    Specifications
    HS Code 284325
    Polymer Type LDPE and LLDPE Blend
    Form Pellets
    Application Film
    Density 0.922 g/cm³
    Melt Flow Index 190 C 2 16 Kg 1.6 g/10 min
    Melting Point 122 °C
    Vicat Softening Temperature 97 °C
    Tensile Strength At Break Md Td 24/22 MPa
    Elongation At Break Md Td 550/650 %
    Dart Impact Strength 110 g
    Elmendorf Tear Strength Md Td 90/140 g
    Haze 8 %
    Gloss 45 65
    Coefficient Of Friction 0.15
    Film Thickness Test 40 µm
    Recommended Extrusion Temperature 180-220 °C

    As an accredited Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Petroquimica Triunfo Trithene® TS 4016 LDPE/LLDPE Film is packaged in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL container loaded with Petroquimica Triunfo Trithene® TS 4016 LDPE/LLDPE blend film resin in securely stacked 25 kg bags.
    Shipping Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film ships as non-hazardous polymer resin in sealed bags, octabins, or bulk containers. It is not regulated by DOT, IMDG, or IATA. Store in a cool, dry, well-ventilated area; protect from moisture, heat, sunlight, and contamination.
    Storage Store in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, flames, and strong oxidizing agents. Keep bags/containers closed and palletized off the floor. Avoid moisture, contaminants, and physical damage. Maintain stable temperature and follow SDS/local regulations. Use first-in, first-out stock rotation. Protect from UV exposure and prolonged heat. Ensure area is clean, dry, and free of ignition sources.
    Shelf Life Shelf life is 12 months when stored in original packaging, in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film

    Trithene® TS 4016 is introduced into monolayer and coextruded blown film lines as an LDPE/LLDPE blend. The LDPE fraction contributes bubble stability and melt pressure reduction. The LLDPE fraction contributes dart impact, puncture resistance, and tear propagation resistance. On production-scale lines using 65 mm to 90 mm single-screw extruders with 24:1 to 30:1 L/D barrier screws and 250 mm annular dies, stable bubble geometry has been observed at die gaps of 1.4 mm to 2.2 mm. Blow-up ratios from 2.0:1 to 3.2:1 are typical. Melt temperatures at the die are held between 190 °C and 215 °C. Specific output rates for this die class generally fall from 0.8 kg/h/mm to 1.4 kg/h/mm of die circumference when internal bubble cooling is active. At 15 wt% to 30 wt% LDPE addition to an LLDPE-rich formulation, extruder head pressure is commonly 10% to 25% lower than for 100 wt% LLDPE at constant screw speed on a 65 mm, 28:1 L/D grooved-feed extruder. Die lip shear rates above approximately 400 s⁻¹ can initiate sharkskin on narrow-molecular-weight LLDPE fractions. The LDPE fraction shifts the melt fracture onset to higher shear rates, typically by 30% to 50%. Film thickness is controlled by non-contacting capacitance sensors with a tolerance of ±5% for 25 µm to 50 µm film. Tensile properties per ISO 527-3 for a 50 µm film commonly show machine-direction tensile yield strength of 11 MPa to 14 MPa and transverse-direction yield strength of 10 MPa to 13 MPa. Elongation at break typically falls between 500% and 650%. Dart impact per ASTM D1709 Method A for a 25 µm film is usually in the 120 g to 180 g range. Elmendorf tear per ASTM D1922 shows clear anisotropy, with machine-direction values of 50 g to 100 g and transverse-direction values of 300 g to 500 g. Haze per ASTM D1003 is commonly 8% to 15% at 25 µm. Coefficient of friction per ASTM D1894 can be maintained between 0.25 and 0.40 by a controlled slip and antiblock package. Drying is not routinely required. Where resin has been stored outdoors at relative humidity above 60%, pre-drying at 60 °C to 70 °C for 2 h to 4 h reduces bubble instability from surface moisture.

    Application classFilm thicknessKey propertyTest methodTypical observed range
    General blown film packaging25 µmDart impactASTM D1709 Method A120 g to 180 g
    Agricultural silage film100 µmPuncture resistanceASTM D574835 N to 55 N
    Collation shrink film45 µmFree shrink MD/TDASTM D273255% to 70% / 15% to 30%
    Heavy-duty shipping sack100 µmElmendorf tear TDASTM D1922600 g to 900 g
    Lamination sealant web40 µmHot tackASTM F19212 N/25 mm to 3.5 N/25 mm
    Frozen food packaging50 µmLow-temperature seal strengthASTM F88 at -18 °C3 N/15 mm to 5 N/15 mm

    Agricultural Silage Film and Greenhouse Cladding Require Controlled Barrier, UV Stabilization, and Tear Resistance

    Agricultural silage film produced from Trithene® TS 4016 is typically run at 80 µm to 150 µm on three-layer blown film lines. The oxygen transmission rate per ASTM D3985 at 23 °C and 0% relative humidity for a 100 µm film is commonly between 1800 cm³/(m²·d·atm) and 3000 cm³/(m²·d·atm). Water vapour transmission rate per ASTM F1249 at 38 °C and 90% relative humidity typically falls from 3 g/(m²·d) to 7 g/(m²·d). Puncture resistance per ASTM D5748 using a 19 mm probe at 250 mm/min is generally 35 N to 55 N for a 100 µm film. Low-temperature brittleness per ASTM D746 remains below -60 °C, which is relevant for winter silage covering. UV stabilization uses hindered amine light stabilizers at 0.2 wt% to 0.4 wt% and UV absorbers at 0.1 wt% to 0.2 wt%. Black silage film generally incorporates carbon black at 2 wt% to 3 wt%. Production experience on 70 mm, 24:1 L/D three-layer lines with 300 mm dies indicates that dusted HALS concentrates can bridge at the feed throat. Pre-dispersed masterbatch or side-feeding is therefore preferred. Exposure to fermentative silage acids such as acetic and lactic acid can accelerate antioxidant extraction at exposed film edges. For long-term greenhouse cladding, UV masterbatch must be selected for the intended exposure zone. Published data for this specific TS 4016 configuration under multi-season greenhouse propagation is limited. The operational boundary is that unstabilized or under-stabilized film should not be used for direct outdoor exposure beyond a single silage season.

    What Limits Gauge Uniformity in Collation Shrink Film Made from LDPE/LLDPE Blends?

    On high-output collation shrink lines, Trithene® TS 4016 film is drawn at thicknesses from 35 µm to 60 µm. Die gap is normally set at 1.2 mm to 1.6 mm, and blow-up ratio is maintained between 2.4:1 and 3.0:1. A high stalk height of 8 to 12 die diameters is used to build transverse-direction orientation. Free shrink per ASTM D2732 after 10 s immersion at 110 °C typically gives machine-direction shrink of 55% to 70% and transverse-direction shrink of 15% to 30%. Gauge uniformity is controlled by die lip concentricity, air-ring velocity distribution, and frost line height. Production audits on LDPE/LLDPE shrink lines with 250 mm dies have shown that raising frost line height from 500 mm to 900 mm can increase transverse orientation but may widen gauge spread from ±4% to ±8% if cooling-air balance is uneven. Melt temperature at the die should remain between 195 °C and 215 °C. Die lip shear rate should be held below 380 s⁻¹ to delay sharkskin. Shrink tunnels are operated at 160 °C to 180 °C with residence times of 3 s to 6 s. Mandrel pre-shrink is a known failure mode if film is stored above 40 °C before conversion. Collation shrink film from this blend is not a substitute for high-shrink EVA-rich formulations in tight multipack contours. Hot wire sealing is preferred over impulse sealing where seal temperatures exceed 150 °C for more than 0.8 s because excessive dwell time can produce edge beading and shrink distortion.

    Heavy-duty shipping sacks produced from Trithene® TS 4016 are converted on side-gusseted, bottom-seal, or pinch-bottom lines for fill weights from 25 kg to 50 kg. Film thickness is typically 80 µm to 150 µm. Dart impact per ASTM D1709 Method A for a 100 µm film is frequently specified above 300 g. Elmendorf tear per ASTM D1922 in the transverse direction is a critical quality gate. For a 100 µm film, transverse-direction tear values of 600 g to 900 g are common. Hot tack and seal strength are evaluated per ASTM F1921 and ASTM F88 respectively. Seal specimens of 25 mm width are clamped at 0.18 MPa for 0.5 s at 130 °C. Peak seal strength for a 100 µm film usually falls between 4 N/15 mm and 6 N/15 mm. The film is processed on high-throughput three-layer lines using 90 mm, 30:1 L/D grooved-feed extruders and 400 mm annular dies. Output rates of 350 kg/h to 500 kg/h are achievable when die gap is held at 2.0 mm to 2.4 mm. Slip and antiblock levels require balance. Erucamide-based slip at 500 ppm to 1000 ppm and silica antiblock at 1000 ppm to 2500 ppm are typical. Above 1200 ppm slip, coefficient of friction can continue to decline during storage and cause turret winder instability. Printed sack performance is sensitive to corona treatment level. Wetting tension per ASTM D2578 should be held at 38 mN/m to 42 mN/m for water-based ink adhesion. Below 36 mN/m, ink rub-off on high-speed flexographic lines becomes a rejection risk. Published data for this specific TS 4016 grade at 150 µm with high ink coverage is limited, so incoming corona decay should be rechecked after 72 h.

    Lamination Sealant Layers and Interlayer Adhesion Control

    In lamination structures where a sealant web is required, Trithene® TS 4016 film is usually corona-treated in line to wetting tension of 38 mN/m to 42 mN/m per ASTM D2578. The treated surface is bonded to aluminium foil, PET, or BOPP using solventless polyurethane adhesives. Seal initiation temperature is measured with a heat-gradient bar on 25 mm strips at 0.25 MPa pressure and 0.5 s dwell. Seal initiation temperature is typically 105 °C to 120 °C. Hot tack strength per ASTM F1921 at 120 °C is often 2 N/25 mm to 3.5 N/25 mm. Peel strength of the laminate is assessed per ASTM D1876. Film-to-aluminium bond strength is commonly 2 N/15 mm to 5 N/15 mm. The sealant web must be substantially free of gel defects larger than 250 µm. Laser scanning or camera-based gel detection is used on slit film at converting speeds up to 300 m/min. Excessive corona treatment above 45 mN/m can create film-to-film blocking during storage. Slip additive migration can lower adhesive anchorage after lamination. Off-line wetting tension should therefore be rechecked after 72 h aging. The formulation should not be combined with primary aromatic amine-containing laminating adhesives that require compliance with specific migration limits under EU Regulation 10/2011. For food-contact laminates, the final structure must meet overall migration limits of 10 mg/dm² and the sealant layer must comply with FDA 21 CFR 177.1520 for olefin polymers. This film functions as a heat-seal layer, not as a gas or moisture barrier layer. In high-barrier laminates, aluminium foil or metallized layers remain the controlling barrier elements.

    When Frozen Food Packaging Demands Low-Temperature Seal Strength and Puncture Resistance

    Frozen food packaging films produced from Trithene® TS 4016 typically range from 40 µm to 70 µm. The film must retain seal integrity after blast freezing at -30 °C. Low-temperature brittleness per ASTM D746 is below -60 °C. Puncture resistance per ASTM D5748 at room temperature is 20 N to 40 N for a 50 µm film. At -20 °C, puncture force may increase by 10% to 20% because of low-temperature stiffening. Gelbo flex pinhole testing per ASTM F392 for 50 cycles typically produces fewer than 5 pinholes per 16 cm² in a 60 µm film. Seal strength per ASTM F88 after 24 h at -18 °C is commonly 3 N/15 mm to 5 N/15 mm for seals made at 130 °C, 0.18 MPa, and 0.5 s. Haze per ASTM D1003 remains at 10% to 18% at 50 µm if no antifog additive is used. When anti-fog performance is required, non-ionic surfactant additives at 0.3 wt% to 0.8 wt% are incorporated, but this can reduce hot tack if the additive blooms excessively. Slip additive levels above 1200 ppm are not recommended for frozen food contact because surface bloom can increase extractables and alter seal consistency. Food-contact compliance requires FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation 10/2011 overall migration limitations. REACH Article 33 supplier communication applies where SVHC content exceeds 0.1 wt%. The film should not be used in direct contact with high-free-fatty-acid foods above 60 °C without migration testing because the LDPE phase may extract under aggressive fatty simulants.

    Regulation or standardScopeKey conditionApplicability to TS 4016 film
    FDA 21 CFR 177.1520Olefin polymers in food contactPolymer composition and extractablesSealant and packaging layers
    EU Regulation 10/2011Plastic food contact materialsOverall migration limit 10 mg/dm²Finished laminate or monolayer film
    EU 2023/2006Good manufacturing practice for food contact materialsTraceability and process controlFilm production and conversion
    REACH Article 33SVHC communicationSubstance above 0.1 wt%Importer and converter declaration
    ASTM D2578Wetting tension of polyolefin films38 mN/m to 42 mN/m before laminationSurface treatment control

    Stretch hood and pallet unitization lines operating with 100 µm to 180 µm Trithene® TS 4016 films require a balance of elastic recovery and tear propagation resistance. Tensile properties per ISO 527-3 at 23 °C show yield stress of 10 MPa to 13 MPa in both machine and transverse directions. Elongation at break exceeds 600%. Hysteresis after 100% extension per ISO 527-3 shows permanent set of 20% to 30% after 60 s relaxation. Tear resistance per ASTM D1922 in the machine direction is typically 80 g to 150 g for a 120 µm film. Puncture resistance per ASTM D5748 is 45 N to 65 N for 120 µm. On four-corner stretch hood machines operating at up to 90 pallets/h, the film is drawn 50% to 80%. Gauge reduction must remain uniform within ±6%. Thin spots at the pallet base can initiate localised tearing under load shift. The LDPE fraction in the blend supports elastic recovery and bubble stability. The LLDPE fraction contributes puncture and tear resistance. Processing uses 100 mm, 30:1 L/D extruders with 400 mm annular dies. Die gap is set at 2.0 mm to 2.4 mm. Blow-up ratio is held between 2.0:1 and 2.8:1. Melt temperature is maintained at 190 °C to 215 °C. Indoor storage at 15 °C to 25 °C for 24 h before palletization stabilises shrink and elastic recovery. Use below -10 °C on unheated loading bays is outside the recommended operating window because elastic recovery decreases at sub-zero temperatures. Published data for this specific TS 4016 configuration under sub-zero stretch hood deployment is limited. The film should not be blended with post-consumer recyclate above 10 wt% for stretch hood service without full tear resistance revalidation per ASTM D1922.

    Free Quote

    Competitive Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Petroquimica Triunfo Trithene® TS 4016 is identified on certificates of analysis as a polyethylene blend of low-density polyethylene, PE-LD, and linear low-density polyethylene, PE-LLD, intended for blown-film conversion. Under ISO 1043-1, the material is classified as a PE-LD/PE-LLD blend rather than a random copolymer. The LLDPE fraction contributes higher dart impact and Elmendorf tear resistance, while the LDPE fraction supplies long-chain branching responsible for melt strength, extensional strain hardening, and shear thinning in the die. Published numerical values for the exact comonomer type, molecular weight distribution, and additive package are limited; the lot-specific certificate of analysis therefore governs incoming inspection and lot acceptance. Typical conversion routes include tubular blown-film lines with spiral mandrel dies, single-layer and coextruded structures, and industrial packaging films above 30 μm where shrink bundling, puncture resistance, and stable bubble geometry are required. The grade is not positioned for cast film, rotational moulding, or injection moulding.

    Which Property Anchors Are Used for Incoming Resin Inspection?

    Incoming inspection for TS 4016 is commonly built around melt-state fingerprints and converted film performance. Density and melt mass-flow rate are measured on pellets under ISO 1183-1:2019 and ISO 1133-1:2022; film properties are measured on a standardized blown-film sample, normally 50 μm gauge, after conditioning at 23 °C and 50% relative humidity for 40 h under ISO 291:2021. The table below is a published property envelope for film-grade LDPE/LLDPE blends, not a lot-specific TS 4016 certificate, and is included to define the analytical scope. Certificates of analysis from the manufacturer or authorized distributor supply the exact values and additive package declaration. Where a receiving laboratory lacks film conversion capability, pellet density and melt mass-flow rate remain the most reproducible screening methods.

    Typical published property envelope for film-grade LDPE/LLDPE blends
    PropertyTest methodUnitTypical published envelope
    Density at 23 °CISO 1183-1:2019g/cm³0.918–0.924
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-1:2022g/10 min1.0–1.6
    Dart impact strength, 50 μm blown filmASTM D1709-22, Method Ag70–120
    Elmendorf tear strength MD/TD, 50 μmASTM D1922-23gf60–140 / 90–180
    Tensile stress at break MD/TDASTM D882-22MPa25–35 / 22–30
    Elongation at break MD/TDASTM D882-22%400–650 / 550–750
    Haze, 50 μmASTM D1003-21%6–14
    Gloss at 60°ASTM D2457-21GU60–80

    When the exact certificate is unavailable, incoming inspection should reject material if pellet contamination exceeds 0.5% by weight, if melt mass-flow rate deviates more than ±10% from the manufacturer’s reference, or if density falls outside the typical LDPE/LLDPE film band. Thickness measurement before film testing should follow ISO 4593:2019, and test specimens for Elmendorf and tensile tests should be cut after the conditioning interval to avoid edge-crack artifacts.

    When Melt Strength Governs Bubble Stability in High-Output Lines

    In blown-film conversion, TS 4016 behaves as an intermediate-melt-strength resin. The LDPE fraction supplies extensional strain hardening; the LLDPE fraction raises extensional viscosity under high draw but lowers bubble tension at low strain, producing a narrower process window than LDPE homopolymer if die gap is reduced below 1.2 mm. On 70 mm single-screw extruders with 30:1 L/D and 350 mm spiral mandrel dies, stable bubbles are obtained with die gaps of 1.6–2.0 mm, melt temperatures of 185–210 °C, and blow-up ratios between 2.0:1 and 2.8:1. Frost line height is commonly maintained between 700 mm and 900 mm above the die to balance MD/TD orientation. Lowering the frost line below 500 mm increases haze and dart impact scatter, while raising it above 1.2 m reduces cooling rate and can generate oscillating gauge bands.

    Use of grooved-feed bushings is required for consistent pellet conveying because LLDPE-rich formulations may exhibit lower bulk density and higher screw torque than LDPE homopolymer. Output limits are usually set by bubble oscillation rather than extruder capacity; at 2.5:1 BUR, web tension fluctuation above ±1.5 N/m indicates that melt temperature or frost line should be adjusted. Specific power consumption in the extruder increases relative to LDPE homopolymer by approximately 5–15% depending on LLDPE content; published data for the exact TS 4016 blend ratio is limited. The apparent shear rate in a 350 mm die with 1.8 mm gap at 150 kg/h is within a range where LDPE long-chain branching suppresses gross melt fracture, but the LLDPE fraction can create sharkskin at the die exit when die pressure approaches the critical shear stress of the melt. Purging after shutdowns longer than 30 min should use LDPE; start-up after an LLDPE-rich grade may require an increase of die gap to 1.0–1.2 mm until melt fracture clears.

    Property trade-offs in collation-shrink and FFS packaging lines

    Comparatively, LDPE homopolymer film at 50 μm typically delivers dart impact in the range of 40–60 g and high elongation but lower Elmendorf tear. LLDPE hexene/octene film at equivalent thickness delivers dart impact above 100 g but reduces bubble stability and increases melt pressure. TS 4016 occupies an intermediate band: the expected dart impact range of 70–120 g and Elmendorf tear retention after transverse orientation make it more resistant to punctures from product corners in bundled beverage multipacks and industrial bag-in-box liners. Seal initiation temperature is governed by the LLDPE fraction and is generally lower than LDPE homopolymer; laboratory heat-seal curves produced with 30 N/mm² seal pressure and 0.5 s dwell on a laboratory impulse sealer show measurable seal strength above 110 °C, but published values for this specific TS 4016 configuration are limited.

    The product is not formulated as a high-clarity grade; haze levels are higher than LDPE homopolymer extrusion film when frost line height is below 500 mm. It differs from slip/antiblock LDPE grades because the exact additive package may contain processing stabilizers; masterbatch dilution with antiblock or slip must be confirmed before use in high-speed packaging machines. In FFS polyethylene sacks, the blend provides puncture resistance during sharp-granule filling, but it does not provide oxygen barrier; where modified atmosphere is required, PA/EVOH coextrusion is necessary. Shrink bundling operations require sufficient MD/TD orientation; typical free shrink for LDPE/LLDPE blends after 120 °C/30 s immersion is 50–60% in MD and 20–30% in TD, though TS 4016-specific values should be confirmed on the converted film.

    Evaluating Surface Treatment and Gauge Profile in High-Speed Conversion

    Polyethylene blown film typically presents initial surface energy between 32 mN/m and 34 mN/m before treatment. Flexographic printing on TS 4016 film generally requires corona discharge treatment to 38–42 mN/m; lamination may require 44–48 mN/m measured with ASTM D2578-23. Treatment decay occurs more rapidly in humid environments and on slip-containing surfaces; inline treatment immediately before printing is therefore preferred to offline batch treatment. Gauge uniformity should be monitored with a beta or capacitance gauge across the web; variation outside ±5% of nominal thickness increases the risk of bag collapse and seal failure in automatic packaging. Winding tension on converting lines should be tapered by 10–15% from core to full roll diameter to prevent blocking and telescoping. Coefficient of friction, when required, can be measured under ASTM D1894-24; if the TS 4016 lot does not contain slip additive, contact surfaces may require masterbatch modification before high-speed bag-making.

    When TS 4016 is supplied into food-contact or high-humidity environments, lot-specific documentation governs. Polyethylene homopolymers and LDPE/LLDPE blends intended for food contact are typically evaluated under U.S. FDA 21 CFR 177.1520 and European Commission Regulation (EU) No 10/2011; TS 4016 should be confirmed against the supplier’s food-contact statement because additive package changes may affect migration test results. REACH registration under Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU apply to the pellet as supplied, but downstream inks, adhesives, and masterbatches require separate compliance assessment. At relative humidity above 60%, surface moisture uptake onto pellets can produce film pinholes; pre-drying at 60–70 °C for 1–2 h in a desiccant or hot-air pellet dryer is required before extrusion. Melt temperature must not exceed 240 °C, and intermittent temperatures above 220 °C should be limited to less than 15 min to avoid local gel formation. Contamination with polypropylene at levels above 5% by weight reduces interlayer weld integrity and increases haze. The resin should be stored below 40 °C, protected from ultraviolet exposure, and used within 12 months of packaging date unless the certificate of analysis states otherwise.