradation of the ester linkage. Thermogravimetric analysis of unfilled and glass-filled PBT generally shows measurable mass loss above 280°C under inert atmosphere, but residence-time effects begin below that threshold in oxidative melt conditions. On a production floor, the practical limit is not the barrel set-point alone; it is the integral of temperature and time in the screw channel, check ring, and hot runner. For a 50-mm screw with 20:1 L/D operating at a cycle time of 20 s to 30 s, the actual melt residence time is commonly 2 to 5 times the shot-capacity residence time when hot-runner dead zones are included. Molding technicians therefore limit buffer volume and avoid shear heating above 10°C to 15°C over barrel set-point. Pre-drying is mandatory: 4 h to 8 h at 120°C in a dehumidifying hopper dryer with a dew point of ≤ −30°C, targeting moisture below 0.02% by mass per ISO 15512:2019. Resin that has exceeded moisture limits during storage at ambient relative humidity > 60% should be re-dried before use. Barrel temperature profiles are normally set from 230°C in the rear zone to 260°C at the nozzle, with rear-barrel cooling to prevent pellet bridging.
In thin-wall connector bodies with nominal wall thickness of 0.8 mm to 1.6 mm, the melting and flow behavior of DURANEX 3300 is controlled by mold temperature and gate design rather than by barrel temperature alone. The glass fibers reduce linear mold shrinkage relative to unfilled PBT; typical parallel-to-flow shrinkage for a 30% glass-filled PBT is in the range of 0.3% to 0.5%, while transverse shrinkage can be 0.7% to 1.0% due to fiber orientation. This differential shrinkage is a primary cause of out-of-plane warpage in box-like housings. Mold temperature of 60°C to 100°C reduces frozen-in orientation and raises surface gloss; lower mold temperatures of 30°C to 50°C shorten cycle time but increase post-mold dimensional change. In electrical connector applications, comparative tracking index tested per IEC 60112:2009 is typically between 250 V and 300 V for PBT-GF30 compositions, but published data for DURANEX 3300 under the exact solution A conditions should be confirmed from the supplier certificate of analysis. Connector designs requiring higher tracking resistance often select a different DURANEX grade, because glass reinforcement near the surface can create insulation weak points if the surface resin layer is depleted during filling or post-mold abrasion.
Measurement of fiber orientation in thin-wall moldings shows that the shell-core structure is asymmetric: fibers align primarily in the flow direction in the shell layer, while the core region may contain more transverse orientation due to fountain flow and jetting. This structure produces anisotropic tensile modulus. For a 30% glass-filled PBT, flow-direction tensile modulus may be 9,000 MPa to 10,000 MPa, while cross-flow modulus may be 6,000 MPa to 7,000 MPa. The ratio between these values, rather than the datasheet average, controls snap-fit deflection and hole-position stability after conditioning. In multi-gate connector housings, weld lines form where melt fronts meet; weld-line tensile strength in glass-filled PBT is commonly 50% to 70% of the virgin tensile strength. Sequential valve gating or moving the weld line to a low-stress region is used when the housing must pass a drop test or thermal shock test per IEC 60068-2-14. Mold flow simulation should be calibrated with measured fiber orientation because standard Cross-WLF viscosity models do not capture fiber mobility. Published data for DURANEX 3300 fiber orientation tensors in specific connector geometries is limited; therefore, tool trials remain necessary for critical dimensions.
The following table compares representative published values for DURANEX 3300 with unfilled PBT. Values are typical at 23°C unless otherwise noted; they should not be used as guaranteed minimum or maximum specification limits without reviewing the supplier’s product data sheet.
| Property | Test standard | DURANEX 3300 GF30 | Unfilled PBT |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 1.53 g/cm³ | 1.31 g/cm³ |
| Tensile stress at break | ISO 527-2:2012 | 140 MPa | 57 MPa |
| Tensile strain at break | ISO 527-2:2012 | 2.5% | >20% |
| Flexural modulus | ISO 178:2019 | 9,000 MPa | 2,400 MPa |
| Flexural strength | ISO 178:2019 | 200 MPa | 80 MPa |
| Charpy notched impact strength | ISO 179-1:2010 | 8.0 kJ/m² | 3.0 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2:2013 | 205°C | 60°C |
| Water absorption, 24 h | ISO 62:2008 | 0.07% | 0.08% |
The tensile stress increase from roughly 57 MPa to 140 MPa is the direct result of fiber-matrix stress transfer; the difference in elongation at break, from a ductile unfilled PBT response to 2.5% for the glass-filled grade, indicates that DURANEX 3300 should not be substituted into snap-fit designs that require large post-yield deformation. Heat deflection temperature under 1.8 MPa shifts from near 60°C for unfilled PBT to approximately 205°C for the 30% glass-reinforced grade, which permits short-term contact with painted or powder-coated metal parts in engine compartments. Notched impact behavior remains sensitive to fiber orientation, gate position, and moisture conditioning; the tabulated 8.0 kJ/m² value is a typical value and may be lower in weld-line regions or at −30°C. Because PBT embrittles when hydrolyzed, values obtained on dry-as-molded specimens may not represent parts conditioned at 85°C/85% RH per IEC 60068-2-78.
For applications currently using an unfilled PBT or a low-glass PBT such as a 10% glass-filled compound, the main processing difference is the higher melt viscosity and faster gate freeze of DURANEX 3300. Melt volume-flow rate for a 30% glass-filled PBT is typically in the range of 12 cm³/10 min to 16 cm³/10 min at 250°C/2.16 kg per ISO 1133-1:2022, compared with higher values for unfilled PBT. Because the glass fibers raise thermal conductivity slightly, the gate sealing time is shorter at the same wall thickness; holding-pressure time must be reduced before full gate solidification to avoid sink marks. A 30% glass-filled PBT generally exhibits lower mold shrinkage than a 10% glass-filled PBT, but the difference between flow and transverse shrinkage is larger, creating more warpage in complex shapes. Compared with mineral-filled PBT grades, DURANEX 3300 has higher tensile strength and lower density, but it also has more visible surface fiber orientation and reduced flow uniformity in long ribs. Compared with impact-modified PBT grades, the 30% glass-filled grade has higher stiffness but lower multiaxial impact resistance; notched Charpy values may be similar at room temperature but degrade more rapidly at subzero temperatures. For parts requiring UL 94 V-0 performance, a flame-retardant DURANEX grade should be selected, because standard PBT-GF30 grades are typically rated HB under UL 94.
Moisture conditioning, chemical exposure, and mechanical load limits must be reviewed before replacing metal or heat-resistant polyamide. PBT ester bonds are susceptible to hydrolysis in hot, humid, and alkaline environments; prolonged exposure above 80°C in water or high-pH coolant can reduce molecular weight and tensile strength. The combination of DURANEX 3300 with amine-based additives or uncoated copper that releases amine complexes should be avoided where long-term thermal aging is required because transesterification or discoloration may occur. Under hood, continuous use temperature for a 30% glass-filled PBT is generally below 140°C, with short-term peaks above 180°C allowed only for limited duration. Resistance to automotive fluids per ISO 175:2010 is composition-dependent; published data for DURANEX 3300 in biodiesel or aggressive acidified condensates is limited, so compatibility testing on finished parts is required. Because black specks, gas streaks, and screw-slippage can occur when the feed zone runs hotter than 90°C to 110°C, rear-barrel cooling should be verified on the production machine.