Petroquimica Triunfo Trilene Ts 8057 Lldpe C4 And Ldpe Blend

Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend

    • Product Name: Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 556861
    Polymer Type LLDPE-C4 and LDPE blend
    Comonomer 1-Butene
    Form Pellets
    Density 0.923 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Break Md 26 MPa
    Tensile Strength At Break Td 22 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Resistance Md 120 g
    Elmendorf Tear Resistance Td 250 g
    Dart Drop Impact 100 g
    Haze 10%
    Gloss 45 65
    Coefficient Of Friction 0.15

    As an accredited Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4/LDPE blend is packaged in 25 kg polyethylene bags, palletized for industrial handling.
    Container Loading (20′ FCL) 20′ FCL loading of Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4/LDPE blend: palletized 25 kg bags, uniformly stowed and secured.
    Shipping Petroquimica Triunfo Trilene® TS 8057 is shipped as non-hazardous polyethylene resin pellets in 25 kg moisture-resistant bags, stretch-wrapped pallets, or bulk bags. Transport by truck, railcar, or container. Store cool and dry, away from ignition sources. Not regulated for DOT, IMDG, or IATA. Secure loads and protect from moisture.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original packaging closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain ambient storage temperatures and follow supplier SDS and local regulations. Use clean handling equipment to preserve product quality. Do not store near strong oxidizers.
    Shelf Life Shelf life is 24 months when stored in original packaging, dry, cool, ventilated conditions, away from direct sunlight and heat.
    Application of Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend

    Food-Contact Blown Film for Low-Temperature Meat and Dairy Packaging

    Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend is converted into food-contact blown film at a melt temperature of 190 °C to 215 °C on a single-screw extruder with L/D 30:1, a 250 mm blown-film die, and a die gap of 1.8 mm. The polymer base is metered at 100 wt% of the polymer phase, with slip masterbatch at 1.0 wt% to 2.0 wt%, antiblock masterbatch at 1.0 wt% to 2.0 wt%, and a fluoropolymer processing aid at 0.04 wt% to 0.08 wt% to suppress die-lip deposit formation. Compliance is anchored to US FDA 21 CFR 177.1520(c) for olefin polymers, European Commission Regulation (EU) No 10/2011 Annex I with overall migration limit 10 mg/dm², and China GB 4806.7-2016. Overall migration testing is conducted according to EN 1186-1:2002, and specific migration of additives is evaluated under EN 13130-1:2004 for dual-export packaging intended for European Union and North American food-contact chains.

    Production-scale failure modes in this sector are concentrated at the screen changer and die lip rather than at the haul-off. On a 90 mm barrier screw with L/D 30:1, melt pressure at the screen pack typically remains between 25 MPa and 35 MPa; when post-industrial regrind exceeds 10 wt%, screen change intervals shorten to 6 h to 8 h because oxidized gel particles from the outer film layers accumulate on the breaker plate. The bubble is stabilized with a dual-lip air ring and internal bubble cooling at a blow-up ratio of 2.2:1 to 2.5:1. Terminal products include vacuum pouches for fresh red meat at 80 μm to 120 μm, frozen poultry bags at 35 μm to 60 μm, and dairy wrapper films at 40 μm to 70 μm. The practical processing window should not exceed 220 °C melt temperature because prolonged residence time above 230 °C generates aldehyde and ketone byproducts that migrate into fatty food simulants under EU No 10/2011 testing.

    StandardRegulatory scopeCritical limit or test condition
    FDA 21 CFR 177.1520(c)Olefin polymers for food-contact useMaximum extractable fraction under specified heptane extraction
    (EU) No 10/2011Plastic materials and articles intended for food contactOverall migration 10 mg/dm²
    GB 4806.7-2016PRC food-contact plastic articlesTotal migration ≤10 mg/dm²
    EN 1186-1:2002Overall migration test methodologySimulant selection based on food type and contact time

    When annular die pressure fluctuations exceed ±0.5 MPa on a 250 mm mono-layer blown-film die, gauge variation in 150 μm industrial liner film becomes the controlling variable for both seal integrity and dart impact resistance under ASTM D1709-16a Method B. In this heavy-duty liner application, the polymer feed comprises 92 wt% to 96 wt% Trilene® TS 8057 and 4 wt% to 8 wt% post-industrial regrind, with a carbon black masterbatch at 2.0 wt% to 3.0 wt% where ultraviolet protection is specified. Melt temperature is held at 200 °C to 225 °C, die gap is 1.8 mm to 2.4 mm, and blow-up ratio is 2.8:1 to 3.5:1; internal bubble cooling stabilizes the stalk above a frost line located 7 to 9 die diameters from the air ring.

    When the liner is inserted into UN-certified fibre drums for dangerous goods, the assembled package is validated under 49 CFR 178.603 drop testing and 49 CFR 178.604 leakproofness testing. The film itself is characterized by tensile yield strength under ISO 527-3:2018 or ASTM D882-18 and by trouser tear strength under ISO 6383-2:1983. Terminal forms include drum liners for chlorinated paraffins, FIBC inner liners for titanium dioxide, and dump-truck body liners used in mineral concentrate transport. Output on a 75 mm grooved-feed extruder with L/D 30:1 ranges from 180 kg/h to 240 kg/h. The addition of more than 8 wt% post-industrial regrind from multi-layer scrap is not recommended because gate pressure and output variations on the grooved-feed section produce gauge bands at the frost line. At relative humidity above 60%, the resin should be pre-dried at 65 °C for 4 h to prevent moisture streaking in thick-gauge liners.

    Why Does Transverse Direction Shrink Force Need to Remain Below 1.8 N/15 mm in Bottle Bundle Structures?

    Transverse direction shrink force in printed bottle bundle film is controlled primarily by blow-up ratio and frost-line residence time. For a 50 μm high-stalk blown film based on Trilene® TS 8057, free shrink measured under ASTM D2732-14 at 150 °C for 15 s falls between 12% and 22% in the transverse direction when blow-up ratio is 3.0:1 to 3.5:1. Keeping shrink force below 1.8 N/15 mm is necessary to prevent PET bottle sidewall compression and label tunnel deformation in high-speed shrink tunnels operating at 140 °C to 155 °C. The polymer phase is used at 100 wt% of the base film, with a slip/antiblock masterbatch added at 1.5 wt% to 2.5 wt%. If shrink force remains above 1.8 N/15 mm, an additional 10 wt% to 20 wt% of fractional-melt LDPE can be let down to reduce shrink tension, but this modification reduces machine-direction tear resistance under ISO 6383-2:1983.

    The process uses a 90 mm extruder with L/D 30:1, a die gap of 1.2 mm to 1.8 mm, and a high-stalk bubble with blow-up ratio up to 4.0:1. The frost line is raised to 6 to 8 die diameters to balance machine-direction and transverse-direction orientation. Terminal products include multi-pack bottle wraps for carbonated soft drinks, can bundles, and printed promotional multi-packs. A double-bubble process is not recommended when the LDPE fraction is below 20 wt% because the C4-LLDPE-rich web re-softens too broadly, causing bubble sag between the hot and cooling zones. Shrink tunnel setpoints above 165 °C produce localized burn-through at edge folds under ASTM D2732-14 free-shrink testing conditions; published data for this exact grade configuration at tunnel temperatures above 160 °C is limited.

    Blow-up ratioTransverse-direction free shrink at 150 °CMachine-direction free shrink at 150 °CShrink force
    2.5:18%–12%55%–65%1.0–1.4 N/15 mm
    3.0:112%–18%48%–58%1.3–1.7 N/15 mm
    3.5:118%–24%40%–50%1.5–2.0 N/15 mm
    4.0:124%–30%35%–45%1.8–2.4 N/15 mm

    Oxygen permeability of a 100 μm silage cover film measured at 23 °C and 0% RH under ASTM D3985-17 remains below 4,000 cm³/(m²·d·atm) when the LDPE fraction in the C4-LLDPE/LDPE blend stays above 15 wt%. For pit silage film and clamp cover use, the polymer phase contains 94 wt% to 96 wt% Trilene® TS 8057 with a UV/HALS masterbatch at 4 wt% to 6 wt%; white films also receive 6 wt% to 8 wt% titanium dioxide masterbatch, while black films receive 2.0 wt% to 2.5 wt% carbon black masterbatch. Blown-film processing on a 1,200 mm die with 2.8:1 to 3.2:1 blow-up ratio and 1.8 mm die gap produces layflat widths up to 12 m at melt temperatures of 200 °C to 230 °C.

    Compliance is evaluated against EN 13206:2017 for thermoplastic films for agricultural use, with weathering resistance measured under ISO 4892-2:2013 and tensile properties under ISO 527-3:2018. Terminal products include pit silage covers, clamp sheets for ensiled forage, and stack covers for baled forage stored outdoors. The material is not specified for round-bale stretch film; for round-bale wrap requiring prestretch above 70%, published industrial data shows C8-LLDPE-rich cast films provide higher tear propagation resistance under ISO 6383-2:1983. Avoid use with sulfur dioxide fumigation in storage environments because HALS stabilizer efficacy decreases under acidic gaseous exposure, which can reduce film service life below the 12-month minimum claimed under EN 13206:2017 class C.

    If Seal Initiation Temperature Must Drop Below 95 °C for High-Speed Form-Fill-Seal Packaging

    The use of Trilene® TS 8057 in extrusion lamination and coating is specified for sealant webs where hot-tack strength and reduced neck-in are more important than narrow low-temperature seal windows. On a 2,400 mm die width extrusion coating line with a polished chili roll at 15 °C to 20 °C, the blend is let down into a fractional-melt LDPE coating resin at 15 wt% to 25 wt%. A fluoropolymer processing aid at 0.05 wt% to 0.1 wt% is added to suppress melt fracture; die gap is set at 0.5 mm to 0.75 mm, melt temperature at 305 °C to 325 °C, and line speed between 200 m/min and 400 m/min. Increasing the TS 8057 fraction above 30 wt% raises extruder backpressure by 15% to 25% and causes edge encapsulation and die-line streaking on a 90 mm extruder with L/D 30:1.

    Food-contact laminates are covered under FDA 21 CFR 177.1520(c) and (EU) No 10/2011, with seal strength measured under ASTM F88/F88M-20 and hot-tack under ASTM F1921/F1921M-18. Terminal products include paper sack liners for petrochemicals, laminated pouches for dried soups, and medical device header bags. Adhesion to aluminium foil requires corona treatment at 44 dyn/cm or a tie resin added at 5 wt% to 10 wt%; without surface treatment, peel strength under ASTM D1876-23 is inconsistent across the web and produces variable failure at the seal interface during form-fill-seal operation.

    Cast film line speed for a 17 μm hand pallet wrap containing C4-LLDPE/LDPE blends is often limited to 350 m/min by web flutter at the air-knife, not by extruder throughput. The polymer phase for economic-grade cast stretch film comprises 20 wt% to 30 wt% Trilene® TS 8057 in a C8-LLDPE base with a tackifier masterbatch at 0.5 wt% to 2.0 wt%; melt temperature is controlled at 250 °C to 275 °C, die gap at 0.6 mm to 0.9 mm, and chill roll temperature at 18 °C to 22 °C. REACH registration is maintained by the resin supplier under Regulation (EC) No 1907/2006.

    Terminal products include hand stretch film from 12 μm to 20 μm, economy machine-grade wrap up to 23 μm, and bundling film for ceramic tiles. Cling and puncture are measured under ASTM D5458-95 and ASTM D5748-95, with tensile elongation under ISO 527-3:2018. The C4-LLDPE/LDPE blend is not recommended for machine-grade prestretch above 200% because core break and dart drop failures increase under ASTM D1709-16a when compared with C8-LLDPE-rich formulations. At ambient temperature below 10 °C, cling force decreases on some cast lines; a secondary winder roller treatment is required if the tackifier level is below 1.0 wt%.

    Free Quote

    Competitive Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Petroquimica Triunfo Trilene® TS 8057 is an ethylene-butene linear low-density polyethylene copolymer blended with low-density polyethylene homopolymer. The butene-derived short-chain branches in the LLDPE fraction depress crystallinity and improve dart impact retention after film orientation, while the long-chain branched LDPE fraction increases melt extensibility and stabilizes the bubble geometry. The grade is supplied as spherical pellets for blown-film and cast-film conversion, particularly where converters require gauge uniformity, puncture resistance, and stable high-speed output from the same resin. The blend differs from a single-component butene-LLDPE by its lower tendency to produce melt fracture and bubble instability at elevated take-off speeds; it differs from high-pressure LDPE by measurably higher transverse-direction tear resistance and dart drop impact energy when films are compared at equivalent thickness under ASTM D1922-15 and ASTM D1709-22.

    As a hybrid architecture, Trilene® TS 8057 occupies a defined processing space between two conventional film resins. The C4-LLDPE fraction contributes linear chains with short-chain branching and a narrow comonomer distribution; the LDPE fraction contributes a branched topology that increases shear sensitivity and elongation at break in the melt. This combination is relevant on production lines where unblended LLDPE-C4 may exhibit surging, edge weave, or variable film thickness because of insufficient melt strength. Published data for this specific product configuration in fully instrumented conversion trials is limited; converter-scale trials therefore remain necessary for definitive output-rate and bubble-stability limits.

    The product model designation TS 8057 does not encode the exact blend ratio. The ratio of LLDPE to LDPE is proprietary to the producer, but the resulting density and melt flow rate are used as routine lot-release parameters. The blend is typically specified for film thicknesses between 15 µm and 50 µm. The lower end of this range is commonly evaluated for stretch-wrap and overwrap formats, while the upper end is evaluated for industrial liners and protective packaging where puncture tolerance and tear propagation resistance are dominant requirements.

    Material Architecture, Specification Envelope, and Monomer Composition

    Trilene® TS 8057 is classified as a film-grade polyolefin blend. The butene comonomer is integrated into the linear polyethylene backbone as pendant ethyl branches after polymerization. The LDPE component is produced through high-pressure free-radical polymerization and contains both short-chain and long-chain branches. The two populations are melt-compounded into a pelletized product. The resulting melt rheology is broader than that of a neat LLDPE-C4, with improved shear thinning at die-lip shear rates. This influences pressure drop, extruder motor load, and the onset of melt fracture.

    For incoming material qualification and extrusion control, the following properties are routinely measured according to the standards listed. The values shown in the table are indicative class-typical ranges for an LLDPE-C4/LDPE film blend of this type and are not a substitute for the producer’s certificate of analysis or the current technical datasheet.

    PropertyTest standardTS 8057 indicative class-typical rangeUnblended butene-LLDPE referenceHigh-pressure LDPE reference
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:2022 / ASTM D1238-200.60–1.0 g/10 min0.80–1.2 g/10 min0.70–2.0 g/10 min
    Density at 23 °CISO 1183-1:2019 / ASTM D792-200.919–0.923 g/cm³0.918–0.922 g/cm³0.919–0.924 g/cm³
    Dart drop impact F50, 25 µm filmASTM D1709-22 Method A100–140 g90–150 g70–110 g
    Tensile strength at break, transverse directionISO 527-3:201820–26 MPa22–30 MPa16–22 MPa
    Elmendorf tear, transverse direction, 25 µm filmASTM D1922-1580–120 gf100–150 gf40–70 gf

    The melt flow rate is not a direct predictor of molecular weight distribution width. In this blend, the LDPE fraction introduces long-chain branching that lowers the power-law index under high shear while retaining acceptable drawability at lower shear. This produces a practical advantage in die-lip cleanliness and bubble stability compared with unblended C4-LLDPE, but it also limits clarity when compared with a single-site LLDPE or a pure high-clarity LDPE film grade.

    In blown-film conversion, the grade is typically processed on a single-screw extruder with a grooved feed section, barrier screw, and 30:1 L/D ratio. A die diameter of 300 mm with a die gap of 1.6–2.0 mm and a blow-up ratio between 2.2:1 and 2.8:1 is a common starting configuration. Melt temperature at the die is maintained between 175 °C and 195 °C, with the die body set at 180–200 °C. Barrel set points are often arranged in a reverse profile: feed zone 140–150 °C, transition 165–175 °C, metering 180–190 °C. This profile reduces premature melting and feed-zone bridging in grooved-barrel machines. Screw speeds from 90 rpm to 120 rpm with outputs of 180–250 kg/h have been reported for similar blends on 75 mm extruders, but throttle settings, screw design, and die geometry shift these values considerably.

    Cast-film conversion of the same resin typically uses a 90 mm or 120 mm extruder with 33:1 L/D, a slot die width of 1200 mm to 1800 mm, and a die gap of 0.5 mm or less. Melt temperature is frequently held at 220–250 °C depending on line speed and draw ratio. The LDPE fraction reduces neck-in and improves edge bead control at line speeds above 300 m/min. However, melt residence time above 240 °C should be minimized because prolonged exposure can increase gel formation, elevate extractables, and shift odor profile. The producer’s processing guide remains the authoritative source for exact set points.

    Why Does the LDPE Fraction Improve Bubble Stability Without Sacrificing Puncture Resistance?

    The principal difference between Trilene® TS 8057 and an unblended C4-LLDPE is the high-pressure LDPE fraction. In melt extension, linear low-density polyethylene lacks the extensional strain hardening that stabilizes a blown-film bubble under rapid draw. The LDPE fraction adds long-chain branching and broadens the relaxation spectrum. As a result, bubble diameter variation, frost-line oscillation, and web tension fluctuations are reduced. This allows the blend to run at higher blow-up ratios and thinner gauges without introducing holes or tear defects.

    At the same time, the LLDPE-C4 fraction preserves solid-state energy absorption. The short-chain branches reduce crystal thickness and increase the number of tie molecules between lamellae. Under impact, the blend dissipates energy through multiple crazing and shear-yielding zones rather than a single catastrophic tear path. This is why the blend class typically shows higher dart drop impact and transverse-direction Elmendorf tear than high-pressure LDPE of comparable density. The trade-off is lower clarity and gloss than a pure LDPE film, and lower ultimate tensile strength in the machine direction than a neat higher-molecular-weight LLDPE-C4 grade. These differences are evaluated using ASTM D1003-21 for haze, ASTM D2457-13 for gloss, ISO 527-3:2018 for film tensile properties, ASTM D1922-15 for tear, and ASTM D5748-19 for puncture resistance.

    On a high-speed blown-film tower with automatic gauge control, the blend’s broader molecular weight distribution can generate higher die swell and a thicker film at the die exit. This must be compensated by adjusting the internal bubble air volume and frost-line height. A frost-line height of 650–850 mm is commonly used for 25 µm film. If the frost line is placed too low, the film may retain excessive orientation and exhibit splitty tear in the machine direction. If the frost line is raised too high, bubble cooling becomes insufficient and the tube may wander. These operational boundaries are equipment-dependent and are not resolved solely by changing the polymer grade.

    When the blend is used in a cast-film process, the LDPE fraction lowers melt tension at the air gap and improves contact with the chill roll. The reduction in neck-in is measurable at draw ratios above 30:1. Additional draw ratio may be required to fully develop the LLDPE orientation and to obtain the desired machine-direction tensile modulus. Too low a draw ratio produces film with poor roll hardness and uneven stretch behavior on power pre-stretch equipment.

    Cast stretch-film lines selecting Trilene® TS 8057 commonly target pre-stretch ratios between 150% and 250% on pallet-wrapping equipment with electronic load-cell tension control. The film is evaluated for puncture, load retention, and tear resistance under ASTM D5748-19 and ASTM D1922-15. In agricultural silage and bale-wrap applications, the blend is typically used as a core layer in coextruded structures, where the surface layers contribute tack or UV stabilization. Published data for this specific product configuration in UV-stabilized silage film is limited; outdoor weathering performance should be established through accelerated testing under ASTM G155-21 and real-exposure trials.

    Blown-film converters also select this grade for industrial liners and heavy-duty packaging where the combination of gauge reduction and puncture resistance offsets the higher clarity requirement. In such applications, the film is frequently specified at 40–50 µm and tested for Elmendorf tear, tensile yield strength, and drop impact. The blend is less suitable for high-clarity retail display film because the LDPE component increases haze and reduces gloss compared with metallocene or single-site LLDPE. It is also not optimized for high-temperature retort packaging because the LDPE fraction lowers the melting point and limits sustained use above 100 °C.

    When Seal Strength and Regulatory Submissions Require Joint Measurement

    Heat-seal performance is a critical downstream property for this blend. The LLDPE-C4 fraction lowers seal initiation temperature relative to high-pressure LDPE. On a laboratory heat sealer with a 3 mm bar width, 0.5 s dwell time, and 0.3 MPa jaw pressure, 25 µm film of this blend class typically exhibits seal initiation below 115 °C. Seal strength is quantified according to ASTM F88/F88M-21. Hot-tack behavior is measured under ASTM F1921-18. These values are strongly dependent on seal-bar geometry, film thickness, and contamination at the seal surface; they must be verified on the converter’s own packaging line.

    The material may be evaluated for food-contact compliance under 21 CFR 177.1520(c) for olefin polymers. In the United States, the specific conditions of use and food type determine whether the structure meets the extractable and end-use limits of 21 CFR 177.1520(c) 3.2a or 3.2b. In the European Union, compliance is assessed under Commission Regulation (EU) No 10/2011, with overall migration limits commonly expressed as 10 mg/dm² for plastic materials in contact with food. RoHS compliance is typically assessed under Directive 2011/65/EU for restricted substances, while REACH obligations are managed under Regulation (EC) No 1907/2006. The producer’s regulatory documentation should be consulted for authorized monomer restrictions and specific migration limits.

    Storage before conversion should avoid direct sunlight, condensation, and prolonged exposure to high-ambient humidity. Polyethylene pellets are generally not hygroscopic, but surface moisture from condensation can produce bubbles and surface defects. If visible condensation is present, accepted practice for polyethylenes is to dry the pellets at 60–70 °C for 2–4 h using a desiccant or hot-air hopper dryer. The resin should not be exposed to amine-based processing aids that are not approved by the producer, because certain nitrogen-containing additives can generate odor, discoloration, or surface exudation in polyolefin films. The working temperature should be kept below 260 °C to minimize oxidative degradation, and purging with a lower-viscosity polyolefin is recommended when transitioning from higher-viscosity engineering polymers.

    Top