| HS Code | 795118 |
| Material Type | High Density Polyethylene (HDPE) |
| Density | 0.950 g/cm3 |
| Melt Flow Rate | 8.0 g/10 min at 190°C/2.16 kg |
| Tensile Strength At Yield | 24-26 MPa |
| Tensile Elongation At Break | 600-800% |
| Flexural Modulus | 1100-1200 MPa |
| Izod Impact Strength Notched | 0.150 J/cm |
| Shore D Hardness | 60-62 |
| Vicat Softening Temperature | 124-125°C |
| Melting Temperature | 130°C |
| Brittleness Temperature | -70°C |
| Thermal Expansion Coefficient | 1.2E-4 /°C |
| Thermal Conductivity | 0.45 W/mK |
| Specific Heat | 1.9 J/g°C |
| Volume Resistivity | 1E15 ohm-cm |
| Dielectric Constant | 2.3 |
| Dielectric Strength | 20 kV/mm |
| Uv Stabilization | Yes |
| Antistatic | Yes |
As an accredited POLIPROPILENO VENEZUELA HDPE 2908APUV factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | POLIPROPILENO VENEZUELA HDPE 2908APUV: typically 25 kg PE-lined woven bags, palletized and stretch-wrapped; 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): POLIPROPILENO VENEZUELA HDPE 2908APUV resin securely palletized/stowed in a full 20-foot container for ocean shipment. |
| Shipping | POLIPROPILENO VENEZUELA HDPE 2908APUV is a non-hazardous polyethylene resin, shipped in 25 kg PP bags or bulk bags on pallets in dry containers. Protect from moisture, sunlight, and heat. Store in a cool, ventilated warehouse. Handle with clean equipment; avoid contamination. No special dangerous goods documentation required. |
| Storage | Store POLIPROPILENO VENEZUELA HDPE 2908APUV in original, sealed containers or bags in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, heat, sparks, flames, and strong oxidizers. Prevent moisture, dirt, and contamination. Keep containers closed when not in use. Avoid physical damage and excessive stacking. Follow first-in, first-out stock rotation and consult the safety data sheet. |
| Shelf Life | Typically, POLIPROPILENO VENEZUELA HDPE 2908APUV has indefinite shelf life when stored cool, dry, ventilated, away from sunlight and contaminants in sealed packaging. |
Extrusion blow molding of 10–30 L HDPE jerricans for solvent and agrochemical filling imposes simultaneous demands on melt strength, stress-crack resistance, and wall-thickness reproducibility. HDPE 2908APUV supplied by POLIPROPILENO VENEZUELA is a UV-stabilized high-density polyethylene blow-molding grade whose lot certification under ISO 1183-1:2019 places it in the HDPE density class above 0.941 g/cm³, while melt flow rate under ISO 1133-1:2022 at 190°C/2.16 kg is held within a narrow blow-molding band. On continuous shuttle lines using 24:1 to 30:1 L/D grooved-barrel extruders fitted with barrier screws and melt pumps, the grade is metered gravimetrically to limit parison length deviation caused by bulk-density fluctuation. When the certified melt flow rate remains within the 0.7–0.9 g/10 min band, the parison can be run at a melt temperature of 190–210°C, a die-head temperature of 185–205°C, and a mold temperature of 10–25°C without excessive sag or pinch-off cracking. For a 20 L jerrican with a calibrated handle pinch-off, blow pressure is set between 0.55 MPa and 0.75 MPa; pre-blow delay and post-blow exhaust are trimmed so that the bottom pinch-off weld does not show crystallized stress whitening. Dimensional stability is checked by neck and body thickness mapping, with no section below 0.4 mm in sidewall corners. The formulation should avoid filler loadings above 1.5 wt% calcium carbonate in the finished wall because filler particles reduce notched impact and increase ESCR sensitivity at the weld line. If external color masterbatch is required, addition is limited to 0.5–1.5 wt% and must use a PE carrier to prevent screw-slipping. Pre-drying is not normally required, but resin stored above 70% relative humidity should be dried at 70–80°C for 2–4 h to avoid melt splay and interfacial voids. Compliance is governed by the UN Model Regulations, specifically test series 6.1.5.3 drop, 6.1.5.5 hydraulic pressure, and 6.1.5.6 stacking, with the design type assigned as 3H1 for non-removable-head jerricans under ADR/IMDG/ICAO. End products include 10 L, 20 L, and 30 L tight-head containers for aliphatic solvents, dilute agrochemicals, and liquid detergents. Continuous service above 60°C is not recommended due to HDPE modulus reduction and potential top-load deformation during pallet stacking.
| UN test series | Reference | Typical 3H1 jerrican requirement |
|---|---|---|
| Drop test | UN 6.1.5.3 | Drop height 1.2 m for PG II/III liquids with relative density ≤1.2, at −18°C conditioning for polyethylene; 1.8 m for PG I X-marked designs |
| Hydraulic pressure | UN 6.1.5.5 | 250 kPa internal pressure for 30 min for X-marked jerricans; lower Y/Z pressures per classification; no leakage allowed |
| Stacking | UN 6.1.5.6 | 40°C for 28 days; load based on stack height and package mass; no collapse or leakage |
Multilayer water storage tanks with a recycled HDPE core and a UV-stabilized virgin cap layer are produced on accumulator-head blow molding machines when the required finished volume exceeds 500 L. In this construction, the inner potable-contact layer is unpigmented virgin HDPE complying with FDA 21 CFR 177.1520(c) and EU 10/2011 for food-contact plastics, while the outer layer carries the UV-stabilization package of HDPE 2908APUV. The layer distribution is typically 10–15% outer virgin, 65–75% recycled core, and 15–20% inner virgin, with the outer cap maintained above 0.3 mm to prevent crack initiation after long-term UV exposure. Incorporation of recycled core requires sieving to 8–10 mm maximum flake size and moisture control below 0.05 wt% because trapped water vapor in the core creates interfacial bubbles under blow pressure and can delaminate the outer cap. Extruder melt temperatures are held at 195–215°C; die-head temperature is reduced by 5–10°C relative to the extruder to increase melt strength and reduce parison drawdown. Mold cooling water is maintained at 10–18°C, with a blow pressure of 0.6–0.8 MPa for large tanks. Ultraviolet exposure verification is conducted under ISO 4892-2, commonly 2,000 h of artificial weathering with no visible surface crazing and Charpy impact retention above 80%, although grade-specific published data for this thickness and core blend are limited. Migration kinetics for the inner layer must satisfy an overall migration limit of 10 mg/dm² under EU 10/2011 testing conditions. Fluorinated barrier treatment should be avoided unless the processor validates interlayer adhesion because fluorine treatment of the inner surface can alter parison welding and reduce the stress-crack resistance of the pinch-off zone. End products include 1,000 L, 2,000 L, and 5,000 L outdoor water storage tanks for irrigation, rainwater collection, and emergency water supply. Operation at continuous hydrostatic head above 40°C is not advised without a validated tank support structure.
For 220 L tight-head, L-ring chemical drums, the primary process boundary is parison wall distribution over a shot weight approaching 8–12 kg. Accumulator-head machines with 30:1 to 35:1 L/D extruders are required to maintain uniform melt quality; the accumulator piston applies high shear and the parison die is programmed with 20–40 axial wall-thickness set points. The grade is processed at a melt temperature of 200–220°C, with the die head kept 10–15°C below the extruder to stabilize parison diameter and reduce sag. A blow pressure of 0.65–0.80 MPa and mold temperature of 15–25°C are used for L-ring drums; bottom pinch-off and top flash pockets require controlled flash thickness so that the weld seam is not thinner than 70% of the nominal adjacent wall. As a 1H1 design type under the UN Model Regulations, the drum must pass 6.1.5.3 drop, 6.1.5.5 hydraulic pressure, and 6.1.5.6 stacking test series. For an X1.4/250 or similar marking, hydraulic pressure is maintained at 250 kPa for 30 minutes; drop height depends on the relative density and packing group. Formulation may include 2.0–2.5 wt% carbon black masterbatch for UV opacity, but carbon black particle size above 25 μm can reduce environmental stress-crack resistance by acting as a stress concentrator. Carbon black masterbatch should be pre-compounded on a twin-screw extruder with 40:1 L/D and dispersive mixing elements to achieve agglomerate size below 25 μm. Addition of post-consumer regrind above 20 wt% requires revalidation of stack and hydraulic tests because low-molecular-weight fractions from prior thermal history reduce melt strength at the pinch-off and shift sag behavior. End products are 200 L and 220 L drums for industrial lubricants, water-treatment chemicals, and non-oxidizing acids. Service temperatures below −30°C require notched impact testing per ASTM D256-10 because HDPE can undergo brittle failure at the bottom chime area under transport vibration, and top-load collapse during stacked storage must be validated after UV exposure.
Automotive suction blow molding lines use HDPE 2908APUV for windshield-washer reservoirs, radiator overflow bottles, and hydraulic clutch fluid reservoirs in the 0.5–3.0 L range. Flow is generated by a vertical or horizontal clamp machine with parison-wall programming, melt temperature of 190–210°C, pre-blow delay of 0.3–0.8 s, and blow air pressure of 0.4–0.6 MPa. The necessary ESCR is evaluated under ASTM D1693-15 condition A or B, with the test fluid specified by the OEM; windshield-washer concentrate containing 30–50 vol% methanol at 60–80°C is one screening medium, with pass/fail thresholds defined by individual OEM material standards. Flammability compliance is tested under FMVSS 302 with a burn rate below 100 mm/min. Heat-aging protocols use ISO 527-2 tensile property retention after 1,000 h at 80°C, and the part must resist vacuum deformation under −20 kPa to −10 kPa at operational temperature. Formulation for under-hood reservoirs excludes plasticizers; high-molecular-weight HDPE with narrow molecular weight distribution is preferred, and the UV stabilization of 2908APUV assists outdoor vehicle exposure when reservoirs are mounted in partially exposed engine bays. The process limitation is clamp tonnage and flash extraction: multi-axis robotic trimming is used to remove top and bottom flash without introducing microcracks in the filler neck or mounting bosses. End products include 2 L windshield washer reservoirs, coolant overflow tanks, and small auxiliary reservoirs. Published third-party data for 2908APUV in specific OEM heat-aging programs are limited; qualification therefore relies on coupon and finished-part tests conducted by the molder according to each OEM material specification.
Blow molded marine fender and buoy shells require a wall thickness of 4–8 mm and a fully fused pinch-off because cyclic compression after foam filling can initiate fatigue cracks at the mold parting line. The process is performed on accumulator-head machines with shot weight up to 20 kg; melt temperature is held at 195–215°C, die head at 185–205°C, and mold temperature at 8–15°C to accelerate shell cooling before foam injection. HDPE 2908APUV is suitable only when the UV stabilization package is verified by ISO 4892-2 cycle 1 or an equivalent ASTM G154 cycle, with a minimum 2,000 h exposure and retention of notched impact strength measured by ISO 179-1/1eA. Salt-spray resistance is screened under ISO 9227 neutral salt spray; the grade does not corrode and acceptance is normally set at mass change below 0.5% after 1,000 h, but the molder must confirm this because published data for the specific compound under marine exposure is limited. Formulation additives include 0.5–1.0 wt% UV masterbatch only if additional protection is specified; antistatic agents must be excluded because they migrate to the surface and increase water absorption at the shell-to-foam interface. The molded shell is filled with polyurethane foam of density 28–35 kg/m³ after wall temperature falls below 45°C; premature foaming at higher wall temperature compresses the foam shell and distorts the outer surface. End products include cylindrical and pneumatic-style boat fenders, navigation buoy floats, and dock impact shells. Service temperature lower than −10°C requires drop-impact testing per ASTM D3029 or ISO 6603-2 because HDPE impact strength declines steeply below the ductile-to-brittle transition when wall thickness constraints and foam backing are present.
In 1,000 L intermediate bulk container inner bottles, extrusion blow molding uses multilayer construction with virgin HDPE 2908APUV in the outer skin, a recycled HDPE core, and an inner virgin layer, typically 20/60/20 or 15/70/15. The outer layer must remain at least 0.25 mm to protect the recycled core from UV-induced surface oxidation during outdoor storage of the IBC. Shell wall thickness ranges from 2.5 mm at the top to 5.0 mm near the base, produced by parison programming with 30–50 control points and an accumulator-head blow molder. Melt temperature is set at 200–220°C, mold cooling at 10–18°C, and blow pressure at 0.6–0.8 MPa. The main process risk is regrind loading from trimmed flash. When flash from previous cycles is ground and mixed into the core at 25–50 wt%, the melt flow rate can shift upward by 5–15% depending on thermal history; this reduces sag resistance and can thin the outer layer below the 0.25 mm minimum under heavy parison drawdown. Barrier integrity is then validated by hydraulic pressure testing under UN 6.5 for IBC design type 31HA1 or 31H1, leakproofness at 20 kPa for 10 minutes, and drop testing on the bottom chime after conditioning at −18°C. The formulation should not exceed 2 wt% external color masterbatch in the outer layer because excessive pigment aggregates nucleate environmental stress cracking. End products are 1,000 L IBC bottles for water-based industrial liquids, detergents, and food-grade liquids; aromatic solvent service above 40°C requires fluorination or an approved barrier layer, and fluorinated inner surfaces must be tested for adhesion after batch fluorination because residual fluorine can weaken the pinch-off weld if not properly neutralized.
Competitive POLIPROPILENO VENEZUELA HDPE 2908APUV prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
POLIPROPILENO VENEZUELA HDPE 2908APUV is a high-density polyethylene grade supplied by Polipropileno Venezuela S.A. and positioned within the high molecular weight extrusion blow moulding and thick sheet product family. Although the producer name contains the term “polipropileno,” the 2908APUV designation refers to an HDPE base resin, not polypropylene. Publicly available certified data for this specific Venezuelan grade are limited; therefore, numerical values provided in this document are representative values for commercial high molecular weight HDPE resins of the same melt flow class and are not a substitute for the supplier certificate of analysis. The grade is typically characterized by a nominal density of 0.958 g/cm³ under ISO 1183-1:2019 and a melt flow rate in the range of 0.7–0.9 g/10 min at 190 °C with 2.16 kg load under ISO 1133-1:2022. The resin is differentiated from standard HDPE blow moulding grades by the presence of a UV stabilization package, a molecular weight distribution tailored for high melt strength, and a density/modulus balance intended for stressed industrial packaging applications.
The pellet bulk density is typically 0.54–0.58 g/cm³, with residual moisture below 0.01% by weight as supplied in closed packaging. The UV package inhibits surface crazing and tensile elongation loss after outdoor exposure, but it does not convert the material into an engineering polymer. The grade is generally recommended for containers, liners, and thick sheet applications requiring resistance to environmental stress cracking in the presence of detergents, diluted acids, alkalis, and aliphatic hydrocarbons; however, chemical compatibility must be validated for each contact matrix. Compared with injection moulding HDPE grades with melt flow rates of 4–8 g/10 min, the 2908APUV class demonstrates significantly higher melt viscosity and parison hang strength. Compared with standard HDPE blow moulding grades without UV stabilizer, it provides longer retention of mechanical properties during outdoor service.
The first distinction is rheological. The melt flow rate of 0.7–0.9 g/10 min measured under ISO 1133-1:2022 at 190 °C with 2.16 kg confirms a high molecular weight resin. This is materially lower than the 4–8 g/10 min range typical of HDPE injection moulding grades and higher in melt viscosity than blow moulding grades with melt flow rates above 1.5 g/10 min. The high melt viscosity reduces parison sag during accumulator retraction and permits the formation of larger preforms with acceptable wall thickness uniformity. The second distinction is environmental stress crack resistance. Resins in this class typically show an F50 failure time exceeding 1000 h in 100% Igepal CO-630 under ASTM D1693-15 Condition B, although actual values depend on comonomer type, molecular weight distribution, and test plaque preparation. The third distinction is UV stabilization. The APUV suffix indicates a light stabilizer package that reduces the loss of tensile elongation at break after accelerated weathering under ISO 4892-2:2013. In many unpigmented HDPE grades without such a package, tensile elongation at break drops below 50% of the original value after 2000 h of xenon arc exposure, while a stabilized grade may retain 70–80% depending on part thickness, pigment concentration, and stabilizer diffusion.
| Property | Test method | Representative range |
|---|---|---|
| Density | ISO 1183-1:2019 | 0.956–0.960 g/cm³ |
| Melt flow rate | ISO 1133-1:2022, 190 °C, 2.16 kg | 0.7–0.9 g/10 min |
| Tensile yield stress | ISO 527-2:2012, 50 mm/min | 26–30 MPa |
| Tensile elongation at break | ISO 527-2:2012, 50 mm/min | >600% |
| Flexural modulus | ISO 178:2019 | 1000–1300 MPa |
| Notched Charpy impact at 23 °C | ISO 179-1:2020 | 5–10 kJ/m² |
| Vicat softening temperature | ISO 306:2013, A50 | 124–128 °C |
| Environmental stress crack resistance | ASTM D1693-15, Condition B | >1000 h |
These representative values are not certified lot-specific data. The differences between 2908APUV and standard HDPE therefore become most visible in applications where tensile elongation retention after weathering, weld-line integrity under stress cracking conditions, and consistent parison stability are simultaneous requirements.
In extrusion blow moulding of 20–30 L industrial containers, the processing window is constrained by melt temperature and parison sag. A grooved-feed single-screw extruder with L/D 30:1 and a barrier screw is commonly operated with barrel temperatures of 190–210 °C, adapter temperature of 205–215 °C, and die head temperature of 200–210 °C. Under these conditions, melt temperature measured at the accumulator head remains between 215 °C and 225 °C, while die-head pressure is generally below 35 MPa. Higher melt temperatures above 230 °C are associated with surface sharkskin, localised gel formation, and reduced parison hang strength. Diverging die tooling with a die gap of 1.5–2.5 mm and a blow ratio between 2.5:1 and 3.5:1 has been reported to produce acceptable wall thickness uniformity in square and cylindrical containers. The melt flow rate of 0.8 g/10 min supports parison stability during accumulator retraction but also increases motor load and melt temperature sensitivity. Screw speed on a 90 mm extruder is typically held between 70 rpm and 90 rpm, depending on back pressure and screw geometry, with back pressure maintained at 10–15 MPa.
For coextrusion structures in which 2908APUV forms a UV-stabilized cap layer over a recycled or lower-cost core layer, the cap layer thickness must be controlled to avoid delamination and stabilizer migration into the food-contact layer. When food-contact approval is required, the finished structure must satisfy FDA 21 CFR 177.1520 and the migration limits of EU 10/2011 as applicable. Published data for this specific configuration are limited, and migration testing on the finished article is required.
When the granulate is stored at relative humidity above 60%, superficial moisture pick-up may occur despite the hydrophobic nature of HDPE. Surface moisture is not chemically bound but can produce blow moulding defects such as bubble formation, silver streaks, and weakened pinch-off welds in thick sections. Pre-drying is not mandatory under closed-warehouse conditions below 60% RH, but sacks exposed to rain or high humidity should be dried in a desiccant or hot-air hopper dryer at 80–85 °C for 2–4 h. The drying air dew point should be below −20 °C. Drying at temperatures above 95 °C is not recommended because pellet agglomeration and additive migration may occur. Storage temperatures above 40 °C and direct sunlight should also be avoided even though the grade is UV-stabilized; stabilizer consumption begins during storage and can shorten the remaining outdoor service life. Avoid deliberate mixing with polypropylene, PET, or PVC regrind because density-based separation is not effective in practice and contamination reduces ESCR and impact performance.
Grade-specific certificates of analysis should be requested from the supplier for each production lot. The following matrix represents test method designations commonly applied to HDPE extrusion blow moulding grades; it is not a complete regulatory declaration for the finished article.
| Standard or regulation | Parameter addressed | Typical application in verification |
|---|---|---|
| ISO 1183-1:2019 | Density | Incoming resin identity and grade confirmation |
| ISO 1133-1:2022 | Melt flow rate | Rheological lot-to-lot consistency |
| ISO 527-2:2012 | Tensile yield and elongation | Mechanical acceptance of moulded specimens |
| ISO 178:2019 | Flexural modulus | Stiffness verification for thick sheet |
| ISO 179-1:2020 | Notched Charpy impact | Low-temperature impact comparison |
| ASTM D1693-15 | Environmental stress crack resistance | Detergent and agrochemical container qualification |
| ISO 306:2013 | Vicat softening temperature | Heat resistance screening |
| ISO 4892-2:2013 | Accelerated xenon arc weathering | UV stabilization performance screening |
| FDA 21 CFR 177.1520 | Olefin polymer food-contact status | Required only when grade-specific approval is confirmed |
| EU 10/2011 | Plastic food-contact migration limits | Required only for finished article in EU food-contact use |
| REACH 1907/2006 | Substances of very high concern | Supplier declaration required for EU market |
| RoHS 2011/65/EU | Restricted heavy metals | Electrical and electronic packaging components |
Where the grade is specified for 200 L intermediate bulk container liners, the combination of high ESCR and UV resistance becomes process-critical. The F50 failure time in 100% Igepal CO-630 under ASTM D1693-15 Condition B exceeds 1000 h for many high molecular weight HDPE resins of this type, but liner qualification must consider weld-line orientation, pinch-off area morphology, and internal stress from the blow ratio. Outdoor exposure of unpigmented HDPE containers for 12–24 months in tropical UV environments has been reported to reduce tensile elongation at break by 20–40% even with UV stabilization; therefore, service life prediction must include thickness reduction and stress cracking, not only UV dose. Published field data for the specific 2908APUV designation in 200 L liner service are limited, and end users should conduct instrumented outdoor exposure trials with destructive testing at defined intervals before committing to extended warranty periods.