    HS Code 285318
    Density 1.47 g/cm³
    Glass Fiber Content 20 %
    Tensile Strength 120 MPa
    Tensile Elongation At Break 3.0 %
    Flexural Modulus 6500 MPa
    Flexural Strength 180 MPa
    Charpy Notched Impact Strength 6 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 200 °C
    Melting Point 224 °C
    Water Absorption After 24 H 0.07 %
    Molding Shrinkage 0.3-0.6 %
    Flammability Rating UL94 HB

    As an accredited Polyplastics DURANEX® PBT+GF20% 3200 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-proof bags, Polyplastics DURANEX® PBT+GF20% 3200 supplied as pellets on pallets.
    Container Loading (20′ FCL) 20′ FCL container loading of Polyplastics DURANEX® PBT+GF20% 3200 resin in bags on pallets, properly secured for export shipment.
    Shipping Polyplastics DURANEX® PBT+GF20% 3200 is shipped as non-hazardous glass-fiber-reinforced PBT pellets in sealed moisture-barrier 25 kg bags, palletized and stretch-wrapped. Keep dry, away from direct sunlight and heat, and handle carefully to avoid bag damage or contamination.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep original containers tightly closed and clearly labeled. Prevent dust generation and static buildup. Avoid contact with strong oxidizers and incompatible chemicals. Maintain good housekeeping and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months when stored dry, cool, and in original unopened packaging, protected from moisture, heat, and sunlight.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF20% 3200 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyplastics DURANEX® PBT+GF20% 3200 is a polybutylene terephthalate injection-moulding compound reinforced with 20% glass fibre by mass. The grade is supplied as cylindrical pellets and is specified where unfilled PBT lacks creep resistance or heat deflection under structural load, but where a 30% glass-fibre PBT would generate excessive melt pressure or anisotropic warpage in flat housings. Manufacturer-published physical data measured to ISO 1183-1:2019 list a density of 1.45 g/cm³. Mechanical properties determined to ISO 527-1/-2 include a tensile stress at break of 95 MPa and a tensile strain at break of 2.5%. Flexural modulus obtained to ISO 178:2019 is reported as 5,600 MPa, with flexural strength near 150 MPa. Heat deflection temperature under 1.8 MPa load to ISO 75-1/-2 is approximately 205 °C. Charpy notched impact strength to ISO 179-1/1eA is published as 5.5 kJ/m². These values are representative lot-average figures; actual moulded part performance depends on gate design, fibre orientation, and thermal history.

    PropertyTest methodRepresentative valueUnit
    DensityISO 1183-1:20191.45g/cm³
    Tensile stress at breakISO 527-1/-295MPa
    Tensile strain at breakISO 527-1/-22.5%
    Flexural modulusISO 178:20195,600MPa
    Flexural strengthISO 178:2019150MPa
    Charpy notched impact strengthISO 179-1/1eA5.5kJ/m²
    Heat deflection temperature, HDT/AISO 75-1/-2205°C

    Before melt processing, moisture must be reduced below 0.02%. PBT hydrolyses rapidly at melt temperature when wet; pellets stored at ambient relative humidity above 60% for more than 30 minutes must be dried in a dehumidifying hopper dryer at 120 °C for 4 to 6 hours, with supply-air dew point below −30 °C. Cylinder settings from rear zone to nozzle are typically 240 °C, 250 °C, 260 °C, and 260 °C; mould-wall temperature is maintained between 40 °C and 80 °C depending on surface finish requirements. Injection speed should be moderate to high, with screw back-pressure between 2 MPa and 5 MPa to avoid glass-fibre attrition. Hold pressure is set at 60–80% of peak injection pressure and held until gate freeze, which in a flat plaque of 2 mm thickness is typically 4 to 8 seconds.

    Production-scale uses reported by injection moulders include automotive relay bases, connector bodies, coil bobbins, sensor housings, and motor brush holders. The glass-fibre mass fraction of 20% supplies sufficient stiffness for snap-fit arms that must retain engagement force after repeated thermal cycling, while still filling sections down to 0.8 mm at practical injection pressures below 100 MPa. In connectors exposed to short-duration vapour-phase heating, the heat deflection temperature above 200 °C reduces softening, but reflow soldering is not a recommended process because the thermal excursion exceeds the continuous-use ceiling for PBT. Published data for long-term hot-oil or hot-air ageing of this specific grade in engine compartments are limited; qualification must therefore be performed under the end-user’s component-specific test protocol.

    What distinguishes the 20% glass-fibre grade from adjacent DURANEX® 3100 and 3300 formulations?

    Within the DURANEX glass-reinforced series, the 3100 formulation at 10% glass fibre carries lower published density near 1.37 g/cm³, tensile stress at break near 75 MPa, and flexural modulus near 3,500 MPa. The 3300 formulation at 30% glass fibre increases density to approximately 1.53 g/cm³, tensile stress at break to 120 MPa, and flexural modulus to 8,000 MPa. The 3200 grade sits between them: its stiffness is roughly 60% higher than the 10% glass-fibre grade, while its melt viscosity is lower than the 30% grade, permitting longer flow lengths before pressure limitation. Heat deflection temperature follows fibre loading, but the increment from 20% to 30% is often only 5 °C to 10 °C; the larger practical difference is mould shrinkage anisotropy. The 20% grade may exhibit flow-direction shrinkage near 0.5% and transverse shrinkage near 0.9%, while higher glass loading can widen directional spread depending on gate design.

    GradeGlass fibre mass fractionDensityTensile stress at breakFlexural modulusHeat deflection temperature, HDT/A
    DURANEX® 310010%1.37 g/cm³75 MPa3,500 MPa195 °C
    DURANEX® 320020%1.45 g/cm³95 MPa5,600 MPa205 °C
    DURANEX® 330030%1.53 g/cm³120 MPa8,000 MPa210 °C

    When replacement of unfilled PBT with 3200 is evaluated, the design group should compare flexural modulus, not tensile strength alone. Unfilled PBT typically has flexural modulus near 2,500 MPa; the 5,600 MPa stiffness of the glass-filled grade changes deflection of a beam or snap-fit by a factor of more than two, which can invalidate existing latch engagement or assembly force calculations. Creep resistance under continuous load is improved, but the glass-filled grade is more notch-sensitive at sharp corners; a fillet radius below 0.3 mm can reduce Charpy notched impact strength from 5.5 kJ/m² to below 3 kJ/m² in moulded parts because fibre ends concentrate stress.

    When the 3200 grade is substituted for unfilled PBT in existing tools

    Substitution into an existing unfilled PBT mould demands revalidation of filling, packing, and gate freeze. The glass-fibre compound’s higher melt viscosity may require increasing nozzle and metering-zone set points by 10 °C to 20 °C; however, melt temperature must not exceed 270 °C for extended hold times because thermal degradation of the polybutylene terephthalate backbone accelerates above 260 °C in the presence of residual oxygen. Screw rotation should be limited to 80 to 120 rpm for a 40 mm diameter screw to reduce fibre breakage. A general-purpose nylon screw with a compression ratio of 2.5:1 is often suitable. The metering section should be free of damaged screw flights or worn non-return valves, because glass-fibre abrasion rapidly enlarges clearance and causes inconsistent shot mass.

    Tool hot-runner systems for 20% glass-filled PBT should use externally heated manifolds with thermal uniformity better than ±5 °C across the nozzle tips; poor thermal uniformity produces non-uniform fibre distribution at knit lines. Cold-runner gates with land lengths below 1.0 mm and sprue pullers with adequate taper reduce hot-tip drool. Vent depths of 0.01 mm to 0.02 mm are recommended along the end-of-fill; deeper vents can flash because the melt crosses the cavity quickly during fast injection. Gas traps can be placed at knit-line intersections to reduce burn marks caused by decomposition of silane-based glass sizing.

    Compared with a 20% glass-fibre polyamide 66 compound, DURANEX® 3200 absorbs significantly less moisture at equilibrium. Data to ISO 62 show PBT water absorption near 0.2% at 23 °C and 50% RH, whereas PA66 glass-fibre grades often reach 1.5–2.0%. This keeps dielectric properties and dimensional changes more stable in humid environments. The trade-off is lower low-temperature toughness: PBT GF20 parts are generally brittle below −20 °C, so impact resistance should be verified to ISO 179-1/1eA if deployment extends to cold climate. PBT’s fast crystallisation also yields shorter moulding cycles than many polyamide formulations.

    Regulatory documentation for DURANEX 3200 must be requested from Polyplastics for each production lot. Typical statements cover RoHS 2011/65/EU and REACH SVHC compliance; FDA food-contact status under 21 CFR 177.166 should not be assumed for all colours and lots, because pigments and glass sizing may differ. Electrical insulation testing on moulded parts is often performed to IEC 60093 for volume resistivity and IEC 60243-1 for dielectric strength; published values for this exact grade may vary with weld lines and moisture content. Unless the part is dried and tested under controlled conditions, surface leakage can dominate.

    Operational boundaries are as follows: residual moisture above 0.02% before moulding leads to splay, reduced tensile strength, and embrittled knit lines; melt temperatures above 270 °C for more than 10 minutes cause black specks from degraded sizing and loss of notched impact strength; regrind levels above 20% in the feed blend can shift mould shrinkage and lower impact strength because glass-fibre length is reduced. Contact with strong alkalis and hot concentrated acids should be avoided; PBT is not recommended for continuous immersion in boiling water without hydrolysis-stabilised grades.