Polyplastics Duranex Pbt Gf15 70g15

Polyplastics DURANEX® PBT+GF15% 70G15

    • Product Name: Polyplastics DURANEX® PBT+GF15% 70G15
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 910581
    Grade 70G15
    Polymer Type Polybutylene terephthalate (PBT)
    Reinforcement Glass fiber
    Glass Fiber Content 15%
    Density 1.41 g/cm³
    Water Absorption 24h 0.20%
    Tensile Strength 100 MPa
    Elongation At Break 3.0%
    Flexural Modulus 5500 MPa
    Flexural Strength 150 MPa
    Charpy Notched Impact Strength 5.0 kJ/m²
    Heat Deflection Temperature 1 82mpa 205 °C
    Melting Point 224 °C
    Mold Shrinkage Parallel 0.4%
    Mold Shrinkage Perpendicular 0.7%
    Volume Resistivity 1×10^16 Ω·cm
    Dielectric Constant 1mhz 3.6
    Dielectric Dissipation Factor 1mhz 0.002

    As an accredited Polyplastics DURANEX® PBT+GF15% 70G15 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Polyplastics DURANEX® PBT+GF15% 70G15 is packed in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of Polyplastics DURANEX® PBT+GF15% 70G15, securely stowed for export shipment.
    Shipping Polyplastics DURANEX® PBT+GF15% 70G15 is supplied as non-hazardous thermoplastic resin pellets, typically in sealed moisture-barrier bags or 25 kg sacks on pallets. Ship dry, protected from heat, sunlight, and moisture; avoid contamination and rough handling. No special transport regulation applies under normal conditions.
    Storage Store DURANEX® PBT+GF15% 70G15 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep material in original unopened packaging or sealed containers to prevent humidity uptake and contamination. Avoid contact with incompatible chemicals and maintain good housekeeping. Use within the manufacturer’s stated shelf life; dry pellets according to processing recommendations before molding.
    Shelf Life Shelf life is typically 12 months when stored dry, unopened, below 30°C, and protected from moisture and sunlight.
    Free Quote

    Competitive Polyplastics DURANEX® PBT+GF15% 70G15 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Polyplastics DURANEX® PBT+GF15% 70G15 is a short-glass-fibre-reinforced polybutylene terephthalate injection moulding compound containing 15% by mass E-glass fibre. The nominal published density is 1.41 g/cm³ to ISO 1183-1. Representative mechanical values measured on injection-moulded specimens are tensile strength 103 MPa to ISO 527-1/-2, flexural modulus 5.0 GPa to ISO 178, flexural strength 165 MPa, and notched Charpy impact 5.0 kJ/m² to ISO 179/1eA. Heat deflection temperature at 1.8 MPa is approximately 200 °C to ISO 75-1/-2. Published water absorption is 0.1% to ISO 62, and the grade carries a UL 94 HB flame rating. These values place 70G15 between the unfilled DURANEX PBT baseline and the 30% glass-reinforced 70G30 grade, providing a balance of stiffness, dimensional stability, and flow that is not available from either the unfilled or the higher-glass material. The product is intended for injection moulding, not blow moulding or profile extrusion, because the glass fibre raises melt viscosity and requires specific thermal and moisture controls.

    What Limits Melt Stability and Drying Requirements in DURANEX 70G15?

    Polybutylene terephthalate is a semicrystalline polyester whose ester linkages undergo hydrolytic chain scission when the melt contains free moisture. For DURANEX 70G15, pellet moisture above 0.02 wt% before plastication causes measurable loss of melt strength, surface splay, and reduced tensile properties. Pellets are dried in a desiccant dryer at 120 °C for 4–6 h, with supply air dew point of -30 °C to -40 °C, and hopper purge using dry air to prevent re-adsorption. In moulding environments where ambient relative humidity exceeds 60%, open hopper residence time is minimised and the feed throat is kept below 50 °C to prevent condensation. A moisture analyser or weight-loss instrument is used to verify dryness; a Karl Fischer titration value below 0.02% is the operational boundary.

    The melt temperature window is 250–270 °C at the nozzle. Barrel settings are typically rear 250 °C, centre 260 °C, front 260 °C, nozzle 255 °C; the temperature at the hot-runner manifold, if used, should not exceed 270 °C. Prolonged melt residence time above 270 °C darkens the resin, releases degradation products, and reduces molecular weight. Published data for this specific configuration is limited, but general PBT processing guides recommend total plastication time below 15 min at upper melt temperatures. Injection pressure is typically 60–100 MPa hydraulic, with back pressure 0.3–0.5 MPa hydraulic to avoid fibre-matrix separation. Mould temperature is maintained at 60–80 °C to obtain sufficient crystallinity and dimensional stability.

    Thermal degradation and hydrolytic degradation interact: moisture shifts the apparent melt viscosity downward during plastication, which can mislead the moulder into lowering barrel temperature. The apparent viscosity reduction is not process-friendly; it is a sign of molecular-weight loss. Melt viscosity should be monitored by in-line pressure drop across the nozzle or by measuring fill weight under fixed conditions. A reduction in fill weight at constant hold pressure of more than 2–3% over a production shift typically indicates either moisture ingress or gradual chain scission. Drying hoppers should be audited at shift change, and return air outlets checked for pellet fines, because fines consume desiccant capacity and produce inconsistent drying.

    Shrinkage Anisotropy at 15 wt% Glass Loading Is a Processing Variable, Not a Fixed Material Constant

    Glass fibres orient in the direction of melt flow during injection moulding, producing a skin layer of high flow-direction fibre alignment and a core with lower orientation. Published mould shrinkage data for DURANEX 70G15 determined on 60 mm × 60 mm × 2 mm plaques to ISO 294-4 are approximately 0.4–0.6% in the flow direction and 0.7–1.0% transverse to flow. The difference between these directional shrinkages is the primary driver of out-of-plane warpage in flat parts. At 15 wt% glass loading, the anisotropy is less severe than in a 30 wt% grade because the lower fibre volume fraction reduces the path-length difference between oriented and unoriented regions. In practice, this means that a connector body or sensor carrier can be moulded with less warp than with 70G30 when the same gate and wall thickness are used.

    The remaining anisotropy is controlled by gate placement, wall thickness uniformity, and packing pressure decay. A single edge gate produces orientation along the length of a rectangular part; a centre gate produces radial orientation and can create saddle-shaped distortion if the packing time is too short. For wall thickness below 1.0 mm, cooling time is not the dominant cycle segment; gate freeze and packing are. Underpacking before gate freeze permits higher flow-direction shrinkage and warpage. Machine control should therefore use switch-over by cavity pressure or screw position, not by timer, to avoid packing inconsistency. The lower fibre content also reduces mould abrasion relative to 30% glass grades, although chrome-plated or bimetallic barrels and screws are still recommended for production runs exceeding 500,000 cycles because the glass still abrades unhardened screw flights.

    Comparative Property Matrix Against Unfilled PBT and 30% Glass Fibre Grade

    The following values are representative published data for injection-moulded specimens. They are not batch certificates and should not be used as specification limits.

    PropertyUnitTest methodDURANEX 70G15DURANEX 3300 unfilled PBTDURANEX 70G30
    Densityg/cm³ISO 1183-11.411.311.52
    Tensile strengthMPaISO 527-1/-210355130
    Flexural modulusMPaISO 1785,0002,4008,500
    Notched Charpy impactkJ/m²ISO 179/1eA5.03.08.0
    Heat deflection temperature at 1.8 MPa°CISO 75-1/-220060205
    Mould shrinkage, flow direction%ISO 294-40.4–0.61.5–2.00.2–0.4
    Mould shrinkage, transverse direction%ISO 294-40.7–1.01.5–2.00.5–0.7
    Water absorption, 24 h%ISO 620.10.10.1

    The matrix shows that 70G15 retains 79% of the tensile strength of 70G30 and 59% of the flexural modulus, while providing lower density and improved mouldability in thin-wall geometries. Static tensile and flexural data do not capture weld-line strength or dynamic fatigue; the lower glass content should not be interpreted as a direct substitution for 30% glass in load-bearing structural brackets without part-level validation. The unfilled baseline is included only to show the reinforcing effect; it is not recommended for applications requiring elevated-temperature load-bearing.

    Electrical insulation characteristics reported for glass-reinforced PBT grades include volume resistivity on the order of 1015 ohm·cm to IEC 60093 and dielectric strength above 15 kV/mm to IEC 60243-1. Comparative tracking index of glass-reinforced PBT is typically 250 V to IEC 60112, although the presence of glass fibres lowers tracking resistance relative to unfilled PBT. For DURANEX 70G15 specifically, batch certificates should be consulted because formulations and pigment packages can shift electrical values. Hydrolytic stability is an operational limitation: continuous service in hot water above 60 °C, steam, or alkaline media attacks the ester linkage and should be excluded from the design envelope. Aromatic hydrocarbons, aliphatic oils, and common automotive greases are generally compatible at normal operating temperatures, but chlorinated solvents and strong acids degrade PBT.

    When the 15% Glass Fibre Grade Replaces a 30% Glass Fibre Grade in Thin-Wall Connectors

    In thin-wall connector housings with wall thickness below 1.0 mm, the lower fibre volume of DURANEX 70G15 reduces apparent melt viscosity and improves feed-system pressure loss compared with DURANEX 70G30. The result is a wider processing window for filling long, thin-wall flow lengths and lower peak cavity pressure at equivalent melt temperature and injection velocity. This is a practical benefit when moulding 64-pin or 96-pin automotive connectors where gate dimensions are restricted and shear heating at the gate is high. Such gates can locally exceed 270 °C melt temperature even with nozzle set points of 260 °C, so melt-temperature monitoring at the nozzle and short hold times are required. The trade-off is lower flexural modulus: a 70G15 connector body will deflect more than a 70G30 body under identical insert loading, and terminal retention force may be lower. Insert-moulded terminal retention is consequently validated by terminal pull-out tests to OEM standards rather than by tensile modulus alone. Weld-line tensile strength is a known limitation in glass-filled PBT; gates should be positioned so that weld lines do not occur at the retention latch or at seals.

    Process experience on injection moulding machines with clamp force 80–120 t for multi-cavity tooling indicates that 70G15 runs with lower screw torque than 70G30 at comparable output. On general-purpose screws with L/D 20:1 and compression ratio 2.0:1–2.5:1, fibre attrition is less severe with 15% glass, which preserves fibre length and improves impact retention after regrind. Regrind should be limited to 25 wt% of total feed unless the application accepts loss of notched Charpy impact. For connector bodies exposed to vibration, the lower fibre loading may improve toughness in thin ribs but reduce creep resistance at elevated temperature compared with 70G30; creep testing to ISO 899-1 is recommended for load-bearing snap-fit arms.

    Automotive underhood sensor carriers, relay sockets, cooling fan brackets, ignition modules, and industrial terminal blocks are among the production applications for DURANEX 70G15. The grade is selected where the part requires the dimensional stability of PBT with a moderate fibre content, reduced warpage relative to 30% glass, and lower density than DURANEX 70G30. In engine compartment environments with continuous air temperatures of 120–140 °C and short-term excursions to 160 °C, the material shows adequate retention of tensile strength for non-structural components, provided the service environment does not include hot water or aggressive alkaline media. For structural brackets or high-load pulleys, the 30% glass grade DURANEX 70G30 or a PBT/ASA blend with higher toughness may be required. The published UL 94 rating for 70G15 is HB; flame-retardant connectors and relay housings should be developed in DURANEX 7407 or another listed UL 94 V-0 grade instead. The operational boundary is therefore not the heat deflection temperature alone but the combination of hydrolysis resistance, weld-line strength, and flammability rating.

    Top